{"id":{"repo_id":"ubc","oai_identifier":"oai:circle.library.ubc.ca:2429/41417"},"canonical_url":"https://search.ndltd.org/etd/ubc/oai:circle.library.ubc.ca:2429/41417","repository":{"repo_id":"ubc","name":"University of British Columbia","base_url":"http://circle.library.ubc.ca/oai/request"},"display":{"title":"Growth and structure of yttrium sesquioxide epitaxial films","abstract":"The use of molecular beam epitaxy as a method for producing solid state host crystals for planar waveguide lasers has been investigated. Single crystal yttrium sesquioxide with a very high degree of structural order has been grown on R-plane sapphire substrates. The (01Ῑ2) Al₂O₃ substrates were annealed in air at 1150°C to generate atomically smooth surfaces with parallel atomic steps. This process was important for maximizing structural quality and minimizing surface roughness of the grown Y₂O₃ ﬁlm. A critical-thickness-like phenomenon was discovered, where the Y₂O₃ would grow in regions with near structural perfection at the beginning of growth. In thicker ﬁlms, the x-ray diffraction peaks became wider, indicating less crystalline uniformity. The maximum equivalent “critical thickness” achieved was 7 nm for a ﬁlm grown at 800°C with a growth rate of 20 nm/hr. The highly ordered material may be present in one uniform layer or distributed in smaller regions throughout the thin ﬁlm. Y₂O₃ ﬁlms on Al₂O₃ were annealed in air at temperatures up to 1400°C to study interdiffusion. By analyzing x-ray diffraction measurements, we found that Al migrated from the substrate into the Y₂O₃ ﬁlm with an approximate activation energy for bulk diffusion of 3.0 eV. Diffusion on the Y₂O₃ surface was estimated to have an activation energy of (0.5 ± 0.3) eV from atomic force microscopy images. After annealing, the presence of Y₄Al₂O₉, YAlO₃, and Y₃Al₅O₁₂ phases was conﬁrmed using x-ray diffraction and photoluminescence measurements. Attempts were made to use molecular hydrogen gas and gallium as surfactants during growth to improve ﬁlm properties. No conclusive beneﬁt was observed. Y₂O₃ ﬁlm surface roughness was observed to increase roughly proportionally to the square root of ﬁlm thickness. A 600 nm thick waveguide layer grown under optimal conditions had a root-mean-square roughness of 5.8 nm. This level of roughness could cause scattering loss at the waveguide core-cladding interface that is problematic for practical applications.","abstract_html":"The use of molecular beam epitaxy as a method for producing solid state host crystals for planar waveguide lasers has been investigated. Single crystal yttrium sesquioxide with a very high degree of structural order has been grown on R-plane sapphire substrates. The (01Ῑ2) Al₂O₃ substrates were annealed in air at 1150°C to generate atomically smooth surfaces with parallel atomic steps. This process was important for maximizing structural quality and minimizing surface roughness of the grown Y₂O₃ ﬁlm. A critical-thickness-like phenomenon was discovered, where the Y₂O₃ would grow in regions with near structural perfection at the beginning of growth. In thicker ﬁlms, the x-ray diffraction peaks became wider, indicating less crystalline uniformity. The maximum equivalent “critical thickness” achieved was 7 nm for a ﬁlm grown at 800°C with a growth rate of 20 nm/hr. The highly ordered material may be present in one uniform layer or distributed in smaller regions throughout the thin ﬁlm. Y₂O₃ ﬁlms on Al₂O₃ were annealed in air at temperatures up to 1400°C to study interdiffusion. By analyzing x-ray diffraction measurements, we found that Al migrated from the substrate into the Y₂O₃ ﬁlm with an approximate activation energy for bulk diffusion of 3.0 eV. Diffusion on the Y₂O₃ surface was estimated to have an activation energy of (0.5 ± 0.3) eV from atomic force microscopy images. After annealing, the presence of Y₄Al₂O₉, YAlO₃, and Y₃Al₅O₁₂ phases was conﬁrmed using x-ray diffraction and photoluminescence measurements. Attempts were made to use molecular hydrogen gas and gallium as surfactants during growth to improve ﬁlm properties. No conclusive beneﬁt was observed. Y₂O₃ ﬁlm surface roughness was observed to increase roughly proportionally to the square root of ﬁlm thickness. A 600 nm thick waveguide layer grown under optimal conditions had a root-mean-square roughness of 5.8 nm. This level of roughness could cause scattering loss at the waveguide core-cladding interface that is problematic for practical applications.","abstract_has_math":false,"creators":["Webster, Scott Elliott"],"institution":"University of British Columbia","degree_name":"Doctor of Philosophy - PhD","degree_level":"doctoral","degree_discipline":"Physics","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2012,"date_issued":"2012","date_published":"2012","updated_at":"2026-11-19T14:51:51Z","subjects":[],"languages":["eng"],"rights":["Attribution-NonCommercial-NoDerivatives 4.0 International"],"rights_urls":["http://creativecommons.org/licenses/by-nc-nd/4.0/"],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/2429/41417","outbound_label":"Handle","outbound_source":"dc:identifier","record_url":"http://hdl.handle.net/2429/41417","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier","download_url":"http://circle.library.ubc.ca/bitstream/2429/41417/3/ubc_2012_spring_webster_scott.pdf","download_label":"Download PDF","download_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"http://circle.library.ubc.ca/oai/request?verb=GetRecord&metadataPrefix=etdms&identifier=oai%3Acircle.library.ubc.ca%3A2429%2F41417","prefix":"etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Webster, Scott Elliott"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2012"]},{"key":"dc:publisher","label":"Institution","values":["University of British Columbia"]},{"key":"dc:type","label":"Dc Type","values":["Text"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Physics"]},{"key":"thesis:degree_level","label":"Degree Level","values":["doctoral"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Doctor of Philosophy - PhD"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of British Columbia"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["eng"]},{"key":"dc:rights","label":"Dc Rights","values":["http://creativecommons.org/licenses/by-nc-nd/4.0/","Attribution-NonCommercial-NoDerivatives 4.0 International"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://hdl.handle.net/2429/41417","http://circle.library.ubc.ca/bitstream/2429/41417/3/ubc_2012_spring_webster_scott.pdf"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["The use of molecular beam epitaxy as a method for producing solid state host crystals for planar waveguide lasers has been investigated. Single crystal yttrium sesquioxide with a very high degree of structural order has been grown on R-plane sapphire substrates. The (01Ῑ2) Al₂O₃ substrates were annealed in air at 1150°C to generate atomically smooth surfaces with parallel atomic steps. This process was important for maximizing structural quality and minimizing surface roughness of the grown Y₂O₃ ﬁlm. A critical-thickness-like phenomenon was discovered, where the Y₂O₃ would grow in regions with near structural perfection at the beginning of growth. In thicker ﬁlms, the x-ray diffraction peaks became wider, indicating less crystalline uniformity. The maximum equivalent “critical thickness” achieved was 7 nm for a ﬁlm grown at 800°C with a growth rate of 20 nm/hr. The highly ordered material may be present in one uniform layer or distributed in smaller regions throughout the thin ﬁlm. Y₂O₃ ﬁlms on Al₂O₃ were annealed in air at temperatures up to 1400°C to study interdiffusion. By analyzing x-ray diffraction measurements, we found that Al migrated from the substrate into the Y₂O₃ ﬁlm with an approximate activation energy for bulk diffusion of 3.0 eV. Diffusion on the Y₂O₃ surface was estimated to have an activation energy of (0.5 ± 0.3) eV from atomic force microscopy images. After annealing, the presence of Y₄Al₂O₉, YAlO₃, and Y₃Al₅O₁₂ phases was conﬁrmed using x-ray diffraction and photoluminescence measurements. Attempts were made to use molecular hydrogen gas and gallium as surfactants during growth to improve ﬁlm properties. No conclusive beneﬁt was observed. Y₂O₃ ﬁlm surface roughness was observed to increase roughly proportionally to the square root of ﬁlm thickness. A 600 nm thick waveguide layer grown under optimal conditions had a root-mean-square roughness of 5.8 nm. This level of roughness could cause scattering loss at the waveguide core-cladding interface that is problematic for practical applications."]},{"key":"dc:format","label":"Dc Format","values":["19885433","application/pdf"]},{"key":"dc:title","label":"Title","values":["Growth and structure of yttrium sesquioxide epitaxial films"]}]}],"canonical_facts":{"dc:creator":["Webster, Scott Elliott"],"dc:date":["2012"],"dc:description":["The use of molecular beam epitaxy as a method for producing solid state host crystals for planar waveguide lasers has been investigated. Single crystal yttrium sesquioxide with a very high degree of structural order has been grown on R-plane sapphire substrates. The (01Ῑ2) Al₂O₃ substrates were annealed in air at 1150°C to generate atomically smooth surfaces with parallel atomic steps. This process was important for maximizing structural quality and minimizing surface roughness of the grown Y₂O₃ ﬁlm. A critical-thickness-like phenomenon was discovered, where the Y₂O₃ would grow in regions with near structural perfection at the beginning of growth. In thicker ﬁlms, the x-ray diffraction peaks became wider, indicating less crystalline uniformity. The maximum equivalent “critical thickness” achieved was 7 nm for a ﬁlm grown at 800°C with a growth rate of 20 nm/hr. The highly ordered material may be present in one uniform layer or distributed in smaller regions throughout the thin ﬁlm. Y₂O₃ ﬁlms on Al₂O₃ were annealed in air at temperatures up to 1400°C to study interdiffusion. By analyzing x-ray diffraction measurements, we found that Al migrated from the substrate into the Y₂O₃ ﬁlm with an approximate activation energy for bulk diffusion of 3.0 eV. Diffusion on the Y₂O₃ surface was estimated to have an activation energy of (0.5 ± 0.3) eV from atomic force microscopy images. After annealing, the presence of Y₄Al₂O₉, YAlO₃, and Y₃Al₅O₁₂ phases was conﬁrmed using x-ray diffraction and photoluminescence measurements. Attempts were made to use molecular hydrogen gas and gallium as surfactants during growth to improve ﬁlm properties. No conclusive beneﬁt was observed. Y₂O₃ ﬁlm surface roughness was observed to increase roughly proportionally to the square root of ﬁlm thickness. A 600 nm thick waveguide layer grown under optimal conditions had a root-mean-square roughness of 5.8 nm. This level of roughness could cause scattering loss at the waveguide core-cladding interface that is problematic for practical applications."],"dc:format":["19885433","application/pdf"],"dc:identifier":["http://hdl.handle.net/2429/41417","http://circle.library.ubc.ca/bitstream/2429/41417/3/ubc_2012_spring_webster_scott.pdf"],"dc:language":["eng"],"dc:publisher":["University of British Columbia"],"dc:rights":["http://creativecommons.org/licenses/by-nc-nd/4.0/","Attribution-NonCommercial-NoDerivatives 4.0 International"],"dc:title":["Growth and structure of yttrium sesquioxide epitaxial films"],"dc:type":["Text"],"thesis:degree_discipline":["Physics"],"thesis:degree_level":["doctoral"],"thesis:degree_name":["Doctor of Philosophy - PhD"],"thesis:institution_name":["University of British Columbia"]},"updated_at":"2026-11-19T14:51:51Z"}