{"id":{"repo_id":"soton","oai_identifier":"oai:eprints.soton.ac.uk:497360"},"canonical_url":"https://search.ndltd.org/etd/soton/oai:eprints.soton.ac.uk:497360","repository":{"repo_id":"soton","name":"University of Southampton","base_url":"https://eprints.soton.ac.uk/cgi/oai2"},"display":{"title":"Development of erbium-doped and bismuth-doped optical fibres for wideband and high-performance amplifiers for telecommunication applications","abstract":"To support the continuously growing demand for data-carrying capacity of optical fibres in telecommunications, developing efficient fibre amplifiers for extended wavelength bands beyond traditional C- and L-bands is crucial. The O-, E-, S-bands (1260-1530 nm), and the extended L-band (1615-1625 nm), within the low-loss transmission window of standard silica fibres, hold significant research and commercial potential. Erbium (Er)-doped fibre amplifiers (EDFAs) are well-studied for the C- and L-bands, but require enhancements in gain flatness, noise, efficiency, and bandwidth extension beyond 1615 nm. Bismuth (Bi)-doped silica fibres, with their ultra-wide near-infrared (NIR) luminescence from various Bi active centres (BACs), offer promising potential for developing wideband Bi-doped fibre amplifiers (BDFAs).<br/>In this thesis, I fabricated Er-doped fibres using the modified chemical vapour deposition (MCVD)-solution doping technique by tailoring the glass core compositions to favour L-band amplification. Fibre spectroscopic properties were characterised including refractive index profile, absorption, background loss, unsaturable loss, fluorescence, lifetime, on/off gain, and Er3+ cross-sections. Using the fabricated EDFs, I developed L-band amplifiers to achieve a high gain of ≥20 dB from 1565-1625 nm in a double-pass configuration, a flat gain ripple of ±0.7 dB from 1580-1615 nm by forming AlPO4 units in the fibre and pumped at 980 nm, an extended operating wavelength up to 1628 nm with a 13.6 dB gain by forming AlPO4 units and pumped at 1480 nm. Er/Yb co-doped fibre amplifier (EYDFA) was built up utilising 1480 nm core-pumping to shorten the L-band device length to 23 m.<br/>High-performance BDFAs were developed using BDFs fabricated by other fabricators. Using Bi-doped germano-silicate fibres (BGSFs) and phospho-silicate fibres (BPSFs), a high gain and high gain-per-unit-length BDFA was demonstrated in the E+S band with shortened device lengths (25.5 m to 48 m), and a high-gain ultra-wideband BDFA was presented in the O+E+S band with a 140 nm 20 dB-gain bandwidth for a -23 dBm input signal, respectively. Spectroscopic properties of various BACs were analysed, and a fully integrated, compact BDFA device box was developed.<br/>Moreover, robust amplifiers were developed to adapt to extreme temperatures and irradiation conditions. For EDFAs, a hybrid configuration was proposed to balance temperature stability and L-band gain, achieving low noise and temperature-insensitive gain flatness from 1585-1615 nm. Radiation tolerance was characterised in various core-composition EDFs after gamma-irradiation to develop radiation-resistant EDFAs in the C- or L-band using cerium (Ce) co-doping. In addition, a radiation-resistant E+S band BDFA was developed with a 35 dB post-irradiation gain. <br/>","abstract_html":"To support the continuously growing demand for data-carrying capacity of optical fibres in telecommunications, developing efficient fibre amplifiers for extended wavelength bands beyond traditional C- and L-bands is crucial. The O-, E-, S-bands (1260-1530 nm), and the extended L-band (1615-1625 nm), within the low-loss transmission window of standard silica fibres, hold significant research and commercial potential. Erbium (Er)-doped fibre amplifiers (EDFAs) are well-studied for the C- and L-bands, but require enhancements in gain flatness, noise, efficiency, and bandwidth extension beyond 1615 nm. Bismuth (Bi)-doped silica fibres, with their ultra-wide near-infrared (NIR) luminescence from various Bi active centres (BACs), offer promising potential for developing wideband Bi-doped fibre amplifiers (BDFAs).&lt;br/&gt;In this thesis, I fabricated Er-doped fibres using the modified chemical vapour deposition (MCVD)-solution doping technique by tailoring the glass core compositions to favour L-band amplification. Fibre spectroscopic properties were characterised including refractive index profile, absorption, background loss, unsaturable loss, fluorescence, lifetime, on/off gain, and Er3+ cross-sections. Using the fabricated EDFs, I developed L-band amplifiers to achieve a high gain of ≥20 dB from 1565-1625 nm in a double-pass configuration, a flat gain ripple of ±0.7 dB from 1580-1615 nm by forming AlPO4 units in the fibre and pumped at 980 nm, an extended operating wavelength up to 1628 nm with a 13.6 dB gain by forming AlPO4 units and pumped at 1480 nm. Er/Yb co-doped fibre amplifier (EYDFA) was built up utilising 1480 nm core-pumping to shorten the L-band device length to 23 m.&lt;br/&gt;High-performance BDFAs were developed using BDFs fabricated by other fabricators. Using Bi-doped germano-silicate fibres (BGSFs) and phospho-silicate fibres (BPSFs), a high gain and high gain-per-unit-length BDFA was demonstrated in the E+S band with shortened device lengths (25.5 m to 48 m), and a high-gain ultra-wideband BDFA was presented in the O+E+S band with a 140 nm 20 dB-gain bandwidth for a -23 dBm input signal, respectively. Spectroscopic properties of various BACs were analysed, and a fully integrated, compact BDFA device box was developed.&lt;br/&gt;Moreover, robust amplifiers were developed to adapt to extreme temperatures and irradiation conditions. For EDFAs, a hybrid configuration was proposed to balance temperature stability and L-band gain, achieving low noise and temperature-insensitive gain flatness from 1585-1615 nm. Radiation tolerance was characterised in various core-composition EDFs after gamma-irradiation to develop radiation-resistant EDFAs in the C- or L-band using cerium (Ce) co-doping. In addition, a radiation-resistant E+S band BDFA was developed with a 35 dB post-irradiation gain. &lt;br/&gt;","abstract_has_math":false,"creators":["Zhai, Ziwei"],"institution":"University of Southampton","degree_name":"Ph.D.","degree_level":"doctoral","degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":["Sahu, Jayanta","Nilsson, Johan"],"committee_chairs":[],"committee_members":[],"year":2025,"date_issued":"2025-01","date_published":"2025-01","updated_at":"2026-11-19T09:55:13Z","subjects":[],"languages":["English","eng"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[{"key":"person:identifier.orcid","label":"ORCID","values":["0000000171287326","0000000335606152","0000000316917959"],"render_values":[{"text":"0000-0001-7128-7326","href":"https://orcid.org/0000-0001-7128-7326","code":true},{"text":"0000-0003-3560-6152","href":"https://orcid.org/0000-0003-3560-6152","code":true},{"text":"0000-0003-1691-7959","href":"https://orcid.org/0000-0003-1691-7959","code":true}]}]},"links":{"outbound_url":null,"outbound_label":null,"outbound_source":null,"record_url":null,"record_label":null,"record_kind":null,"record_source":null,"download_url":"https://eprints.soton.ac.uk/id/eprint/497360/1/THESIS_FINAL_ZZ.pdf","download_label":"Download PDF","download_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://eprints.soton.ac.uk/cgi/oai2?verb=GetRecord&metadataPrefix=uketd_dc&identifier=oai%3Aeprints.soton.ac.uk%3A497360","prefix":"uketd_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Sahu, Jayanta","Nilsson, Johan"]},{"key":"dc:creator","label":"Author","values":["Zhai, Ziwei"]},{"key":"person:identifier.orcid","label":"ORCID","values":["0000000171287326","0000000335606152","0000000316917959"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2025-01"]},{"key":"dc:date.issued","label":"Date","values":["2025-01"]},{"key":"dc:publisher.commercial","label":"Dc Publisher Commercial","values":["University of Southampton"]},{"key":"dc:publisher.department","label":"Dc Publisher Department","values":["Optoelectronics Research Centre"]},{"key":"dc:publisher.institution","label":"Dc Publisher Institution","values":["University of Southampton"]},{"key":"dc:relation.isreferencedby","label":"Dc Relation Isreferencedby","values":["https://eprints.soton.ac.uk/id/eprint/497360/"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"dc:type.qualificationlevel","label":"Dc Type Qualificationlevel","values":["doctoral"]},{"key":"dc:type.qualificationname","label":"Dc Type Qualificationname","values":["Ph.D."]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:language.dcterms_iso639_2","label":"Language (ISO 639-2)","values":["eng"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://eprints.soton.ac.uk/id/eprint/497360/1/THESIS_FINAL_ZZ.pdf","https://eprints.soton.ac.uk/id/eprint/497360/2/Final-thesis-submission-Examination-Ms-Ziwei-Zhai.pdf"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["To support the continuously growing demand for data-carrying capacity of optical fibres in telecommunications, developing efficient fibre amplifiers for extended wavelength bands beyond traditional C- and L-bands is crucial. The O-, E-, S-bands (1260-1530 nm), and the extended L-band (1615-1625 nm), within the low-loss transmission window of standard silica fibres, hold significant research and commercial potential. Erbium (Er)-doped fibre amplifiers (EDFAs) are well-studied for the C- and L-bands, but require enhancements in gain flatness, noise, efficiency, and bandwidth extension beyond 1615 nm. Bismuth (Bi)-doped silica fibres, with their ultra-wide near-infrared (NIR) luminescence from various Bi active centres (BACs), offer promising potential for developing wideband Bi-doped fibre amplifiers (BDFAs).<br/>In this thesis, I fabricated Er-doped fibres using the modified chemical vapour deposition (MCVD)-solution doping technique by tailoring the glass core compositions to favour L-band amplification. Fibre spectroscopic properties were characterised including refractive index profile, absorption, background loss, unsaturable loss, fluorescence, lifetime, on/off gain, and Er3+ cross-sections. Using the fabricated EDFs, I developed L-band amplifiers to achieve a high gain of ≥20 dB from 1565-1625 nm in a double-pass configuration, a flat gain ripple of ±0.7 dB from 1580-1615 nm by forming AlPO4 units in the fibre and pumped at 980 nm, an extended operating wavelength up to 1628 nm with a 13.6 dB gain by forming AlPO4 units and pumped at 1480 nm. Er/Yb co-doped fibre amplifier (EYDFA) was built up utilising 1480 nm core-pumping to shorten the L-band device length to 23 m.<br/>High-performance BDFAs were developed using BDFs fabricated by other fabricators. Using Bi-doped germano-silicate fibres (BGSFs) and phospho-silicate fibres (BPSFs), a high gain and high gain-per-unit-length BDFA was demonstrated in the E+S band with shortened device lengths (25.5 m to 48 m), and a high-gain ultra-wideband BDFA was presented in the O+E+S band with a 140 nm 20 dB-gain bandwidth for a -23 dBm input signal, respectively. Spectroscopic properties of various BACs were analysed, and a fully integrated, compact BDFA device box was developed.<br/>Moreover, robust amplifiers were developed to adapt to extreme temperatures and irradiation conditions. For EDFAs, a hybrid configuration was proposed to balance temperature stability and L-band gain, achieving low noise and temperature-insensitive gain flatness from 1585-1615 nm. Radiation tolerance was characterised in various core-composition EDFs after gamma-irradiation to develop radiation-resistant EDFAs in the C- or L-band using cerium (Ce) co-doping. In addition, a radiation-resistant E+S band BDFA was developed with a 35 dB post-irradiation gain. <br/>"]},{"key":"dc:format","label":"Dc Format","values":["text"]},{"key":"dcterms:accessrights","label":"Dcterms Accessrights","values":["public","staffonly"]},{"key":"dc:title","label":"Title","values":["Development of erbium-doped and bismuth-doped optical fibres for wideband and high-performance amplifiers for telecommunication applications"]}]}],"canonical_facts":{"dc:contributor.advisor":["Sahu, Jayanta","Nilsson, Johan"],"dc:creator":["Zhai, Ziwei"],"dc:date":["2025-01"],"dc:date.issued":["2025-01"],"dc:description.abstract":["To support the continuously growing demand for data-carrying capacity of optical fibres in telecommunications, developing efficient fibre amplifiers for extended wavelength bands beyond traditional C- and L-bands is crucial. The O-, E-, S-bands (1260-1530 nm), and the extended L-band (1615-1625 nm), within the low-loss transmission window of standard silica fibres, hold significant research and commercial potential. Erbium (Er)-doped fibre amplifiers (EDFAs) are well-studied for the C- and L-bands, but require enhancements in gain flatness, noise, efficiency, and bandwidth extension beyond 1615 nm. Bismuth (Bi)-doped silica fibres, with their ultra-wide near-infrared (NIR) luminescence from various Bi active centres (BACs), offer promising potential for developing wideband Bi-doped fibre amplifiers (BDFAs).<br/>In this thesis, I fabricated Er-doped fibres using the modified chemical vapour deposition (MCVD)-solution doping technique by tailoring the glass core compositions to favour L-band amplification. Fibre spectroscopic properties were characterised including refractive index profile, absorption, background loss, unsaturable loss, fluorescence, lifetime, on/off gain, and Er3+ cross-sections. Using the fabricated EDFs, I developed L-band amplifiers to achieve a high gain of ≥20 dB from 1565-1625 nm in a double-pass configuration, a flat gain ripple of ±0.7 dB from 1580-1615 nm by forming AlPO4 units in the fibre and pumped at 980 nm, an extended operating wavelength up to 1628 nm with a 13.6 dB gain by forming AlPO4 units and pumped at 1480 nm. Er/Yb co-doped fibre amplifier (EYDFA) was built up utilising 1480 nm core-pumping to shorten the L-band device length to 23 m.<br/>High-performance BDFAs were developed using BDFs fabricated by other fabricators. Using Bi-doped germano-silicate fibres (BGSFs) and phospho-silicate fibres (BPSFs), a high gain and high gain-per-unit-length BDFA was demonstrated in the E+S band with shortened device lengths (25.5 m to 48 m), and a high-gain ultra-wideband BDFA was presented in the O+E+S band with a 140 nm 20 dB-gain bandwidth for a -23 dBm input signal, respectively. Spectroscopic properties of various BACs were analysed, and a fully integrated, compact BDFA device box was developed.<br/>Moreover, robust amplifiers were developed to adapt to extreme temperatures and irradiation conditions. For EDFAs, a hybrid configuration was proposed to balance temperature stability and L-band gain, achieving low noise and temperature-insensitive gain flatness from 1585-1615 nm. Radiation tolerance was characterised in various core-composition EDFs after gamma-irradiation to develop radiation-resistant EDFAs in the C- or L-band using cerium (Ce) co-doping. In addition, a radiation-resistant E+S band BDFA was developed with a 35 dB post-irradiation gain. <br/>"],"dc:format":["text"],"dc:identifier.uri":["https://eprints.soton.ac.uk/id/eprint/497360/1/THESIS_FINAL_ZZ.pdf","https://eprints.soton.ac.uk/id/eprint/497360/2/Final-thesis-submission-Examination-Ms-Ziwei-Zhai.pdf"],"dc:language":["English"],"dc:language.dcterms_iso639_2":["eng"],"dc:publisher.commercial":["University of Southampton"],"dc:publisher.department":["Optoelectronics Research Centre"],"dc:publisher.institution":["University of Southampton"],"dc:relation.isreferencedby":["https://eprints.soton.ac.uk/id/eprint/497360/"],"dcterms:accessrights":["public","staffonly"],"dc:title":["Development of erbium-doped and bismuth-doped optical fibres for wideband and high-performance amplifiers for telecommunication applications"],"dc:type":["Thesis"],"dc:type.qualificationlevel":["doctoral"],"dc:type.qualificationname":["Ph.D."],"person:identifier.orcid":["0000000171287326","0000000335606152","0000000316917959"]},"updated_at":"2026-11-19T09:55:13Z"}