{"id":{"repo_id":"njit","oai_identifier":"oai:digitalcommons.njit.edu:theses-2048"},"canonical_url":"https://search.ndltd.org/etd/njit/oai:digitalcommons.njit.edu:theses-2048","repository":{"repo_id":"njit","name":"NJIT","base_url":"https://digitalcommons.njit.edu/do/oai/"},"display":{"title":"Synthesis and characterization of phosphosilicate glass films by LPCVD for sensor application","abstract":"This study was dedicated to the synthesis of the thin film materials required to fabricate the waveguide and the reference arm barrier for integrated optical sensor. Phosphosilicate glass (PSG) thin films were synthesized on silicon and quartz wafers by LPCVD using Ditertiarybutylsilane(DTBS), Trimethylphosphite(TMP) and oxygen as precursors. The films were processed at different temperatures between 600 C and 700 C at a constant pressure, and at different flow rate of TMP. The effect of TMP flow rate and deposition temperature on deposition parameters and the properties of PSG films were investigated. The films deposited were uniform, amorphous, low stress and the composition of the films varied with deposition temperature and TMP flow rate. The deposition rate increased with increasing TMP flow rate and had a maximum of deposition rate at 650 C. It was suggested that the addition of TMP catalyzes the deposition. Refractive index increased with increasing deposition temperature and phosphorus concentration. A less transparent film at higher temperatures also suggested presence of carbon at higher temperatures, This may be due to a possible decomposition reaction of TMP or DTBS. The PSG films showed around 100% transparency when deposited at 650 C.","abstract_html":"This study was dedicated to the synthesis of the thin film materials required to fabricate the waveguide and the reference arm barrier for integrated optical sensor. Phosphosilicate glass (PSG) thin films were synthesized on silicon and quartz wafers by LPCVD using Ditertiarybutylsilane(DTBS), Trimethylphosphite(TMP) and oxygen as precursors. The films were processed at different temperatures between 600 C and 700 C at a constant pressure, and at different flow rate of TMP. The effect of TMP flow rate and deposition temperature on deposition parameters and the properties of PSG films were investigated. The films deposited were uniform, amorphous, low stress and the composition of the films varied with deposition temperature and TMP flow rate. The deposition rate increased with increasing TMP flow rate and had a maximum of deposition rate at 650 C. It was suggested that the addition of TMP catalyzes the deposition. Refractive index increased with increasing deposition temperature and phosphorus concentration. A less transparent film at higher temperatures also suggested presence of carbon at higher temperatures, This may be due to a possible decomposition reaction of TMP or DTBS. The PSG films showed around 100% transparency when deposited at 650 C.","abstract_has_math":false,"creators":["Wu, Hui"],"institution":null,"degree_name":"Master of Science in Materials Science and Engineering - (M.S.)","degree_level":null,"degree_discipline":"Committee for the Interdisciplinary Program in Materials Science and Engineering","degree_department":null,"school":null,"contributors":["Roland A. Levy","John Francis Federici","Lev N. Krasnoperov"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T08:40:28Z","subjects":["Silicon-carbide thin films.","Silicon-carbide thin films--Effect of temperature on.","Materials Science and Engineering"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://digitalcommons.njit.edu/theses/1049","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://digitalcommons.njit.edu/theses/1049","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digitalcommons.njit.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Adigitalcommons.njit.edu%3Atheses-2048","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Roland A. Levy","John Francis Federici","Lev N. Krasnoperov"]},{"key":"dc:creator","label":"Author","values":["Wu, Hui"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["1997-10-31T08:00:00Z"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Committee for the Interdisciplinary Program in Materials Science and Engineering"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science in Materials Science and Engineering - (M.S.)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Silicon-carbide thin films.","Silicon-carbide thin films--Effect of temperature on.","Materials Science and Engineering"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digitalcommons.njit.edu/theses/1049"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["This study was dedicated to the synthesis of the thin film materials required to fabricate the waveguide and the reference arm barrier for integrated optical sensor. Phosphosilicate glass (PSG) thin films were synthesized on silicon and quartz wafers by LPCVD using Ditertiarybutylsilane(DTBS), Trimethylphosphite(TMP) and oxygen as precursors. The films were processed at different temperatures between 600 C and 700 C at a constant pressure, and at different flow rate of TMP. The effect of TMP flow rate and deposition temperature on deposition parameters and the properties of PSG films were investigated. The films deposited were uniform, amorphous, low stress and the composition of the films varied with deposition temperature and TMP flow rate. The deposition rate increased with increasing TMP flow rate and had a maximum of deposition rate at 650 C. It was suggested that the addition of TMP catalyzes the deposition. Refractive index increased with increasing deposition temperature and phosphorus concentration. A less transparent film at higher temperatures also suggested presence of carbon at higher temperatures, This may be due to a possible decomposition reaction of TMP or DTBS. The PSG films showed around 100% transparency when deposited at 650 C."]},{"key":"dc:title","label":"Title","values":["Synthesis and characterization of phosphosilicate glass films by LPCVD for sensor application"]}]}],"canonical_facts":{"dc:contributor":["Roland A. Levy","John Francis Federici","Lev N. Krasnoperov"],"dc:creator":["Wu, Hui"],"dc:date.created":["1997-10-31T08:00:00Z"],"dc:description.abstract":["This study was dedicated to the synthesis of the thin film materials required to fabricate the waveguide and the reference arm barrier for integrated optical sensor. Phosphosilicate glass (PSG) thin films were synthesized on silicon and quartz wafers by LPCVD using Ditertiarybutylsilane(DTBS), Trimethylphosphite(TMP) and oxygen as precursors. The films were processed at different temperatures between 600 C and 700 C at a constant pressure, and at different flow rate of TMP. The effect of TMP flow rate and deposition temperature on deposition parameters and the properties of PSG films were investigated. The films deposited were uniform, amorphous, low stress and the composition of the films varied with deposition temperature and TMP flow rate. The deposition rate increased with increasing TMP flow rate and had a maximum of deposition rate at 650 C. It was suggested that the addition of TMP catalyzes the deposition. Refractive index increased with increasing deposition temperature and phosphorus concentration. A less transparent film at higher temperatures also suggested presence of carbon at higher temperatures, This may be due to a possible decomposition reaction of TMP or DTBS. The PSG films showed around 100% transparency when deposited at 650 C."],"dc:identifier":["https://digitalcommons.njit.edu/theses/1049"],"dc:subject":["Silicon-carbide thin films.","Silicon-carbide thin films--Effect of temperature on.","Materials Science and Engineering"],"dc:title":["Synthesis and characterization of phosphosilicate glass films by LPCVD for sensor application"],"dc:type":["Thesis"],"thesis:degree_discipline":["Committee for the Interdisciplinary Program in Materials Science and Engineering"],"thesis:degree_name":["Master of Science in Materials Science and Engineering - (M.S.)"]},"updated_at":"2026-11-19T08:40:28Z"}