{"id":{"repo_id":"uab","oai_identifier":"oai:digitalcommons.library.uab.edu:etd-collection-3246"},"canonical_url":"https://search.ndltd.org/etd/uab/oai:digitalcommons.library.uab.edu:etd-collection-3246","repository":{"repo_id":"uab","name":"University of Alabama Birmingham","base_url":"https://digitalcommons.library.uab.edu/do/oai/"},"display":{"title":"Edge-Wave Formation During Multi-Stand Tube Mill Operation","abstract":"Cold-Formed (CF), High-Frequency (HF), Electric-Resistance-Welded (ERW) tubing is manufactured using a continuous roll forming process where a flat steel strip is progressively formed into a round which is then passed through an induction coil to be heated prior to having the heated edges forged to make a weld. A somewhat common issue, particularly as the thickness decreases and outside dimension increases, is an elastic edge wave that ultimately sets into a plastically deformed strip edge that cannot be successfully joined into a welded tube. Many variables can cause or exacerbate this effect including strip not centered in the mill, significant thickness variation across the width of the strip, tooling not properly lined up in the mill and tooling design issues. Herein, material properties and tube mill lateral alignment are examined regarding the formation of edge wave and poor quality. Material properties, within a specific range, do not have a noticeable impact on poor quality. Tube mill alignment (in the horizontal plane) does have a noticeable impact and poor alignment does contribute to the formation of edge wave.","abstract_html":"Cold-Formed (CF), High-Frequency (HF), Electric-Resistance-Welded (ERW) tubing is manufactured using a continuous roll forming process where a flat steel strip is progressively formed into a round which is then passed through an induction coil to be heated prior to having the heated edges forged to make a weld. A somewhat common issue, particularly as the thickness decreases and outside dimension increases, is an elastic edge wave that ultimately sets into a plastically deformed strip edge that cannot be successfully joined into a welded tube. Many variables can cause or exacerbate this effect including strip not centered in the mill, significant thickness variation across the width of the strip, tooling not properly lined up in the mill and tooling design issues. Herein, material properties and tube mill lateral alignment are examined regarding the formation of edge wave and poor quality. Material properties, within a specific range, do not have a noticeable impact on poor quality. Tube mill alignment (in the horizontal plane) does have a noticeable impact and poor alignment does contribute to the formation of edge wave.","abstract_has_math":false,"creators":["Lerew, Daniel"],"institution":null,"degree_name":null,"degree_level":"Thesis","degree_discipline":null,"degree_department":null,"school":null,"contributors":["Charles Monroe","Robin Foley","Haibin Ning"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T09:26:44Z","subjects":["Cold Formed","Electric Resistance Welded","Multi-Stand Tube Mill","Roll Forming","Engineering"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://digitalcommons.library.uab.edu/etd-collection/2254","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://digitalcommons.library.uab.edu/etd-collection/2254","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digitalcommons.library.uab.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Adigitalcommons.library.uab.edu%3Aetd-collection-3246","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Charles Monroe","Robin Foley","Haibin Ning"]},{"key":"dc:creator","label":"Author","values":["Lerew, Daniel"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["2018-01-01T08:00:00Z"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Thesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Cold Formed","Electric Resistance Welded","Multi-Stand Tube Mill","Roll Forming","Engineering"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digitalcommons.library.uab.edu/etd-collection/2254"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Cold-Formed (CF), High-Frequency (HF), Electric-Resistance-Welded (ERW) tubing is manufactured using a continuous roll forming process where a flat steel strip is progressively formed into a round which is then passed through an induction coil to be heated prior to having the heated edges forged to make a weld. A somewhat common issue, particularly as the thickness decreases and outside dimension increases, is an elastic edge wave that ultimately sets into a plastically deformed strip edge that cannot be successfully joined into a welded tube. Many variables can cause or exacerbate this effect including strip not centered in the mill, significant thickness variation across the width of the strip, tooling not properly lined up in the mill and tooling design issues. Herein, material properties and tube mill lateral alignment are examined regarding the formation of edge wave and poor quality. Material properties, within a specific range, do not have a noticeable impact on poor quality. Tube mill alignment (in the horizontal plane) does have a noticeable impact and poor alignment does contribute to the formation of edge wave."]},{"key":"dc:description.note","label":"Dc Description Note","values":["etdadmin_upload_603226"]},{"key":"dc:title","label":"Title","values":["Edge-Wave Formation During Multi-Stand Tube Mill Operation"]}]}],"canonical_facts":{"dc:contributor":["Charles Monroe","Robin Foley","Haibin Ning"],"dc:creator":["Lerew, Daniel"],"dc:date.created":["2018-01-01T08:00:00Z"],"dc:description.abstract":["Cold-Formed (CF), High-Frequency (HF), Electric-Resistance-Welded (ERW) tubing is manufactured using a continuous roll forming process where a flat steel strip is progressively formed into a round which is then passed through an induction coil to be heated prior to having the heated edges forged to make a weld. A somewhat common issue, particularly as the thickness decreases and outside dimension increases, is an elastic edge wave that ultimately sets into a plastically deformed strip edge that cannot be successfully joined into a welded tube. Many variables can cause or exacerbate this effect including strip not centered in the mill, significant thickness variation across the width of the strip, tooling not properly lined up in the mill and tooling design issues. Herein, material properties and tube mill lateral alignment are examined regarding the formation of edge wave and poor quality. Material properties, within a specific range, do not have a noticeable impact on poor quality. Tube mill alignment (in the horizontal plane) does have a noticeable impact and poor alignment does contribute to the formation of edge wave."],"dc:description.note":["etdadmin_upload_603226"],"dc:identifier":["https://digitalcommons.library.uab.edu/etd-collection/2254"],"dc:subject":["Cold Formed","Electric Resistance Welded","Multi-Stand Tube Mill","Roll Forming","Engineering"],"dc:title":["Edge-Wave Formation During Multi-Stand Tube Mill Operation"],"thesis:degree_level":["Thesis"]},"updated_at":"2026-11-19T09:26:44Z"}