{"id":{"repo_id":"njit","oai_identifier":"oai:digitalcommons.njit.edu:dissertations-2144"},"canonical_url":"https://search.ndltd.org/etd/njit/oai:digitalcommons.njit.edu:dissertations-2144","repository":{"repo_id":"njit","name":"NJIT","base_url":"https://digitalcommons.njit.edu/do/oai/"},"display":{"title":"Investigation of paraelectric PTL thin films using reactive magnetron sputtering","abstract":"The study of methods to prepare paraelectric perovskite PLT (Pb_{1-x}La_xTi_{1-x/4}O_3; x=0.28) thin films has been important because thin films of this high dielectric strength material are required to make high density capacitors for dynamic random access memory. In this research, paraelectric PLT thin films were prepared on multi-layer (Pt/Ti/SiO_2/Si) and MgO substrates in a unique way by the reactive magnetron sputtering method using a multi-component metal target. The individual control of each metal area on the sputtering target had considerable influence on the stoichiometry and electrical properties of the thin films. The effect of post-deposition annealing on as-deposited amorphous PLT films was studied as a function of temperature in the range of 450 C to 750 C. The interdependent relationship of the composition, crystalline structure and surface morphology in the films was studied as a function of annealing conditions. The chemical composition of the as-deposited and annealed films was measured by Rutherford back-scattering (RBS) and Auger electron spectroscopy (AES). The composition of PLT (28) thin film was: Pb, 0.73; La, 0.28; Ti, 0.88; 0, 2.9. The dielectric constant ([epsilon]r) and dissipation factor (tan [delta]) at low electric field measurement (500 V/cm) of the capacitors with the highest dielectric properties were 1216 and 0.018, respectively. Single crystal film at 650 C were smooth and had the lowest leakage current density, 0.1 uA/cm^2, at the electric field of 0.25 MV/cm. However, the highest dielectric constant, 1216, and the highest charge storage density, 12.5 uC/cm^2, obtained with an annealing temperature of 750 C. The research showed that magnetron sputtering can be used to prepare paraelectric perovskite PLT (28) thin films with high dielectric constant, large charge storage density and relatively low leakage current for capacitor applications in active DRAM cells.","abstract_html":"The study of methods to prepare paraelectric perovskite PLT (Pb_{1-x}La_xTi_{1-x/4}O_3; x=0.28) thin films has been important because thin films of this high dielectric strength material are required to make high density capacitors for dynamic random access memory. In this research, paraelectric PLT thin films were prepared on multi-layer (Pt/Ti/SiO_2/Si) and MgO substrates in a unique way by the reactive magnetron sputtering method using a multi-component metal target. The individual control of each metal area on the sputtering target had considerable influence on the stoichiometry and electrical properties of the thin films. The effect of post-deposition annealing on as-deposited amorphous PLT films was studied as a function of temperature in the range of 450 C to 750 C. The interdependent relationship of the composition, crystalline structure and surface morphology in the films was studied as a function of annealing conditions. The chemical composition of the as-deposited and annealed films was measured by Rutherford back-scattering (RBS) and Auger electron spectroscopy (AES). The composition of PLT (28) thin film was: Pb, 0.73; La, 0.28; Ti, 0.88; 0, 2.9. The dielectric constant ([epsilon]r) and dissipation factor (tan [delta]) at low electric field measurement (500 V/cm) of the capacitors with the highest dielectric properties were 1216 and 0.018, respectively. Single crystal film at 650 C were smooth and had the lowest leakage current density, 0.1 uA/cm^2, at the electric field of 0.25 MV/cm. However, the highest dielectric constant, 1216, and the highest charge storage density, 12.5 uC/cm^2, obtained with an annealing temperature of 750 C. The research showed that magnetron sputtering can be used to prepare paraelectric perovskite PLT (28) thin films with high dielectric constant, large charge storage density and relatively low leakage current for capacitor applications in active DRAM cells.","abstract_has_math":false,"creators":["Kim, Hyun Hoo"],"institution":null,"degree_name":"Doctor of Philosophy in Electrical Engineering - (Ph.D.)","degree_level":null,"degree_discipline":"Electrical and Computer Engineering","degree_department":null,"school":null,"contributors":["Kenneth Sohn","Roy H. Cornely","Haim Grebel"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T08:40:00Z","subjects":["Thin films.","Thin films--Electric properties.","Sputtering (Physics)","Electrical and Electronics"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://digitalcommons.njit.edu/dissertations/1089","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://digitalcommons.njit.edu/dissertations/1089","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digitalcommons.njit.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Adigitalcommons.njit.edu%3Adissertations-2144","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Kenneth Sohn","Roy H. Cornely","Haim Grebel"]},{"key":"dc:creator","label":"Author","values":["Kim, Hyun Hoo"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["1994-05-31T07:00:00Z"]},{"key":"dc:type","label":"Dc Type","values":["Dissertation"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Electrical and Computer Engineering"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Doctor of Philosophy in Electrical Engineering - (Ph.D.)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Thin films.","Thin films--Electric properties.","Sputtering (Physics)","Electrical and Electronics"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digitalcommons.njit.edu/dissertations/1089"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["The study of methods to prepare paraelectric perovskite PLT (Pb_{1-x}La_xTi_{1-x/4}O_3; x=0.28) thin films has been important because thin films of this high dielectric strength material are required to make high density capacitors for dynamic random access memory. In this research, paraelectric PLT thin films were prepared on multi-layer (Pt/Ti/SiO_2/Si) and MgO substrates in a unique way by the reactive magnetron sputtering method using a multi-component metal target. The individual control of each metal area on the sputtering target had considerable influence on the stoichiometry and electrical properties of the thin films. The effect of post-deposition annealing on as-deposited amorphous PLT films was studied as a function of temperature in the range of 450 C to 750 C. The interdependent relationship of the composition, crystalline structure and surface morphology in the films was studied as a function of annealing conditions. The chemical composition of the as-deposited and annealed films was measured by Rutherford back-scattering (RBS) and Auger electron spectroscopy (AES). The composition of PLT (28) thin film was: Pb, 0.73; La, 0.28; Ti, 0.88; 0, 2.9. The dielectric constant ([epsilon]r) and dissipation factor (tan [delta]) at low electric field measurement (500 V/cm) of the capacitors with the highest dielectric properties were 1216 and 0.018, respectively. Single crystal film at 650 C were smooth and had the lowest leakage current density, 0.1 uA/cm^2, at the electric field of 0.25 MV/cm. However, the highest dielectric constant, 1216, and the highest charge storage density, 12.5 uC/cm^2, obtained with an annealing temperature of 750 C. The research showed that magnetron sputtering can be used to prepare paraelectric perovskite PLT (28) thin films with high dielectric constant, large charge storage density and relatively low leakage current for capacitor applications in active DRAM cells."]},{"key":"dc:title","label":"Title","values":["Investigation of paraelectric PTL thin films using reactive magnetron sputtering"]}]}],"canonical_facts":{"dc:contributor":["Kenneth Sohn","Roy H. Cornely","Haim Grebel"],"dc:creator":["Kim, Hyun Hoo"],"dc:date.created":["1994-05-31T07:00:00Z"],"dc:description.abstract":["The study of methods to prepare paraelectric perovskite PLT (Pb_{1-x}La_xTi_{1-x/4}O_3; x=0.28) thin films has been important because thin films of this high dielectric strength material are required to make high density capacitors for dynamic random access memory. In this research, paraelectric PLT thin films were prepared on multi-layer (Pt/Ti/SiO_2/Si) and MgO substrates in a unique way by the reactive magnetron sputtering method using a multi-component metal target. The individual control of each metal area on the sputtering target had considerable influence on the stoichiometry and electrical properties of the thin films. The effect of post-deposition annealing on as-deposited amorphous PLT films was studied as a function of temperature in the range of 450 C to 750 C. The interdependent relationship of the composition, crystalline structure and surface morphology in the films was studied as a function of annealing conditions. The chemical composition of the as-deposited and annealed films was measured by Rutherford back-scattering (RBS) and Auger electron spectroscopy (AES). The composition of PLT (28) thin film was: Pb, 0.73; La, 0.28; Ti, 0.88; 0, 2.9. The dielectric constant ([epsilon]r) and dissipation factor (tan [delta]) at low electric field measurement (500 V/cm) of the capacitors with the highest dielectric properties were 1216 and 0.018, respectively. Single crystal film at 650 C were smooth and had the lowest leakage current density, 0.1 uA/cm^2, at the electric field of 0.25 MV/cm. However, the highest dielectric constant, 1216, and the highest charge storage density, 12.5 uC/cm^2, obtained with an annealing temperature of 750 C. The research showed that magnetron sputtering can be used to prepare paraelectric perovskite PLT (28) thin films with high dielectric constant, large charge storage density and relatively low leakage current for capacitor applications in active DRAM cells."],"dc:identifier":["https://digitalcommons.njit.edu/dissertations/1089"],"dc:subject":["Thin films.","Thin films--Electric properties.","Sputtering (Physics)","Electrical and Electronics"],"dc:title":["Investigation of paraelectric PTL thin films using reactive magnetron sputtering"],"dc:type":["Dissertation"],"thesis:degree_discipline":["Electrical and Computer Engineering"],"thesis:degree_name":["Doctor of Philosophy in Electrical Engineering - (Ph.D.)"]},"updated_at":"2026-11-19T08:40:00Z"}