{"id":{"repo_id":"maryland","oai_identifier":"oai:drum.lib.umd.edu:1903/15432"},"canonical_url":"https://search.ndltd.org/etd/maryland/oai:drum.lib.umd.edu:1903/15432","repository":{"repo_id":"maryland","name":"University of Maryland","base_url":"https://api.drum.lib.umd.edu/server/oai/request"},"display":{"title":"Ultra-High Molecular Weight Nonlinear Bisphenol A Polycarbonates by Solid State Polymerization in Micro-Layers","abstract":"The solid-state polymerization of bisphenol A polycarbonate (BPAPC) has been studied in amorphous and partially crystallized micro-layers (SSP<sub>m</sub>) of low molecular weight prepolymers in presence of LiOH.H<sub>2</sub>O catalyst at a temperature between the glass transition temperature and the melting point. When the prepolymers (14,000 g/mol) in micro-layers of a thickness range from 5 &mu;m to 35 &mu;m were solid-state polymerized at 230 °C, the polymer molecular weight increased rapidly to above 100,000 g/mol, exceeding the highest molecular weight obtainable by the conventional solid-state polymerization in micro-particles. It has also been observed that the final molecular weight reached as high as 600,000 g/mol even in presence of significant stoichiometric imbalances of end group mole ratios when the prepolymer having 21,000 g/mol is used at 230°C under low pressure (10 mmHg). Most notably, amorphous prepolymer micro-layers showed significantly higher increase in molecular weight than partially crystallized prepolymer micro-layers. The chain branching and partially cross-linked structures in high molecular weight polycarbonates have been confirmed by <super>1</super>H-NMR spectroscopic analysis as well as pyrolysis-gas chromatography mass spectrometry (Py-GC/MS). <super>13</super>C-NMR analysis and SSP theoretical model simulation have shown that conventional linear step-growth polymerization is not responsible for the additional increase in molecular weight beyond 50,000 g/mol of polycarbonate MW. The ultra-high molecular weight is contributed to the formation of branched and partially cross-linked structures via Fries or Kolbe-Schmitt rearrangement reactions and radical recombination reaction, respectively. Micro-radical polycarbonate species can be produced via chain scission reaction and hydrogen abstraction at the solid-state polymerization temperature. The formation of cross-linked polymers by radical recombination reactions was attributed to the near complete removal of phenol (i.e. radical scavenger) from the micro-layers during the solid state polymerization. Branched structure polycarbonate was also confirmed by atomic force microscopy (AFM). The presence of branched and cross-linked polymers contributed to the insolubility of the polymer in solvents such as chloroform, tetrahydrofuran (THF), and methlylene chloride. As SSP<sub>m</sub> process extends for a long reaction time at 230°C, about 95% of the polymer was insoluble with excellent transparency (90-93% light transmission). Properties of ultra-high molecular weight nonlinear polycarbonates (SSP<sub>m</sub> PCs) have been investigated by differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), and rheometer. The development of Multi-Layer Deposit and Reaction (MLDR) technique has shown that the SSP<sub>m</sub> process is not limited to 5-35&mu;m scale. The layer thickness can be expanded while keeping the merits (e.g. high transparency, good solvent resistance, and obtaining high molecular weight in short reaction time) of the SSP<sub>m</sub> technique developed in this study.","abstract_html":"The solid-state polymerization of bisphenol A polycarbonate (BPAPC) has been studied in amorphous and partially crystallized micro-layers (SSP&lt;sub&gt;m&lt;/sub&gt;) of low molecular weight prepolymers in presence of LiOH.H&lt;sub&gt;2&lt;/sub&gt;O catalyst at a temperature between the glass transition temperature and the melting point. When the prepolymers (14,000 g/mol) in micro-layers of a thickness range from 5 &amp;mu;m to 35 &amp;mu;m were solid-state polymerized at 230 °C, the polymer molecular weight increased rapidly to above 100,000 g/mol, exceeding the highest molecular weight obtainable by the conventional solid-state polymerization in micro-particles. It has also been observed that the final molecular weight reached as high as 600,000 g/mol even in presence of significant stoichiometric imbalances of end group mole ratios when the prepolymer having 21,000 g/mol is used at 230°C under low pressure (10 mmHg). Most notably, amorphous prepolymer micro-layers showed significantly higher increase in molecular weight than partially crystallized prepolymer micro-layers. The chain branching and partially cross-linked structures in high molecular weight polycarbonates have been confirmed by &lt;super&gt;1&lt;/super&gt;H-NMR spectroscopic analysis as well as pyrolysis-gas chromatography mass spectrometry (Py-GC/MS). &lt;super&gt;13&lt;/super&gt;C-NMR analysis and SSP theoretical model simulation have shown that conventional linear step-growth polymerization is not responsible for the additional increase in molecular weight beyond 50,000 g/mol of polycarbonate MW. The ultra-high molecular weight is contributed to the formation of branched and partially cross-linked structures via Fries or Kolbe-Schmitt rearrangement reactions and radical recombination reaction, respectively. Micro-radical polycarbonate species can be produced via chain scission reaction and hydrogen abstraction at the solid-state polymerization temperature. The formation of cross-linked polymers by radical recombination reactions was attributed to the near complete removal of phenol (i.e. radical scavenger) from the micro-layers during the solid state polymerization. Branched structure polycarbonate was also confirmed by atomic force microscopy (AFM). The presence of branched and cross-linked polymers contributed to the insolubility of the polymer in solvents such as chloroform, tetrahydrofuran (THF), and methlylene chloride. As SSP&lt;sub&gt;m&lt;/sub&gt; process extends for a long reaction time at 230°C, about 95% of the polymer was insoluble with excellent transparency (90-93% light transmission). Properties of ultra-high molecular weight nonlinear polycarbonates (SSP&lt;sub&gt;m&lt;/sub&gt; PCs) have been investigated by differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), and rheometer. The development of Multi-Layer Deposit and Reaction (MLDR) technique has shown that the SSP&lt;sub&gt;m&lt;/sub&gt; process is not limited to 5-35&amp;mu;m scale. The layer thickness can be expanded while keeping the merits (e.g. high transparency, good solvent resistance, and obtaining high molecular weight in short reaction time) of the SSP&lt;sub&gt;m&lt;/sub&gt; technique developed in this study.","abstract_has_math":false,"creators":["Baick, In Hak"],"institution":"Digital Repository at the University of Maryland","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":"Chemical Engineering","school":null,"contributors":[],"advisors":["Choi, Kyu Yong"],"committee_chairs":[],"committee_members":[],"year":2013,"date_issued":"2013","date_published":"2013","updated_at":"2026-11-19T08:53:11Z","subjects":[],"languages":["en"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/1903/15432","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/1903/15432","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Amaryland%3Aoai%3Adrum.lib.umd.edu%3A1903%2F15432","prefix":"oai_dc"},"source_record":{"url":"https://api.drum.lib.umd.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Adrum.lib.umd.edu%3A1903%2F15432","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Choi, Kyu Yong"]},{"key":"dc:contributor.department","label":"Department","values":["Chemical Engineering"]},{"key":"dc:creator","label":"Author","values":["Baick, In Hak"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2014-06-26T05:31:38Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2014-06-26T05:31:38Z"]},{"key":"dc:date.issued","label":"Date","values":["2013"]},{"key":"dc:publisher","label":"Institution","values":["Digital Repository at the University of Maryland","University of Maryland (College Park, Md.)"]},{"key":"dc:type","label":"Dc Type","values":["Dissertation"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject.keyword","label":"Dc Subject Keyword","values":["Amorphous state","Bisphenol A Polycarbonates","insoluble polycarbonates","micro-layers","partial cross-linking","step-growth polymerization"]},{"key":"dc:subject.proquest","label":"Dc Subject Proquest","values":["Chemical engineering","Polymer chemistry"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/1903/15432"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["The solid-state polymerization of bisphenol A polycarbonate (BPAPC) has been studied in amorphous and partially crystallized micro-layers (SSP<sub>m</sub>) of low molecular weight prepolymers in presence of LiOH.H<sub>2</sub>O catalyst at a temperature between the glass transition temperature and the melting point. When the prepolymers (14,000 g/mol) in micro-layers of a thickness range from 5 &mu;m to 35 &mu;m were solid-state polymerized at 230 °C, the polymer molecular weight increased rapidly to above 100,000 g/mol, exceeding the highest molecular weight obtainable by the conventional solid-state polymerization in micro-particles. It has also been observed that the final molecular weight reached as high as 600,000 g/mol even in presence of significant stoichiometric imbalances of end group mole ratios when the prepolymer having 21,000 g/mol is used at 230°C under low pressure (10 mmHg). Most notably, amorphous prepolymer micro-layers showed significantly higher increase in molecular weight than partially crystallized prepolymer micro-layers. The chain branching and partially cross-linked structures in high molecular weight polycarbonates have been confirmed by <super>1</super>H-NMR spectroscopic analysis as well as pyrolysis-gas chromatography mass spectrometry (Py-GC/MS). <super>13</super>C-NMR analysis and SSP theoretical model simulation have shown that conventional linear step-growth polymerization is not responsible for the additional increase in molecular weight beyond 50,000 g/mol of polycarbonate MW. The ultra-high molecular weight is contributed to the formation of branched and partially cross-linked structures via Fries or Kolbe-Schmitt rearrangement reactions and radical recombination reaction, respectively. Micro-radical polycarbonate species can be produced via chain scission reaction and hydrogen abstraction at the solid-state polymerization temperature. The formation of cross-linked polymers by radical recombination reactions was attributed to the near complete removal of phenol (i.e. radical scavenger) from the micro-layers during the solid state polymerization. Branched structure polycarbonate was also confirmed by atomic force microscopy (AFM). The presence of branched and cross-linked polymers contributed to the insolubility of the polymer in solvents such as chloroform, tetrahydrofuran (THF), and methlylene chloride. As SSP<sub>m</sub> process extends for a long reaction time at 230°C, about 95% of the polymer was insoluble with excellent transparency (90-93% light transmission). Properties of ultra-high molecular weight nonlinear polycarbonates (SSP<sub>m</sub> PCs) have been investigated by differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), and rheometer. The development of Multi-Layer Deposit and Reaction (MLDR) technique has shown that the SSP<sub>m</sub> process is not limited to 5-35&mu;m scale. The layer thickness can be expanded while keeping the merits (e.g. high transparency, good solvent resistance, and obtaining high molecular weight in short reaction time) of the SSP<sub>m</sub> technique developed in this study."]},{"key":"dc:title","label":"Title","values":["Ultra-High Molecular Weight Nonlinear Bisphenol A Polycarbonates by Solid State Polymerization in Micro-Layers"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:contributor.advisor":["Choi, Kyu Yong"],"dc:contributor.department":["Chemical Engineering"],"dc:creator":["Baick, In Hak"],"dc:date.accessioned":["2014-06-26T05:31:38Z"],"dc:date.available":["2014-06-26T05:31:38Z"],"dc:date.issued":["2013"],"dc:description.abstract":["The solid-state polymerization of bisphenol A polycarbonate (BPAPC) has been studied in amorphous and partially crystallized micro-layers (SSP<sub>m</sub>) of low molecular weight prepolymers in presence of LiOH.H<sub>2</sub>O catalyst at a temperature between the glass transition temperature and the melting point. When the prepolymers (14,000 g/mol) in micro-layers of a thickness range from 5 &mu;m to 35 &mu;m were solid-state polymerized at 230 °C, the polymer molecular weight increased rapidly to above 100,000 g/mol, exceeding the highest molecular weight obtainable by the conventional solid-state polymerization in micro-particles. It has also been observed that the final molecular weight reached as high as 600,000 g/mol even in presence of significant stoichiometric imbalances of end group mole ratios when the prepolymer having 21,000 g/mol is used at 230°C under low pressure (10 mmHg). Most notably, amorphous prepolymer micro-layers showed significantly higher increase in molecular weight than partially crystallized prepolymer micro-layers. The chain branching and partially cross-linked structures in high molecular weight polycarbonates have been confirmed by <super>1</super>H-NMR spectroscopic analysis as well as pyrolysis-gas chromatography mass spectrometry (Py-GC/MS). <super>13</super>C-NMR analysis and SSP theoretical model simulation have shown that conventional linear step-growth polymerization is not responsible for the additional increase in molecular weight beyond 50,000 g/mol of polycarbonate MW. The ultra-high molecular weight is contributed to the formation of branched and partially cross-linked structures via Fries or Kolbe-Schmitt rearrangement reactions and radical recombination reaction, respectively. Micro-radical polycarbonate species can be produced via chain scission reaction and hydrogen abstraction at the solid-state polymerization temperature. The formation of cross-linked polymers by radical recombination reactions was attributed to the near complete removal of phenol (i.e. radical scavenger) from the micro-layers during the solid state polymerization. Branched structure polycarbonate was also confirmed by atomic force microscopy (AFM). The presence of branched and cross-linked polymers contributed to the insolubility of the polymer in solvents such as chloroform, tetrahydrofuran (THF), and methlylene chloride. As SSP<sub>m</sub> process extends for a long reaction time at 230°C, about 95% of the polymer was insoluble with excellent transparency (90-93% light transmission). Properties of ultra-high molecular weight nonlinear polycarbonates (SSP<sub>m</sub> PCs) have been investigated by differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), and rheometer. The development of Multi-Layer Deposit and Reaction (MLDR) technique has shown that the SSP<sub>m</sub> process is not limited to 5-35&mu;m scale. The layer thickness can be expanded while keeping the merits (e.g. high transparency, good solvent resistance, and obtaining high molecular weight in short reaction time) of the SSP<sub>m</sub> technique developed in this study."],"dc:identifier.uri":["http://hdl.handle.net/1903/15432"],"dc:language.iso":["en"],"dc:publisher":["Digital Repository at the University of Maryland","University of Maryland (College Park, Md.)"],"dc:subject.keyword":["Amorphous state","Bisphenol A Polycarbonates","insoluble polycarbonates","micro-layers","partial cross-linking","step-growth polymerization"],"dc:subject.proquest":["Chemical engineering","Polymer chemistry"],"dc:title":["Ultra-High Molecular Weight Nonlinear Bisphenol A Polycarbonates by Solid State Polymerization in Micro-Layers"],"dc:type":["Dissertation"],"others:access_status":["open.access"]},"updated_at":"2026-11-19T08:53:11Z"}