{"id":{"repo_id":"mcmaster","oai_identifier":"oai:macsphere.mcmaster.ca:11375/8776"},"canonical_url":"https://search.ndltd.org/etd/mcmaster/oai:macsphere.mcmaster.ca:11375/8776","repository":{"repo_id":"mcmaster","name":"McMaster University","base_url":"https://macsphere.mcmaster.ca/server/oai/request"},"display":{"title":"The Properties of Lead Titanate Thin Films produced by Chemical Vapour Deposition","abstract":"<p>This project focused on advancing the knowledge of chemical vapour<br />deposition (CVD) PbTiO₃ thin films for future work on lead zirconate titanate or PZT<br />(PbZrᵪT₁_ᵪO₃) through an understanding of the structural, chemical and electrical<br />properties of the material.</p> <p>A study of the individual oxides, TiO₂ and PbOᵪ, prepared also by CVD, was<br />made using transmission electron microscopy (TEM), scanning electron microscopy<br />(SEM), Raman spectroscopy and x-ray diffraction (XRD), before a low pressure, low<br />temperature process for PbTiO₃ was developed. The major factors in controlling the<br />film composition and thickness uniformity were identified. The formation sequence<br />for CVO PbTiO₃ films involved individual oxides of Ti and Pb, rather than<br />pyrochlore-type phases. A Pb-rich composition ensured the formation of perovskite,<br />however it resulted in the formation of a thin PbOᵪ surface layer. Removal of this<br />layer by etching gave improved electrical properties. Capacitance measurements<br />typically varied less than 1% over the frequency range and gave ε' values from<br />60-155. At 1 kHz, tan δ was ~0.01 and the resistivity was ~10¹¹Ω.cm.</p> <p>TEM examination of as-deposited films of PbTiO₃ revealed no macro-domains existed. After post-deposition annealing twinned structures acting as domains were<br />found in grains, ~0.1 μm in size. The origin of the theoretical minimum grain size<br />for twinning in PbTiO₃ thin films is discussed. A classification scheme for domain structures was developed based on thin films of PbTiO₃ and PZT. Similarities were<br />drawn between these domain structures and their bulk counterparts.</p> <p>The multi-layered bottom electrode of Pt and Ti used in this study was found<br />to react at temperatures ≤515°C. At higher temperatures (698°C), the Ti layer was<br />completely consumed, however the top surface of the Pt layer remained unaffected.</p>","abstract_html":"&lt;p&gt;This project focused on advancing the knowledge of chemical vapour&lt;br /&gt;deposition (CVD) PbTiO₃ thin films for future work on lead zirconate titanate or PZT&lt;br /&gt;(PbZrᵪT₁_ᵪO₃) through an understanding of the structural, chemical and electrical&lt;br /&gt;properties of the material.&lt;/p&gt; &lt;p&gt;A study of the individual oxides, TiO₂ and PbOᵪ, prepared also by CVD, was&lt;br /&gt;made using transmission electron microscopy (TEM), scanning electron microscopy&lt;br /&gt;(SEM), Raman spectroscopy and x-ray diffraction (XRD), before a low pressure, low&lt;br /&gt;temperature process for PbTiO₃ was developed. The major factors in controlling the&lt;br /&gt;film composition and thickness uniformity were identified. The formation sequence&lt;br /&gt;for CVO PbTiO₃ films involved individual oxides of Ti and Pb, rather than&lt;br /&gt;pyrochlore-type phases. A Pb-rich composition ensured the formation of perovskite,&lt;br /&gt;however it resulted in the formation of a thin PbOᵪ surface layer. Removal of this&lt;br /&gt;layer by etching gave improved electrical properties. Capacitance measurements&lt;br /&gt;typically varied less than 1% over the frequency range and gave ε&#x27; values from&lt;br /&gt;60-155. At 1 kHz, tan δ was ~0.01 and the resistivity was ~10¹¹Ω.cm.&lt;/p&gt; &lt;p&gt;TEM examination of as-deposited films of PbTiO₃ revealed no macro-domains existed. After post-deposition annealing twinned structures acting as domains were&lt;br /&gt;found in grains, ~0.1 μm in size. The origin of the theoretical minimum grain size&lt;br /&gt;for twinning in PbTiO₃ thin films is discussed. A classification scheme for domain structures was developed based on thin films of PbTiO₃ and PZT. Similarities were&lt;br /&gt;drawn between these domain structures and their bulk counterparts.&lt;/p&gt; &lt;p&gt;The multi-layered bottom electrode of Pt and Ti used in this study was found&lt;br /&gt;to react at temperatures ≤515°C. At higher temperatures (698°C), the Ti layer was&lt;br /&gt;completely consumed, however the top surface of the Pt layer remained unaffected.&lt;/p&gt;","abstract_has_math":false,"creators":["Madsen, Lynnette D."],"institution":null,"degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":"Materials Science and Engineering","school":null,"contributors":[],"advisors":["Weatherly, G.C.","Emesh, I."],"committee_chairs":[],"committee_members":[],"year":1994,"date_issued":"1994-06","date_published":"1994-06","updated_at":"2026-11-18T19:32:04Z","subjects":[],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://doi.org/10.71548/11012"],"render_values":[{"text":"https://doi.org/10.71548/11012","href":"https://doi.org/10.71548/11012","code":true}]},{"key":"dc:identifier.other","label":"Dc Identifier Other","values":["opendissertations/3952","4969","1859365"],"render_values":[{"text":"opendissertations/3952","href":null,"code":true},{"text":"4969","href":null,"code":true},{"text":"1859365","href":null,"code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/11375/8776","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"http://hdl.handle.net/11375/8776","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://macsphere.mcmaster.ca/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Amacsphere.mcmaster.ca%3A11375%2F8776","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Weatherly, G.C.","Emesh, I."]},{"key":"dc:contributor.department","label":"Department","values":["Materials Science and Engineering"]},{"key":"dc:creator","label":"Author","values":["Madsen, Lynnette D."]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2014-06-18T16:43:56Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2014-06-18T16:43:56Z"]},{"key":"dc:date.created","label":"Dc Date Created","values":["2011-03-08"]},{"key":"dc:date.issued","label":"Date","values":["1994-06"]},{"key":"dc:type","label":"Dc Type","values":["thesis"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.other","label":"Dc Identifier Other","values":["opendissertations/3952","4969","1859365"]},{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/11375/8776","https://doi.org/10.71548/11012"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["<p>This project focused on advancing the knowledge of chemical vapour<br />deposition (CVD) PbTiO₃ thin films for future work on lead zirconate titanate or PZT<br />(PbZrᵪT₁_ᵪO₃) through an understanding of the structural, chemical and electrical<br />properties of the material.</p> <p>A study of the individual oxides, TiO₂ and PbOᵪ, prepared also by CVD, was<br />made using transmission electron microscopy (TEM), scanning electron microscopy<br />(SEM), Raman spectroscopy and x-ray diffraction (XRD), before a low pressure, low<br />temperature process for PbTiO₃ was developed. The major factors in controlling the<br />film composition and thickness uniformity were identified. The formation sequence<br />for CVO PbTiO₃ films involved individual oxides of Ti and Pb, rather than<br />pyrochlore-type phases. A Pb-rich composition ensured the formation of perovskite,<br />however it resulted in the formation of a thin PbOᵪ surface layer. Removal of this<br />layer by etching gave improved electrical properties. Capacitance measurements<br />typically varied less than 1% over the frequency range and gave ε' values from<br />60-155. At 1 kHz, tan δ was ~0.01 and the resistivity was ~10¹¹Ω.cm.</p> <p>TEM examination of as-deposited films of PbTiO₃ revealed no macro-domains existed. After post-deposition annealing twinned structures acting as domains were<br />found in grains, ~0.1 μm in size. The origin of the theoretical minimum grain size<br />for twinning in PbTiO₃ thin films is discussed. A classification scheme for domain structures was developed based on thin films of PbTiO₃ and PZT. Similarities were<br />drawn between these domain structures and their bulk counterparts.</p> <p>The multi-layered bottom electrode of Pt and Ti used in this study was found<br />to react at temperatures ≤515°C. At higher temperatures (698°C), the Ti layer was<br />completely consumed, however the top surface of the Pt layer remained unaffected.</p>"]},{"key":"dc:description.degree","label":"Dc Description Degree","values":["Doctor of Philosophy (PhD)"]},{"key":"dc:title","label":"Title","values":["The Properties of Lead Titanate Thin Films produced by Chemical Vapour Deposition"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:contributor.advisor":["Weatherly, G.C.","Emesh, I."],"dc:contributor.department":["Materials Science and Engineering"],"dc:creator":["Madsen, Lynnette D."],"dc:date.accessioned":["2014-06-18T16:43:56Z"],"dc:date.available":["2014-06-18T16:43:56Z"],"dc:date.created":["2011-03-08"],"dc:date.issued":["1994-06"],"dc:description.abstract":["<p>This project focused on advancing the knowledge of chemical vapour<br />deposition (CVD) PbTiO₃ thin films for future work on lead zirconate titanate or PZT<br />(PbZrᵪT₁_ᵪO₃) through an understanding of the structural, chemical and electrical<br />properties of the material.</p> <p>A study of the individual oxides, TiO₂ and PbOᵪ, prepared also by CVD, was<br />made using transmission electron microscopy (TEM), scanning electron microscopy<br />(SEM), Raman spectroscopy and x-ray diffraction (XRD), before a low pressure, low<br />temperature process for PbTiO₃ was developed. The major factors in controlling the<br />film composition and thickness uniformity were identified. The formation sequence<br />for CVO PbTiO₃ films involved individual oxides of Ti and Pb, rather than<br />pyrochlore-type phases. A Pb-rich composition ensured the formation of perovskite,<br />however it resulted in the formation of a thin PbOᵪ surface layer. Removal of this<br />layer by etching gave improved electrical properties. Capacitance measurements<br />typically varied less than 1% over the frequency range and gave ε' values from<br />60-155. At 1 kHz, tan δ was ~0.01 and the resistivity was ~10¹¹Ω.cm.</p> <p>TEM examination of as-deposited films of PbTiO₃ revealed no macro-domains existed. After post-deposition annealing twinned structures acting as domains were<br />found in grains, ~0.1 μm in size. The origin of the theoretical minimum grain size<br />for twinning in PbTiO₃ thin films is discussed. A classification scheme for domain structures was developed based on thin films of PbTiO₃ and PZT. Similarities were<br />drawn between these domain structures and their bulk counterparts.</p> <p>The multi-layered bottom electrode of Pt and Ti used in this study was found<br />to react at temperatures ≤515°C. At higher temperatures (698°C), the Ti layer was<br />completely consumed, however the top surface of the Pt layer remained unaffected.</p>"],"dc:description.degree":["Doctor of Philosophy (PhD)"],"dc:identifier.other":["opendissertations/3952","4969","1859365"],"dc:identifier.uri":["http://hdl.handle.net/11375/8776","https://doi.org/10.71548/11012"],"dc:title":["The Properties of Lead Titanate Thin Films produced by Chemical Vapour Deposition"],"dc:type":["thesis"],"others:access_status":["open.access"]},"updated_at":"2026-11-18T19:32:04Z"}