{"id":{"repo_id":"mcmaster","oai_identifier":"oai:macsphere.mcmaster.ca:11375/18389"},"canonical_url":"https://search.ndltd.org/etd/mcmaster/oai:macsphere.mcmaster.ca:11375/18389","repository":{"repo_id":"mcmaster","name":"McMaster University","base_url":"https://macsphere.mcmaster.ca/server/oai/request"},"display":{"title":"THE EFFECT OF H2SO4 SURFACE PRE-TREATMENT ON THE STRESS CORROSION CRACKING OF MAGNESIUM ALLOY AZ31B","abstract":"The stress corrosion cracking (SCC) behaviour of Mg alloy AZ31B was investigated with respect to surface condition. Salt fog U-bend testing was used to identify changes in SCC as a result of surface conditioning pre-treatments. Six surface conditions were investigated: as-received, mechanically-polished, sulphuric acid (H2SO4)-cleaned, mechanically-polished then H2SO4-cleaned, aged H2SO4-cleaned, and acetic acid (C2H4O2)-cleaned. Results showed that the rate of SCC was accelerated and the SCC mode was intergranular for all surface conditioning treatments involving H2SO4-cleaning. It was found that the accelerated intergranular SCC was a result of three contributing factors: a low pH, the presence of aggressive ions, and a porous film which allowed direct contact between the metal surface and the electrolyte. Characterization of the surfaces using potentiodynamic polarization and cross-sectional images of sample surfaces showed that in the absence of one of these three contributing factors intergranular SCC would not occur.","abstract_html":"The stress corrosion cracking (SCC) behaviour of Mg alloy AZ31B was investigated with respect to surface condition. Salt fog U-bend testing was used to identify changes in SCC as a result of surface conditioning pre-treatments. Six surface conditions were investigated: as-received, mechanically-polished, sulphuric acid (H2SO4)-cleaned, mechanically-polished then H2SO4-cleaned, aged H2SO4-cleaned, and acetic acid (C2H4O2)-cleaned. Results showed that the rate of SCC was accelerated and the SCC mode was intergranular for all surface conditioning treatments involving H2SO4-cleaning. It was found that the accelerated intergranular SCC was a result of three contributing factors: a low pH, the presence of aggressive ions, and a porous film which allowed direct contact between the metal surface and the electrolyte. Characterization of the surfaces using potentiodynamic polarization and cross-sectional images of sample surfaces showed that in the absence of one of these three contributing factors intergranular SCC would not occur.","abstract_has_math":false,"creators":["Wilson, Brycklin"],"institution":null,"degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":"Materials Science and Engineering","school":null,"contributors":[],"advisors":["Kish, Joseph","McDermid, Joseph"],"committee_chairs":[],"committee_members":[],"year":2015,"date_issued":"2015-11","date_published":"2015-11","updated_at":"2026-11-18T19:39:05Z","subjects":["Magnesium","Stress Corrosion Cracking"],"languages":["en"],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://doi.org/10.71548/22713"],"render_values":[{"text":"https://doi.org/10.71548/22713","href":"https://doi.org/10.71548/22713","code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/11375/18389","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"http://hdl.handle.net/11375/18389","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://macsphere.mcmaster.ca/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Amacsphere.mcmaster.ca%3A11375%2F18389","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Kish, Joseph","McDermid, Joseph"]},{"key":"dc:contributor.department","label":"Department","values":["Materials Science and Engineering"]},{"key":"dc:creator","label":"Author","values":["Wilson, Brycklin"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2015-10-08T19:26:52Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2015-10-08T19:26:52Z"]},{"key":"dc:date.issued","label":"Date","values":["2015-11"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Magnesium","Stress Corrosion Cracking"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/11375/18389","https://doi.org/10.71548/22713"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["The stress corrosion cracking (SCC) behaviour of Mg alloy AZ31B was investigated with respect to surface condition. Salt fog U-bend testing was used to identify changes in SCC as a result of surface conditioning pre-treatments. Six surface conditions were investigated: as-received, mechanically-polished, sulphuric acid (H2SO4)-cleaned, mechanically-polished then H2SO4-cleaned, aged H2SO4-cleaned, and acetic acid (C2H4O2)-cleaned. Results showed that the rate of SCC was accelerated and the SCC mode was intergranular for all surface conditioning treatments involving H2SO4-cleaning. It was found that the accelerated intergranular SCC was a result of three contributing factors: a low pH, the presence of aggressive ions, and a porous film which allowed direct contact between the metal surface and the electrolyte. Characterization of the surfaces using potentiodynamic polarization and cross-sectional images of sample surfaces showed that in the absence of one of these three contributing factors intergranular SCC would not occur."]},{"key":"dc:description.degree","label":"Dc Description Degree","values":["Master of Applied Science (MASc)"]},{"key":"dc:title","label":"Title","values":["THE EFFECT OF H2SO4 SURFACE PRE-TREATMENT ON THE STRESS CORROSION CRACKING OF MAGNESIUM ALLOY AZ31B"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:contributor.advisor":["Kish, Joseph","McDermid, Joseph"],"dc:contributor.department":["Materials Science and Engineering"],"dc:creator":["Wilson, Brycklin"],"dc:date.accessioned":["2015-10-08T19:26:52Z"],"dc:date.available":["2015-10-08T19:26:52Z"],"dc:date.issued":["2015-11"],"dc:description.abstract":["The stress corrosion cracking (SCC) behaviour of Mg alloy AZ31B was investigated with respect to surface condition. Salt fog U-bend testing was used to identify changes in SCC as a result of surface conditioning pre-treatments. Six surface conditions were investigated: as-received, mechanically-polished, sulphuric acid (H2SO4)-cleaned, mechanically-polished then H2SO4-cleaned, aged H2SO4-cleaned, and acetic acid (C2H4O2)-cleaned. Results showed that the rate of SCC was accelerated and the SCC mode was intergranular for all surface conditioning treatments involving H2SO4-cleaning. It was found that the accelerated intergranular SCC was a result of three contributing factors: a low pH, the presence of aggressive ions, and a porous film which allowed direct contact between the metal surface and the electrolyte. Characterization of the surfaces using potentiodynamic polarization and cross-sectional images of sample surfaces showed that in the absence of one of these three contributing factors intergranular SCC would not occur."],"dc:description.degree":["Master of Applied Science (MASc)"],"dc:identifier.uri":["http://hdl.handle.net/11375/18389","https://doi.org/10.71548/22713"],"dc:language.iso":["en"],"dc:subject":["Magnesium","Stress Corrosion Cracking"],"dc:title":["THE EFFECT OF H2SO4 SURFACE PRE-TREATMENT ON THE STRESS CORROSION CRACKING OF MAGNESIUM ALLOY AZ31B"],"dc:type":["Thesis"],"others:access_status":["open.access"]},"updated_at":"2026-11-18T19:39:05Z"}