{"id":{"repo_id":"gatech","oai_identifier":"oai:repository.gatech.edu:1853/72615"},"canonical_url":"https://search.ndltd.org/etd/gatech/oai:repository.gatech.edu:1853/72615","repository":{"repo_id":"gatech","name":"Georgia Tech","base_url":"https://repository.gatech.edu/server/oai/request"},"display":{"title":"Enhancing the Stability and Performance of Solid Oxide Cells by Tailoring Surfaces and Interfaces through Surface Modification","abstract":"Reversible solid oxide cells (RSOCs) are an extremely promising solution for efficient electric grid storage; however, breakthroughs in materials innovation are required for RSOCs to be implemented on a large scale, as several challenges remain to be fully resolved. The air electrode is one area of focus, as the kinetics of oxygen reduction and evolution reactions are notoriously sluggish, resulting in low energy efficiency. To combat these problems, a surface sol-gel (SSG) process was developed to achieve layer-by-layer deposition of catalytically active catalysts (e.g., PrOx and BaO) on the surface of a porous air electrode, reducing the polarization resistance while increasing the stability of the electrode. For example, the application of an SSG coating of PrOx to a La0.6Sr0.4Co0.2Fe0.8O3-δ (LSCF) electrode reduced the polarization resistance from 1.136 to 0.117 Ω cm2 at 600 °C and the degradation rate from 1.13×10-3 to 2.67×10-4 Ω cm2 h-1 at 650 °C. The interface between the electrolyte and the air electrode is the other area of focus, where the electrolyte experiences degradation due to exposure to high concentrations of water during water electrolysis. Here, a dense and highly stable electrolyte composition, BaHf0.8Yb0.2O3 (BHYb), was deposited on the surface of a more conductive electrolyte, BaZr0.1Ce0.7Y0.1Yb0.1O3-δ, creating a bilayer electrolyte. The epitaxial, dense, and uniform BHYb layer is effective in preventing electrolyte degradation against high concentrations of steam and CO2 present in the air electrode, greatly enhancing the chemical stability while maintaining high electrochemical performance.","abstract_html":"Reversible solid oxide cells (RSOCs) are an extremely promising solution for efficient electric grid storage; however, breakthroughs in materials innovation are required for RSOCs to be implemented on a large scale, as several challenges remain to be fully resolved. The air electrode is one area of focus, as the kinetics of oxygen reduction and evolution reactions are notoriously sluggish, resulting in low energy efficiency. To combat these problems, a surface sol-gel (SSG) process was developed to achieve layer-by-layer deposition of catalytically active catalysts (e.g., PrOx and BaO) on the surface of a porous air electrode, reducing the polarization resistance while increasing the stability of the electrode. For example, the application of an SSG coating of PrOx to a La0.6Sr0.4Co0.2Fe0.8O3-δ (LSCF) electrode reduced the polarization resistance from 1.136 to 0.117 Ω cm2 at 600 °C and the degradation rate from 1.13×10-3 to 2.67×10-4 Ω cm2 h-1 at 650 °C. The interface between the electrolyte and the air electrode is the other area of focus, where the electrolyte experiences degradation due to exposure to high concentrations of water during water electrolysis. Here, a dense and highly stable electrolyte composition, BaHf0.8Yb0.2O3 (BHYb), was deposited on the surface of a more conductive electrolyte, BaZr0.1Ce0.7Y0.1Yb0.1O3-δ, creating a bilayer electrolyte. The epitaxial, dense, and uniform BHYb layer is effective in preventing electrolyte degradation against high concentrations of steam and CO2 present in the air electrode, greatly enhancing the chemical stability while maintaining high electrochemical performance.","abstract_has_math":false,"creators":["Kane, Nicholas John"],"institution":"Georgia Institute of Technology","degree_name":null,"degree_level":"Doctoral","degree_discipline":null,"degree_department":"Materials Science and Engineering","school":null,"contributors":[],"advisors":["Liu, Meilin"],"committee_chairs":[],"committee_members":["Fuller, Thomas","Losego, Mark","McDowell, Matthew","Singh, Preet"],"year":2022,"date_issued":"2022-07-21","date_published":"2022-07-21","updated_at":"2026-11-19T05:59:11Z","subjects":["Surface modification","Surface sol-gel","Solid oxide fuel cell","Catalysts","Sputtering"],"languages":["en_US"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/1853/72615","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/1853/72615","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://repository.gatech.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Arepository.gatech.edu%3A1853%2F72615","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Liu, Meilin"]},{"key":"dc:contributor.committeemember","label":"Committee Member","values":["Fuller, Thomas","Losego, Mark","McDowell, Matthew","Singh, Preet"]},{"key":"dc:contributor.department","label":"Department","values":["Materials Science and Engineering"]},{"key":"dc:contributor.other","label":"Dc Contributor Other","values":["College of Engineering","School of Materials Science and Engineering"]},{"key":"dc:creator","label":"Author","values":["Kane, Nicholas John"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2023-09-06T19:43:59Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2023-09-06T19:43:59Z"]},{"key":"dc:date.created","label":"Dc Date Created","values":["2022-08"]},{"key":"dc:date.issued","label":"Date","values":["2022-07-21"]},{"key":"dc:date.submitted","label":"Dc Date Submitted","values":["August 2022"]},{"key":"dc:date.updated","label":"Dc Date Updated","values":["2023-09-06T19:44:00Z"]},{"key":"dc:publisher","label":"Institution","values":["Georgia Institute of Technology"]},{"key":"dc:relation.advisorentity","label":"Dc Relation Advisorentity","values":["30dd1bbc-edf1-406a-9183-d985863cbab3"]},{"key":"dc:relation.orgunit","label":"Dc Relation Orgunit","values":["7c022d60-21d5-497c-b552-95e489a06569","21b5a45b-0b8a-4b69-a36b-6556f8426a35"]},{"key":"dc:type","label":"Dc Type","values":["Text","Dissertation"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Doctoral"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Surface modification","Surface sol-gel","Solid oxide fuel cell","Catalysts","Sputtering"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en_US"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/1853/72615"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Reversible solid oxide cells (RSOCs) are an extremely promising solution for efficient electric grid storage; however, breakthroughs in materials innovation are required for RSOCs to be implemented on a large scale, as several challenges remain to be fully resolved. The air electrode is one area of focus, as the kinetics of oxygen reduction and evolution reactions are notoriously sluggish, resulting in low energy efficiency. To combat these problems, a surface sol-gel (SSG) process was developed to achieve layer-by-layer deposition of catalytically active catalysts (e.g., PrOx and BaO) on the surface of a porous air electrode, reducing the polarization resistance while increasing the stability of the electrode. For example, the application of an SSG coating of PrOx to a La0.6Sr0.4Co0.2Fe0.8O3-δ (LSCF) electrode reduced the polarization resistance from 1.136 to 0.117 Ω cm2 at 600 °C and the degradation rate from 1.13×10-3 to 2.67×10-4 Ω cm2 h-1 at 650 °C. The interface between the electrolyte and the air electrode is the other area of focus, where the electrolyte experiences degradation due to exposure to high concentrations of water during water electrolysis. Here, a dense and highly stable electrolyte composition, BaHf0.8Yb0.2O3 (BHYb), was deposited on the surface of a more conductive electrolyte, BaZr0.1Ce0.7Y0.1Yb0.1O3-δ, creating a bilayer electrolyte. The epitaxial, dense, and uniform BHYb layer is effective in preventing electrolyte degradation against high concentrations of steam and CO2 present in the air electrode, greatly enhancing the chemical stability while maintaining high electrochemical performance."]},{"key":"dc:description.degree","label":"Dc Description Degree","values":["Ph.D."]},{"key":"dc:format.mimetype","label":"Dc Format Mimetype","values":["application/pdf"]},{"key":"dc:title","label":"Title","values":["Enhancing the Stability and Performance of Solid Oxide Cells by Tailoring Surfaces and Interfaces through Surface Modification"]},{"key":"dspace:entity.type","label":"Dspace Entity Type","values":["Publication"]}]}],"canonical_facts":{"dc:contributor.advisor":["Liu, Meilin"],"dc:contributor.committeemember":["Fuller, Thomas","Losego, Mark","McDowell, Matthew","Singh, Preet"],"dc:contributor.department":["Materials Science and Engineering"],"dc:contributor.other":["College of Engineering","School of Materials Science and Engineering"],"dc:creator":["Kane, Nicholas John"],"dc:date.accessioned":["2023-09-06T19:43:59Z"],"dc:date.available":["2023-09-06T19:43:59Z"],"dc:date.created":["2022-08"],"dc:date.issued":["2022-07-21"],"dc:date.submitted":["August 2022"],"dc:date.updated":["2023-09-06T19:44:00Z"],"dc:description.abstract":["Reversible solid oxide cells (RSOCs) are an extremely promising solution for efficient electric grid storage; however, breakthroughs in materials innovation are required for RSOCs to be implemented on a large scale, as several challenges remain to be fully resolved. The air electrode is one area of focus, as the kinetics of oxygen reduction and evolution reactions are notoriously sluggish, resulting in low energy efficiency. To combat these problems, a surface sol-gel (SSG) process was developed to achieve layer-by-layer deposition of catalytically active catalysts (e.g., PrOx and BaO) on the surface of a porous air electrode, reducing the polarization resistance while increasing the stability of the electrode. For example, the application of an SSG coating of PrOx to a La0.6Sr0.4Co0.2Fe0.8O3-δ (LSCF) electrode reduced the polarization resistance from 1.136 to 0.117 Ω cm2 at 600 °C and the degradation rate from 1.13×10-3 to 2.67×10-4 Ω cm2 h-1 at 650 °C. The interface between the electrolyte and the air electrode is the other area of focus, where the electrolyte experiences degradation due to exposure to high concentrations of water during water electrolysis. Here, a dense and highly stable electrolyte composition, BaHf0.8Yb0.2O3 (BHYb), was deposited on the surface of a more conductive electrolyte, BaZr0.1Ce0.7Y0.1Yb0.1O3-δ, creating a bilayer electrolyte. The epitaxial, dense, and uniform BHYb layer is effective in preventing electrolyte degradation against high concentrations of steam and CO2 present in the air electrode, greatly enhancing the chemical stability while maintaining high electrochemical performance."],"dc:description.degree":["Ph.D."],"dc:format.mimetype":["application/pdf"],"dc:identifier.uri":["https://hdl.handle.net/1853/72615"],"dc:language.iso":["en_US"],"dc:publisher":["Georgia Institute of Technology"],"dc:relation.advisorentity":["30dd1bbc-edf1-406a-9183-d985863cbab3"],"dc:relation.orgunit":["7c022d60-21d5-497c-b552-95e489a06569","21b5a45b-0b8a-4b69-a36b-6556f8426a35"],"dc:subject":["Surface modification","Surface sol-gel","Solid oxide fuel cell","Catalysts","Sputtering"],"dc:title":["Enhancing the Stability and Performance of Solid Oxide Cells by Tailoring Surfaces and Interfaces through Surface Modification"],"dc:type":["Text","Dissertation"],"dspace:entity.type":["Publication"],"thesis:degree_level":["Doctoral"]},"updated_at":"2026-11-19T05:59:11Z"}