{"id":{"repo_id":"nps","oai_identifier":"oai:calhoun.nps.edu:10945/12089"},"canonical_url":"https://search.ndltd.org/etd/nps/oai:calhoun.nps.edu:10945/12089","repository":{"repo_id":"nps","name":"Naval Postgraduate School","base_url":"https://calhoun.nps.edu/server/oai/request"},"display":{"title":"Electrical resistivity and Hall effect of cuprous sulfide and bismuth telluride in the temperature range from 290K to 670K.","abstract":"An instrumentation and experimental technique for the measurements of electrical resistivity and the Hall effect at elevated temperatures is described. These two temperature-dependent properties are uniquely determined for non-isothermal conditions and thereby are evaluations at computed average temperatures within the specimens. The results of this investigation of cuprous sulfide and bismuth telluride in the temperature range from 290°K to 670°K are presented and compared with known published data. Resistivities are determined from measurements of potential differences between selected points along the current path through the specimens, while Hall effects are presented in terms of the Hall coefficient, R(H⁹), evaluated by Hall's equation, V(h)=R(h)IH/d. Both cuprous sulfide and bismuth telluride show resistivities on the order of 10ˉ³ ohm centimeters, characteristic of semiconductor materials, while the Hall coefficient for cuprous sulfide is established at values less than 0.179 cubic centimeters per coulomb, and the Hall coefficient for bismuth telluride decreases continuously with increasing temperature from about 0.5 cubic centimeters per coulomb. The instrumentation and investigation was conducted at the U.S. Naval Postgraduate School, Monterey, California, during the winter and spring of 1961.","abstract_html":"An instrumentation and experimental technique for the measurements of electrical resistivity and the Hall effect at elevated temperatures is described. These two temperature-dependent properties are uniquely determined for non-isothermal conditions and thereby are evaluations at computed average temperatures within the specimens. The results of this investigation of cuprous sulfide and bismuth telluride in the temperature range from 290°K to 670°K are presented and compared with known published data. Resistivities are determined from measurements of potential differences between selected points along the current path through the specimens, while Hall effects are presented in terms of the Hall coefficient, R(H⁹), evaluated by Hall&#x27;s equation, V(h)=R(h)IH/d. Both cuprous sulfide and bismuth telluride show resistivities on the order of 10ˉ³ ohm centimeters, characteristic of semiconductor materials, while the Hall coefficient for cuprous sulfide is established at values less than 0.179 cubic centimeters per coulomb, and the Hall coefficient for bismuth telluride decreases continuously with increasing temperature from about 0.5 cubic centimeters per coulomb. The instrumentation and investigation was conducted at the U.S. Naval Postgraduate School, Monterey, California, during the winter and spring of 1961.","abstract_has_math":false,"creators":["Erickson, Philip W."],"institution":"Monterey, California: U.S. Naval Postgraduate School","degree_name":"M.S. in Mechanical Engineering","degree_level":"Masters","degree_discipline":"Mechanical Engineering","degree_department":"Mechanical Engineering","school":null,"contributors":[],"advisors":["Pucci, Paul"],"committee_chairs":[],"committee_members":[],"year":1961,"date_issued":"1961","date_published":"1961","updated_at":"2026-11-21T23:44:27Z","subjects":["Electronics"],"languages":[],"rights":["This publication is a work of the U.S. Government as defined in Title 17, United States Code, Section 101. Copyright protection is not available for this work in the United States.","Approved for public release; distribution is unlimited."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/10945/12089","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/10945/12089","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Anps%3Aoai%3Acalhoun.nps.edu%3A10945%2F12089","prefix":"oai_dc"},"source_record":{"url":"https://calhoun.nps.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Acalhoun.nps.edu%3A10945%2F12089","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Pucci, Paul"]},{"key":"dc:contributor.department","label":"Department","values":["Mechanical Engineering"]},{"key":"dc:contributor.other","label":"Dc Contributor Other","values":["Naval Postgraduate School (U.S.)"]},{"key":"dc:creator","label":"Author","values":["Erickson, Philip W."]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["1961"]},{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2012-08-29T23:31:00Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2012-08-29T23:31:00Z"]},{"key":"dc:date.issued","label":"Date","values":["1961"]},{"key":"dc:publisher","label":"Institution","values":["Monterey, California: U.S. Naval Postgraduate School"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Mechanical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Masters"]},{"key":"thesis:degree_name","label":"Degree Name","values":["M.S. in Mechanical Engineering"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["Naval Postgraduate School"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject.lcsh","label":"Dc Subject Lcsh","values":["Electronics"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:rights","label":"Dc Rights","values":["This publication is a work of the U.S. Government as defined in Title 17, United States Code, Section 101. Copyright protection is not available for this work in the United States.","Approved for public release; distribution is unlimited."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/10945/12089"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["An instrumentation and experimental technique for the measurements of electrical resistivity and the Hall effect at elevated temperatures is described. These two temperature-dependent properties are uniquely determined for non-isothermal conditions and thereby are evaluations at computed average temperatures within the specimens. The results of this investigation of cuprous sulfide and bismuth telluride in the temperature range from 290°K to 670°K are presented and compared with known published data. Resistivities are determined from measurements of potential differences between selected points along the current path through the specimens, while Hall effects are presented in terms of the Hall coefficient, R(H⁹), evaluated by Hall's equation, V(h)=R(h)IH/d. Both cuprous sulfide and bismuth telluride show resistivities on the order of 10ˉ³ ohm centimeters, characteristic of semiconductor materials, while the Hall coefficient for cuprous sulfide is established at values less than 0.179 cubic centimeters per coulomb, and the Hall coefficient for bismuth telluride decreases continuously with increasing temperature from about 0.5 cubic centimeters per coulomb. The instrumentation and investigation was conducted at the U.S. Naval Postgraduate School, Monterey, California, during the winter and spring of 1961."]},{"key":"dc:description.uri","label":"Dc Description URI","values":["http://archive.org/details/electricalresist1094512089"]},{"key":"dc:title","label":"Title","values":["Electrical resistivity and Hall effect of cuprous sulfide and bismuth telluride in the temperature range from 290K to 670K."]},{"key":"dspace:entity.type","label":"Dspace Entity Type","values":["Publication"]},{"key":"local:contributor.affiliation","label":"Local Contributor Affiliation","values":["U.S. Navy (U.S.N.) author.","Lieutenant Commander, United States Navy"]}]}],"canonical_facts":{"dc:contributor.advisor":["Pucci, Paul"],"dc:contributor.department":["Mechanical Engineering"],"dc:contributor.other":["Naval Postgraduate School (U.S.)"],"dc:creator":["Erickson, Philip W."],"dc:date":["1961"],"dc:date.accessioned":["2012-08-29T23:31:00Z"],"dc:date.available":["2012-08-29T23:31:00Z"],"dc:date.issued":["1961"],"dc:description.abstract":["An instrumentation and experimental technique for the measurements of electrical resistivity and the Hall effect at elevated temperatures is described. These two temperature-dependent properties are uniquely determined for non-isothermal conditions and thereby are evaluations at computed average temperatures within the specimens. The results of this investigation of cuprous sulfide and bismuth telluride in the temperature range from 290°K to 670°K are presented and compared with known published data. Resistivities are determined from measurements of potential differences between selected points along the current path through the specimens, while Hall effects are presented in terms of the Hall coefficient, R(H⁹), evaluated by Hall's equation, V(h)=R(h)IH/d. Both cuprous sulfide and bismuth telluride show resistivities on the order of 10ˉ³ ohm centimeters, characteristic of semiconductor materials, while the Hall coefficient for cuprous sulfide is established at values less than 0.179 cubic centimeters per coulomb, and the Hall coefficient for bismuth telluride decreases continuously with increasing temperature from about 0.5 cubic centimeters per coulomb. The instrumentation and investigation was conducted at the U.S. Naval Postgraduate School, Monterey, California, during the winter and spring of 1961."],"dc:description.uri":["http://archive.org/details/electricalresist1094512089"],"dc:identifier.uri":["https://hdl.handle.net/10945/12089"],"dc:publisher":["Monterey, California: U.S. Naval Postgraduate School"],"dc:rights":["This publication is a work of the U.S. Government as defined in Title 17, United States Code, Section 101. Copyright protection is not available for this work in the United States.","Approved for public release; distribution is unlimited."],"dc:subject.lcsh":["Electronics"],"dc:title":["Electrical resistivity and Hall effect of cuprous sulfide and bismuth telluride in the temperature range from 290K to 670K."],"dc:type":["Thesis"],"dspace:entity.type":["Publication"],"local:contributor.affiliation":["U.S. Navy (U.S.N.) author.","Lieutenant Commander, United States Navy"],"thesis:degree_discipline":["Mechanical Engineering"],"thesis:degree_level":["Masters"],"thesis:degree_name":["M.S. in Mechanical Engineering"],"thesis:institution_name":["Naval Postgraduate School"]},"updated_at":"2026-11-21T23:44:27Z"}