{"id":{"repo_id":"guelph","oai_identifier":"oai:atrium.lib.uoguelph.ca:10214/26685"},"canonical_url":"https://search.ndltd.org/etd/guelph/oai:atrium.lib.uoguelph.ca:10214/26685","repository":{"repo_id":"guelph","name":"University of Guelph","base_url":"https://atrium.lib.uoguelph.ca/server/oai/request"},"display":{"title":"Tracking the Effect of Accelerated Aging on Cross-Linked Polyethylene Pipe using Fourier Transform Infrared Microscopy","abstract":"Cross-linked polyethylene (PEX-a) pipes have been quickly replacing metal piping in home and industrial applications due their cost-effective manufacturing process, ease of installation, and long projected lifetimes. However, PEX-a pipes are not immune to oxidative degradation from their environment while in-use, creating the opportunity for premature failure. Therefore, understanding the degradation process is critical to helping extend lifetimes and prevent expensive failures. We have developed several experimental protocols to accelerate the ageing process in-house in our efforts towards this goal, isolating the effects from various environmental stresses present during in-service conditions. By conducting FTIR microscopy measurements on unused/virgin pipes, as well as both in-service and in-house aged pipes, we have found several key indicators of an aged pipe that play a role in pipe failure. Principal component analysis (PCA) was conducted to identify characteristics of PEX-a pipes subjected to these various ageing environments.","abstract_html":"Cross-linked polyethylene (PEX-a) pipes have been quickly replacing metal piping in home and industrial applications due their cost-effective manufacturing process, ease of installation, and long projected lifetimes. However, PEX-a pipes are not immune to oxidative degradation from their environment while in-use, creating the opportunity for premature failure. Therefore, understanding the degradation process is critical to helping extend lifetimes and prevent expensive failures. We have developed several experimental protocols to accelerate the ageing process in-house in our efforts towards this goal, isolating the effects from various environmental stresses present during in-service conditions. By conducting FTIR microscopy measurements on unused/virgin pipes, as well as both in-service and in-house aged pipes, we have found several key indicators of an aged pipe that play a role in pipe failure. Principal component analysis (PCA) was conducted to identify characteristics of PEX-a pipes subjected to these various ageing environments.","abstract_has_math":false,"creators":["D'Amico, Joseph"],"institution":"University of Guelph","degree_name":"Master of Science","degree_level":null,"degree_discipline":null,"degree_department":"Department of Physics","school":null,"contributors":[],"advisors":["Dutcher, John"],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T08:26:04Z","subjects":["PEX-a pipe","accelerated ageing","FTIR microscopy","polymer degradation","principal component analysis"],"languages":["en"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/10214/26685","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/10214/26685","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aguelph%3Aoai%3Aatrium.lib.uoguelph.ca%3A10214%2F26685","prefix":"oai_dc"},"source_record":{"url":"https://atrium.lib.uoguelph.ca/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Aatrium.lib.uoguelph.ca%3A10214%2F26685","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Dutcher, John"]},{"key":"dc:creator","label":"Author","values":["D'Amico, Joseph"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2022-01-13T21:25:50Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2022-01-13T21:25:50Z"]},{"key":"dc:date.copyright","label":"Dc Date Copyright","values":["2022-01"]},{"key":"dc:date.created","label":"Dc Date Created","values":["2022-01-11"]},{"key":"dc:publisher","label":"Institution","values":["University of Guelph"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_department","label":"Department","values":["Department of Physics"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science"]},{"key":"thesis:degree_program","label":"Thesis Degree Program","values":["Physics"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of Guelph"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["PEX-a pipe","accelerated ageing","FTIR microscopy","polymer degradation","principal component analysis"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en"]},{"key":"dc:rights.license","label":"Dc Rights License","values":["All items in the Atrium are protected by copyright with all rights reserved unless otherwise indicated."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/10214/26685"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Cross-linked polyethylene (PEX-a) pipes have been quickly replacing metal piping in home and industrial applications due their cost-effective manufacturing process, ease of installation, and long projected lifetimes. However, PEX-a pipes are not immune to oxidative degradation from their environment while in-use, creating the opportunity for premature failure. Therefore, understanding the degradation process is critical to helping extend lifetimes and prevent expensive failures. We have developed several experimental protocols to accelerate the ageing process in-house in our efforts towards this goal, isolating the effects from various environmental stresses present during in-service conditions. By conducting FTIR microscopy measurements on unused/virgin pipes, as well as both in-service and in-house aged pipes, we have found several key indicators of an aged pipe that play a role in pipe failure. Principal component analysis (PCA) was conducted to identify characteristics of PEX-a pipes subjected to these various ageing environments."]},{"key":"dc:title","label":"Title","values":["Tracking the Effect of Accelerated Aging on Cross-Linked Polyethylene Pipe using Fourier Transform Infrared Microscopy"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:contributor.advisor":["Dutcher, John"],"dc:creator":["D'Amico, Joseph"],"dc:date.accessioned":["2022-01-13T21:25:50Z"],"dc:date.available":["2022-01-13T21:25:50Z"],"dc:date.copyright":["2022-01"],"dc:date.created":["2022-01-11"],"dc:description.abstract":["Cross-linked polyethylene (PEX-a) pipes have been quickly replacing metal piping in home and industrial applications due their cost-effective manufacturing process, ease of installation, and long projected lifetimes. However, PEX-a pipes are not immune to oxidative degradation from their environment while in-use, creating the opportunity for premature failure. Therefore, understanding the degradation process is critical to helping extend lifetimes and prevent expensive failures. We have developed several experimental protocols to accelerate the ageing process in-house in our efforts towards this goal, isolating the effects from various environmental stresses present during in-service conditions. By conducting FTIR microscopy measurements on unused/virgin pipes, as well as both in-service and in-house aged pipes, we have found several key indicators of an aged pipe that play a role in pipe failure. Principal component analysis (PCA) was conducted to identify characteristics of PEX-a pipes subjected to these various ageing environments."],"dc:identifier.uri":["https://hdl.handle.net/10214/26685"],"dc:language.iso":["en"],"dc:publisher":["University of Guelph"],"dc:rights.license":["All items in the Atrium are protected by copyright with all rights reserved unless otherwise indicated."],"dc:subject":["PEX-a pipe","accelerated ageing","FTIR microscopy","polymer degradation","principal component analysis"],"dc:title":["Tracking the Effect of Accelerated Aging on Cross-Linked Polyethylene Pipe using Fourier Transform Infrared Microscopy"],"dc:type":["Thesis"],"others:access_status":["open.access"],"thesis:degree_department":["Department of Physics"],"thesis:degree_name":["Master of Science"],"thesis:degree_program":["Physics"],"thesis:institution_name":["University of Guelph"]},"updated_at":"2026-11-19T08:26:04Z"}