{"id":{"repo_id":"mtu","oai_identifier":"oai:digitalcommons.mtu.edu:etds-1027"},"canonical_url":"https://search.ndltd.org/etd/mtu/oai:digitalcommons.mtu.edu:etds-1027","repository":{"repo_id":"mtu","name":"Michigan Technological University","base_url":"https://digitalcommons.mtu.edu/do/oai/"},"display":{"title":"Processing and mechanical properties of cast aluminum containing scandium, zirconium, and ytterbium","abstract":"A series of aluminum alloys containing additions of scandium, zirconium, and ytterbium were cast to evaluate the effect of partial ytterbium substitution for scandium on tensile behavior. Due to the high price of scandium, a crucible-melt interaction study was performed to ensure no scandium was lost in graphite, alumina, magnesia, or zirconia crucibles after holding a liquid Al-Sc master alloy for 8 hours at 900 °C in an argon atmosphere. The alloys were subjected to an isochronal aging treatment and tested for conductivity and Vickers microhardness after each increment. For scandium-containing alloys, peak hardnesses of 520-790 MPa, and peak tensile stresses of 138-234 MPa were observed after aging from 150-350 °C for 3 hours in increments of 50 °C, and for alloys without scandium, peak hardnesses of 217-335 MPa and peak tensile stresses of 45-63 MPa were observed after a 3 hour, 150 °C aging treatment. The hardness and tensile strength of the ytterbium containing alloy was found to be lower than in the alloy with no ytterbium substitution.","abstract_html":"A series of aluminum alloys containing additions of scandium, zirconium, and ytterbium were cast to evaluate the effect of partial ytterbium substitution for scandium on tensile behavior. Due to the high price of scandium, a crucible-melt interaction study was performed to ensure no scandium was lost in graphite, alumina, magnesia, or zirconia crucibles after holding a liquid Al-Sc master alloy for 8 hours at 900 °C in an argon atmosphere. The alloys were subjected to an isochronal aging treatment and tested for conductivity and Vickers microhardness after each increment. For scandium-containing alloys, peak hardnesses of 520-790 MPa, and peak tensile stresses of 138-234 MPa were observed after aging from 150-350 °C for 3 hours in increments of 50 °C, and for alloys without scandium, peak hardnesses of 217-335 MPa and peak tensile stresses of 45-63 MPa were observed after a 3 hour, 150 °C aging treatment. The hardness and tensile strength of the ytterbium containing alloy was found to be lower than in the alloy with no ytterbium substitution.","abstract_has_math":false,"creators":["Johnson, Nicholas D."],"institution":null,"degree_name":"Master of Science in Materials Science and Engineering (MS)","degree_level":"Master's Thesis","degree_discipline":"Department of Materials Science and Engineering","degree_department":null,"school":null,"contributors":["Paul George Sanders"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T08:14:43Z","subjects":["Engineering","Engineering Science and Materials"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digitalcommons.mtu.edu/etds/28"],"render_values":[{"text":"https://digitalcommons.mtu.edu/etds/28","href":"https://digitalcommons.mtu.edu/etds/28","code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://doi.org/10.37099/mtu.dc.etds/28","outbound_label":"DOI","outbound_source":"dc:identifier","record_url":"https://doi.org/10.37099/mtu.dc.etds/28","record_label":"Repository record","record_kind":"doi","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digitalcommons.mtu.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Adigitalcommons.mtu.edu%3Aetds-1027","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Paul George Sanders"]},{"key":"dc:creator","label":"Author","values":["Johnson, Nicholas D."]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["2011-01-01T08:00:00Z"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Department of Materials Science and Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Master's Thesis"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science in Materials Science and Engineering (MS)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Engineering","Engineering Science and Materials"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["10.37099/mtu.dc.etds/28","https://digitalcommons.mtu.edu/etds/28"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["A series of aluminum alloys containing additions of scandium, zirconium, and ytterbium were cast to evaluate the effect of partial ytterbium substitution for scandium on tensile behavior. Due to the high price of scandium, a crucible-melt interaction study was performed to ensure no scandium was lost in graphite, alumina, magnesia, or zirconia crucibles after holding a liquid Al-Sc master alloy for 8 hours at 900 °C in an argon atmosphere. The alloys were subjected to an isochronal aging treatment and tested for conductivity and Vickers microhardness after each increment. For scandium-containing alloys, peak hardnesses of 520-790 MPa, and peak tensile stresses of 138-234 MPa were observed after aging from 150-350 °C for 3 hours in increments of 50 °C, and for alloys without scandium, peak hardnesses of 217-335 MPa and peak tensile stresses of 45-63 MPa were observed after a 3 hour, 150 °C aging treatment. The hardness and tensile strength of the ytterbium containing alloy was found to be lower than in the alloy with no ytterbium substitution."]},{"key":"dc:title","label":"Title","values":["Processing and mechanical properties of cast aluminum containing scandium, zirconium, and ytterbium"]}]}],"canonical_facts":{"dc:contributor":["Paul George Sanders"],"dc:creator":["Johnson, Nicholas D."],"dc:date.created":["2011-01-01T08:00:00Z"],"dc:description.abstract":["A series of aluminum alloys containing additions of scandium, zirconium, and ytterbium were cast to evaluate the effect of partial ytterbium substitution for scandium on tensile behavior. Due to the high price of scandium, a crucible-melt interaction study was performed to ensure no scandium was lost in graphite, alumina, magnesia, or zirconia crucibles after holding a liquid Al-Sc master alloy for 8 hours at 900 °C in an argon atmosphere. The alloys were subjected to an isochronal aging treatment and tested for conductivity and Vickers microhardness after each increment. For scandium-containing alloys, peak hardnesses of 520-790 MPa, and peak tensile stresses of 138-234 MPa were observed after aging from 150-350 °C for 3 hours in increments of 50 °C, and for alloys without scandium, peak hardnesses of 217-335 MPa and peak tensile stresses of 45-63 MPa were observed after a 3 hour, 150 °C aging treatment. The hardness and tensile strength of the ytterbium containing alloy was found to be lower than in the alloy with no ytterbium substitution."],"dc:identifier":["10.37099/mtu.dc.etds/28","https://digitalcommons.mtu.edu/etds/28"],"dc:subject":["Engineering","Engineering Science and Materials"],"dc:title":["Processing and mechanical properties of cast aluminum containing scandium, zirconium, and ytterbium"],"thesis:degree_discipline":["Department of Materials Science and Engineering"],"thesis:degree_level":["Master's Thesis"],"thesis:degree_name":["Master of Science in Materials Science and Engineering (MS)"]},"updated_at":"2026-11-19T08:14:43Z"}