{"id":{"repo_id":"nps","oai_identifier":"oai:calhoun.nps.edu:10945/3120"},"canonical_url":"https://search.ndltd.org/etd/nps/oai:calhoun.nps.edu:10945/3120","repository":{"repo_id":"nps","name":"Naval Postgraduate School","base_url":"https://calhoun.nps.edu/server/oai/request"},"display":{"title":"The \"Lazy S\" feature in Friction Stir Welding of AA2099 Aluminum-Lithium alloy","abstract":"The addition of Lithium to Aluminum-Lithium (Al-Li) alloys results in reduced density as well as increased stiffness and strength, and so these materials are attractive for selected aerospace structures. Friction Stir Welding (FSW) of Al-Li alloys may provide high join efficiency in such structures but potential FSW defects must be understood. This thesis examines the occurrence of the \"Lazy S\" feature, which may be a defect. Welds were made after various treatments of the faying surfaces and with different FSW procedures. These welds were examined and their microstructures were characterized by optical microscopy and orientation imaging microscopy. Microhardness data were acquired as well. The Lazy S feature arises as the faying surfaces are deformed and spread out during FSW. Inadequate bonding along these surfaces will constitute a weld defect.","abstract_html":"The addition of Lithium to Aluminum-Lithium (Al-Li) alloys results in reduced density as well as increased stiffness and strength, and so these materials are attractive for selected aerospace structures. Friction Stir Welding (FSW) of Al-Li alloys may provide high join efficiency in such structures but potential FSW defects must be understood. This thesis examines the occurrence of the &quot;Lazy S&quot; feature, which may be a defect. Welds were made after various treatments of the faying surfaces and with different FSW procedures. These welds were examined and their microstructures were characterized by optical microscopy and orientation imaging microscopy. Microhardness data were acquired as well. The Lazy S feature arises as the faying surfaces are deformed and spread out during FSW. Inadequate bonding along these surfaces will constitute a weld defect.","abstract_has_math":false,"creators":["Klages, Holli K."],"institution":"Monterey, California. Naval Postgraduate School","degree_name":"M.S.","degree_level":"Masters","degree_discipline":"Mechanical Engineering","degree_department":null,"school":null,"contributors":[],"advisors":["McNelley, Terry"],"committee_chairs":[],"committee_members":[],"year":2007,"date_issued":"2007-12","date_published":"2007-12","updated_at":"2026-11-19T06:32:39Z","subjects":["Mechanical engineering","Lithium alloys","Microstructure"],"languages":[],"rights":["Approved for public release; distribution is unlimited."],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier.oclc","label":"OCLC","values":["191091968"],"render_values":[{"text":"191091968","href":null,"code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/10945/3120","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/10945/3120","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Anps%3Aoai%3Acalhoun.nps.edu%3A10945%2F3120","prefix":"oai_dc"},"source_record":{"url":"https://calhoun.nps.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Acalhoun.nps.edu%3A10945%2F3120","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["McNelley, Terry"]},{"key":"dc:contributor.other","label":"Dc Contributor Other","values":["Naval Postgraduate School (U.S.)"]},{"key":"dc:creator","label":"Author","values":["Klages, Holli K."]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2012-03-14T17:37:22Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2012-03-14T17:37:22Z"]},{"key":"dc:date.issued","label":"Date","values":["2007-12"]},{"key":"dc:publisher","label":"Institution","values":["Monterey, California. Naval Postgraduate School"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Mechanical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Masters"]},{"key":"thesis:degree_name","label":"Degree Name","values":["M.S."]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["Naval Postgraduate School"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject.lcsh","label":"Dc Subject Lcsh","values":["Mechanical engineering","Lithium alloys","Microstructure"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:rights","label":"Dc Rights","values":["Approved for public release; distribution is unlimited."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.oclc","label":"OCLC","values":["191091968"]},{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/10945/3120"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["The addition of Lithium to Aluminum-Lithium (Al-Li) alloys results in reduced density as well as increased stiffness and strength, and so these materials are attractive for selected aerospace structures. Friction Stir Welding (FSW) of Al-Li alloys may provide high join efficiency in such structures but potential FSW defects must be understood. This thesis examines the occurrence of the \"Lazy S\" feature, which may be a defect. Welds were made after various treatments of the faying surfaces and with different FSW procedures. These welds were examined and their microstructures were characterized by optical microscopy and orientation imaging microscopy. Microhardness data were acquired as well. The Lazy S feature arises as the faying surfaces are deformed and spread out during FSW. Inadequate bonding along these surfaces will constitute a weld defect."]},{"key":"dc:description.uri","label":"Dc Description URI","values":["http://archive.org/details/thelazysfeaturei109453120"]},{"key":"dc:format.extent","label":"Dc Format Extent","values":["xiv, 47 p. : col. ill. ;"]},{"key":"dc:title","label":"Title","values":["The \"Lazy S\" feature in Friction Stir Welding of AA2099 Aluminum-Lithium alloy"]},{"key":"dspace:entity.type","label":"Dspace Entity Type","values":["Publication"]},{"key":"local:contributor.affiliation","label":"Local Contributor Affiliation","values":["US Navy (USN) author."]},{"key":"local:etd.verified","label":"Local Etd Verified","values":["no"]}]}],"canonical_facts":{"dc:contributor.advisor":["McNelley, Terry"],"dc:contributor.other":["Naval Postgraduate School (U.S.)"],"dc:creator":["Klages, Holli K."],"dc:date.accessioned":["2012-03-14T17:37:22Z"],"dc:date.available":["2012-03-14T17:37:22Z"],"dc:date.issued":["2007-12"],"dc:description.abstract":["The addition of Lithium to Aluminum-Lithium (Al-Li) alloys results in reduced density as well as increased stiffness and strength, and so these materials are attractive for selected aerospace structures. Friction Stir Welding (FSW) of Al-Li alloys may provide high join efficiency in such structures but potential FSW defects must be understood. This thesis examines the occurrence of the \"Lazy S\" feature, which may be a defect. Welds were made after various treatments of the faying surfaces and with different FSW procedures. These welds were examined and their microstructures were characterized by optical microscopy and orientation imaging microscopy. Microhardness data were acquired as well. The Lazy S feature arises as the faying surfaces are deformed and spread out during FSW. Inadequate bonding along these surfaces will constitute a weld defect."],"dc:description.uri":["http://archive.org/details/thelazysfeaturei109453120"],"dc:format.extent":["xiv, 47 p. : col. ill. ;"],"dc:identifier.oclc":["191091968"],"dc:identifier.uri":["https://hdl.handle.net/10945/3120"],"dc:publisher":["Monterey, California. Naval Postgraduate School"],"dc:rights":["Approved for public release; distribution is unlimited."],"dc:subject.lcsh":["Mechanical engineering","Lithium alloys","Microstructure"],"dc:title":["The \"Lazy S\" feature in Friction Stir Welding of AA2099 Aluminum-Lithium alloy"],"dc:type":["Thesis"],"dspace:entity.type":["Publication"],"local:contributor.affiliation":["US Navy (USN) author."],"local:etd.verified":["no"],"thesis:degree_discipline":["Mechanical Engineering"],"thesis:degree_level":["Masters"],"thesis:degree_name":["M.S."],"thesis:institution_name":["Naval Postgraduate School"]},"updated_at":"2026-11-19T06:32:39Z"}