{"id":{"repo_id":"manitoba","oai_identifier":"oai:mspace.lib.umanitoba.ca:1993/39665"},"canonical_url":"https://search.ndltd.org/etd/manitoba/oai:mspace.lib.umanitoba.ca:1993/39665","repository":{"repo_id":"manitoba","name":"University of Manitoba","base_url":"https://mspace.lib.umanitoba.ca/oai/request"},"display":{"title":"Valorizing underutilized canola crop residue for fibres and polymer composites: closed-loop retting, enzymatic degradation, and structure–processing–properties relationships","abstract":"The use of canola fibres, obtained from discarded stalks, in textiles and composites is limited due to insufficient knowledge of sustainable fibre extraction technologies, processing chemistry, and structure-processing-properties relationships. The objectives of this study were to: (i) develop a closed-loop water-retting system and optimise retting parameters; (ii) integrate water or field-retting with mechanical decortication to establish a scalable extraction process, and conduct enzymatic post-treatment on canola fibres following water-retting and decortication to understand the kinetics of catalytic degradation and optimise processing conditions; (iii) investigate the effect of fibre processing method and fibre geometry on the properties of nonwoven mats and composites. Water-retted and hand-extracted canola fibres exhibited 10.7±0.3 % fibre yield under optimal retting conditions. The fibre crystallinity index increased, while the linear density decreased with increasing retting time, temperature, and water flow rate. Canola fibres obtained through mechanical decortication following water or field-retting exhibited greater fibre length and marginally lower fibre diameter compared to hand-extracted fibres. The rate of change in pectin concentration determined the degree of fibre degradation during enzymatic treatment with pectinase, conducted on water-retted and decorticated fibres. The fibre degradation process exhibited a rapid initial decay due to higher starting pectin concentration, followed by a progressive slowdown of degradation rate in the remaining phase due to depletion of pectin within the fibres. Unlike pectinase, pectate lyase exhibited substantial differences in degradation effectiveness across various crop varieties. Enzymatic pectinase post-treatment on canola fibres after water-retting and decortication resulted in approximately 87% reduction in fibre diameter and about 80% reduction in linear density, leading to significant improvements in fibre flexibility (∼1148%) and tensile modulus and strength (~94%). For a given fibre length, composites manufactured from water-retted-decorticated (WRD) fibres exhibited the lowest modulus and strength, while those manufactured from WRD-enzyme treated fibres showed the highest. Composites manufactured from field-retted-decorticated fibre fell in between, primarily owing to variations in fibre modulus and consolidation behaviour in that order, which were caused by the differences in fibre chemical composition and diameter resulting from fibre processing and needle punching.","abstract_html":"The use of canola fibres, obtained from discarded stalks, in textiles and composites is limited due to insufficient knowledge of sustainable fibre extraction technologies, processing chemistry, and structure-processing-properties relationships. The objectives of this study were to: (i) develop a closed-loop water-retting system and optimise retting parameters; (ii) integrate water or field-retting with mechanical decortication to establish a scalable extraction process, and conduct enzymatic post-treatment on canola fibres following water-retting and decortication to understand the kinetics of catalytic degradation and optimise processing conditions; (iii) investigate the effect of fibre processing method and fibre geometry on the properties of nonwoven mats and composites. Water-retted and hand-extracted canola fibres exhibited 10.7±0.3 % fibre yield under optimal retting conditions. The fibre crystallinity index increased, while the linear density decreased with increasing retting time, temperature, and water flow rate. Canola fibres obtained through mechanical decortication following water or field-retting exhibited greater fibre length and marginally lower fibre diameter compared to hand-extracted fibres. The rate of change in pectin concentration determined the degree of fibre degradation during enzymatic treatment with pectinase, conducted on water-retted and decorticated fibres. The fibre degradation process exhibited a rapid initial decay due to higher starting pectin concentration, followed by a progressive slowdown of degradation rate in the remaining phase due to depletion of pectin within the fibres. Unlike pectinase, pectate lyase exhibited substantial differences in degradation effectiveness across various crop varieties. Enzymatic pectinase post-treatment on canola fibres after water-retting and decortication resulted in approximately 87% reduction in fibre diameter and about 80% reduction in linear density, leading to significant improvements in fibre flexibility (∼1148%) and tensile modulus and strength (~94%). For a given fibre length, composites manufactured from water-retted-decorticated (WRD) fibres exhibited the lowest modulus and strength, while those manufactured from WRD-enzyme treated fibres showed the highest. Composites manufactured from field-retted-decorticated fibre fell in between, primarily owing to variations in fibre modulus and consolidation behaviour in that order, which were caused by the differences in fibre chemical composition and diameter resulting from fibre processing and needle punching.","abstract_has_math":false,"creators":["Shadhin, Md"],"institution":null,"degree_name":null,"degree_level":"Doctor of Philosophy (Ph.D.)","degree_discipline":"Biosystems Engineering","degree_department":null,"school":null,"contributors":[],"advisors":["Rahman, Mashiur","Jayaraman, Raghavan"],"committee_chairs":[],"committee_members":["Foster, Johan (Chemical and Biological Engineering, University of British Columbia)","Chen, Ying (Biosystems Engineering)","Mann, Danny (Biosystems Engineering)","Zhong, Wen (Biosystems Engineering)"],"year":2026,"date_issued":"2026-03-16","date_published":"2026-03-16","updated_at":"2026-11-19T09:03:53Z","subjects":["Canola","Fibers","Composites","Closed-loop system","Enzymatic degradation"],"languages":["eng"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/1993/39665","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/1993/39665","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Amanitoba%3Aoai%3Amspace.lib.umanitoba.ca%3A1993%2F39665","prefix":"oai_dc"},"source_record":{"url":"https://mspace.lib.umanitoba.ca/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Amspace.lib.umanitoba.ca%3A1993%2F39665","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.committeemember","label":"Committee Member","values":["Foster, Johan (Chemical and Biological Engineering, University of British Columbia)","Chen, Ying (Biosystems Engineering)","Mann, Danny (Biosystems Engineering)","Zhong, Wen (Biosystems Engineering)"]},{"key":"dc:contributor.supervisor","label":"Supervisor","values":["Rahman, Mashiur","Jayaraman, Raghavan"]},{"key":"dc:creator","label":"Author","values":["Shadhin, Md"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2026-03-18T20:18:24Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2026-03-18T20:18:24Z"]},{"key":"dc:date.issued","label":"Date","values":["2026-03-16"]},{"key":"dc:date.submitted","label":"Dc Date Submitted","values":["2026-03-16T18:54:26Z"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Biosystems Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Doctor of Philosophy (Ph.D.)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Canola","Fibers","Composites","Closed-loop system","Enzymatic degradation"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["eng"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/1993/39665"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"crisitem:project.funder","label":"Crisitem Project Funder","values":["University of Manitoba"]},{"key":"crisitem:project.funderid","label":"Crisitem Project Funderid","values":["https://doi.org/10.13039/100010318"]},{"key":"crisitem:project.title","label":"Crisitem Project Title","values":["University of Manitoba Graduate Fellowship (UMGF)"]},{"key":"dc:description.abstract","label":"Abstract","values":["The use of canola fibres, obtained from discarded stalks, in textiles and composites is limited due to insufficient knowledge of sustainable fibre extraction technologies, processing chemistry, and structure-processing-properties relationships. The objectives of this study were to: (i) develop a closed-loop water-retting system and optimise retting parameters; (ii) integrate water or field-retting with mechanical decortication to establish a scalable extraction process, and conduct enzymatic post-treatment on canola fibres following water-retting and decortication to understand the kinetics of catalytic degradation and optimise processing conditions; (iii) investigate the effect of fibre processing method and fibre geometry on the properties of nonwoven mats and composites. Water-retted and hand-extracted canola fibres exhibited 10.7±0.3 % fibre yield under optimal retting conditions. The fibre crystallinity index increased, while the linear density decreased with increasing retting time, temperature, and water flow rate. Canola fibres obtained through mechanical decortication following water or field-retting exhibited greater fibre length and marginally lower fibre diameter compared to hand-extracted fibres. The rate of change in pectin concentration determined the degree of fibre degradation during enzymatic treatment with pectinase, conducted on water-retted and decorticated fibres. The fibre degradation process exhibited a rapid initial decay due to higher starting pectin concentration, followed by a progressive slowdown of degradation rate in the remaining phase due to depletion of pectin within the fibres. Unlike pectinase, pectate lyase exhibited substantial differences in degradation effectiveness across various crop varieties. Enzymatic pectinase post-treatment on canola fibres after water-retting and decortication resulted in approximately 87% reduction in fibre diameter and about 80% reduction in linear density, leading to significant improvements in fibre flexibility (∼1148%) and tensile modulus and strength (~94%). For a given fibre length, composites manufactured from water-retted-decorticated (WRD) fibres exhibited the lowest modulus and strength, while those manufactured from WRD-enzyme treated fibres showed the highest. Composites manufactured from field-retted-decorticated fibre fell in between, primarily owing to variations in fibre modulus and consolidation behaviour in that order, which were caused by the differences in fibre chemical composition and diameter resulting from fibre processing and needle punching."]},{"key":"dc:description.note","label":"Dc Description Note","values":["May 2026"]},{"key":"dc:title","label":"Title","values":["Valorizing underutilized canola crop residue for fibres and polymer composites: closed-loop retting, enzymatic degradation, and structure–processing–properties relationships"]},{"key":"local:admin","label":"Local Admin","values":["yes"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"crisitem:project.funder":["University of Manitoba"],"crisitem:project.funderid":["https://doi.org/10.13039/100010318"],"crisitem:project.title":["University of Manitoba Graduate Fellowship (UMGF)"],"dc:contributor.committeemember":["Foster, Johan (Chemical and Biological Engineering, University of British Columbia)","Chen, Ying (Biosystems Engineering)","Mann, Danny (Biosystems Engineering)","Zhong, Wen (Biosystems Engineering)"],"dc:contributor.supervisor":["Rahman, Mashiur","Jayaraman, Raghavan"],"dc:creator":["Shadhin, Md"],"dc:date.accessioned":["2026-03-18T20:18:24Z"],"dc:date.available":["2026-03-18T20:18:24Z"],"dc:date.issued":["2026-03-16"],"dc:date.submitted":["2026-03-16T18:54:26Z"],"dc:description.abstract":["The use of canola fibres, obtained from discarded stalks, in textiles and composites is limited due to insufficient knowledge of sustainable fibre extraction technologies, processing chemistry, and structure-processing-properties relationships. The objectives of this study were to: (i) develop a closed-loop water-retting system and optimise retting parameters; (ii) integrate water or field-retting with mechanical decortication to establish a scalable extraction process, and conduct enzymatic post-treatment on canola fibres following water-retting and decortication to understand the kinetics of catalytic degradation and optimise processing conditions; (iii) investigate the effect of fibre processing method and fibre geometry on the properties of nonwoven mats and composites. Water-retted and hand-extracted canola fibres exhibited 10.7±0.3 % fibre yield under optimal retting conditions. The fibre crystallinity index increased, while the linear density decreased with increasing retting time, temperature, and water flow rate. Canola fibres obtained through mechanical decortication following water or field-retting exhibited greater fibre length and marginally lower fibre diameter compared to hand-extracted fibres. The rate of change in pectin concentration determined the degree of fibre degradation during enzymatic treatment with pectinase, conducted on water-retted and decorticated fibres. The fibre degradation process exhibited a rapid initial decay due to higher starting pectin concentration, followed by a progressive slowdown of degradation rate in the remaining phase due to depletion of pectin within the fibres. Unlike pectinase, pectate lyase exhibited substantial differences in degradation effectiveness across various crop varieties. Enzymatic pectinase post-treatment on canola fibres after water-retting and decortication resulted in approximately 87% reduction in fibre diameter and about 80% reduction in linear density, leading to significant improvements in fibre flexibility (∼1148%) and tensile modulus and strength (~94%). For a given fibre length, composites manufactured from water-retted-decorticated (WRD) fibres exhibited the lowest modulus and strength, while those manufactured from WRD-enzyme treated fibres showed the highest. Composites manufactured from field-retted-decorticated fibre fell in between, primarily owing to variations in fibre modulus and consolidation behaviour in that order, which were caused by the differences in fibre chemical composition and diameter resulting from fibre processing and needle punching."],"dc:description.note":["May 2026"],"dc:identifier.uri":["http://hdl.handle.net/1993/39665"],"dc:language.iso":["eng"],"dc:subject":["Canola","Fibers","Composites","Closed-loop system","Enzymatic degradation"],"dc:title":["Valorizing underutilized canola crop residue for fibres and polymer composites: closed-loop retting, enzymatic degradation, and structure–processing–properties relationships"],"local:admin":["yes"],"others:access_status":["open.access"],"thesis:degree_discipline":["Biosystems Engineering"],"thesis:degree_level":["Doctor of Philosophy (Ph.D.)"]},"updated_at":"2026-11-19T09:03:53Z"}