{"id":{"repo_id":"soton","oai_identifier":"oai:eprints.soton.ac.uk:432273"},"canonical_url":"https://search.ndltd.org/etd/soton/oai:eprints.soton.ac.uk:432273","repository":{"repo_id":"soton","name":"University of Southampton","base_url":"https://eprints.soton.ac.uk/cgi/oai2"},"display":{"title":"Tantalum pentoxide integrated photonic devices","abstract":"This thesis investigates tantalum pentoxide (Ta<sub>2</sub>O<sub>5</sub>) as a material for realising integrated photonic devices on a silicon platform, as a basis for realising photonics integrated circuits with multiple functionalities on a single monolithic chip. In particular, achieving gain and lasing, and electro-optic functionalities were studied. To further investigate the integration of these functionalities onto a silicon platform, a grating-assisted coupler was explored.<br/><br/>Ta<sub>2</sub>O<sub>5</sub> thin films were deposited on oxidised silicon wafer using RF sputtering and waveguides were realised using lithography and ion beam milling. An optimisation of the etching process to reduce waveguide sidewall roughness was performed.<br/><br/>Thulium-doped Ta<sub>2</sub>O<sub>5</sub> was investigated to provide gain and lasing at around 2 μm by pumping at around 790 nm. With a thulium-doping concentration of 9x10<sup>20</sup> ions/cm<sup>3</sup>, the highest peak photoluminescence power and lifetime was achieved with sample annealed at 650 °C for 12 hours. The excited-state lifetime of this sample was 477 ± 40 μs. Emission centred around 1.85 μm and a high emission cross-section of 2.99x10<sup>-20</sup> cm<sup>2</sup> was attained. The absorption cross-section were 8.05x10<sup>-21</sup> cm<sup>2</sup> at 792 nm and 1.09x10<sup>-20</sup> cm<sup>2</sup> at a wavelength of 1756 nm.<br/><br/>Second-order nonlinearity was achieved in Ta<sub>2</sub>O<sub>5</sub> by thermal poling, 0.46 and 0.34 pm/V was achieved with sodium-doped and undoped Ta<sub>2</sub>O<sub>5</sub> respectively. The effect of sodium-doping and annealing on the induced second-order nonlinearity was studied.<br/><br/>A grating-assisted coupler was designed and fabricated to couple between 750 by 750 nm Ta<sub>2</sub>O<sub>5</sub> and a 400 by 250 nm Si channel waveguides. Simulations show that a grating period of 2.361 μm was required for coupling to occur.<br/><br/>The results show that tantalum pentoxide is a promising medium for realising integrated lasers and amplifiers, electro-optic applications on a silicon platform.","abstract_html":"This thesis investigates tantalum pentoxide (Ta&lt;sub&gt;2&lt;/sub&gt;O&lt;sub&gt;5&lt;/sub&gt;) as a material for realising integrated photonic devices on a silicon platform, as a basis for realising photonics integrated circuits with multiple functionalities on a single monolithic chip. In particular, achieving gain and lasing, and electro-optic functionalities were studied. To further investigate the integration of these functionalities onto a silicon platform, a grating-assisted coupler was explored.&lt;br/&gt;&lt;br/&gt;Ta&lt;sub&gt;2&lt;/sub&gt;O&lt;sub&gt;5&lt;/sub&gt; thin films were deposited on oxidised silicon wafer using RF sputtering and waveguides were realised using lithography and ion beam milling. An optimisation of the etching process to reduce waveguide sidewall roughness was performed.&lt;br/&gt;&lt;br/&gt;Thulium-doped Ta&lt;sub&gt;2&lt;/sub&gt;O&lt;sub&gt;5&lt;/sub&gt; was investigated to provide gain and lasing at around 2 μm by pumping at around 790 nm. With a thulium-doping concentration of 9x10&lt;sup&gt;20&lt;/sup&gt; ions/cm&lt;sup&gt;3&lt;/sup&gt;, the highest peak photoluminescence power and lifetime was achieved with sample annealed at 650 °C for 12 hours. The excited-state lifetime of this sample was 477 ± 40 μs. Emission centred around 1.85 μm and a high emission cross-section of 2.99x10&lt;sup&gt;-20&lt;/sup&gt; cm&lt;sup&gt;2&lt;/sup&gt; was attained. The absorption cross-section were 8.05x10&lt;sup&gt;-21&lt;/sup&gt; cm&lt;sup&gt;2&lt;/sup&gt; at 792 nm and 1.09x10&lt;sup&gt;-20&lt;/sup&gt; cm&lt;sup&gt;2&lt;/sup&gt; at a wavelength of 1756 nm.&lt;br/&gt;&lt;br/&gt;Second-order nonlinearity was achieved in Ta&lt;sub&gt;2&lt;/sub&gt;O&lt;sub&gt;5&lt;/sub&gt; by thermal poling, 0.46 and 0.34 pm/V was achieved with sodium-doped and undoped Ta&lt;sub&gt;2&lt;/sub&gt;O&lt;sub&gt;5&lt;/sub&gt; respectively. The effect of sodium-doping and annealing on the induced second-order nonlinearity was studied.&lt;br/&gt;&lt;br/&gt;A grating-assisted coupler was designed and fabricated to couple between 750 by 750 nm Ta&lt;sub&gt;2&lt;/sub&gt;O&lt;sub&gt;5&lt;/sub&gt; and a 400 by 250 nm Si channel waveguides. Simulations show that a grating period of 2.361 μm was required for coupling to occur.&lt;br/&gt;&lt;br/&gt;The results show that tantalum pentoxide is a promising medium for realising integrated lasers and amplifiers, electro-optic applications on a silicon platform.","abstract_has_math":false,"creators":["Tong, Amy Sen Kay"],"institution":"University of Southampton","degree_name":"Ph.D.","degree_level":"doctoral","degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":["Wilkinson, James S."],"committee_chairs":[],"committee_members":[],"year":2019,"date_issued":"2019-03","date_published":"2019-03","updated_at":"2026-11-19T09:33:57Z","subjects":[],"languages":["English","eng"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[{"key":"person:identifier.orcid","label":"ORCID","values":["0000000347121697"],"render_values":[{"text":"0000-0003-4712-1697","href":"https://orcid.org/0000-0003-4712-1697","code":true}]}]},"links":{"outbound_url":null,"outbound_label":null,"outbound_source":null,"record_url":null,"record_label":null,"record_kind":null,"record_source":null,"download_url":"https://eprints.soton.ac.uk/id/eprint/432273/1/Final_thesis.pdf","download_label":"Download PDF","download_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://eprints.soton.ac.uk/cgi/oai2?verb=GetRecord&metadataPrefix=uketd_dc&identifier=oai%3Aeprints.soton.ac.uk%3A432273","prefix":"uketd_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Wilkinson, James S."]},{"key":"dc:creator","label":"Author","values":["Tong, Amy Sen Kay"]},{"key":"person:identifier.orcid","label":"ORCID","values":["0000000347121697"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2019-03"]},{"key":"dc:date.issued","label":"Date","values":["2019-03"]},{"key":"dc:publisher.commercial","label":"Dc Publisher Commercial","values":["University of Southampton"]},{"key":"dc:publisher.department","label":"Dc Publisher Department","values":["Zepler Institute for Photonics and Nanoelectronics"]},{"key":"dc:publisher.institution","label":"Dc Publisher Institution","values":["University of Southampton"]},{"key":"dc:relation.isreferencedby","label":"Dc Relation Isreferencedby","values":["https://eprints.soton.ac.uk/id/eprint/432273/"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"dc:type.qualificationlevel","label":"Dc Type Qualificationlevel","values":["doctoral"]},{"key":"dc:type.qualificationname","label":"Dc Type Qualificationname","values":["Ph.D."]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:language.dcterms_iso639_2","label":"Language (ISO 639-2)","values":["eng"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://eprints.soton.ac.uk/id/eprint/432273/1/Final_thesis.pdf"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["This thesis investigates tantalum pentoxide (Ta<sub>2</sub>O<sub>5</sub>) as a material for realising integrated photonic devices on a silicon platform, as a basis for realising photonics integrated circuits with multiple functionalities on a single monolithic chip. In particular, achieving gain and lasing, and electro-optic functionalities were studied. To further investigate the integration of these functionalities onto a silicon platform, a grating-assisted coupler was explored.<br/><br/>Ta<sub>2</sub>O<sub>5</sub> thin films were deposited on oxidised silicon wafer using RF sputtering and waveguides were realised using lithography and ion beam milling. An optimisation of the etching process to reduce waveguide sidewall roughness was performed.<br/><br/>Thulium-doped Ta<sub>2</sub>O<sub>5</sub> was investigated to provide gain and lasing at around 2 μm by pumping at around 790 nm. With a thulium-doping concentration of 9x10<sup>20</sup> ions/cm<sup>3</sup>, the highest peak photoluminescence power and lifetime was achieved with sample annealed at 650 °C for 12 hours. The excited-state lifetime of this sample was 477 ± 40 μs. Emission centred around 1.85 μm and a high emission cross-section of 2.99x10<sup>-20</sup> cm<sup>2</sup> was attained. The absorption cross-section were 8.05x10<sup>-21</sup> cm<sup>2</sup> at 792 nm and 1.09x10<sup>-20</sup> cm<sup>2</sup> at a wavelength of 1756 nm.<br/><br/>Second-order nonlinearity was achieved in Ta<sub>2</sub>O<sub>5</sub> by thermal poling, 0.46 and 0.34 pm/V was achieved with sodium-doped and undoped Ta<sub>2</sub>O<sub>5</sub> respectively. The effect of sodium-doping and annealing on the induced second-order nonlinearity was studied.<br/><br/>A grating-assisted coupler was designed and fabricated to couple between 750 by 750 nm Ta<sub>2</sub>O<sub>5</sub> and a 400 by 250 nm Si channel waveguides. Simulations show that a grating period of 2.361 μm was required for coupling to occur.<br/><br/>The results show that tantalum pentoxide is a promising medium for realising integrated lasers and amplifiers, electro-optic applications on a silicon platform."]},{"key":"dc:format","label":"Dc Format","values":["text"]},{"key":"dcterms:accessrights","label":"Dcterms Accessrights","values":["public"]},{"key":"dc:title","label":"Title","values":["Tantalum pentoxide integrated photonic devices"]}]}],"canonical_facts":{"dc:contributor.advisor":["Wilkinson, James S."],"dc:creator":["Tong, Amy Sen Kay"],"dc:date":["2019-03"],"dc:date.issued":["2019-03"],"dc:description.abstract":["This thesis investigates tantalum pentoxide (Ta<sub>2</sub>O<sub>5</sub>) as a material for realising integrated photonic devices on a silicon platform, as a basis for realising photonics integrated circuits with multiple functionalities on a single monolithic chip. In particular, achieving gain and lasing, and electro-optic functionalities were studied. To further investigate the integration of these functionalities onto a silicon platform, a grating-assisted coupler was explored.<br/><br/>Ta<sub>2</sub>O<sub>5</sub> thin films were deposited on oxidised silicon wafer using RF sputtering and waveguides were realised using lithography and ion beam milling. An optimisation of the etching process to reduce waveguide sidewall roughness was performed.<br/><br/>Thulium-doped Ta<sub>2</sub>O<sub>5</sub> was investigated to provide gain and lasing at around 2 μm by pumping at around 790 nm. With a thulium-doping concentration of 9x10<sup>20</sup> ions/cm<sup>3</sup>, the highest peak photoluminescence power and lifetime was achieved with sample annealed at 650 °C for 12 hours. The excited-state lifetime of this sample was 477 ± 40 μs. Emission centred around 1.85 μm and a high emission cross-section of 2.99x10<sup>-20</sup> cm<sup>2</sup> was attained. The absorption cross-section were 8.05x10<sup>-21</sup> cm<sup>2</sup> at 792 nm and 1.09x10<sup>-20</sup> cm<sup>2</sup> at a wavelength of 1756 nm.<br/><br/>Second-order nonlinearity was achieved in Ta<sub>2</sub>O<sub>5</sub> by thermal poling, 0.46 and 0.34 pm/V was achieved with sodium-doped and undoped Ta<sub>2</sub>O<sub>5</sub> respectively. The effect of sodium-doping and annealing on the induced second-order nonlinearity was studied.<br/><br/>A grating-assisted coupler was designed and fabricated to couple between 750 by 750 nm Ta<sub>2</sub>O<sub>5</sub> and a 400 by 250 nm Si channel waveguides. Simulations show that a grating period of 2.361 μm was required for coupling to occur.<br/><br/>The results show that tantalum pentoxide is a promising medium for realising integrated lasers and amplifiers, electro-optic applications on a silicon platform."],"dc:format":["text"],"dc:identifier.uri":["https://eprints.soton.ac.uk/id/eprint/432273/1/Final_thesis.pdf"],"dc:language":["English"],"dc:language.dcterms_iso639_2":["eng"],"dc:publisher.commercial":["University of Southampton"],"dc:publisher.department":["Zepler Institute for Photonics and Nanoelectronics"],"dc:publisher.institution":["University of Southampton"],"dc:relation.isreferencedby":["https://eprints.soton.ac.uk/id/eprint/432273/"],"dcterms:accessrights":["public"],"dc:title":["Tantalum pentoxide integrated photonic devices"],"dc:type":["Thesis"],"dc:type.qualificationlevel":["doctoral"],"dc:type.qualificationname":["Ph.D."],"person:identifier.orcid":["0000000347121697"]},"updated_at":"2026-11-19T09:33:57Z"}