{"id":{"repo_id":"ubc","oai_identifier":"oai:circle.library.ubc.ca:2429/39557"},"canonical_url":"https://search.ndltd.org/etd/ubc/oai:circle.library.ubc.ca:2429/39557","repository":{"repo_id":"ubc","name":"University of British Columbia","base_url":"http://circle.library.ubc.ca/oai/request"},"display":{"title":"Ductility and chemical reactions at the interface between nickel and magnesium oxide single crystals","abstract":"An investigation was conducted on the interaction between nickel metal and single crystals of magnesium oxide. The nickel was cleaned with purified hydrogen gas at 800°C and melted under vacuum (5 x 10⁻⁵ mm. Hg) in contact with the magnesium oxide. The interface was examined metallographic-ally. The formation of compounds at the interface was examined by X-ray diffraction techniques. The magnesium oxide was plastically deformed by thermal stresses which occurred on cooling. Slip occurred on four slip planes only. The slip sources were present in the surface at a depth not exceeding ten microns. They were in the form of dislocation half-loops introduced in the surface during cleavage. The introduction of these half-loops was due to the formation of cleavage steps. Rows of dislocation half-loops were due to the multiplication of a half-loop on a slip plane oriented in the direction of propagation of the cleavage crack. Bond formation consisted of the formation of a magnesium-nickel compound (Mg₂Ni). The bond strength exceeded the stress for brittle fracture of magnesium oxide. Attack of the magnesium oxide occurred preferentially at the perimeter of the interface. This led to groove-formation, which resulted in a large hysteresis of wetting. The diffusion of nickel into magnesium oxide seemed to take place mainly by diffusion along dislocations.","abstract_html":"An investigation was conducted on the interaction between nickel metal and single crystals of magnesium oxide. The nickel was cleaned with purified hydrogen gas at 800°C and melted under vacuum (5 x 10⁻⁵ mm. Hg) in contact with the magnesium oxide. The interface was examined metallographic-ally. The formation of compounds at the interface was examined by X-ray diffraction techniques. The magnesium oxide was plastically deformed by thermal stresses which occurred on cooling. Slip occurred on four slip planes only. The slip sources were present in the surface at a depth not exceeding ten microns. They were in the form of dislocation half-loops introduced in the surface during cleavage. The introduction of these half-loops was due to the formation of cleavage steps. Rows of dislocation half-loops were due to the multiplication of a half-loop on a slip plane oriented in the direction of propagation of the cleavage crack. Bond formation consisted of the formation of a magnesium-nickel compound (Mg₂Ni). The bond strength exceeded the stress for brittle fracture of magnesium oxide. Attack of the magnesium oxide occurred preferentially at the perimeter of the interface. This led to groove-formation, which resulted in a large hysteresis of wetting. The diffusion of nickel into magnesium oxide seemed to take place mainly by diffusion along dislocations.","abstract_has_math":false,"creators":["Hasselman, Didericus Petrus Hermannus"],"institution":"University of British Columbia","degree_name":"Master of Applied Science - MASc","degree_level":"master's","degree_discipline":"Metals and Materials Engineering","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":1959,"date_issued":"1959","date_published":"1959","updated_at":"2026-11-19T14:50:50Z","subjects":[],"languages":["eng"],"rights":["For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/2429/39557","outbound_label":"Handle","outbound_source":"dc:identifier","record_url":"http://hdl.handle.net/2429/39557","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier","download_url":"http://circle.library.ubc.ca/bitstream/2429/39557/1/UBC_1960_A7+H25+D8.pdf","download_label":"Download PDF","download_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"http://circle.library.ubc.ca/oai/request?verb=GetRecord&metadataPrefix=etdms&identifier=oai%3Acircle.library.ubc.ca%3A2429%2F39557","prefix":"etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Hasselman, Didericus Petrus Hermannus"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["1959"]},{"key":"dc:publisher","label":"Institution","values":["University of British Columbia"]},{"key":"dc:type","label":"Dc Type","values":["Text"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Metals and Materials Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["master's"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Applied Science - MASc"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of British Columbia"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["eng"]},{"key":"dc:rights","label":"Dc Rights","values":["For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://hdl.handle.net/2429/39557","http://circle.library.ubc.ca/bitstream/2429/39557/1/UBC_1960_A7+H25+D8.pdf"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["An investigation was conducted on the interaction between nickel metal and single crystals of magnesium oxide. The nickel was cleaned with purified hydrogen gas at 800°C and melted under vacuum (5 x 10⁻⁵ mm. Hg) in contact with the magnesium oxide. The interface was examined metallographic-ally. The formation of compounds at the interface was examined by X-ray diffraction techniques. The magnesium oxide was plastically deformed by thermal stresses which occurred on cooling. Slip occurred on four slip planes only. The slip sources were present in the surface at a depth not exceeding ten microns. They were in the form of dislocation half-loops introduced in the surface during cleavage. The introduction of these half-loops was due to the formation of cleavage steps. Rows of dislocation half-loops were due to the multiplication of a half-loop on a slip plane oriented in the direction of propagation of the cleavage crack. Bond formation consisted of the formation of a magnesium-nickel compound (Mg₂Ni). The bond strength exceeded the stress for brittle fracture of magnesium oxide. Attack of the magnesium oxide occurred preferentially at the perimeter of the interface. This led to groove-formation, which resulted in a large hysteresis of wetting. The diffusion of nickel into magnesium oxide seemed to take place mainly by diffusion along dislocations."]},{"key":"dc:format","label":"Dc Format","values":["13443111","application/pdf"]},{"key":"dc:title","label":"Title","values":["Ductility and chemical reactions at the interface between nickel and magnesium oxide single crystals"]}]}],"canonical_facts":{"dc:creator":["Hasselman, Didericus Petrus Hermannus"],"dc:date":["1959"],"dc:description":["An investigation was conducted on the interaction between nickel metal and single crystals of magnesium oxide. The nickel was cleaned with purified hydrogen gas at 800°C and melted under vacuum (5 x 10⁻⁵ mm. Hg) in contact with the magnesium oxide. The interface was examined metallographic-ally. The formation of compounds at the interface was examined by X-ray diffraction techniques. The magnesium oxide was plastically deformed by thermal stresses which occurred on cooling. Slip occurred on four slip planes only. The slip sources were present in the surface at a depth not exceeding ten microns. They were in the form of dislocation half-loops introduced in the surface during cleavage. The introduction of these half-loops was due to the formation of cleavage steps. Rows of dislocation half-loops were due to the multiplication of a half-loop on a slip plane oriented in the direction of propagation of the cleavage crack. Bond formation consisted of the formation of a magnesium-nickel compound (Mg₂Ni). The bond strength exceeded the stress for brittle fracture of magnesium oxide. Attack of the magnesium oxide occurred preferentially at the perimeter of the interface. This led to groove-formation, which resulted in a large hysteresis of wetting. The diffusion of nickel into magnesium oxide seemed to take place mainly by diffusion along dislocations."],"dc:format":["13443111","application/pdf"],"dc:identifier":["http://hdl.handle.net/2429/39557","http://circle.library.ubc.ca/bitstream/2429/39557/1/UBC_1960_A7+H25+D8.pdf"],"dc:language":["eng"],"dc:publisher":["University of British Columbia"],"dc:rights":["For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use."],"dc:title":["Ductility and chemical reactions at the interface between nickel and magnesium oxide single crystals"],"dc:type":["Text"],"thesis:degree_discipline":["Metals and Materials Engineering"],"thesis:degree_level":["master's"],"thesis:degree_name":["Master of Applied Science - MASc"],"thesis:institution_name":["University of British Columbia"]},"updated_at":"2026-11-19T14:50:50Z"}