{"id":{"repo_id":"greece","oai_identifier":"oai:10442/1020"},"canonical_url":"https://search.ndltd.org/etd/greece/oai:10442/1020","repository":{"repo_id":"greece","name":"Greek National Archive of PhD Theses","base_url":"https://phdtheses.ekt.gr/eadd_oai/request"},"display":{"title":"ΜΕΛΕΤΗ ΤΗΣ ΔΟΜΗΣ ΗΛΕΚΤΡΟΛΥΤΙΚΩΝ ΑΠΟΘΕΜΑΤΩΝ ΝΙΚΕΛΙΟΥ","abstract":"THE PURPOSE OF THIS THESIS IS TO CONTRIBUTE TO THE STUDY OF THE STRUCTURE AND THE PROPERTIES OF ELECTROLYTIC NICKEL DEPOSITS. THE X-RAY ANALYSIS OF DEPOSITS PREPARED FROM A BATH OF PURE NICKEL SULPHATE (1,22M), ALLOWED THE TRACING OF A DIAGRAM DEPICTING THE PREFERRED ORIENTATIONS, WHERE THE ORIENTATIONS [110]A., [100], [210] AND [110]B. ARE NOTICED. A PREVIOUS DIAGRAM WITH THE RESPECTIVELY DIAGRAMS, OF THE PREFERRED ORIENTATIONS OF THE DEPOSITS FROM A WATTS BATH, ONE MAY NOTE THE APPEARANCE OF THE ORIENTATION [100] IN TWO WELL DISTINGUISHED REGIONS, THE EXTENSION OF THE ORIENTATION [210] IN MUCH LESS ACIDIC SOLUTIONS AND THECOMPLETELY DISAPPEARANCE OF THE ORIENTATION [211]. THE PRESENCE OF 2-BUTYNE-DIOL 1,4 PROVOKES THE DRASTIC LIMITATION OF THE ORIENTATION [210], WHILE THE ORIENTATION [111] PRESENTS A NOTICEABLE STABILITY. THE PRESENCE OF BENZYNE SULPHONATE PROVOKES THE DRASTIC LIMITATION OF THE ORIENTATION [100]. IT WAS ALSO NOTED THAT THE MECHANICAL PROPERTIES (HARDNESS- ROUGHNESS) DEPEND ON THE CONDITIONS OF THE ELECTROLYSIS AND THE PRESENCE OF ORGANIC ADDITIVES. THE HARD DEPOSITS CORRESPOND TO THE PREFERRED ORIENTATIONS AFFECTED BY INHIBITORS, WHILE THE BRIGHT DEPOSITS ARE MICROCRYSTALLINE.","abstract_html":"THE PURPOSE OF THIS THESIS IS TO CONTRIBUTE TO THE STUDY OF THE STRUCTURE AND THE PROPERTIES OF ELECTROLYTIC NICKEL DEPOSITS. THE X-RAY ANALYSIS OF DEPOSITS PREPARED FROM A BATH OF PURE NICKEL SULPHATE (1,22M), ALLOWED THE TRACING OF A DIAGRAM DEPICTING THE PREFERRED ORIENTATIONS, WHERE THE ORIENTATIONS [110]A., [100], [210] AND [110]B. ARE NOTICED. A PREVIOUS DIAGRAM WITH THE RESPECTIVELY DIAGRAMS, OF THE PREFERRED ORIENTATIONS OF THE DEPOSITS FROM A WATTS BATH, ONE MAY NOTE THE APPEARANCE OF THE ORIENTATION [100] IN TWO WELL DISTINGUISHED REGIONS, THE EXTENSION OF THE ORIENTATION [210] IN MUCH LESS ACIDIC SOLUTIONS AND THECOMPLETELY DISAPPEARANCE OF THE ORIENTATION [211]. THE PRESENCE OF 2-BUTYNE-DIOL 1,4 PROVOKES THE DRASTIC LIMITATION OF THE ORIENTATION [210], WHILE THE ORIENTATION [111] PRESENTS A NOTICEABLE STABILITY. THE PRESENCE OF BENZYNE SULPHONATE PROVOKES THE DRASTIC LIMITATION OF THE ORIENTATION [100]. IT WAS ALSO NOTED THAT THE MECHANICAL PROPERTIES (HARDNESS- ROUGHNESS) DEPEND ON THE CONDITIONS OF THE ELECTROLYSIS AND THE PRESENCE OF ORGANIC ADDITIVES. THE HARD DEPOSITS CORRESPOND TO THE PREFERRED ORIENTATIONS AFFECTED BY INHIBITORS, WHILE THE BRIGHT DEPOSITS ARE MICROCRYSTALLINE.","abstract_has_math":false,"creators":["Αργυρίου, Αργύριος"],"institution":"National Technical University of Athens (NTUA)","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":1988,"date_issued":"1988","date_published":"1988","updated_at":"2026-11-18T20:20:43Z","subjects":["ALL SULPHATE BATHS","BRIGHTNERS","ELECTROCRYSTALLIZATION OF NICKEL","ELECTRODEPOSITION OF NICKEL","ELECTROPLATING","Hardness","LEVELLING AGENTS","ORGANIC ADDITIVES","PREFERRED ORIENTATIONS","Roughness","ΕΚΛΕΚΤΙΚΟΣ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΣ","Ηλεκτροαπόθεση νικελίου","ΗΛΕΚΤΡΟΚΡΥΣΤΑΛΛΩΣΗ ΤΟΥ ΝΙΚΕΛΙΟΥ","ΗΛΕΚΤΡΟΛΥΤΙΚΗ ΕΠΙΜΕΤΑΛΛΩΣΗ","ΛΕΙΑΝΤΙΚΑ","ΛΟΥΤΡΟ ΚΑΘΑΡΟΥ ΘΕΙΙΚΟΥ ΝΙΚΕΛΙΟΥ","Οργανικά πρόσθετα","Σκληρότητα","ΣΤΙΛΒΩΤΙΚΑ","Τραχύτητα","Επιστήμες Μηχανικού και Τεχνολογία","Επιστήμη Χημικού Μηχανικού","Engineering and Technology","Chemical Engineering"],"languages":["gre"],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["10.12681/eadd/1020"],"render_values":[{"text":"10.12681/eadd/1020","href":"https://doi.org/10.12681/eadd/1020","code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/10442/hedi/1020","outbound_label":"Handle","outbound_source":"dc:identifier","record_url":"http://hdl.handle.net/10442/hedi/1020","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://phdtheses.ekt.gr/eadd_oai/request?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3A10442%2F1020","prefix":"oai_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Αργυρίου, Αργύριος"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["1988"]},{"key":"dc:publisher","label":"Institution","values":["National Technical University of Athens (NTUA)","Εθνικό Μετσόβιο Πολυτεχνείο (ΕΜΠ)"]},{"key":"dc:type","label":"Dc Type","values":["PhD Thesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["ALL SULPHATE BATHS","BRIGHTNERS","ELECTROCRYSTALLIZATION OF NICKEL","ELECTRODEPOSITION OF NICKEL","ELECTROPLATING","Hardness","LEVELLING AGENTS","ORGANIC ADDITIVES","PREFERRED ORIENTATIONS","Roughness","ΕΚΛΕΚΤΙΚΟΣ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΣ","Ηλεκτροαπόθεση νικελίου","ΗΛΕΚΤΡΟΚΡΥΣΤΑΛΛΩΣΗ ΤΟΥ ΝΙΚΕΛΙΟΥ","ΗΛΕΚΤΡΟΛΥΤΙΚΗ ΕΠΙΜΕΤΑΛΛΩΣΗ","ΛΕΙΑΝΤΙΚΑ","ΛΟΥΤΡΟ ΚΑΘΑΡΟΥ ΘΕΙΙΚΟΥ ΝΙΚΕΛΙΟΥ","Οργανικά πρόσθετα","Σκληρότητα","ΣΤΙΛΒΩΤΙΚΑ","Τραχύτητα","Επιστήμες Μηχανικού και Τεχνολογία","Επιστήμη Χημικού Μηχανικού","Engineering and Technology","Chemical Engineering"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["gre"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["10.12681/eadd/1020","http://hdl.handle.net/10442/hedi/1020"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["THE PURPOSE OF THIS THESIS IS TO CONTRIBUTE TO THE STUDY OF THE STRUCTURE AND THE PROPERTIES OF ELECTROLYTIC NICKEL DEPOSITS. THE X-RAY ANALYSIS OF DEPOSITS PREPARED FROM A BATH OF PURE NICKEL SULPHATE (1,22M), ALLOWED THE TRACING OF A DIAGRAM DEPICTING THE PREFERRED ORIENTATIONS, WHERE THE ORIENTATIONS [110]A., [100], [210] AND [110]B. ARE NOTICED. A PREVIOUS DIAGRAM WITH THE RESPECTIVELY DIAGRAMS, OF THE PREFERRED ORIENTATIONS OF THE DEPOSITS FROM A WATTS BATH, ONE MAY NOTE THE APPEARANCE OF THE ORIENTATION [100] IN TWO WELL DISTINGUISHED REGIONS, THE EXTENSION OF THE ORIENTATION [210] IN MUCH LESS ACIDIC SOLUTIONS AND THECOMPLETELY DISAPPEARANCE OF THE ORIENTATION [211]. THE PRESENCE OF 2-BUTYNE-DIOL 1,4 PROVOKES THE DRASTIC LIMITATION OF THE ORIENTATION [210], WHILE THE ORIENTATION [111] PRESENTS A NOTICEABLE STABILITY. THE PRESENCE OF BENZYNE SULPHONATE PROVOKES THE DRASTIC LIMITATION OF THE ORIENTATION [100]. IT WAS ALSO NOTED THAT THE MECHANICAL PROPERTIES (HARDNESS- ROUGHNESS) DEPEND ON THE CONDITIONS OF THE ELECTROLYSIS AND THE PRESENCE OF ORGANIC ADDITIVES. THE HARD DEPOSITS CORRESPOND TO THE PREFERRED ORIENTATIONS AFFECTED BY INHIBITORS, WHILE THE BRIGHT DEPOSITS ARE MICROCRYSTALLINE.","Η ΕΡΓΑΣΙΑ ΑΥΤΗ ΕΧΕΙ ΩΣ ΣΤΟΧΟ ΝΑ ΣΥΜΒΑΛΛΕΙ ΣΤΗΝ ΜΕΛΕΤΗ ΤΗΣ ΔΟΜΗΣ ΚΑΙ ΤΩΝ ΙΔΙΟΤΗΤΩΝ ΤΩΝ ΗΛΕΚΤΡΟΛΥΤΙΚΩΝ ΑΠΟΘΕΜΑΤΩΝ ΝΙΚΕΛΙΟΥ. Η ΑΚΤΙΝΟΚΡΥΣΤΑΛΛΟΓΡΑΦΙΚΗ ΑΝΑΛΥΣΗ ΤΩΝΑΠΟΘΕΜΑΤΩΝ ΠΟΥ ΠΑΡΑΣΚΕΥΑΣΘΗΚΑΝ ΑΠΟ ΛΟΥΤΡΟ ΚΑΘΑΡΟΥ ΘΕΙΙΚΟΥ ΝΙΚΕΛΙΟΥ (1,224) ΕΠΕΤΡΕΨΕ ΤΗΝ ΧΑΡΑΞΗ ΤΟΥ ΔΙΑΓΡΑΜΜΑΤΟΣ ΕΚΛΕΚΤΙΚΩΝ ΠΡΟΣΑΝΑΤΟΛΙΣΜΩΝ ΕΙΣ ΤΟ ΟΠΟΙΟ ΕΜΦΑΝΙΖΟΝΤΑΙ ΟΙ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΙ [110].Α, [100], [210] ΚΑΙ 110]Β. ΑΠΟ ΤΗΝ ΣΥΓΚΡΙΣΗ ΤΟΥ ΔΙΑΓΡΑΜΜΑΤΟΣ ΑΥΤΟΥ ΜΕ ΤΑ ΑΝΤΙΣΤΟΙΧΑ ΔΙΑΓΡΑΜΜΑΤΑ ΕΚΛΕΚΤΙΚΩΝ ΠΡΟΣΑΝΑΤΟΛΙΣΜΩΝ ΤΩΝ ΑΠΟΘΕΜΑΤΩΝ ΑΠΟ ΛΟΥΤΡΟ ΤΟΥ WATTS ΔΙΑΠΙΣΤΩΝΕΤΑΙ Η ΕΜΦΑΝΙΣΗ ΤΟΥ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΥ [100] ΣΕ ΔΥΟ ΔΙΑΚΕΚΡΙΜΕΝΕΣ ΜΕΤΑΞΥ ΤΟΥΣ ΠΕΡΙΟΧΕΣ, Η ΕΠΕΚΤΑΣΗ ΤΟΥ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΥ[210] ΣΕ ΠΟΛΥ ΛΙΓΟΤΕΡΟ ΟΞΙΝΑ ΔΙΑΛΥΜΑΤΑ ΚΑΙ Η ΠΛΗΡΗΣ ΕΞΑΦΑΝΙΣΗ ΤΟΥ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΥ [211]. Η ΠΑΡΟΥΣΙΑ ΤΗΣ Ζ- ΒΟΥΤΙΝΟ-ΔΙΟΛΗΣ 1,4 ΠΕΡΙΟΡΙΖΕΙ ΔΡΑΣΤΙΚΑ ΤΟΝ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟ [210], ΕΝΩ Ο ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΣ [111] ΕΜΦΑΝΙΖΕΙ ΑΞΙΟΣΗΜΕΙΩΤΗ ΣΤΑΘΕΡΟΤΗΤΑ. Η ΠΑΡΟΥΣΙΑ ΤΟΥ ΒΕΝΖΟΣΟΥΛΦΟΝΙΚΟΥ ΝΑΤΡΙΟΥ ΠΕΡΙΟΡΙΖΕΙ ΔΡΑΣΤΙΚΑ ΤΟΝ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟ [100]. ΔΙΑΠΙΣΤΩΘΗΚΕ ΕΠΙΣΗΣ, ΟΤΙ ΟΙ ΜΗΧΑΝΙΚΕΣ ΙΔΙΟΤΗΤΕΣ ΤΩΝ ΑΠΟΘΕΜΑΤΩΝ (ΣΚΛΗΡΟΤΗΤΑ-ΤΡΑΧΥΤΗΤΑ) ΕΞΑΡΤΩΝΤΑΙ ΑΠΟ ΤΙΣ ΣΥΝΘΗΚΕΣ ΤΗΣ ΗΛΕΚΤΡΟΛΥΣΗΣ ΚΑΙ ΤΗΝ ΠΑΡΟΥΣΙΑ ΟΡΓΑΝΙΚΩΝ ΠΡΟΣΘΕΤΩΝ. ΤΑ ΣΚΛΗΡΑ ΑΠΟΘΕΜΑΤΑ ΑΝΤΙΣΤΟΙΧΟΥΝ ΣΕ ΕΚΛΕΚΤΙΚΟΥΣ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΥΣ ΕΝΤΟΝΑ ΠΑΡΕΜΠΟΔΙΖΟΜΕΝΟΥΣ, ΕΝΩ ΤΑ ΣΤΙΛΠΝΑ ΑΠΟΘΕΜΑΤΑ ΕΙΝΑΙ ΜΙΚΡΟΚΡΥΣΤΑΛΛΙΚΑ."]},{"key":"dc:title","label":"Title","values":["ΜΕΛΕΤΗ ΤΗΣ ΔΟΜΗΣ ΗΛΕΚΤΡΟΛΥΤΙΚΩΝ ΑΠΟΘΕΜΑΤΩΝ ΝΙΚΕΛΙΟΥ","STUDY OF STRUCTURE OF NICKEL ELECTRODEPOSITS"]}]}],"canonical_facts":{"dc:creator":["Αργυρίου, Αργύριος"],"dc:date":["1988"],"dc:description":["THE PURPOSE OF THIS THESIS IS TO CONTRIBUTE TO THE STUDY OF THE STRUCTURE AND THE PROPERTIES OF ELECTROLYTIC NICKEL DEPOSITS. THE X-RAY ANALYSIS OF DEPOSITS PREPARED FROM A BATH OF PURE NICKEL SULPHATE (1,22M), ALLOWED THE TRACING OF A DIAGRAM DEPICTING THE PREFERRED ORIENTATIONS, WHERE THE ORIENTATIONS [110]A., [100], [210] AND [110]B. ARE NOTICED. A PREVIOUS DIAGRAM WITH THE RESPECTIVELY DIAGRAMS, OF THE PREFERRED ORIENTATIONS OF THE DEPOSITS FROM A WATTS BATH, ONE MAY NOTE THE APPEARANCE OF THE ORIENTATION [100] IN TWO WELL DISTINGUISHED REGIONS, THE EXTENSION OF THE ORIENTATION [210] IN MUCH LESS ACIDIC SOLUTIONS AND THECOMPLETELY DISAPPEARANCE OF THE ORIENTATION [211]. THE PRESENCE OF 2-BUTYNE-DIOL 1,4 PROVOKES THE DRASTIC LIMITATION OF THE ORIENTATION [210], WHILE THE ORIENTATION [111] PRESENTS A NOTICEABLE STABILITY. THE PRESENCE OF BENZYNE SULPHONATE PROVOKES THE DRASTIC LIMITATION OF THE ORIENTATION [100]. IT WAS ALSO NOTED THAT THE MECHANICAL PROPERTIES (HARDNESS- ROUGHNESS) DEPEND ON THE CONDITIONS OF THE ELECTROLYSIS AND THE PRESENCE OF ORGANIC ADDITIVES. THE HARD DEPOSITS CORRESPOND TO THE PREFERRED ORIENTATIONS AFFECTED BY INHIBITORS, WHILE THE BRIGHT DEPOSITS ARE MICROCRYSTALLINE.","Η ΕΡΓΑΣΙΑ ΑΥΤΗ ΕΧΕΙ ΩΣ ΣΤΟΧΟ ΝΑ ΣΥΜΒΑΛΛΕΙ ΣΤΗΝ ΜΕΛΕΤΗ ΤΗΣ ΔΟΜΗΣ ΚΑΙ ΤΩΝ ΙΔΙΟΤΗΤΩΝ ΤΩΝ ΗΛΕΚΤΡΟΛΥΤΙΚΩΝ ΑΠΟΘΕΜΑΤΩΝ ΝΙΚΕΛΙΟΥ. Η ΑΚΤΙΝΟΚΡΥΣΤΑΛΛΟΓΡΑΦΙΚΗ ΑΝΑΛΥΣΗ ΤΩΝΑΠΟΘΕΜΑΤΩΝ ΠΟΥ ΠΑΡΑΣΚΕΥΑΣΘΗΚΑΝ ΑΠΟ ΛΟΥΤΡΟ ΚΑΘΑΡΟΥ ΘΕΙΙΚΟΥ ΝΙΚΕΛΙΟΥ (1,224) ΕΠΕΤΡΕΨΕ ΤΗΝ ΧΑΡΑΞΗ ΤΟΥ ΔΙΑΓΡΑΜΜΑΤΟΣ ΕΚΛΕΚΤΙΚΩΝ ΠΡΟΣΑΝΑΤΟΛΙΣΜΩΝ ΕΙΣ ΤΟ ΟΠΟΙΟ ΕΜΦΑΝΙΖΟΝΤΑΙ ΟΙ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΙ [110].Α, [100], [210] ΚΑΙ 110]Β. ΑΠΟ ΤΗΝ ΣΥΓΚΡΙΣΗ ΤΟΥ ΔΙΑΓΡΑΜΜΑΤΟΣ ΑΥΤΟΥ ΜΕ ΤΑ ΑΝΤΙΣΤΟΙΧΑ ΔΙΑΓΡΑΜΜΑΤΑ ΕΚΛΕΚΤΙΚΩΝ ΠΡΟΣΑΝΑΤΟΛΙΣΜΩΝ ΤΩΝ ΑΠΟΘΕΜΑΤΩΝ ΑΠΟ ΛΟΥΤΡΟ ΤΟΥ WATTS ΔΙΑΠΙΣΤΩΝΕΤΑΙ Η ΕΜΦΑΝΙΣΗ ΤΟΥ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΥ [100] ΣΕ ΔΥΟ ΔΙΑΚΕΚΡΙΜΕΝΕΣ ΜΕΤΑΞΥ ΤΟΥΣ ΠΕΡΙΟΧΕΣ, Η ΕΠΕΚΤΑΣΗ ΤΟΥ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΥ[210] ΣΕ ΠΟΛΥ ΛΙΓΟΤΕΡΟ ΟΞΙΝΑ ΔΙΑΛΥΜΑΤΑ ΚΑΙ Η ΠΛΗΡΗΣ ΕΞΑΦΑΝΙΣΗ ΤΟΥ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΥ [211]. Η ΠΑΡΟΥΣΙΑ ΤΗΣ Ζ- ΒΟΥΤΙΝΟ-ΔΙΟΛΗΣ 1,4 ΠΕΡΙΟΡΙΖΕΙ ΔΡΑΣΤΙΚΑ ΤΟΝ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟ [210], ΕΝΩ Ο ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΣ [111] ΕΜΦΑΝΙΖΕΙ ΑΞΙΟΣΗΜΕΙΩΤΗ ΣΤΑΘΕΡΟΤΗΤΑ. Η ΠΑΡΟΥΣΙΑ ΤΟΥ ΒΕΝΖΟΣΟΥΛΦΟΝΙΚΟΥ ΝΑΤΡΙΟΥ ΠΕΡΙΟΡΙΖΕΙ ΔΡΑΣΤΙΚΑ ΤΟΝ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟ [100]. ΔΙΑΠΙΣΤΩΘΗΚΕ ΕΠΙΣΗΣ, ΟΤΙ ΟΙ ΜΗΧΑΝΙΚΕΣ ΙΔΙΟΤΗΤΕΣ ΤΩΝ ΑΠΟΘΕΜΑΤΩΝ (ΣΚΛΗΡΟΤΗΤΑ-ΤΡΑΧΥΤΗΤΑ) ΕΞΑΡΤΩΝΤΑΙ ΑΠΟ ΤΙΣ ΣΥΝΘΗΚΕΣ ΤΗΣ ΗΛΕΚΤΡΟΛΥΣΗΣ ΚΑΙ ΤΗΝ ΠΑΡΟΥΣΙΑ ΟΡΓΑΝΙΚΩΝ ΠΡΟΣΘΕΤΩΝ. ΤΑ ΣΚΛΗΡΑ ΑΠΟΘΕΜΑΤΑ ΑΝΤΙΣΤΟΙΧΟΥΝ ΣΕ ΕΚΛΕΚΤΙΚΟΥΣ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΥΣ ΕΝΤΟΝΑ ΠΑΡΕΜΠΟΔΙΖΟΜΕΝΟΥΣ, ΕΝΩ ΤΑ ΣΤΙΛΠΝΑ ΑΠΟΘΕΜΑΤΑ ΕΙΝΑΙ ΜΙΚΡΟΚΡΥΣΤΑΛΛΙΚΑ."],"dc:identifier":["10.12681/eadd/1020","http://hdl.handle.net/10442/hedi/1020"],"dc:language":["gre"],"dc:publisher":["National Technical University of Athens (NTUA)","Εθνικό Μετσόβιο Πολυτεχνείο (ΕΜΠ)"],"dc:subject":["ALL SULPHATE BATHS","BRIGHTNERS","ELECTROCRYSTALLIZATION OF NICKEL","ELECTRODEPOSITION OF NICKEL","ELECTROPLATING","Hardness","LEVELLING AGENTS","ORGANIC ADDITIVES","PREFERRED ORIENTATIONS","Roughness","ΕΚΛΕΚΤΙΚΟΣ ΠΡΟΣΑΝΑΤΟΛΙΣΜΟΣ","Ηλεκτροαπόθεση νικελίου","ΗΛΕΚΤΡΟΚΡΥΣΤΑΛΛΩΣΗ ΤΟΥ ΝΙΚΕΛΙΟΥ","ΗΛΕΚΤΡΟΛΥΤΙΚΗ ΕΠΙΜΕΤΑΛΛΩΣΗ","ΛΕΙΑΝΤΙΚΑ","ΛΟΥΤΡΟ ΚΑΘΑΡΟΥ ΘΕΙΙΚΟΥ ΝΙΚΕΛΙΟΥ","Οργανικά πρόσθετα","Σκληρότητα","ΣΤΙΛΒΩΤΙΚΑ","Τραχύτητα","Επιστήμες Μηχανικού και Τεχνολογία","Επιστήμη Χημικού Μηχανικού","Engineering and Technology","Chemical Engineering"],"dc:title":["ΜΕΛΕΤΗ ΤΗΣ ΔΟΜΗΣ ΗΛΕΚΤΡΟΛΥΤΙΚΩΝ ΑΠΟΘΕΜΑΤΩΝ ΝΙΚΕΛΙΟΥ","STUDY OF STRUCTURE OF NICKEL ELECTRODEPOSITS"],"dc:type":["PhD Thesis"]},"updated_at":"2026-11-18T20:20:43Z"}