{"id":{"repo_id":"njit","oai_identifier":"oai:digitalcommons.njit.edu:theses-2123"},"canonical_url":"https://search.ndltd.org/etd/njit/oai:digitalcommons.njit.edu:theses-2123","repository":{"repo_id":"njit","name":"NJIT","base_url":"https://digitalcommons.njit.edu/do/oai/"},"display":{"title":"Residual stress analysis of sputtered Tantalum Silicide thin film","abstract":"The influence of different argon pressures on the residual stress, microstructure, and resisitivity of sputtered tantalum silicide thin films has been investigated. TaSi_2 films were deposited onto Si wafers by dc magnetron sputtering. The deposition temperature was assumed to be 300 C. The thickness was about 0.5 um. The residual stresses in the films deposited at different argon pressures were determined by curvature measurement method. The compressive intrinsic stress of 1033.4MPa was measured at P_{Ar} = 0.5 mTorr. The intrinsic stress in the films seemed to change from compression to tension as P_{Ar} increased above 8mTorr. A maximum tensile intrinsic stress of 221MPa was obtained at 10 mTon and the tensile intrinsic stress decreased at the higher argon pressure. SEM showed an accompanying microstructural change from a dense structure at the low pressures to an open growth structure with some gaps between grains at the highest pressure. The electrical resistivity exhibited a sputtering-pressure dependence and seemed to be closely related to the microstructure of films.","abstract_html":"The influence of different argon pressures on the residual stress, microstructure, and resisitivity of sputtered tantalum silicide thin films has been investigated. TaSi_2 films were deposited onto Si wafers by dc magnetron sputtering. The deposition temperature was assumed to be 300 C. The thickness was about 0.5 um. The residual stresses in the films deposited at different argon pressures were determined by curvature measurement method. The compressive intrinsic stress of 1033.4MPa was measured at P_{Ar} = 0.5 mTorr. The intrinsic stress in the films seemed to change from compression to tension as P_{Ar} increased above 8mTorr. A maximum tensile intrinsic stress of 221MPa was obtained at 10 mTon and the tensile intrinsic stress decreased at the higher argon pressure. SEM showed an accompanying microstructural change from a dense structure at the low pressures to an open growth structure with some gaps between grains at the highest pressure. The electrical resistivity exhibited a sputtering-pressure dependence and seemed to be closely related to the microstructure of films.","abstract_has_math":false,"creators":["Song, Young Joo"],"institution":null,"degree_name":"Master of Science in Electrical Engineering - (M.S.)","degree_level":null,"degree_discipline":"Electrical Engineering","degree_department":null,"school":null,"contributors":["Kenneth Sohn","Roy H. Cornely","Robert Boris Marcus"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T08:40:35Z","subjects":["Silicides.","Tantalum films.","Electrical and Electronics"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://digitalcommons.njit.edu/theses/1124","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://digitalcommons.njit.edu/theses/1124","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digitalcommons.njit.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Adigitalcommons.njit.edu%3Atheses-2123","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Kenneth Sohn","Roy H. Cornely","Robert Boris Marcus"]},{"key":"dc:creator","label":"Author","values":["Song, Young Joo"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["1996-10-31T08:00:00Z"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Electrical Engineering"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science in Electrical Engineering - (M.S.)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Silicides.","Tantalum films.","Electrical and Electronics"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digitalcommons.njit.edu/theses/1124"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["The influence of different argon pressures on the residual stress, microstructure, and resisitivity of sputtered tantalum silicide thin films has been investigated. TaSi_2 films were deposited onto Si wafers by dc magnetron sputtering. The deposition temperature was assumed to be 300 C. The thickness was about 0.5 um. The residual stresses in the films deposited at different argon pressures were determined by curvature measurement method. The compressive intrinsic stress of 1033.4MPa was measured at P_{Ar} = 0.5 mTorr. The intrinsic stress in the films seemed to change from compression to tension as P_{Ar} increased above 8mTorr. A maximum tensile intrinsic stress of 221MPa was obtained at 10 mTon and the tensile intrinsic stress decreased at the higher argon pressure. SEM showed an accompanying microstructural change from a dense structure at the low pressures to an open growth structure with some gaps between grains at the highest pressure. The electrical resistivity exhibited a sputtering-pressure dependence and seemed to be closely related to the microstructure of films."]},{"key":"dc:title","label":"Title","values":["Residual stress analysis of sputtered Tantalum Silicide thin film"]}]}],"canonical_facts":{"dc:contributor":["Kenneth Sohn","Roy H. Cornely","Robert Boris Marcus"],"dc:creator":["Song, Young Joo"],"dc:date.created":["1996-10-31T08:00:00Z"],"dc:description.abstract":["The influence of different argon pressures on the residual stress, microstructure, and resisitivity of sputtered tantalum silicide thin films has been investigated. TaSi_2 films were deposited onto Si wafers by dc magnetron sputtering. The deposition temperature was assumed to be 300 C. The thickness was about 0.5 um. The residual stresses in the films deposited at different argon pressures were determined by curvature measurement method. The compressive intrinsic stress of 1033.4MPa was measured at P_{Ar} = 0.5 mTorr. The intrinsic stress in the films seemed to change from compression to tension as P_{Ar} increased above 8mTorr. A maximum tensile intrinsic stress of 221MPa was obtained at 10 mTon and the tensile intrinsic stress decreased at the higher argon pressure. SEM showed an accompanying microstructural change from a dense structure at the low pressures to an open growth structure with some gaps between grains at the highest pressure. The electrical resistivity exhibited a sputtering-pressure dependence and seemed to be closely related to the microstructure of films."],"dc:identifier":["https://digitalcommons.njit.edu/theses/1124"],"dc:subject":["Silicides.","Tantalum films.","Electrical and Electronics"],"dc:title":["Residual stress analysis of sputtered Tantalum Silicide thin film"],"dc:type":["Thesis"],"thesis:degree_discipline":["Electrical Engineering"],"thesis:degree_name":["Master of Science in Electrical Engineering - (M.S.)"]},"updated_at":"2026-11-19T08:40:35Z"}