{"id":{"repo_id":"sjsu","oai_identifier":"oai:scholarworks.sjsu.edu:etd_theses-7834"},"canonical_url":"https://search.ndltd.org/etd/sjsu/oai:scholarworks.sjsu.edu:etd_theses-7834","repository":{"repo_id":"sjsu","name":"San Jose State University","base_url":"https://scholarworks.sjsu.edu/do/oai/"},"display":{"title":"The Effect of Surface Treatment on Nickel Leaching from Nitinol","abstract":"Nitinol is widely used as a biomaterial for implantable medical devices but can be susceptible to nickel leaching. Our research was aimed at determining nickel leaching from surface treated Nitinol samples, treated as follows: mechanical polishing (untreated), oxidation, and nitriding+oxidation (5 different nitriding temperatures). Five specimens from each category were immersed in 40 mL PBS solution and incubated at 37°C over 91 days. Nickel concentration readings were taken at regular intervals. After 91 days, the average nickel concentration in the PBS solution was (a) 0.223 mg/L, SD 0.017, untreated, (b) 7.68 mg/L, SD 6.405, 1000°C nitriding+oxidation, and (c) 3.914 mg/L, SD 1.78, oxidation-only. The concentration readings had large standard deviations implying differences in surface characteristics after treatment. The increased nickel leaching from treated samples was thought to be due to atomic diffusion and exposure of the nickel-rich sublayers to PBS after oxide layer delamination. These sublayers formed after formation of thick (>1 µm) TiO2 layers during oxidation.","abstract_html":"Nitinol is widely used as a biomaterial for implantable medical devices but can be susceptible to nickel leaching. Our research was aimed at determining nickel leaching from surface treated Nitinol samples, treated as follows: mechanical polishing (untreated), oxidation, and nitriding+oxidation (5 different nitriding temperatures). Five specimens from each category were immersed in 40 mL PBS solution and incubated at 37°C over 91 days. Nickel concentration readings were taken at regular intervals. After 91 days, the average nickel concentration in the PBS solution was (a) 0.223 mg/L, SD 0.017, untreated, (b) 7.68 mg/L, SD 6.405, 1000°C nitriding+oxidation, and (c) 3.914 mg/L, SD 1.78, oxidation-only. The concentration readings had large standard deviations implying differences in surface characteristics after treatment. The increased nickel leaching from treated samples was thought to be due to atomic diffusion and exposure of the nickel-rich sublayers to PBS after oxide layer delamination. These sublayers formed after formation of thick (&gt;1 µm) TiO2 layers during oxidation.","abstract_has_math":false,"creators":["Madamba, Daniel Lawrence Leobrera"],"institution":null,"degree_name":"Master of Science (MS)","degree_level":null,"degree_discipline":"General Engineering","degree_department":null,"school":null,"contributors":["Guna S. Selvaduray"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-26T13:59:51Z","subjects":["Nickel Leaching","Nitinol","Nitriding","Oxidation","Surface Modification"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["https://scholarworks.sjsu.edu/etd_theses/4287"],"render_values":[{"text":"https://scholarworks.sjsu.edu/etd_theses/4287","href":"https://scholarworks.sjsu.edu/etd_theses/4287","code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://doi.org/10.31979/etd.uyvh-6h8x","outbound_label":"DOI","outbound_source":"dc:identifier","record_url":"https://doi.org/10.31979/etd.uyvh-6h8x","record_label":"Repository record","record_kind":"doi","record_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Asjsu%3Aoai%3Ascholarworks.sjsu.edu%3Aetd_theses-7834","prefix":"oai_dc"},"source_record":{"url":"https://scholarworks.sjsu.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Ascholarworks.sjsu.edu%3Aetd_theses-7834","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Guna S. Selvaduray"]},{"key":"dc:creator","label":"Author","values":["Madamba, Daniel Lawrence Leobrera"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["2013-01-01T08:00:00Z"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["General Engineering"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science (MS)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Nickel Leaching","Nitinol","Nitriding","Oxidation","Surface Modification"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://doi.org/10.31979/etd.uyvh-6h8x","https://scholarworks.sjsu.edu/etd_theses/4287"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Nitinol is widely used as a biomaterial for implantable medical devices but can be susceptible to nickel leaching. Our research was aimed at determining nickel leaching from surface treated Nitinol samples, treated as follows: mechanical polishing (untreated), oxidation, and nitriding+oxidation (5 different nitriding temperatures). Five specimens from each category were immersed in 40 mL PBS solution and incubated at 37°C over 91 days. Nickel concentration readings were taken at regular intervals. After 91 days, the average nickel concentration in the PBS solution was (a) 0.223 mg/L, SD 0.017, untreated, (b) 7.68 mg/L, SD 6.405, 1000°C nitriding+oxidation, and (c) 3.914 mg/L, SD 1.78, oxidation-only. The concentration readings had large standard deviations implying differences in surface characteristics after treatment. The increased nickel leaching from treated samples was thought to be due to atomic diffusion and exposure of the nickel-rich sublayers to PBS after oxide layer delamination. These sublayers formed after formation of thick (>1 µm) TiO2 layers during oxidation."]},{"key":"dc:title","label":"Title","values":["The Effect of Surface Treatment on Nickel Leaching from Nitinol"]}]}],"canonical_facts":{"dc:contributor":["Guna S. Selvaduray"],"dc:creator":["Madamba, Daniel Lawrence Leobrera"],"dc:date.created":["2013-01-01T08:00:00Z"],"dc:description.abstract":["Nitinol is widely used as a biomaterial for implantable medical devices but can be susceptible to nickel leaching. Our research was aimed at determining nickel leaching from surface treated Nitinol samples, treated as follows: mechanical polishing (untreated), oxidation, and nitriding+oxidation (5 different nitriding temperatures). Five specimens from each category were immersed in 40 mL PBS solution and incubated at 37°C over 91 days. Nickel concentration readings were taken at regular intervals. After 91 days, the average nickel concentration in the PBS solution was (a) 0.223 mg/L, SD 0.017, untreated, (b) 7.68 mg/L, SD 6.405, 1000°C nitriding+oxidation, and (c) 3.914 mg/L, SD 1.78, oxidation-only. The concentration readings had large standard deviations implying differences in surface characteristics after treatment. The increased nickel leaching from treated samples was thought to be due to atomic diffusion and exposure of the nickel-rich sublayers to PBS after oxide layer delamination. These sublayers formed after formation of thick (>1 µm) TiO2 layers during oxidation."],"dc:identifier":["https://doi.org/10.31979/etd.uyvh-6h8x","https://scholarworks.sjsu.edu/etd_theses/4287"],"dc:subject":["Nickel Leaching","Nitinol","Nitriding","Oxidation","Surface Modification"],"dc:title":["The Effect of Surface Treatment on Nickel Leaching from Nitinol"],"dc:type":["Thesis"],"thesis:degree_discipline":["General Engineering"],"thesis:degree_name":["Master of Science (MS)"]},"updated_at":"2026-11-26T13:59:51Z"}