{"id":{"repo_id":"sdstate","oai_identifier":"oai:openprairie.sdstate.edu:etd2-3100"},"canonical_url":"https://search.ndltd.org/etd/sdstate/oai:openprairie.sdstate.edu:etd2-3100","repository":{"repo_id":"sdstate","name":"South Dakota State University","base_url":"https://openprairie.sdstate.edu/do/oai/"},"display":{"title":"Initial Light Induced Degradation of N-type Dendritic Web Photovoltaic Solar Modules","abstract":"Initial light induced degradation (ILID) has been observed in p-type single crystalline and multicrystalline solar cells. ILID is strongly correlated with high boron and oxygen content in the solar cell even though gallium-doped solar cells have experienced ILID. Recent theories suggest that n-type antimony-doped solar cells should be much less susceptible to ILID due to absence of boron. In addition, initial degradation of PV module of n-type solar cells has not been reported as of date. Using indoor solar simulation, PV modules containing n-type antimony-doped dendritic web silicon solar cells were studied for the presence of ILID. 1-V curve measurements were • made as the modules received their first light exposure. No degradation in V oc was observed, but a small amount of degradation up to 2% did appear in 15c and P max· The mechanism behind this very low level of degradation was unclear.","abstract_html":"Initial light induced degradation (ILID) has been observed in p-type single crystalline and multicrystalline solar cells. ILID is strongly correlated with high boron and oxygen content in the solar cell even though gallium-doped solar cells have experienced ILID. Recent theories suggest that n-type antimony-doped solar cells should be much less susceptible to ILID due to absence of boron. In addition, initial degradation of PV module of n-type solar cells has not been reported as of date. Using indoor solar simulation, PV modules containing n-type antimony-doped dendritic web silicon solar cells were studied for the presence of ILID. 1-V curve measurements were • made as the modules received their first light exposure. No degradation in V oc was observed, but a small amount of degradation up to 2% did appear in 15c and P max· The mechanism behind this very low level of degradation was unclear.","abstract_has_math":false,"creators":["Kim, Na-Young"],"institution":null,"degree_name":"Master of Science (MS)","degree_level":"Thesis - University Access Only","degree_discipline":"Electrical Engineering and Computer Science","degree_department":null,"school":null,"contributors":["Michael E. Ropp"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T09:06:03Z","subjects":[],"languages":[],"rights":[],"rights_urls":["http://rightsstatements.org/vocab/InC/1.0/"],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://openprairie.sdstate.edu/etd2/2087","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://openprairie.sdstate.edu/etd2/2087","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://openprairie.sdstate.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Aopenprairie.sdstate.edu%3Aetd2-3100","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Michael E. Ropp"]},{"key":"dc:creator","label":"Author","values":["Kim, Na-Young"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.available","label":"Dc Date Available","values":["2026-05-27T07:00:00Z"]},{"key":"dc:date.created","label":"Dc Date Created","values":["2006-01-01T08:00:00Z"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Electrical Engineering and Computer Science"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Thesis - University Access Only"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science (MS)"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:rights","label":"Dc Rights","values":["http://rightsstatements.org/vocab/InC/1.0/"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://openprairie.sdstate.edu/etd2/2087"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Initial light induced degradation (ILID) has been observed in p-type single crystalline and multicrystalline solar cells. ILID is strongly correlated with high boron and oxygen content in the solar cell even though gallium-doped solar cells have experienced ILID. Recent theories suggest that n-type antimony-doped solar cells should be much less susceptible to ILID due to absence of boron. In addition, initial degradation of PV module of n-type solar cells has not been reported as of date. Using indoor solar simulation, PV modules containing n-type antimony-doped dendritic web silicon solar cells were studied for the presence of ILID. 1-V curve measurements were • made as the modules received their first light exposure. No degradation in V oc was observed, but a small amount of degradation up to 2% did appear in 15c and P max· The mechanism behind this very low level of degradation was unclear."]},{"key":"dc:title","label":"Title","values":["Initial Light Induced Degradation of N-type Dendritic Web Photovoltaic Solar Modules"]}]}],"canonical_facts":{"dc:contributor":["Michael E. Ropp"],"dc:creator":["Kim, Na-Young"],"dc:date.available":["2026-05-27T07:00:00Z"],"dc:date.created":["2006-01-01T08:00:00Z"],"dc:description.abstract":["Initial light induced degradation (ILID) has been observed in p-type single crystalline and multicrystalline solar cells. ILID is strongly correlated with high boron and oxygen content in the solar cell even though gallium-doped solar cells have experienced ILID. Recent theories suggest that n-type antimony-doped solar cells should be much less susceptible to ILID due to absence of boron. In addition, initial degradation of PV module of n-type solar cells has not been reported as of date. Using indoor solar simulation, PV modules containing n-type antimony-doped dendritic web silicon solar cells were studied for the presence of ILID. 1-V curve measurements were • made as the modules received their first light exposure. No degradation in V oc was observed, but a small amount of degradation up to 2% did appear in 15c and P max· The mechanism behind this very low level of degradation was unclear."],"dc:identifier":["https://openprairie.sdstate.edu/etd2/2087"],"dc:rights":["http://rightsstatements.org/vocab/InC/1.0/"],"dc:title":["Initial Light Induced Degradation of N-type Dendritic Web Photovoltaic Solar Modules"],"thesis:degree_discipline":["Electrical Engineering and Computer Science"],"thesis:degree_level":["Thesis - University Access Only"],"thesis:degree_name":["Master of Science (MS)"]},"updated_at":"2026-11-19T09:06:03Z"}