{"id":{"repo_id":"ohiolink","oai_identifier":"oai:etd.ohiolink.edu:akron1398093214"},"canonical_url":"https://search.ndltd.org/etd/ohiolink/oai:etd.ohiolink.edu:akron1398093214","repository":{"repo_id":"ohiolink","name":"OhioLINK","base_url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai"},"display":{"title":"In Situ Infrared Studies of Photooxidation of Ethanol and Bacteria on TiO2-Based Catalysts","abstract":"TiO<sub>2</sub> is modified to Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> to test two hypotheses: i) Fe-doped TiO<sub>2</sub> can enhance photocatalytic activity under visible light due to the adsorption of visible light and ii) external layer of TiO<sub>2</sub> on Fe-doped TiO<sub>2</sub> can enhance photocatalytic activity of catalyst by providing more active sites. Photocatalytic activity of catalysts was characterized by the rate of ethanol photooxidation. The results showed that Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> have adsorption on visible light range, but do not have visible light photoactivity. This could be explained by that Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> do not have enough rutile crystal structure. In addition, external layer on ALD Fe-doped TiO<sub>2</sub> does not enhance photocatalytic activity. It can be explained by remaining organic compound on the surface of ALD Fe-doped TiO<sub>2</sub> block some active sites. Sol-gel TiO<sub>2</sub> and anatase are used to test two hypotheses: i) morphology of catalyst has effect on bacteria degradation and ii) water can facilitate the bacteria degradation on sol-gel TiO<sub>2</sub>. The results showed bacteria degradation on sol-gel TiO<sub>2</sub> is faster than that on anatase, which validated the first hypothesis. It can be explained by that sol-gel TiO<sub>2</sub> (rhombus-shaped TiO<sub>2</sub> with small particle size) has more effective contact surface with bacteria than anatase (sphere-shaped TiO<sub>2</sub> with big particle size). In addition, the presence of water can increase the degradation rate of bacteria, which validated the second hypothesis. Holes produced from UV illumination can react with H2O to produce &#x2022;OH, and more &#x2022;OH can facilitate the degradation of bacteria. In-situ diffuse reflectance infrared fourier transform (DRIFT) infrared spectroscopy is the main characterization method in this study to monitor the photooxidation of ethanol and degradation of bacteria. Peak height change was used as quantitative indicator of photooxidation and degradation.","abstract_html":"TiO&lt;sub&gt;2&lt;/sub&gt; is modified to Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; and ALD Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; to test two hypotheses: i) Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; can enhance photocatalytic activity under visible light due to the adsorption of visible light and ii) external layer of TiO&lt;sub&gt;2&lt;/sub&gt; on Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; can enhance photocatalytic activity of catalyst by providing more active sites. Photocatalytic activity of catalysts was characterized by the rate of ethanol photooxidation. The results showed that Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; and ALD Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; have adsorption on visible light range, but do not have visible light photoactivity. This could be explained by that Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; and ALD Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; do not have enough rutile crystal structure. In addition, external layer on ALD Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; does not enhance photocatalytic activity. It can be explained by remaining organic compound on the surface of ALD Fe-doped TiO&lt;sub&gt;2&lt;/sub&gt; block some active sites. Sol-gel TiO&lt;sub&gt;2&lt;/sub&gt; and anatase are used to test two hypotheses: i) morphology of catalyst has effect on bacteria degradation and ii) water can facilitate the bacteria degradation on sol-gel TiO&lt;sub&gt;2&lt;/sub&gt;. The results showed bacteria degradation on sol-gel TiO&lt;sub&gt;2&lt;/sub&gt; is faster than that on anatase, which validated the first hypothesis. It can be explained by that sol-gel TiO&lt;sub&gt;2&lt;/sub&gt; (rhombus-shaped TiO&lt;sub&gt;2&lt;/sub&gt; with small particle size) has more effective contact surface with bacteria than anatase (sphere-shaped TiO&lt;sub&gt;2&lt;/sub&gt; with big particle size). In addition, the presence of water can increase the degradation rate of bacteria, which validated the second hypothesis. Holes produced from UV illumination can react with H2O to produce &amp;#x2022;OH, and more &amp;#x2022;OH can facilitate the degradation of bacteria. In-situ diffuse reflectance infrared fourier transform (DRIFT) infrared spectroscopy is the main characterization method in this study to monitor the photooxidation of ethanol and degradation of bacteria. Peak height change was used as quantitative indicator of photooxidation and degradation.","abstract_has_math":false,"creators":["Huang, Dan"],"institution":"University of Akron","degree_name":"Master of Science","degree_level":"masters","degree_discipline":"Polymer Science","degree_department":null,"school":null,"contributors":[],"advisors":["Chuang, Steven"],"committee_chairs":[],"committee_members":[],"year":2014,"date_issued":"2014-05-16","date_published":"2014-05-16","updated_at":"2026-11-27T04:39:37Z","subjects":["Chemical Engineering","Chemistry","Polymer Chemistry","Polymers"],"languages":["English"],"rights":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://rave.ohiolink.edu/etdc/view?acc_num=akron1398093214","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"http://rave.ohiolink.edu/etdc/view?acc_num=akron1398093214","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aohiolink%3Aoai%3Aetd.ohiolink.edu%3Aakron1398093214","prefix":"oai_dc"},"source_record":{"url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Aetd.ohiolink.edu%3Aakron1398093214","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Chuang, Steven"]},{"key":"dc:creator","label":"Author","values":["Huang, Dan"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2014-05-16"]},{"key":"dc:publisher","label":"Institution","values":["University of Akron / OhioLINK"]},{"key":"dc:type","label":"Dc Type","values":["Electronic Thesis or Dissertation"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Polymer Science"]},{"key":"thesis:degree_level","label":"Degree Level","values":["masters"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of Akron"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Chemical Engineering","Chemistry","Polymer Chemistry","Polymers"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:rights","label":"Dc Rights","values":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://rave.ohiolink.edu/etdc/view?acc_num=akron1398093214"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["TiO<sub>2</sub> is modified to Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> to test two hypotheses: i) Fe-doped TiO<sub>2</sub> can enhance photocatalytic activity under visible light due to the adsorption of visible light and ii) external layer of TiO<sub>2</sub> on Fe-doped TiO<sub>2</sub> can enhance photocatalytic activity of catalyst by providing more active sites. Photocatalytic activity of catalysts was characterized by the rate of ethanol photooxidation. The results showed that Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> have adsorption on visible light range, but do not have visible light photoactivity. This could be explained by that Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> do not have enough rutile crystal structure. In addition, external layer on ALD Fe-doped TiO<sub>2</sub> does not enhance photocatalytic activity. It can be explained by remaining organic compound on the surface of ALD Fe-doped TiO<sub>2</sub> block some active sites. Sol-gel TiO<sub>2</sub> and anatase are used to test two hypotheses: i) morphology of catalyst has effect on bacteria degradation and ii) water can facilitate the bacteria degradation on sol-gel TiO<sub>2</sub>. The results showed bacteria degradation on sol-gel TiO<sub>2</sub> is faster than that on anatase, which validated the first hypothesis. It can be explained by that sol-gel TiO<sub>2</sub> (rhombus-shaped TiO<sub>2</sub> with small particle size) has more effective contact surface with bacteria than anatase (sphere-shaped TiO<sub>2</sub> with big particle size). In addition, the presence of water can increase the degradation rate of bacteria, which validated the second hypothesis. Holes produced from UV illumination can react with H2O to produce &#x2022;OH, and more &#x2022;OH can facilitate the degradation of bacteria. In-situ diffuse reflectance infrared fourier transform (DRIFT) infrared spectroscopy is the main characterization method in this study to monitor the photooxidation of ethanol and degradation of bacteria. Peak height change was used as quantitative indicator of photooxidation and degradation."]},{"key":"dc:format","label":"Dc Format","values":["application/pdf","p.83","1.7 MB"]},{"key":"dc:title","label":"Title","values":["In Situ Infrared Studies of Photooxidation of Ethanol and Bacteria on TiO2-Based Catalysts"]}]}],"canonical_facts":{"dc:contributor.advisor":["Chuang, Steven"],"dc:creator":["Huang, Dan"],"dc:date":["2014-05-16"],"dc:description":["TiO<sub>2</sub> is modified to Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> to test two hypotheses: i) Fe-doped TiO<sub>2</sub> can enhance photocatalytic activity under visible light due to the adsorption of visible light and ii) external layer of TiO<sub>2</sub> on Fe-doped TiO<sub>2</sub> can enhance photocatalytic activity of catalyst by providing more active sites. Photocatalytic activity of catalysts was characterized by the rate of ethanol photooxidation. The results showed that Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> have adsorption on visible light range, but do not have visible light photoactivity. This could be explained by that Fe-doped TiO<sub>2</sub> and ALD Fe-doped TiO<sub>2</sub> do not have enough rutile crystal structure. In addition, external layer on ALD Fe-doped TiO<sub>2</sub> does not enhance photocatalytic activity. It can be explained by remaining organic compound on the surface of ALD Fe-doped TiO<sub>2</sub> block some active sites. Sol-gel TiO<sub>2</sub> and anatase are used to test two hypotheses: i) morphology of catalyst has effect on bacteria degradation and ii) water can facilitate the bacteria degradation on sol-gel TiO<sub>2</sub>. The results showed bacteria degradation on sol-gel TiO<sub>2</sub> is faster than that on anatase, which validated the first hypothesis. It can be explained by that sol-gel TiO<sub>2</sub> (rhombus-shaped TiO<sub>2</sub> with small particle size) has more effective contact surface with bacteria than anatase (sphere-shaped TiO<sub>2</sub> with big particle size). In addition, the presence of water can increase the degradation rate of bacteria, which validated the second hypothesis. Holes produced from UV illumination can react with H2O to produce &#x2022;OH, and more &#x2022;OH can facilitate the degradation of bacteria. In-situ diffuse reflectance infrared fourier transform (DRIFT) infrared spectroscopy is the main characterization method in this study to monitor the photooxidation of ethanol and degradation of bacteria. Peak height change was used as quantitative indicator of photooxidation and degradation."],"dc:format":["application/pdf","p.83","1.7 MB"],"dc:identifier":["http://rave.ohiolink.edu/etdc/view?acc_num=akron1398093214"],"dc:language":["English"],"dc:publisher":["University of Akron / OhioLINK"],"dc:rights":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."],"dc:subject":["Chemical Engineering","Chemistry","Polymer Chemistry","Polymers"],"dc:title":["In Situ Infrared Studies of Photooxidation of Ethanol and Bacteria on TiO2-Based Catalysts"],"dc:type":["Electronic Thesis or Dissertation"],"thesis:degree_discipline":["Polymer Science"],"thesis:degree_level":["masters"],"thesis:degree_name":["Master of Science"],"thesis:institution_name":["University of Akron"]},"updated_at":"2026-11-27T04:39:37Z"}