{"id":{"repo_id":"ohiolink","oai_identifier":"oai:etd.ohiolink.edu:case1054825028"},"canonical_url":"https://search.ndltd.org/etd/ohiolink/oai:etd.ohiolink.edu:case1054825028","repository":{"repo_id":"ohiolink","name":"OhioLINK","base_url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai"},"display":{"title":"Priming and temperature loss of steel in a cellular ceramic filter","abstract":"Ceramic filters have been accepted as a successful method of reducing or eliminating inclusions from steel and other metal castings. For a filter to function when it is placed in the gating system of the casting, it is necessary that the steel flow through this filter without freezing or that the filter prime properly. This priming and the factors that influence it is the subject of this thesis. Cellular ceramic filters of various cell sizes and thicknesses were used in this study to investigate the relationships among superheat, filter parameters and priming conditions. The heat loss was the major factor to cause freezing of metal and the cessation of flow at the filter. An increase of static head does not help much to improve priming. A solid shell model was proposed to describe the various primed flow rates. The priming or no priming was not a simple occurrence. Priming depends on the conditions in the overall metal mold-filter system and is considered as four categories: fully primed, gradually primed, gradually unprimed and completely unprimed. Criteria for priming were also discussed. The temperature loss of liquid steel across the filter under various conditions was studied. This temperature loss between the metal entering and leaving the filter was both measured and calculated using appropriate heat flow equations. The calcu lated temperature loss was proved to be a very good base line to obtain the required superheat for obtaining a fully primed condition under various conditions.","abstract_html":"Ceramic filters have been accepted as a successful method of reducing or eliminating inclusions from steel and other metal castings. For a filter to function when it is placed in the gating system of the casting, it is necessary that the steel flow through this filter without freezing or that the filter prime properly. This priming and the factors that influence it is the subject of this thesis. Cellular ceramic filters of various cell sizes and thicknesses were used in this study to investigate the relationships among superheat, filter parameters and priming conditions. The heat loss was the major factor to cause freezing of metal and the cessation of flow at the filter. An increase of static head does not help much to improve priming. A solid shell model was proposed to describe the various primed flow rates. The priming or no priming was not a simple occurrence. Priming depends on the conditions in the overall metal mold-filter system and is considered as four categories: fully primed, gradually primed, gradually unprimed and completely unprimed. Criteria for priming were also discussed. The temperature loss of liquid steel across the filter under various conditions was studied. This temperature loss between the metal entering and leaving the filter was both measured and calculated using appropriate heat flow equations. The calcu lated temperature loss was proved to be a very good base line to obtain the required superheat for obtaining a fully primed condition under various conditions.","abstract_has_math":false,"creators":["Nieh, Cuo-Yo"],"institution":"Case Western Reserve University School of Graduate Studies","degree_name":"Doctor of Philosophy","degree_level":"doctoral","degree_discipline":"Materials Science and Engineering","degree_department":null,"school":null,"contributors":[],"advisors":["Wallace, John"],"committee_chairs":[],"committee_members":[],"year":1990,"date_issued":"1990","date_published":"1990","updated_at":"2026-11-27T04:14:08Z","subjects":["Engineering, Metallurgy","Priming","temperature loss","cellular ceramic filter"],"languages":["English"],"rights":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://rave.ohiolink.edu/etdc/view?acc_num=case1054825028","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"http://rave.ohiolink.edu/etdc/view?acc_num=case1054825028","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aohiolink%3Aoai%3Aetd.ohiolink.edu%3Acase1054825028","prefix":"oai_dc"},"source_record":{"url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Aetd.ohiolink.edu%3Acase1054825028","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Wallace, John"]},{"key":"dc:creator","label":"Author","values":["Nieh, Cuo-Yo"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["1990"]},{"key":"dc:publisher","label":"Institution","values":["Case Western Reserve University School of Graduate Studies / OhioLINK"]},{"key":"dc:type","label":"Dc Type","values":["Electronic Thesis or Dissertation"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Materials Science and Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["doctoral"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Doctor of Philosophy"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["Case Western Reserve University School of Graduate Studies"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Engineering, Metallurgy","Priming","temperature loss","cellular ceramic filter"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:rights","label":"Dc Rights","values":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://rave.ohiolink.edu/etdc/view?acc_num=case1054825028"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["Ceramic filters have been accepted as a successful method of reducing or eliminating inclusions from steel and other metal castings. For a filter to function when it is placed in the gating system of the casting, it is necessary that the steel flow through this filter without freezing or that the filter prime properly. This priming and the factors that influence it is the subject of this thesis. Cellular ceramic filters of various cell sizes and thicknesses were used in this study to investigate the relationships among superheat, filter parameters and priming conditions. The heat loss was the major factor to cause freezing of metal and the cessation of flow at the filter. An increase of static head does not help much to improve priming. A solid shell model was proposed to describe the various primed flow rates. The priming or no priming was not a simple occurrence. Priming depends on the conditions in the overall metal mold-filter system and is considered as four categories: fully primed, gradually primed, gradually unprimed and completely unprimed. Criteria for priming were also discussed. The temperature loss of liquid steel across the filter under various conditions was studied. This temperature loss between the metal entering and leaving the filter was both measured and calculated using appropriate heat flow equations. The calcu lated temperature loss was proved to be a very good base line to obtain the required superheat for obtaining a fully primed condition under various conditions."]},{"key":"dc:format","label":"Dc Format","values":["application/pdf","p.127","2.8 MB"]},{"key":"dc:title","label":"Title","values":["Priming and temperature loss of steel in a cellular ceramic filter"]}]}],"canonical_facts":{"dc:contributor.advisor":["Wallace, John"],"dc:creator":["Nieh, Cuo-Yo"],"dc:date":["1990"],"dc:description":["Ceramic filters have been accepted as a successful method of reducing or eliminating inclusions from steel and other metal castings. For a filter to function when it is placed in the gating system of the casting, it is necessary that the steel flow through this filter without freezing or that the filter prime properly. This priming and the factors that influence it is the subject of this thesis. Cellular ceramic filters of various cell sizes and thicknesses were used in this study to investigate the relationships among superheat, filter parameters and priming conditions. The heat loss was the major factor to cause freezing of metal and the cessation of flow at the filter. An increase of static head does not help much to improve priming. A solid shell model was proposed to describe the various primed flow rates. The priming or no priming was not a simple occurrence. Priming depends on the conditions in the overall metal mold-filter system and is considered as four categories: fully primed, gradually primed, gradually unprimed and completely unprimed. Criteria for priming were also discussed. The temperature loss of liquid steel across the filter under various conditions was studied. This temperature loss between the metal entering and leaving the filter was both measured and calculated using appropriate heat flow equations. The calcu lated temperature loss was proved to be a very good base line to obtain the required superheat for obtaining a fully primed condition under various conditions."],"dc:format":["application/pdf","p.127","2.8 MB"],"dc:identifier":["http://rave.ohiolink.edu/etdc/view?acc_num=case1054825028"],"dc:language":["English"],"dc:publisher":["Case Western Reserve University School of Graduate Studies / OhioLINK"],"dc:rights":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."],"dc:subject":["Engineering, Metallurgy","Priming","temperature loss","cellular ceramic filter"],"dc:title":["Priming and temperature loss of steel in a cellular ceramic filter"],"dc:type":["Electronic Thesis or Dissertation"],"thesis:degree_discipline":["Materials Science and Engineering"],"thesis:degree_level":["doctoral"],"thesis:degree_name":["Doctor of Philosophy"],"thesis:institution_name":["Case Western Reserve University School of Graduate Studies"]},"updated_at":"2026-11-27T04:14:08Z"}