{"id":{"repo_id":"ohiolink","oai_identifier":"oai:etd.ohiolink.edu:osu1243885964"},"canonical_url":"https://search.ndltd.org/etd/ohiolink/oai:etd.ohiolink.edu:osu1243885964","repository":{"repo_id":"ohiolink","name":"OhioLINK","base_url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai"},"display":{"title":"An Experimental Investigation of Materials and Surface Treatments on Gear contact Fatigue Life","abstract":"<p>This study consists of experimental studies involving two modes of gear contact fatigue failure: gear pitting (spalling) and gear scuffing. For pitting studies, several materials and surface treatments were investigated at various stress levels. These surface treatments included (i) hobbed and shaved (baseline), (ii) chemically polished, (iii) shot peened and plastic honed, and (iv) ground gears. Pitting fatigue lives of chemically polished gears were greater than those of baseline specimens. Both shot peened and plastic honed gears and ground gears were shown to have greater pitting fatigue lives than baseline gears. The improved pitting fatigue life of ground gears over baseline gears appears related to the improved involute profile shapes of the specimens.</p><p>For gear scuffing experiments, the standard ISO 14635-1 FZG Scuffing Test was performed on AISI 8620 type A spur gears. These experiments included four uncoated gear pairs and one gear pair coated with an experimental PVD coating. Uncoated gears encountered scuffing during Stages 11 and 12. A high correlation between temperature and scuffing results was detected for both coated and uncoated specimens.</p>","abstract_html":"&lt;p&gt;This study consists of experimental studies involving two modes of gear contact fatigue failure: gear pitting (spalling) and gear scuffing. For pitting studies, several materials and surface treatments were investigated at various stress levels. These surface treatments included (i) hobbed and shaved (baseline), (ii) chemically polished, (iii) shot peened and plastic honed, and (iv) ground gears. Pitting fatigue lives of chemically polished gears were greater than those of baseline specimens. Both shot peened and plastic honed gears and ground gears were shown to have greater pitting fatigue lives than baseline gears. The improved pitting fatigue life of ground gears over baseline gears appears related to the improved involute profile shapes of the specimens.&lt;/p&gt;&lt;p&gt;For gear scuffing experiments, the standard ISO 14635-1 FZG Scuffing Test was performed on AISI 8620 type A spur gears. These experiments included four uncoated gear pairs and one gear pair coated with an experimental PVD coating. Uncoated gears encountered scuffing during Stages 11 and 12. A high correlation between temperature and scuffing results was detected for both coated and uncoated specimens.&lt;/p&gt;","abstract_has_math":false,"creators":["Klein, Mark Andrew"],"institution":"The Ohio State University","degree_name":"Master of Science","degree_level":"masters","degree_discipline":"Mechanical Engineering","degree_department":null,"school":null,"contributors":[],"advisors":["Kahraman, Ahmet"],"committee_chairs":[],"committee_members":[],"year":2009,"date_issued":"2009-09-03","date_published":"2009-09-03","updated_at":"2026-11-27T04:34:13Z","subjects":["Mechanical Engineering","gear","scuffing","spalling","pitting","fatigue contact","spur gears","FZG"],"languages":["English"],"rights":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://rave.ohiolink.edu/etdc/view?acc_num=osu1243885964","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"http://rave.ohiolink.edu/etdc/view?acc_num=osu1243885964","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aohiolink%3Aoai%3Aetd.ohiolink.edu%3Aosu1243885964","prefix":"oai_dc"},"source_record":{"url":"https://etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Aetd.ohiolink.edu%3Aosu1243885964","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Kahraman, Ahmet"]},{"key":"dc:creator","label":"Author","values":["Klein, Mark Andrew"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2009-09-03"]},{"key":"dc:publisher","label":"Institution","values":["The Ohio State University / OhioLINK"]},{"key":"dc:type","label":"Dc Type","values":["Electronic Thesis or Dissertation"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Mechanical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["masters"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["The Ohio State University"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Mechanical Engineering","gear","scuffing","spalling","pitting","fatigue contact","spur gears","FZG"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:rights","label":"Dc Rights","values":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://rave.ohiolink.edu/etdc/view?acc_num=osu1243885964"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["<p>This study consists of experimental studies involving two modes of gear contact fatigue failure: gear pitting (spalling) and gear scuffing. For pitting studies, several materials and surface treatments were investigated at various stress levels. These surface treatments included (i) hobbed and shaved (baseline), (ii) chemically polished, (iii) shot peened and plastic honed, and (iv) ground gears. Pitting fatigue lives of chemically polished gears were greater than those of baseline specimens. Both shot peened and plastic honed gears and ground gears were shown to have greater pitting fatigue lives than baseline gears. The improved pitting fatigue life of ground gears over baseline gears appears related to the improved involute profile shapes of the specimens.</p><p>For gear scuffing experiments, the standard ISO 14635-1 FZG Scuffing Test was performed on AISI 8620 type A spur gears. These experiments included four uncoated gear pairs and one gear pair coated with an experimental PVD coating. Uncoated gears encountered scuffing during Stages 11 and 12. A high correlation between temperature and scuffing results was detected for both coated and uncoated specimens.</p>"]},{"key":"dc:format","label":"Dc Format","values":["application/pdf","p.124","4.04 MB"]},{"key":"dc:title","label":"Title","values":["An Experimental Investigation of Materials and Surface Treatments on Gear contact Fatigue Life"]}]}],"canonical_facts":{"dc:contributor.advisor":["Kahraman, Ahmet"],"dc:creator":["Klein, Mark Andrew"],"dc:date":["2009-09-03"],"dc:description":["<p>This study consists of experimental studies involving two modes of gear contact fatigue failure: gear pitting (spalling) and gear scuffing. For pitting studies, several materials and surface treatments were investigated at various stress levels. These surface treatments included (i) hobbed and shaved (baseline), (ii) chemically polished, (iii) shot peened and plastic honed, and (iv) ground gears. Pitting fatigue lives of chemically polished gears were greater than those of baseline specimens. Both shot peened and plastic honed gears and ground gears were shown to have greater pitting fatigue lives than baseline gears. The improved pitting fatigue life of ground gears over baseline gears appears related to the improved involute profile shapes of the specimens.</p><p>For gear scuffing experiments, the standard ISO 14635-1 FZG Scuffing Test was performed on AISI 8620 type A spur gears. These experiments included four uncoated gear pairs and one gear pair coated with an experimental PVD coating. Uncoated gears encountered scuffing during Stages 11 and 12. A high correlation between temperature and scuffing results was detected for both coated and uncoated specimens.</p>"],"dc:format":["application/pdf","p.124","4.04 MB"],"dc:identifier":["http://rave.ohiolink.edu/etdc/view?acc_num=osu1243885964"],"dc:language":["English"],"dc:publisher":["The Ohio State University / OhioLINK"],"dc:rights":["unrestricted","This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws."],"dc:subject":["Mechanical Engineering","gear","scuffing","spalling","pitting","fatigue contact","spur gears","FZG"],"dc:title":["An Experimental Investigation of Materials and Surface Treatments on Gear contact Fatigue Life"],"dc:type":["Electronic Thesis or Dissertation"],"thesis:degree_discipline":["Mechanical Engineering"],"thesis:degree_level":["masters"],"thesis:degree_name":["Master of Science"],"thesis:institution_name":["The Ohio State University"]},"updated_at":"2026-11-27T04:34:13Z"}