{"id":{"repo_id":"pohang","oai_identifier":"oai:oasis.postech.ac.kr:2014.oak/2132"},"canonical_url":"https://search.ndltd.org/etd/pohang/oai:oasis.postech.ac.kr:2014.oak/2132","repository":{"repo_id":"pohang","name":"Pohang University of Science and Technology","base_url":"http://oasis.postech.ac.kr/oai/request"},"display":{"title":"Gaseous Reduction of Hematite Ores containing High Phosphorus","abstract":"In the current study, the reduction behavior of high P iron ore pellets by CO-H2 gas mixtures was investigated. Total porosity, pore size distribution and surface area of the pellets were measured using the mercury pressure porosimeter. The reduction was carried out using the thermogravimetric analyses (TGA). The reduction rate increased with increase in temperature and was highest when 100%H2 was used. The reduction behavior could not be explained in terms of a single rate determination step. In the initial stage the reaction rate was controlled by chemical reaction and by diffusion in the later part of the reduction process. The calculated activation energy values range from 20.8 to 50.2 kJ/ mol. The elemental distribution in the reduced pellet of the ore was clarified using the EPMA.","abstract_html":"In the current study, the reduction behavior of high P iron ore pellets by CO-H2 gas mixtures was investigated. Total porosity, pore size distribution and surface area of the pellets were measured using the mercury pressure porosimeter. The reduction was carried out using the thermogravimetric analyses (TGA). The reduction rate increased with increase in temperature and was highest when 100%H2 was used. The reduction behavior could not be explained in terms of a single rate determination step. In the initial stage the reaction rate was controlled by chemical reaction and by diffusion in the later part of the reduction process. The calculated activation energy values range from 20.8 to 50.2 kJ/ mol. The elemental distribution in the reduced pellet of the ore was clarified using the EPMA.","abstract_has_math":false,"creators":["Chiwandika, Kugara Edson"],"institution":null,"degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2014,"date_issued":"2014","date_published":"2014","updated_at":"2026-11-26T04:05:45Z","subjects":[],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["hdl:2014.oak/2132"],"render_values":[{"text":"hdl:2014.oak/2132","href":null,"code":true}]},{"key":"mods:identifier.other","label":"Mods Identifier Other","values":["OAK-2014-01630"],"render_values":[{"text":"OAK-2014-01630","href":null,"code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"http://postech.dcollection.net/jsp/common/DcLoOrgPer.jsp?sItemId=000001675047","outbound_label":"Repository record","outbound_source":"mods:identifier.uri","record_url":"http://postech.dcollection.net/jsp/common/DcLoOrgPer.jsp?sItemId=000001675047","record_label":"Repository record","record_kind":"record","record_source":"mods:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Apohang%3Aoai%3Aoasis.postech.ac.kr%3A2014.oak%2F2132","prefix":"oai_dc"},"source_record":{"url":"http://oasis.postech.ac.kr/oai/request?verb=GetRecord&metadataPrefix=mets&identifier=oai%3Aoasis.postech.ac.kr%3A2014.oak%2F2132","prefix":"mets"},"metadata_groups":[{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.issued","label":"Date","values":["2014"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["hdl:2014.oak/2132"]},{"key":"mods:identifier.other","label":"Mods Identifier Other","values":["OAK-2014-01630"]},{"key":"mods:identifier.uri","label":"Mods Identifier URI","values":["http://postech.dcollection.net/jsp/common/DcLoOrgPer.jsp?sItemId=000001675047"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.other","label":"Dc Description Other","values":["In the current study, the reduction behavior of high P iron ore pellets by CO-H2 gas mixtures was investigated. Total porosity, pore size distribution and surface area of the pellets were measured using the mercury pressure porosimeter. The reduction was carried out using the thermogravimetric analyses (TGA). The reduction rate increased with increase in temperature and was highest when 100%H2 was used. The reduction behavior could not be explained in terms of a single rate determination step. In the initial stage the reaction rate was controlled by chemical reaction and by diffusion in the later part of the reduction process. The calculated activation energy values range from 20.8 to 50.2 kJ/ mol. The elemental distribution in the reduced pellet of the ore was clarified using the EPMA."]},{"key":"dc:title","label":"Title","values":["Gaseous Reduction of Hematite Ores containing High Phosphorus"]},{"key":"mods:accesscondition.useandreproduction","label":"Mods Accesscondition Useandreproduction","values":["BY_NC_ND"]},{"key":"mods:dateaccessioned","label":"Mods Dateaccessioned","values":["2014-12-01T11:49:09Z"]},{"key":"mods:dateavailable","label":"Mods Dateavailable","values":["2014-12-01T11:49:09Z"]},{"key":"mods:namepart","label":"Mods Namepart","values":["Chiwandika, Kugara Edson","철강대학원 철강학과","Graduate Istitute of Ferrous Technology POSTECH"]},{"key":"mods:roleterm.text","label":"Mods Roleterm Text","values":["author","college","department"]}]}],"canonical_facts":{"dc:date.issued":["2014"],"dc:description.other":["In the current study, the reduction behavior of high P iron ore pellets by CO-H2 gas mixtures was investigated. Total porosity, pore size distribution and surface area of the pellets were measured using the mercury pressure porosimeter. The reduction was carried out using the thermogravimetric analyses (TGA). The reduction rate increased with increase in temperature and was highest when 100%H2 was used. The reduction behavior could not be explained in terms of a single rate determination step. In the initial stage the reaction rate was controlled by chemical reaction and by diffusion in the later part of the reduction process. The calculated activation energy values range from 20.8 to 50.2 kJ/ mol. The elemental distribution in the reduced pellet of the ore was clarified using the EPMA."],"dc:identifier":["hdl:2014.oak/2132"],"dc:title":["Gaseous Reduction of Hematite Ores containing High Phosphorus"],"dc:type":["Thesis"],"mods:accesscondition.useandreproduction":["BY_NC_ND"],"mods:dateaccessioned":["2014-12-01T11:49:09Z"],"mods:dateavailable":["2014-12-01T11:49:09Z"],"mods:identifier.other":["OAK-2014-01630"],"mods:identifier.uri":["http://postech.dcollection.net/jsp/common/DcLoOrgPer.jsp?sItemId=000001675047"],"mods:namepart":["Chiwandika, Kugara Edson","철강대학원 철강학과","Graduate Istitute of Ferrous Technology POSTECH"],"mods:roleterm.text":["author","college","department"]},"updated_at":"2026-11-26T04:05:45Z"}