{"id":{"repo_id":"uab","oai_identifier":"oai:digitalcommons.library.uab.edu:etd-collection-4000"},"canonical_url":"https://search.ndltd.org/etd/uab/oai:digitalcommons.library.uab.edu:etd-collection-4000","repository":{"repo_id":"uab","name":"University of Alabama Birmingham","base_url":"https://digitalcommons.library.uab.edu/do/oai/"},"display":{"title":"Retention Of Cad/Cam Crowns Luted With Resin Cements And Rmgi","abstract":"Objectives: To measure retention of lithium disilicate (IPS e.max CAD, Ivoclar Viva-dent) and zirconia reinforced lithium disilicate (CELTRATM DUO, Dentsply) copings luted using resin cements and resin-modified glass ionomer cement. Methods: 110 Extracted human, non-carious mandibular 2nd premolars (n=10) were embedded in PVC cylinders with acrylic resin and placed into a lathe to produce a uni-form crown preparation (22°-convergence & 3mm-height). Following the orientation groove placement (69L bur), preparations were scanned and milled using a CEREC 3D/Sirona machine to produce e.max and CELTRATM DUO crowns. Preparations were imaged with a digital microscope (Keyence/VHX-600-20X) and the surface area of each crown was calculated. IPS e.max crowns and CELTRATM DUO crowns were cemented using the cements as in Tables 1 & 2. Specimens were stored (distilled water/37°C/24h) and thermocycled (10,000cycles/5-50°C/30secs) before debonding in tension at crosshead speed-5mm/min (INSTRON Model/5565). The bond strength was calculated by dividing the failure load with preparation surface area. The CELTRATM DUO and e.max data were compared separately with 1-way ANOVA and Tukey post-hoc analysis (alpha=0.05). Results: The simulated crown strength test results for e.max were: Calibra=4.89±2.35a; ExpE(TE)=3.70±2.08a,b; ExpSE=3.18±2.03a,b RelyXLP=3.11±1.99a,b; ExpE(Self-Etch)=2.74±1.23a,b; Multilink=2.66±1.72a,b; RelyXU=2.65±1.46a,b; Re-lyXLP/HF=1.91±0.70b. For CELTRATM: Exp/S=4.73±2.45a; Exp/S/E=4.40±1.76a,b; Re-lyXLP/HF=3.34±1.65a,b,c; Exp=1.79±0.70b,c; and RelyXLP=0.95±0.58c. The ANOVA showed some significant differences between groups (p=0.01) where the same letter denotes similar groups. Conclusions: The Calibra material resulted in significantly higher retention with the than RelyXLP/HF for the coping fabricated from emax. The experimental resin cement with silane when compared to Exp and RelyXLP resulted in significantly higher test retention strength for the CELTRATM DUO.","abstract_html":"Objectives: To measure retention of lithium disilicate (IPS e.max CAD, Ivoclar Viva-dent) and zirconia reinforced lithium disilicate (CELTRATM DUO, Dentsply) copings luted using resin cements and resin-modified glass ionomer cement. Methods: 110 Extracted human, non-carious mandibular 2nd premolars (n=10) were embedded in PVC cylinders with acrylic resin and placed into a lathe to produce a uni-form crown preparation (22°-convergence &amp; 3mm-height). Following the orientation groove placement (69L bur), preparations were scanned and milled using a CEREC 3D/Sirona machine to produce e.max and CELTRATM DUO crowns. Preparations were imaged with a digital microscope (Keyence/VHX-600-20X) and the surface area of each crown was calculated. IPS e.max crowns and CELTRATM DUO crowns were cemented using the cements as in Tables 1 &amp; 2. Specimens were stored (distilled water/37°C/24h) and thermocycled (10,000cycles/5-50°C/30secs) before debonding in tension at crosshead speed-5mm/min (INSTRON Model/5565). The bond strength was calculated by dividing the failure load with preparation surface area. The CELTRATM DUO and e.max data were compared separately with 1-way ANOVA and Tukey post-hoc analysis (alpha=0.05). Results: The simulated crown strength test results for e.max were: Calibra=4.89±2.35a; ExpE(TE)=3.70±2.08a,b; ExpSE=3.18±2.03a,b RelyXLP=3.11±1.99a,b; ExpE(Self-Etch)=2.74±1.23a,b; Multilink=2.66±1.72a,b; RelyXU=2.65±1.46a,b; Re-lyXLP/HF=1.91±0.70b. For CELTRATM: Exp/S=4.73±2.45a; Exp/S/E=4.40±1.76a,b; Re-lyXLP/HF=3.34±1.65a,b,c; Exp=1.79±0.70b,c; and RelyXLP=0.95±0.58c. The ANOVA showed some significant differences between groups (p=0.01) where the same letter denotes similar groups. Conclusions: The Calibra material resulted in significantly higher retention with the than RelyXLP/HF for the coping fabricated from emax. The experimental resin cement with silane when compared to Exp and RelyXLP resulted in significantly higher test retention strength for the CELTRATM DUO.","abstract_has_math":false,"creators":["Sonavane, Shruti Sushilkumar"],"institution":null,"degree_name":null,"degree_level":"Thesis","degree_discipline":null,"degree_department":null,"school":null,"contributors":["John O Burgess","Amjad Javed","Jack E Lemons","Lance Ramp","Nathaniel C Lawson"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T09:24:20Z","subjects":["Adhesion","Biomaterials","CAD/CAM","Cements","Ceramics","Dentistry"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://digitalcommons.library.uab.edu/etd-collection/3008","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://digitalcommons.library.uab.edu/etd-collection/3008","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digitalcommons.library.uab.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Adigitalcommons.library.uab.edu%3Aetd-collection-4000","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["John O Burgess","Amjad Javed","Jack E Lemons","Lance Ramp","Nathaniel C Lawson"]},{"key":"dc:creator","label":"Author","values":["Sonavane, Shruti Sushilkumar"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["2015-01-01T08:00:00Z"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Thesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Adhesion","Biomaterials","CAD/CAM","Cements","Ceramics","Dentistry"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digitalcommons.library.uab.edu/etd-collection/3008"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Objectives: To measure retention of lithium disilicate (IPS e.max CAD, Ivoclar Viva-dent) and zirconia reinforced lithium disilicate (CELTRATM DUO, Dentsply) copings luted using resin cements and resin-modified glass ionomer cement. Methods: 110 Extracted human, non-carious mandibular 2nd premolars (n=10) were embedded in PVC cylinders with acrylic resin and placed into a lathe to produce a uni-form crown preparation (22°-convergence & 3mm-height). Following the orientation groove placement (69L bur), preparations were scanned and milled using a CEREC 3D/Sirona machine to produce e.max and CELTRATM DUO crowns. Preparations were imaged with a digital microscope (Keyence/VHX-600-20X) and the surface area of each crown was calculated. IPS e.max crowns and CELTRATM DUO crowns were cemented using the cements as in Tables 1 & 2. Specimens were stored (distilled water/37°C/24h) and thermocycled (10,000cycles/5-50°C/30secs) before debonding in tension at crosshead speed-5mm/min (INSTRON Model/5565). The bond strength was calculated by dividing the failure load with preparation surface area. The CELTRATM DUO and e.max data were compared separately with 1-way ANOVA and Tukey post-hoc analysis (alpha=0.05). Results: The simulated crown strength test results for e.max were: Calibra=4.89±2.35a; ExpE(TE)=3.70±2.08a,b; ExpSE=3.18±2.03a,b RelyXLP=3.11±1.99a,b; ExpE(Self-Etch)=2.74±1.23a,b; Multilink=2.66±1.72a,b; RelyXU=2.65±1.46a,b; Re-lyXLP/HF=1.91±0.70b. For CELTRATM: Exp/S=4.73±2.45a; Exp/S/E=4.40±1.76a,b; Re-lyXLP/HF=3.34±1.65a,b,c; Exp=1.79±0.70b,c; and RelyXLP=0.95±0.58c. The ANOVA showed some significant differences between groups (p=0.01) where the same letter denotes similar groups. Conclusions: The Calibra material resulted in significantly higher retention with the than RelyXLP/HF for the coping fabricated from emax. The experimental resin cement with silane when compared to Exp and RelyXLP resulted in significantly higher test retention strength for the CELTRATM DUO."]},{"key":"dc:description.note","label":"Dc Description Note","values":["etdadmin_upload_341613"]},{"key":"dc:title","label":"Title","values":["Retention Of Cad/Cam Crowns Luted With Resin Cements And Rmgi"]}]}],"canonical_facts":{"dc:contributor":["John O Burgess","Amjad Javed","Jack E Lemons","Lance Ramp","Nathaniel C Lawson"],"dc:creator":["Sonavane, Shruti Sushilkumar"],"dc:date.created":["2015-01-01T08:00:00Z"],"dc:description.abstract":["Objectives: To measure retention of lithium disilicate (IPS e.max CAD, Ivoclar Viva-dent) and zirconia reinforced lithium disilicate (CELTRATM DUO, Dentsply) copings luted using resin cements and resin-modified glass ionomer cement. Methods: 110 Extracted human, non-carious mandibular 2nd premolars (n=10) were embedded in PVC cylinders with acrylic resin and placed into a lathe to produce a uni-form crown preparation (22°-convergence & 3mm-height). Following the orientation groove placement (69L bur), preparations were scanned and milled using a CEREC 3D/Sirona machine to produce e.max and CELTRATM DUO crowns. Preparations were imaged with a digital microscope (Keyence/VHX-600-20X) and the surface area of each crown was calculated. IPS e.max crowns and CELTRATM DUO crowns were cemented using the cements as in Tables 1 & 2. Specimens were stored (distilled water/37°C/24h) and thermocycled (10,000cycles/5-50°C/30secs) before debonding in tension at crosshead speed-5mm/min (INSTRON Model/5565). The bond strength was calculated by dividing the failure load with preparation surface area. The CELTRATM DUO and e.max data were compared separately with 1-way ANOVA and Tukey post-hoc analysis (alpha=0.05). Results: The simulated crown strength test results for e.max were: Calibra=4.89±2.35a; ExpE(TE)=3.70±2.08a,b; ExpSE=3.18±2.03a,b RelyXLP=3.11±1.99a,b; ExpE(Self-Etch)=2.74±1.23a,b; Multilink=2.66±1.72a,b; RelyXU=2.65±1.46a,b; Re-lyXLP/HF=1.91±0.70b. For CELTRATM: Exp/S=4.73±2.45a; Exp/S/E=4.40±1.76a,b; Re-lyXLP/HF=3.34±1.65a,b,c; Exp=1.79±0.70b,c; and RelyXLP=0.95±0.58c. The ANOVA showed some significant differences between groups (p=0.01) where the same letter denotes similar groups. Conclusions: The Calibra material resulted in significantly higher retention with the than RelyXLP/HF for the coping fabricated from emax. The experimental resin cement with silane when compared to Exp and RelyXLP resulted in significantly higher test retention strength for the CELTRATM DUO."],"dc:description.note":["etdadmin_upload_341613"],"dc:identifier":["https://digitalcommons.library.uab.edu/etd-collection/3008"],"dc:subject":["Adhesion","Biomaterials","CAD/CAM","Cements","Ceramics","Dentistry"],"dc:title":["Retention Of Cad/Cam Crowns Luted With Resin Cements And Rmgi"],"thesis:degree_level":["Thesis"]},"updated_at":"2026-11-19T09:24:20Z"}