{"id":{"repo_id":"ohiolink","oai_identifier":"oai:etd.ohiolink.edu:case1425046485"},"canonical_url":"https://search.ndltd.org/etd/ohiolink/oai:etd.ohiolink.edu:case1425046485","repository":{"repo_id":"ohiolink","name":"OhioLINK","base_url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai"},"display":{"title":"Fundamental and Flow Battery Studies for Non-Aqueous Redox Systems","abstract":"Non-aqueous redox flow battery systems are being considered for grid level energy storage applications. Non-aqueous electrolytes have exhibited the ability to support redox reactions with cell potentials > 2 V, and therefore hold promise for enabling high energy and power density redox flow batteries. The increased cell potential is considered the primary advantage of non-aqueous electrolytes over aqueous electrolytes, which are constrained to cell potentials ~1.6 V due to the electrochemical stability of water. Although reversible and promising kinetic couples have been reported in the literature, practical cell-level operation demonstrations are limited because often low conductivity anion exchange membranes (<0.5 mS cm-1) and impractical cell designs (H-type cells) have been used. The motivation of this research is to obtain fundamental understanding of the key factors limiting the performance of non-aqueous redox flow battery systems in realistic flow battery designs. A model non-aqueous redox system of vanadium acetylacetonate in acetonitrile with a cell potential of ~2.2 V, was demonstrated in an energy storage device.We modified a cation exchange membrane and a microporous polymer film for use in a non-aqueous electrolyte. This is one of the early studies reporting measured conductivities of membranes for application in non-aqueous flow battery. The conductivity of the microporous separators was found to be 1.5 times greater than a modified TEA-Nafion cation exchange membrane, and over 34 times greater than anion exchange membranes similar to those typically used in the literature. There is an operational trade-off of a lower cost higher conductivity microporous separator with a higher cost but lower conductivity and higher permselectivity (low active species crossover) cation exchange membrane. The two types of membranes have been examined in two prototype flow battery designs (flow-through and flow-by electrodes) and energy storage performance in these realistic devices were measured. An acceptable 79-88% energy storage efficiency was demonstrated at current densities of 10 mA cm-2, which represents a current density greater than 100-fold over previous literature. These results represent operation of a non-aqueous flow battery at power densities that might be practical. The source of the overpotentials were identified, with electrolyte/membrane conductivity being the controlling resistance. However, we observed a significant capacity fade that has been attributed to increased activation and concentration overpotentials during cycling to a constant cell potential, primarily in the positive half-cell. The source of the capacity decay was found to be caused mainly by the degradation of the active (and perhaps inactive) species. The understanding of the source of energy storage capacity loss identified in this research provides insight for exploring deeper understanding of redox couples, supporting electrolytes, and solvent effects that should lead to flow battery systems for stable high energy efficiencies, high power densities, and stable high storage capacities.","abstract_html":"Non-aqueous redox flow battery systems are being considered for grid level energy storage applications. Non-aqueous electrolytes have exhibited the ability to support redox reactions with cell potentials &gt; 2 V, and therefore hold promise for enabling high energy and power density redox flow batteries. The increased cell potential is considered the primary advantage of non-aqueous electrolytes over aqueous electrolytes, which are constrained to cell potentials ~1.6 V due to the electrochemical stability of water. Although reversible and promising kinetic couples have been reported in the literature, practical cell-level operation demonstrations are limited because often low conductivity anion exchange membranes (&lt;0.5 mS cm-1) and impractical cell designs (H-type cells) have been used. The motivation of this research is to obtain fundamental understanding of the key factors limiting the performance of non-aqueous redox flow battery systems in realistic flow battery designs. A model non-aqueous redox system of vanadium acetylacetonate in acetonitrile with a cell potential of ~2.2 V, was demonstrated in an energy storage device.We modified a cation exchange membrane and a microporous polymer film for use in a non-aqueous electrolyte. This is one of the early studies reporting measured conductivities of membranes for application in non-aqueous flow battery. The conductivity of the microporous separators was found to be 1.5 times greater than a modified TEA-Nafion cation exchange membrane, and over 34 times greater than anion exchange membranes similar to those typically used in the literature. There is an operational trade-off of a lower cost higher conductivity microporous separator with a higher cost but lower conductivity and higher permselectivity (low active species crossover) cation exchange membrane. The two types of membranes have been examined in two prototype flow battery designs (flow-through and flow-by electrodes) and energy storage performance in these realistic devices were measured. An acceptable 79-88% energy storage efficiency was demonstrated at current densities of 10 mA cm-2, which represents a current density greater than 100-fold over previous literature. These results represent operation of a non-aqueous flow battery at power densities that might be practical. The source of the overpotentials were identified, with electrolyte/membrane conductivity being the controlling resistance. However, we observed a significant capacity fade that has been attributed to increased activation and concentration overpotentials during cycling to a constant cell potential, primarily in the positive half-cell. The source of the capacity decay was found to be caused mainly by the degradation of the active (and perhaps inactive) species. The understanding of the source of energy storage capacity loss identified in this research provides insight for exploring deeper understanding of redox couples, supporting electrolytes, and solvent effects that should lead to flow battery systems for stable high energy efficiencies, high power densities, and stable high storage capacities.","abstract_has_math":false,"creators":["Escalante García, Ismailia Leilani"],"institution":"Case Western Reserve University School of Graduate Studies","degree_name":"Doctor of Philosophy","degree_level":"doctoral","degree_discipline":"Chemical Engineering","degree_department":null,"school":null,"contributors":[],"advisors":["Savinell, Robert"],"committee_chairs":[],"committee_members":[],"year":2015,"date_issued":"2015-06-03","date_published":"2015-06-03","updated_at":"2026-11-27T04:40:11Z","subjects":["Energy","Chemical Engineering","Flow batteries, non-aqueous electrolytes, separators"],"languages":["English"],"rights":["unrestricted","This thesis or dissertation is protected by copyright: some rights reserved. It is licensed for use under a Creative Commons license. Specific terms and permissions are available from this document's record in the OhioLINK ETD Center."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://rave.ohiolink.edu/etdc/view?acc_num=case1425046485","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"http://rave.ohiolink.edu/etdc/view?acc_num=case1425046485","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aohiolink%3Aoai%3Aetd.ohiolink.edu%3Acase1425046485","prefix":"oai_dc"},"source_record":{"url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Aetd.ohiolink.edu%3Acase1425046485","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Savinell, Robert"]},{"key":"dc:creator","label":"Author","values":["Escalante García, Ismailia Leilani"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2015-06-03"]},{"key":"dc:publisher","label":"Institution","values":["Case Western Reserve University School of Graduate Studies / OhioLINK"]},{"key":"dc:type","label":"Dc Type","values":["Electronic Thesis or Dissertation"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Chemical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["doctoral"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Doctor of Philosophy"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["Case Western Reserve University School of Graduate Studies"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Energy","Chemical Engineering","Flow batteries, non-aqueous electrolytes, separators"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:rights","label":"Dc Rights","values":["unrestricted","This thesis or dissertation is protected by copyright: some rights reserved. It is licensed for use under a Creative Commons license. Specific terms and permissions are available from this document's record in the OhioLINK ETD Center."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://rave.ohiolink.edu/etdc/view?acc_num=case1425046485"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["Non-aqueous redox flow battery systems are being considered for grid level energy storage applications. Non-aqueous electrolytes have exhibited the ability to support redox reactions with cell potentials > 2 V, and therefore hold promise for enabling high energy and power density redox flow batteries. The increased cell potential is considered the primary advantage of non-aqueous electrolytes over aqueous electrolytes, which are constrained to cell potentials ~1.6 V due to the electrochemical stability of water. Although reversible and promising kinetic couples have been reported in the literature, practical cell-level operation demonstrations are limited because often low conductivity anion exchange membranes (<0.5 mS cm-1) and impractical cell designs (H-type cells) have been used. The motivation of this research is to obtain fundamental understanding of the key factors limiting the performance of non-aqueous redox flow battery systems in realistic flow battery designs. A model non-aqueous redox system of vanadium acetylacetonate in acetonitrile with a cell potential of ~2.2 V, was demonstrated in an energy storage device.We modified a cation exchange membrane and a microporous polymer film for use in a non-aqueous electrolyte. This is one of the early studies reporting measured conductivities of membranes for application in non-aqueous flow battery. The conductivity of the microporous separators was found to be 1.5 times greater than a modified TEA-Nafion cation exchange membrane, and over 34 times greater than anion exchange membranes similar to those typically used in the literature. There is an operational trade-off of a lower cost higher conductivity microporous separator with a higher cost but lower conductivity and higher permselectivity (low active species crossover) cation exchange membrane. The two types of membranes have been examined in two prototype flow battery designs (flow-through and flow-by electrodes) and energy storage performance in these realistic devices were measured. An acceptable 79-88% energy storage efficiency was demonstrated at current densities of 10 mA cm-2, which represents a current density greater than 100-fold over previous literature. These results represent operation of a non-aqueous flow battery at power densities that might be practical. The source of the overpotentials were identified, with electrolyte/membrane conductivity being the controlling resistance. However, we observed a significant capacity fade that has been attributed to increased activation and concentration overpotentials during cycling to a constant cell potential, primarily in the positive half-cell. The source of the capacity decay was found to be caused mainly by the degradation of the active (and perhaps inactive) species. The understanding of the source of energy storage capacity loss identified in this research provides insight for exploring deeper understanding of redox couples, supporting electrolytes, and solvent effects that should lead to flow battery systems for stable high energy efficiencies, high power densities, and stable high storage capacities."]},{"key":"dc:format","label":"Dc Format","values":["application/pdf","p.209","3.9 MB"]},{"key":"dc:title","label":"Title","values":["Fundamental and Flow Battery Studies for Non-Aqueous Redox Systems"]}]}],"canonical_facts":{"dc:contributor.advisor":["Savinell, Robert"],"dc:creator":["Escalante García, Ismailia Leilani"],"dc:date":["2015-06-03"],"dc:description":["Non-aqueous redox flow battery systems are being considered for grid level energy storage applications. Non-aqueous electrolytes have exhibited the ability to support redox reactions with cell potentials > 2 V, and therefore hold promise for enabling high energy and power density redox flow batteries. The increased cell potential is considered the primary advantage of non-aqueous electrolytes over aqueous electrolytes, which are constrained to cell potentials ~1.6 V due to the electrochemical stability of water. Although reversible and promising kinetic couples have been reported in the literature, practical cell-level operation demonstrations are limited because often low conductivity anion exchange membranes (<0.5 mS cm-1) and impractical cell designs (H-type cells) have been used. The motivation of this research is to obtain fundamental understanding of the key factors limiting the performance of non-aqueous redox flow battery systems in realistic flow battery designs. A model non-aqueous redox system of vanadium acetylacetonate in acetonitrile with a cell potential of ~2.2 V, was demonstrated in an energy storage device.We modified a cation exchange membrane and a microporous polymer film for use in a non-aqueous electrolyte. This is one of the early studies reporting measured conductivities of membranes for application in non-aqueous flow battery. The conductivity of the microporous separators was found to be 1.5 times greater than a modified TEA-Nafion cation exchange membrane, and over 34 times greater than anion exchange membranes similar to those typically used in the literature. There is an operational trade-off of a lower cost higher conductivity microporous separator with a higher cost but lower conductivity and higher permselectivity (low active species crossover) cation exchange membrane. The two types of membranes have been examined in two prototype flow battery designs (flow-through and flow-by electrodes) and energy storage performance in these realistic devices were measured. An acceptable 79-88% energy storage efficiency was demonstrated at current densities of 10 mA cm-2, which represents a current density greater than 100-fold over previous literature. These results represent operation of a non-aqueous flow battery at power densities that might be practical. The source of the overpotentials were identified, with electrolyte/membrane conductivity being the controlling resistance. However, we observed a significant capacity fade that has been attributed to increased activation and concentration overpotentials during cycling to a constant cell potential, primarily in the positive half-cell. The source of the capacity decay was found to be caused mainly by the degradation of the active (and perhaps inactive) species. The understanding of the source of energy storage capacity loss identified in this research provides insight for exploring deeper understanding of redox couples, supporting electrolytes, and solvent effects that should lead to flow battery systems for stable high energy efficiencies, high power densities, and stable high storage capacities."],"dc:format":["application/pdf","p.209","3.9 MB"],"dc:identifier":["http://rave.ohiolink.edu/etdc/view?acc_num=case1425046485"],"dc:language":["English"],"dc:publisher":["Case Western Reserve University School of Graduate Studies / OhioLINK"],"dc:rights":["unrestricted","This thesis or dissertation is protected by copyright: some rights reserved. It is licensed for use under a Creative Commons license. Specific terms and permissions are available from this document's record in the OhioLINK ETD Center."],"dc:subject":["Energy","Chemical Engineering","Flow batteries, non-aqueous electrolytes, separators"],"dc:title":["Fundamental and Flow Battery Studies for Non-Aqueous Redox Systems"],"dc:type":["Electronic Thesis or Dissertation"],"thesis:degree_discipline":["Chemical Engineering"],"thesis:degree_level":["doctoral"],"thesis:degree_name":["Doctor of Philosophy"],"thesis:institution_name":["Case Western Reserve University School of Graduate Studies"]},"updated_at":"2026-11-27T04:40:11Z"}