{"id":{"repo_id":"sask","oai_identifier":"oai:harvest.usask.ca:10388/15432"},"canonical_url":"https://search.ndltd.org/etd/sask/oai:harvest.usask.ca:10388/15432","repository":{"repo_id":"sask","name":"University of Saskatchewan","base_url":"https://harvest.usask.ca/server/oai/request"},"display":{"title":"Tribological and Corrosion Behavior of Cold Sprayed Fe-Based Bulk Metallic Glass Coating on Aluminum Alloy","abstract":"Aluminum alloys are vital to the aerospace, marine and automobile industries due to their lightweight, high specific strength, and good corrosion resistance. However, despite these favorable characteristics, they suffer rapid deterioration under severe friction and wear conditions, making surface engineering and coating imperative for use in several industrial applications where high wear resistance is a design requirement. Although several surface modification techniques and coating materials exist for aluminum alloys, bulk metallic glasses (BMGs) have gained attention as promising coating materials due to their superior mechanical properties and excellent wear and corrosion resistance. In this study, Fe87.55C0.75Si6.68Cr2.51B2.51 MG powder was deposited on AA5086-H32 plates at room temperature using a cold spray process. Optical microscopy, hardness testing, X-ray computed tomography (CT), and X-ray diffraction were employed to characterize the thickness, hardness, porosity, and amorphous nature of the resulting coating. Sliding wear tests were conducted against Si3N4 ceramic counterface in dry and wet (3.5 wt.% NaCl solution) conditions under three different applied loads of 10 N, 20 N, and 30 N. Furthermore, electrochemical corrosion performance of the coating, substrate and reference (A2 tool steel) in 3.5 wt.% NaCl solution was investigated using a potentiodynamic polarization test. Electrochemical parameters obtained from the resulting Tafel plots were used in calculating the corrosion rates of Fe-based BMG coating, substrate material and reference material. The microstructure, morphology and chemical composition of the resulting worn surfaces were examined using surface profilometry, scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) to determine the wear characteristics and wear mechanisms. The surfaces of the corroded test specimens were also examined using SEM. The results obtained showed that the cold spray process produced dense amorphous Fe-based BMG coating with an average thickness of 721 μm, porosity of 0.38% and hardness value of 698 HV0.3 (~ 8 times that of the substrate). The coated AA5086-H32 alloy exhibited the best wear resistance in dry and wet conditions, with wear rates less than that of the substrate by a magnitude of 10^2. XRD analysis of the worn surfaces of the Fe-MG coating showed that load-induced crystallization did not occur during the dry sliding wear test. Temperature measurements and EDS analysis showed evidence of room-temperature oxidation of the Fe-MG coating. The results of the potentiodynamic tests showed that AA5086-H32 had the lowest corrosion rate in 3.5 wt.% NaCl solution, followed by the coating and A2 tool steel. In conclusion, Fe-based BMG coatings offer a potential solution to expanding the use of aluminum alloys in applications requiring excellent wear resistance. Although the corrosion resistance of the coating was lower than the substrate, it performed better than A2 tool steel, a conventional material used in industrial wear applications.","abstract_html":"Aluminum alloys are vital to the aerospace, marine and automobile industries due to their lightweight, high specific strength, and good corrosion resistance. However, despite these favorable characteristics, they suffer rapid deterioration under severe friction and wear conditions, making surface engineering and coating imperative for use in several industrial applications where high wear resistance is a design requirement. Although several surface modification techniques and coating materials exist for aluminum alloys, bulk metallic glasses (BMGs) have gained attention as promising coating materials due to their superior mechanical properties and excellent wear and corrosion resistance. In this study, Fe87.55C0.75Si6.68Cr2.51B2.51 MG powder was deposited on AA5086-H32 plates at room temperature using a cold spray process. Optical microscopy, hardness testing, X-ray computed tomography (CT), and X-ray diffraction were employed to characterize the thickness, hardness, porosity, and amorphous nature of the resulting coating. Sliding wear tests were conducted against Si3N4 ceramic counterface in dry and wet (3.5 wt.% NaCl solution) conditions under three different applied loads of 10 N, 20 N, and 30 N. Furthermore, electrochemical corrosion performance of the coating, substrate and reference (A2 tool steel) in 3.5 wt.% NaCl solution was investigated using a potentiodynamic polarization test. Electrochemical parameters obtained from the resulting Tafel plots were used in calculating the corrosion rates of Fe-based BMG coating, substrate material and reference material. The microstructure, morphology and chemical composition of the resulting worn surfaces were examined using surface profilometry, scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) to determine the wear characteristics and wear mechanisms. The surfaces of the corroded test specimens were also examined using SEM. The results obtained showed that the cold spray process produced dense amorphous Fe-based BMG coating with an average thickness of 721 μm, porosity of 0.38% and hardness value of 698 HV0.3 (~ 8 times that of the substrate). The coated AA5086-H32 alloy exhibited the best wear resistance in dry and wet conditions, with wear rates less than that of the substrate by a magnitude of 10^2. XRD analysis of the worn surfaces of the Fe-MG coating showed that load-induced crystallization did not occur during the dry sliding wear test. Temperature measurements and EDS analysis showed evidence of room-temperature oxidation of the Fe-MG coating. The results of the potentiodynamic tests showed that AA5086-H32 had the lowest corrosion rate in 3.5 wt.% NaCl solution, followed by the coating and A2 tool steel. In conclusion, Fe-based BMG coatings offer a potential solution to expanding the use of aluminum alloys in applications requiring excellent wear resistance. Although the corrosion resistance of the coating was lower than the substrate, it performed better than A2 tool steel, a conventional material used in industrial wear applications.","abstract_has_math":false,"creators":["Adesola, Oluwasegun Emmanuel"],"institution":"University of Saskatchewan","degree_name":"Master of Science (M.Sc.)","degree_level":"Masters","degree_discipline":"Mechanical Engineering","degree_department":"Mechanical Engineering","school":null,"contributors":[],"advisors":["Oguocha, Ikechukwuka"],"committee_chairs":[],"committee_members":["Cree, Duncan duncan.cree@usask.ca","Odeshi, Akindele","Evitts, Richard"],"year":2024,"date_issued":"2024-01-15","date_published":"2024-01-15","updated_at":"2026-11-19T10:13:52Z","subjects":["Bulk metallic glasses (BMGs), Iron-based BMGs, Cold spray, Coatings, Wear, Corrosion, AA5086-H32"],"languages":["en"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[{"key":"person:identifier.orcid","label":"ORCID","values":["0009-0003-5407-7599"],"render_values":[{"text":"0009-0003-5407-7599","href":"https://orcid.org/0009-0003-5407-7599","code":true}]}]},"links":{"outbound_url":"https://hdl.handle.net/10388/15432","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/10388/15432","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","access_status":"embargoed","embargo_until":"2025-01-15","access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Asask%3Aoai%3Aharvest.usask.ca%3A10388%2F15432","prefix":"oai_dc"},"source_record":{"url":"https://harvest.usask.ca/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Aharvest.usask.ca%3A10388%2F15432","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Oguocha, Ikechukwuka"]},{"key":"dc:contributor.committeemember","label":"Committee Member","values":["Cree, Duncan duncan.cree@usask.ca","Odeshi, Akindele","Evitts, Richard"]},{"key":"dc:creator","label":"Author","values":["Adesola, Oluwasegun Emmanuel"]},{"key":"person:identifier.orcid","label":"ORCID","values":["0009-0003-5407-7599"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2024-01-16T02:53:07Z"]},{"key":"dc:date.copyright","label":"Dc Date Copyright","values":["2023"]},{"key":"dc:date.created","label":"Dc Date Created","values":["2024-01"]},{"key":"dc:date.embargo","label":"Dc Date Embargo","values":["2025-01-15"]},{"key":"dc:date.issued","label":"Date","values":["2024-01-15"]},{"key":"dc:date.liftdate","label":"Dc Date Liftdate","values":["2025-01-15"]},{"key":"dc:date.submitted","label":"Dc Date Submitted","values":["January 2024"]},{"key":"dc:date.updated","label":"Dc Date Updated","values":["2024-01-16T02:53:07Z"]},{"key":"dc:type","label":"Dc Type","values":["Thesis","text"]},{"key":"thesis:degree_department","label":"Department","values":["Mechanical Engineering"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Mechanical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Masters"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science (M.Sc.)"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of Saskatchewan"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Bulk metallic glasses (BMGs), Iron-based BMGs, Cold spray, Coatings, Wear, Corrosion, AA5086-H32"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/10388/15432"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Aluminum alloys are vital to the aerospace, marine and automobile industries due to their lightweight, high specific strength, and good corrosion resistance. However, despite these favorable characteristics, they suffer rapid deterioration under severe friction and wear conditions, making surface engineering and coating imperative for use in several industrial applications where high wear resistance is a design requirement. Although several surface modification techniques and coating materials exist for aluminum alloys, bulk metallic glasses (BMGs) have gained attention as promising coating materials due to their superior mechanical properties and excellent wear and corrosion resistance. In this study, Fe87.55C0.75Si6.68Cr2.51B2.51 MG powder was deposited on AA5086-H32 plates at room temperature using a cold spray process. Optical microscopy, hardness testing, X-ray computed tomography (CT), and X-ray diffraction were employed to characterize the thickness, hardness, porosity, and amorphous nature of the resulting coating. Sliding wear tests were conducted against Si3N4 ceramic counterface in dry and wet (3.5 wt.% NaCl solution) conditions under three different applied loads of 10 N, 20 N, and 30 N. Furthermore, electrochemical corrosion performance of the coating, substrate and reference (A2 tool steel) in 3.5 wt.% NaCl solution was investigated using a potentiodynamic polarization test. Electrochemical parameters obtained from the resulting Tafel plots were used in calculating the corrosion rates of Fe-based BMG coating, substrate material and reference material. The microstructure, morphology and chemical composition of the resulting worn surfaces were examined using surface profilometry, scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) to determine the wear characteristics and wear mechanisms. The surfaces of the corroded test specimens were also examined using SEM. The results obtained showed that the cold spray process produced dense amorphous Fe-based BMG coating with an average thickness of 721 μm, porosity of 0.38% and hardness value of 698 HV0.3 (~ 8 times that of the substrate). The coated AA5086-H32 alloy exhibited the best wear resistance in dry and wet conditions, with wear rates less than that of the substrate by a magnitude of 10^2. XRD analysis of the worn surfaces of the Fe-MG coating showed that load-induced crystallization did not occur during the dry sliding wear test. Temperature measurements and EDS analysis showed evidence of room-temperature oxidation of the Fe-MG coating. The results of the potentiodynamic tests showed that AA5086-H32 had the lowest corrosion rate in 3.5 wt.% NaCl solution, followed by the coating and A2 tool steel. In conclusion, Fe-based BMG coatings offer a potential solution to expanding the use of aluminum alloys in applications requiring excellent wear resistance. Although the corrosion resistance of the coating was lower than the substrate, it performed better than A2 tool steel, a conventional material used in industrial wear applications."]},{"key":"dc:format.mimetype","label":"Dc Format Mimetype","values":["application/pdf"]},{"key":"dc:title","label":"Title","values":["Tribological and Corrosion Behavior of Cold Sprayed Fe-Based Bulk Metallic Glass Coating on Aluminum Alloy"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:contributor.advisor":["Oguocha, Ikechukwuka"],"dc:contributor.committeemember":["Cree, Duncan duncan.cree@usask.ca","Odeshi, Akindele","Evitts, Richard"],"dc:creator":["Adesola, Oluwasegun Emmanuel"],"dc:date.accessioned":["2024-01-16T02:53:07Z"],"dc:date.copyright":["2023"],"dc:date.created":["2024-01"],"dc:date.embargo":["2025-01-15"],"dc:date.issued":["2024-01-15"],"dc:date.liftdate":["2025-01-15"],"dc:date.submitted":["January 2024"],"dc:date.updated":["2024-01-16T02:53:07Z"],"dc:description.abstract":["Aluminum alloys are vital to the aerospace, marine and automobile industries due to their lightweight, high specific strength, and good corrosion resistance. However, despite these favorable characteristics, they suffer rapid deterioration under severe friction and wear conditions, making surface engineering and coating imperative for use in several industrial applications where high wear resistance is a design requirement. Although several surface modification techniques and coating materials exist for aluminum alloys, bulk metallic glasses (BMGs) have gained attention as promising coating materials due to their superior mechanical properties and excellent wear and corrosion resistance. In this study, Fe87.55C0.75Si6.68Cr2.51B2.51 MG powder was deposited on AA5086-H32 plates at room temperature using a cold spray process. Optical microscopy, hardness testing, X-ray computed tomography (CT), and X-ray diffraction were employed to characterize the thickness, hardness, porosity, and amorphous nature of the resulting coating. Sliding wear tests were conducted against Si3N4 ceramic counterface in dry and wet (3.5 wt.% NaCl solution) conditions under three different applied loads of 10 N, 20 N, and 30 N. Furthermore, electrochemical corrosion performance of the coating, substrate and reference (A2 tool steel) in 3.5 wt.% NaCl solution was investigated using a potentiodynamic polarization test. Electrochemical parameters obtained from the resulting Tafel plots were used in calculating the corrosion rates of Fe-based BMG coating, substrate material and reference material. The microstructure, morphology and chemical composition of the resulting worn surfaces were examined using surface profilometry, scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) to determine the wear characteristics and wear mechanisms. The surfaces of the corroded test specimens were also examined using SEM. The results obtained showed that the cold spray process produced dense amorphous Fe-based BMG coating with an average thickness of 721 μm, porosity of 0.38% and hardness value of 698 HV0.3 (~ 8 times that of the substrate). The coated AA5086-H32 alloy exhibited the best wear resistance in dry and wet conditions, with wear rates less than that of the substrate by a magnitude of 10^2. XRD analysis of the worn surfaces of the Fe-MG coating showed that load-induced crystallization did not occur during the dry sliding wear test. Temperature measurements and EDS analysis showed evidence of room-temperature oxidation of the Fe-MG coating. The results of the potentiodynamic tests showed that AA5086-H32 had the lowest corrosion rate in 3.5 wt.% NaCl solution, followed by the coating and A2 tool steel. In conclusion, Fe-based BMG coatings offer a potential solution to expanding the use of aluminum alloys in applications requiring excellent wear resistance. Although the corrosion resistance of the coating was lower than the substrate, it performed better than A2 tool steel, a conventional material used in industrial wear applications."],"dc:format.mimetype":["application/pdf"],"dc:identifier.uri":["https://hdl.handle.net/10388/15432"],"dc:language.iso":["en"],"dc:subject":["Bulk metallic glasses (BMGs), Iron-based BMGs, Cold spray, Coatings, Wear, Corrosion, AA5086-H32"],"dc:title":["Tribological and Corrosion Behavior of Cold Sprayed Fe-Based Bulk Metallic Glass Coating on Aluminum Alloy"],"dc:type":["Thesis","text"],"others:access_status":["open.access"],"person:identifier.orcid":["0009-0003-5407-7599"],"thesis:degree_department":["Mechanical Engineering"],"thesis:degree_discipline":["Mechanical Engineering"],"thesis:degree_level":["Masters"],"thesis:degree_name":["Master of Science (M.Sc.)"],"thesis:institution_name":["University of Saskatchewan"]},"updated_at":"2026-11-19T10:13:52Z"}