{"id":{"repo_id":"ohiolink","oai_identifier":"oai:etd.ohiolink.edu:case152302739582634"},"canonical_url":"https://search.ndltd.org/etd/ohiolink/oai:etd.ohiolink.edu:case152302739582634","repository":{"repo_id":"ohiolink","name":"OhioLINK","base_url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai"},"display":{"title":"Mechanical Behavior and Microstructural Evolution during Hot Deformation of Aluminum 2070","abstract":"A third generation Ag-free Al-Li alloy, 2070, is the focus of this dissertation. To determine its suitability for a range of applications, this alloy was first qualified through a series of room temperature mechanical tests. Samples from each orientation (e.g., L, T, or S) were excised from each section of an H-forging to determine the effects of prior work and degree of anisotropy. Samples were then tested at room temperature in tension, compression, and Charpy impact. Room temperature mechanical behavior of as-received H-forgings of 2070 was found to meet or exceed properties of second and third generation Al-Li alloys.The primary focus of this dissertation was to determine the effects of forging conditions (i.e., temperature and strain rate) on flow stress and microstructural evolution during/after hot deformation of this material. Subscale right circular cylinder samples were deformation processed under isothermal conditions at a range of temperatures (T = 300/425/450/475°C) and strain rates (0.01/s, 0.1/s, 5.0/s) to 100% true strain in order to determine these effects on the resulting flow stress and microstructure. Activation energy and power dissipation coefficients were determined for each temperature and strain rate combination followed by microstructure analyses via optical and scanning electron microscopy (SEM).Microstructure analyses included EBSD (electron backscatter diffraction) to determine the degree of dynamic recrystallization (DRX) or dynamic recovery (DRV) present after deformation processing at different temperatures and strain rates. Dynamic recovery was found to be the dominant deformation mechanism for the sample tested at 450°C and 0.01/s. Samples tested at 450°C and 5.0/s or 300°C and any strain rate (0.01, 0.1, or 5.0/s) were found to be dominated by dynamic recrystallization, with a large area fraction of unresolved highly deformed grains. When samples were solution heat treated (at 510°C for 1 hour) after deformation processing, the sample processed at 450°C and 0.01/s was found to have little microstructural change, while the sample processed at 300°C and 5.0/s showed substantial static recrystallization.","abstract_html":"A third generation Ag-free Al-Li alloy, 2070, is the focus of this dissertation. To determine its suitability for a range of applications, this alloy was first qualified through a series of room temperature mechanical tests. Samples from each orientation (e.g., L, T, or S) were excised from each section of an H-forging to determine the effects of prior work and degree of anisotropy. Samples were then tested at room temperature in tension, compression, and Charpy impact. Room temperature mechanical behavior of as-received H-forgings of 2070 was found to meet or exceed properties of second and third generation Al-Li alloys.The primary focus of this dissertation was to determine the effects of forging conditions (i.e., temperature and strain rate) on flow stress and microstructural evolution during/after hot deformation of this material. Subscale right circular cylinder samples were deformation processed under isothermal conditions at a range of temperatures (T = 300/425/450/475°C) and strain rates (0.01/s, 0.1/s, 5.0/s) to 100% true strain in order to determine these effects on the resulting flow stress and microstructure. Activation energy and power dissipation coefficients were determined for each temperature and strain rate combination followed by microstructure analyses via optical and scanning electron microscopy (SEM).Microstructure analyses included EBSD (electron backscatter diffraction) to determine the degree of dynamic recrystallization (DRX) or dynamic recovery (DRV) present after deformation processing at different temperatures and strain rates. Dynamic recovery was found to be the dominant deformation mechanism for the sample tested at 450°C and 0.01/s. Samples tested at 450°C and 5.0/s or 300°C and any strain rate (0.01, 0.1, or 5.0/s) were found to be dominated by dynamic recrystallization, with a large area fraction of unresolved highly deformed grains. When samples were solution heat treated (at 510°C for 1 hour) after deformation processing, the sample processed at 450°C and 0.01/s was found to have little microstructural change, while the sample processed at 300°C and 5.0/s showed substantial static recrystallization.","abstract_has_math":false,"creators":["Neilson, Henry Jathuren"],"institution":"Case Western Reserve University School of Graduate Studies","degree_name":"Doctor of Philosophy","degree_level":"doctoral","degree_discipline":"Materials Science and Engineering","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":["Lewandowski, John"],"committee_members":[],"year":2018,"date_issued":"2018-06-01","date_published":"2018-06-01","updated_at":"2026-11-27T04:48:26Z","subjects":["Materials Science","Hot deformation","aluminum","lithium","processing","forging","microstructural analysis","mechanical behavior"],"languages":["English"],"rights":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://rave.ohiolink.edu/etdc/view?acc_num=case152302739582634","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"http://rave.ohiolink.edu/etdc/view?acc_num=case152302739582634","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aohiolink%3Aoai%3Aetd.ohiolink.edu%3Acase152302739582634","prefix":"oai_dc"},"source_record":{"url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Aetd.ohiolink.edu%3Acase152302739582634","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.committeechair","label":"Committee Chair","values":["Lewandowski, John"]},{"key":"dc:creator","label":"Author","values":["Neilson, Henry Jathuren"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2018-06-01"]},{"key":"dc:publisher","label":"Institution","values":["Case Western Reserve University School of Graduate Studies / OhioLINK"]},{"key":"dc:type","label":"Dc Type","values":["Electronic Thesis or Dissertation"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Materials Science and Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["doctoral"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Doctor of Philosophy"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["Case Western Reserve University School of Graduate Studies"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Materials Science","Hot deformation","aluminum","lithium","processing","forging","microstructural analysis","mechanical behavior"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:rights","label":"Dc Rights","values":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://rave.ohiolink.edu/etdc/view?acc_num=case152302739582634"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["A third generation Ag-free Al-Li alloy, 2070, is the focus of this dissertation. To determine its suitability for a range of applications, this alloy was first qualified through a series of room temperature mechanical tests. Samples from each orientation (e.g., L, T, or S) were excised from each section of an H-forging to determine the effects of prior work and degree of anisotropy. Samples were then tested at room temperature in tension, compression, and Charpy impact. Room temperature mechanical behavior of as-received H-forgings of 2070 was found to meet or exceed properties of second and third generation Al-Li alloys.The primary focus of this dissertation was to determine the effects of forging conditions (i.e., temperature and strain rate) on flow stress and microstructural evolution during/after hot deformation of this material. Subscale right circular cylinder samples were deformation processed under isothermal conditions at a range of temperatures (T = 300/425/450/475°C) and strain rates (0.01/s, 0.1/s, 5.0/s) to 100% true strain in order to determine these effects on the resulting flow stress and microstructure. Activation energy and power dissipation coefficients were determined for each temperature and strain rate combination followed by microstructure analyses via optical and scanning electron microscopy (SEM).Microstructure analyses included EBSD (electron backscatter diffraction) to determine the degree of dynamic recrystallization (DRX) or dynamic recovery (DRV) present after deformation processing at different temperatures and strain rates. Dynamic recovery was found to be the dominant deformation mechanism for the sample tested at 450°C and 0.01/s. Samples tested at 450°C and 5.0/s or 300°C and any strain rate (0.01, 0.1, or 5.0/s) were found to be dominated by dynamic recrystallization, with a large area fraction of unresolved highly deformed grains. When samples were solution heat treated (at 510°C for 1 hour) after deformation processing, the sample processed at 450°C and 0.01/s was found to have little microstructural change, while the sample processed at 300°C and 5.0/s showed substantial static recrystallization."]},{"key":"dc:format","label":"Dc Format","values":["application/pdf","p.235","31.56 MB"]},{"key":"dc:title","label":"Title","values":["Mechanical Behavior and Microstructural Evolution during Hot Deformation of Aluminum 2070"]}]}],"canonical_facts":{"dc:contributor.committeechair":["Lewandowski, John"],"dc:creator":["Neilson, Henry Jathuren"],"dc:date":["2018-06-01"],"dc:description":["A third generation Ag-free Al-Li alloy, 2070, is the focus of this dissertation. To determine its suitability for a range of applications, this alloy was first qualified through a series of room temperature mechanical tests. Samples from each orientation (e.g., L, T, or S) were excised from each section of an H-forging to determine the effects of prior work and degree of anisotropy. Samples were then tested at room temperature in tension, compression, and Charpy impact. Room temperature mechanical behavior of as-received H-forgings of 2070 was found to meet or exceed properties of second and third generation Al-Li alloys.The primary focus of this dissertation was to determine the effects of forging conditions (i.e., temperature and strain rate) on flow stress and microstructural evolution during/after hot deformation of this material. Subscale right circular cylinder samples were deformation processed under isothermal conditions at a range of temperatures (T = 300/425/450/475°C) and strain rates (0.01/s, 0.1/s, 5.0/s) to 100% true strain in order to determine these effects on the resulting flow stress and microstructure. Activation energy and power dissipation coefficients were determined for each temperature and strain rate combination followed by microstructure analyses via optical and scanning electron microscopy (SEM).Microstructure analyses included EBSD (electron backscatter diffraction) to determine the degree of dynamic recrystallization (DRX) or dynamic recovery (DRV) present after deformation processing at different temperatures and strain rates. Dynamic recovery was found to be the dominant deformation mechanism for the sample tested at 450°C and 0.01/s. Samples tested at 450°C and 5.0/s or 300°C and any strain rate (0.01, 0.1, or 5.0/s) were found to be dominated by dynamic recrystallization, with a large area fraction of unresolved highly deformed grains. When samples were solution heat treated (at 510°C for 1 hour) after deformation processing, the sample processed at 450°C and 0.01/s was found to have little microstructural change, while the sample processed at 300°C and 5.0/s showed substantial static recrystallization."],"dc:format":["application/pdf","p.235","31.56 MB"],"dc:identifier":["http://rave.ohiolink.edu/etdc/view?acc_num=case152302739582634"],"dc:language":["English"],"dc:publisher":["Case Western Reserve University School of Graduate Studies / OhioLINK"],"dc:rights":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."],"dc:subject":["Materials Science","Hot deformation","aluminum","lithium","processing","forging","microstructural analysis","mechanical behavior"],"dc:title":["Mechanical Behavior and Microstructural Evolution during Hot Deformation of Aluminum 2070"],"dc:type":["Electronic Thesis or Dissertation"],"thesis:degree_discipline":["Materials Science and Engineering"],"thesis:degree_level":["doctoral"],"thesis:degree_name":["Doctor of Philosophy"],"thesis:institution_name":["Case Western Reserve University School of Graduate Studies"]},"updated_at":"2026-11-27T04:48:26Z"}