{"id":{"repo_id":"ubc","oai_identifier":"oai:circle.library.ubc.ca:2429/36326"},"canonical_url":"https://search.ndltd.org/etd/ubc/oai:circle.library.ubc.ca:2429/36326","repository":{"repo_id":"ubc","name":"University of British Columbia","base_url":"http://circle.library.ubc.ca/oai/request"},"display":{"title":"Longitudinal permeability within Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) growth increments","abstract":"An apparatus was constructed to measure the longitudinal gas-permeability of wood microsections about 150 microns thick. This apparatus was used to examine low surface tension drying methods of wood (freeze-drying and alcohol-benzene extraction) believed to maintain the bordered pit tori of Douglas fir (Pseudotsuga menziesii (Mirb.) Franco) in the non-aspirated condition. Results were compared with drying methods believed to aspirate tori (air-drying, oven-drying and boiling-under-vacuum). Dry nitrogen gas-permeability measurements were made under \"steady state\" conditions. Similar drying techniques were used to prepare gross specimens which were subsequently subjected to “non-steady state\" pressure treatment in end-penetration. Sapwood and heartwood specimens from impermeable interior-type and permeable coast-type Douglas fir were tested. With both gross sections and microsections, the two low surface tension drying methods provided more permeable wood than did air-drying. Boiling-under-vacuum was as effective as low surface tension methods in improving gas-permeability, but not creosote-permeability, whereas oven-drying was as effective as low surface tension methods in improving creosote-permeability, but not gas-permeability. The improvement was most striking in all sapwood samples, less in coast-type heartwood, and nil or not measurable in interior-type heartwood. Under the experimental conditions, latewood gas-permeability was about 2 darcies for all specimens and drying methods. Heartwood early-wood gas-permeability ranged from 0.02 to 2 darcies but was unaffected by drying methods. Sapwood earlywood gas-permeability was improved from 8 to 30 times by low surface tension drying. The greatest gas-permeability was found in the first-formed earlywood, which ranged from 2 to 100 darcies. The later-formed earlywood ranged from 0.02 to 100 darcies, depending on wood origin and drying method. Creosote-permeability of interior-type heartwood was uniformly low by all drying methods. Interior-type sapwood and coast-type sapwood and heartwood were much more permeable after low surface tension drying or oven-drying. By visual observations, after all drying methods, latewood was more permeable than earlywood. Low surface tension drying methods improve earlywood gas-permeability of sapwood, and latewood creosote-permeability of sapwood and coast-type heartwood.","abstract_html":"An apparatus was constructed to measure the longitudinal gas-permeability of wood microsections about 150 microns thick. This apparatus was used to examine low surface tension drying methods of wood (freeze-drying and alcohol-benzene extraction) believed to maintain the bordered pit tori of Douglas fir (Pseudotsuga menziesii (Mirb.) Franco) in the non-aspirated condition. Results were compared with drying methods believed to aspirate tori (air-drying, oven-drying and boiling-under-vacuum). Dry nitrogen gas-permeability measurements were made under &quot;steady state&quot; conditions. Similar drying techniques were used to prepare gross specimens which were subsequently subjected to “non-steady state&quot; pressure treatment in end-penetration. Sapwood and heartwood specimens from impermeable interior-type and permeable coast-type Douglas fir were tested. With both gross sections and microsections, the two low surface tension drying methods provided more permeable wood than did air-drying. Boiling-under-vacuum was as effective as low surface tension methods in improving gas-permeability, but not creosote-permeability, whereas oven-drying was as effective as low surface tension methods in improving creosote-permeability, but not gas-permeability. The improvement was most striking in all sapwood samples, less in coast-type heartwood, and nil or not measurable in interior-type heartwood. Under the experimental conditions, latewood gas-permeability was about 2 darcies for all specimens and drying methods. Heartwood early-wood gas-permeability ranged from 0.02 to 2 darcies but was unaffected by drying methods. Sapwood earlywood gas-permeability was improved from 8 to 30 times by low surface tension drying. The greatest gas-permeability was found in the first-formed earlywood, which ranged from 2 to 100 darcies. The later-formed earlywood ranged from 0.02 to 100 darcies, depending on wood origin and drying method. Creosote-permeability of interior-type heartwood was uniformly low by all drying methods. Interior-type sapwood and coast-type sapwood and heartwood were much more permeable after low surface tension drying or oven-drying. By visual observations, after all drying methods, latewood was more permeable than earlywood. Low surface tension drying methods improve earlywood gas-permeability of sapwood, and latewood creosote-permeability of sapwood and coast-type heartwood.","abstract_has_math":false,"creators":["Bramhall, George"],"institution":"University of British Columbia","degree_name":"Master of Science - MSc","degree_level":"master's","degree_discipline":"Forestry","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":1967,"date_issued":"1967","date_published":"1967","updated_at":"2026-11-19T14:49:21Z","subjects":[],"languages":["eng"],"rights":["For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/2429/36326","outbound_label":"Handle","outbound_source":"dc:identifier","record_url":"http://hdl.handle.net/2429/36326","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier","download_url":"http://circle.library.ubc.ca/bitstream/2429/36326/1/UBC_1967_A6_7+B63.pdf","download_label":"Download PDF","download_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"http://circle.library.ubc.ca/oai/request?verb=GetRecord&metadataPrefix=etdms&identifier=oai%3Acircle.library.ubc.ca%3A2429%2F36326","prefix":"etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Bramhall, George"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["1967"]},{"key":"dc:publisher","label":"Institution","values":["University of British Columbia"]},{"key":"dc:type","label":"Dc Type","values":["Text"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Forestry"]},{"key":"thesis:degree_level","label":"Degree Level","values":["master's"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science - MSc"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of British Columbia"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["eng"]},{"key":"dc:rights","label":"Dc Rights","values":["For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://hdl.handle.net/2429/36326","http://circle.library.ubc.ca/bitstream/2429/36326/1/UBC_1967_A6_7+B63.pdf"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["An apparatus was constructed to measure the longitudinal gas-permeability of wood microsections about 150 microns thick. This apparatus was used to examine low surface tension drying methods of wood (freeze-drying and alcohol-benzene extraction) believed to maintain the bordered pit tori of Douglas fir (Pseudotsuga menziesii (Mirb.) Franco) in the non-aspirated condition. Results were compared with drying methods believed to aspirate tori (air-drying, oven-drying and boiling-under-vacuum). Dry nitrogen gas-permeability measurements were made under \"steady state\" conditions. Similar drying techniques were used to prepare gross specimens which were subsequently subjected to “non-steady state\" pressure treatment in end-penetration. Sapwood and heartwood specimens from impermeable interior-type and permeable coast-type Douglas fir were tested. With both gross sections and microsections, the two low surface tension drying methods provided more permeable wood than did air-drying. Boiling-under-vacuum was as effective as low surface tension methods in improving gas-permeability, but not creosote-permeability, whereas oven-drying was as effective as low surface tension methods in improving creosote-permeability, but not gas-permeability. The improvement was most striking in all sapwood samples, less in coast-type heartwood, and nil or not measurable in interior-type heartwood. Under the experimental conditions, latewood gas-permeability was about 2 darcies for all specimens and drying methods. Heartwood early-wood gas-permeability ranged from 0.02 to 2 darcies but was unaffected by drying methods. Sapwood earlywood gas-permeability was improved from 8 to 30 times by low surface tension drying. The greatest gas-permeability was found in the first-formed earlywood, which ranged from 2 to 100 darcies. The later-formed earlywood ranged from 0.02 to 100 darcies, depending on wood origin and drying method. Creosote-permeability of interior-type heartwood was uniformly low by all drying methods. Interior-type sapwood and coast-type sapwood and heartwood were much more permeable after low surface tension drying or oven-drying. By visual observations, after all drying methods, latewood was more permeable than earlywood. Low surface tension drying methods improve earlywood gas-permeability of sapwood, and latewood creosote-permeability of sapwood and coast-type heartwood."]},{"key":"dc:format","label":"Dc Format","values":["7357784","application/pdf"]},{"key":"dc:title","label":"Title","values":["Longitudinal permeability within Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) growth increments"]}]}],"canonical_facts":{"dc:creator":["Bramhall, George"],"dc:date":["1967"],"dc:description":["An apparatus was constructed to measure the longitudinal gas-permeability of wood microsections about 150 microns thick. This apparatus was used to examine low surface tension drying methods of wood (freeze-drying and alcohol-benzene extraction) believed to maintain the bordered pit tori of Douglas fir (Pseudotsuga menziesii (Mirb.) Franco) in the non-aspirated condition. Results were compared with drying methods believed to aspirate tori (air-drying, oven-drying and boiling-under-vacuum). Dry nitrogen gas-permeability measurements were made under \"steady state\" conditions. Similar drying techniques were used to prepare gross specimens which were subsequently subjected to “non-steady state\" pressure treatment in end-penetration. Sapwood and heartwood specimens from impermeable interior-type and permeable coast-type Douglas fir were tested. With both gross sections and microsections, the two low surface tension drying methods provided more permeable wood than did air-drying. Boiling-under-vacuum was as effective as low surface tension methods in improving gas-permeability, but not creosote-permeability, whereas oven-drying was as effective as low surface tension methods in improving creosote-permeability, but not gas-permeability. The improvement was most striking in all sapwood samples, less in coast-type heartwood, and nil or not measurable in interior-type heartwood. Under the experimental conditions, latewood gas-permeability was about 2 darcies for all specimens and drying methods. Heartwood early-wood gas-permeability ranged from 0.02 to 2 darcies but was unaffected by drying methods. Sapwood earlywood gas-permeability was improved from 8 to 30 times by low surface tension drying. The greatest gas-permeability was found in the first-formed earlywood, which ranged from 2 to 100 darcies. The later-formed earlywood ranged from 0.02 to 100 darcies, depending on wood origin and drying method. Creosote-permeability of interior-type heartwood was uniformly low by all drying methods. Interior-type sapwood and coast-type sapwood and heartwood were much more permeable after low surface tension drying or oven-drying. By visual observations, after all drying methods, latewood was more permeable than earlywood. Low surface tension drying methods improve earlywood gas-permeability of sapwood, and latewood creosote-permeability of sapwood and coast-type heartwood."],"dc:format":["7357784","application/pdf"],"dc:identifier":["http://hdl.handle.net/2429/36326","http://circle.library.ubc.ca/bitstream/2429/36326/1/UBC_1967_A6_7+B63.pdf"],"dc:language":["eng"],"dc:publisher":["University of British Columbia"],"dc:rights":["For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use."],"dc:title":["Longitudinal permeability within Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) growth increments"],"dc:type":["Text"],"thesis:degree_discipline":["Forestry"],"thesis:degree_level":["master's"],"thesis:degree_name":["Master of Science - MSc"],"thesis:institution_name":["University of British Columbia"]},"updated_at":"2026-11-19T14:49:21Z"}