{"id":{"repo_id":"ubc","oai_identifier":"oai:circle.library.ubc.ca:2429/58950"},"canonical_url":"https://search.ndltd.org/etd/ubc/oai:circle.library.ubc.ca:2429/58950","repository":{"repo_id":"ubc","name":"University of British Columbia","base_url":"http://circle.library.ubc.ca/oai/request"},"display":{"title":"Effect of H₂O on CH₄ oxidation over PdO/Al₂O₃ and CeOx/PdO/Al₂O₃ catalysts","abstract":"Natural gas is a promising alternative fuel for transportation systems because of reduced CO, CO₂, SO₂, and NOx emissions into the environment, and its abundance and low cost compared with gasoline and diesel. A significant obstacle in the use of NG for vehicle fuels is that CH₄ is difficult to oxidize in the presence of CO₂ and H₂O and at the low exhaust gas temperature (500-550°C) of natural gas vehicles (NGV). Although Pd is the most active catalyst for CH₄ oxidation, the presence of H₂O suppresses the catalyst activity. The effect of H₂O on the activity of Pd/Al₂O₃ catalysts with Pd loadings of 0.3, 2.6 and 6.5Pd (wt.%) and corresponding dispersions of 57%, 48%, and 33%, was well described by a kinetic model that accounted for the effect of H₂O. Langmuir adsorption was assumed to determine the amount of H₂O adsorbed on active sites for the catalysts with different Pd dispersions under wet and dry reaction conditions. The estimated kinetic parameters of apparent activation energy, Ea of 60.6±11.5 kJ.mol-¹ and heat of H₂O adsorption, ∆H(H₂O) of -81.5±9.1 kJ.mol-¹ indicate that CH₄ oxidation is independent of Pd dispersion. Using different preparation methods and varying Ce:Pd ratios, it was found that sequential impregnation of the Al₂O₃ support by Ce and Pd, with Ce:Pd ratio of 5, yielded a catalyst that had the least inhibition by H₂O. H₂O adsorption is the dominant mechanism for activity loss, although some sintering of the support may also occur. In a Time-on-Stream (TOS) study with extra H₂O added to the feed gas, the chemical and physical properties of the catalysts showed only small changes before and after use. The less negative effect of H₂O at higher temperature and at lower H₂O concentration was also confirmed by the kinetic study. The kinetic model is consistent with a Langmuir mechanism in which H₂O adsorption suppresses C-H bond activation on the active sites. The kinetic analysis shows that the Ce added to the PdO/Al₂O₃ catalyst suppresses the amount of H₂O adsorbed onto the catalyst, thereby reducing the H₂O inhibition effect in the presence of Ce.","abstract_html":"Natural gas is a promising alternative fuel for transportation systems because of reduced CO, CO₂, SO₂, and NOx emissions into the environment, and its abundance and low cost compared with gasoline and diesel. A significant obstacle in the use of NG for vehicle fuels is that CH₄ is difficult to oxidize in the presence of CO₂ and H₂O and at the low exhaust gas temperature (500-550°C) of natural gas vehicles (NGV). Although Pd is the most active catalyst for CH₄ oxidation, the presence of H₂O suppresses the catalyst activity. The effect of H₂O on the activity of Pd/Al₂O₃ catalysts with Pd loadings of 0.3, 2.6 and 6.5Pd (wt.%) and corresponding dispersions of 57%, 48%, and 33%, was well described by a kinetic model that accounted for the effect of H₂O. Langmuir adsorption was assumed to determine the amount of H₂O adsorbed on active sites for the catalysts with different Pd dispersions under wet and dry reaction conditions. The estimated kinetic parameters of apparent activation energy, Ea of 60.6±11.5 kJ.mol-¹ and heat of H₂O adsorption, ∆H(H₂O) of -81.5±9.1 kJ.mol-¹ indicate that CH₄ oxidation is independent of Pd dispersion. Using different preparation methods and varying Ce:Pd ratios, it was found that sequential impregnation of the Al₂O₃ support by Ce and Pd, with Ce:Pd ratio of 5, yielded a catalyst that had the least inhibition by H₂O. H₂O adsorption is the dominant mechanism for activity loss, although some sintering of the support may also occur. In a Time-on-Stream (TOS) study with extra H₂O added to the feed gas, the chemical and physical properties of the catalysts showed only small changes before and after use. The less negative effect of H₂O at higher temperature and at lower H₂O concentration was also confirmed by the kinetic study. The kinetic model is consistent with a Langmuir mechanism in which H₂O adsorption suppresses C-H bond activation on the active sites. The kinetic analysis shows that the Ce added to the PdO/Al₂O₃ catalyst suppresses the amount of H₂O adsorbed onto the catalyst, thereby reducing the H₂O inhibition effect in the presence of Ce.","abstract_has_math":false,"creators":["Alyani, Mina"],"institution":"University of British Columbia","degree_name":"Doctor of Philosophy - PhD","degree_level":"doctoral","degree_discipline":"Chemical and Biological Engineering","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2016,"date_issued":"2016","date_published":"2016","updated_at":"2026-11-19T15:00:29Z","subjects":[],"languages":["eng"],"rights":["Attribution-NonCommercial-NoDerivatives 4.0 International"],"rights_urls":["http://creativecommons.org/licenses/by-nc-nd/4.0/"],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/2429/58950","outbound_label":"Handle","outbound_source":"dc:identifier","record_url":"http://hdl.handle.net/2429/58950","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier","download_url":"http://circle.library.ubc.ca/bitstream/2429/58950/4/ubc_2016_september_alyani_mina.pdf","download_label":"Download PDF","download_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"http://circle.library.ubc.ca/oai/request?verb=GetRecord&metadataPrefix=etdms&identifier=oai%3Acircle.library.ubc.ca%3A2429%2F58950","prefix":"etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Alyani, Mina"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2016"]},{"key":"dc:publisher","label":"Institution","values":["University of British Columbia"]},{"key":"dc:type","label":"Dc Type","values":["Text"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Chemical and Biological Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["doctoral"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Doctor of Philosophy - PhD"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of British Columbia"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["eng"]},{"key":"dc:rights","label":"Dc Rights","values":["http://creativecommons.org/licenses/by-nc-nd/4.0/","Attribution-NonCommercial-NoDerivatives 4.0 International"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["http://hdl.handle.net/2429/58950","http://circle.library.ubc.ca/bitstream/2429/58950/4/ubc_2016_september_alyani_mina.pdf"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["Natural gas is a promising alternative fuel for transportation systems because of reduced CO, CO₂, SO₂, and NOx emissions into the environment, and its abundance and low cost compared with gasoline and diesel. A significant obstacle in the use of NG for vehicle fuels is that CH₄ is difficult to oxidize in the presence of CO₂ and H₂O and at the low exhaust gas temperature (500-550°C) of natural gas vehicles (NGV). Although Pd is the most active catalyst for CH₄ oxidation, the presence of H₂O suppresses the catalyst activity. The effect of H₂O on the activity of Pd/Al₂O₃ catalysts with Pd loadings of 0.3, 2.6 and 6.5Pd (wt.%) and corresponding dispersions of 57%, 48%, and 33%, was well described by a kinetic model that accounted for the effect of H₂O. Langmuir adsorption was assumed to determine the amount of H₂O adsorbed on active sites for the catalysts with different Pd dispersions under wet and dry reaction conditions. The estimated kinetic parameters of apparent activation energy, Ea of 60.6±11.5 kJ.mol-¹ and heat of H₂O adsorption, ∆H(H₂O) of -81.5±9.1 kJ.mol-¹ indicate that CH₄ oxidation is independent of Pd dispersion. Using different preparation methods and varying Ce:Pd ratios, it was found that sequential impregnation of the Al₂O₃ support by Ce and Pd, with Ce:Pd ratio of 5, yielded a catalyst that had the least inhibition by H₂O. H₂O adsorption is the dominant mechanism for activity loss, although some sintering of the support may also occur. In a Time-on-Stream (TOS) study with extra H₂O added to the feed gas, the chemical and physical properties of the catalysts showed only small changes before and after use. The less negative effect of H₂O at higher temperature and at lower H₂O concentration was also confirmed by the kinetic study. The kinetic model is consistent with a Langmuir mechanism in which H₂O adsorption suppresses C-H bond activation on the active sites. The kinetic analysis shows that the Ce added to the PdO/Al₂O₃ catalyst suppresses the amount of H₂O adsorbed onto the catalyst, thereby reducing the H₂O inhibition effect in the presence of Ce."]},{"key":"dc:format","label":"Dc Format","values":["4050763","application/pdf"]},{"key":"dc:title","label":"Title","values":["Effect of H₂O on CH₄ oxidation over PdO/Al₂O₃ and CeOx/PdO/Al₂O₃ catalysts"]}]}],"canonical_facts":{"dc:creator":["Alyani, Mina"],"dc:date":["2016"],"dc:description":["Natural gas is a promising alternative fuel for transportation systems because of reduced CO, CO₂, SO₂, and NOx emissions into the environment, and its abundance and low cost compared with gasoline and diesel. A significant obstacle in the use of NG for vehicle fuels is that CH₄ is difficult to oxidize in the presence of CO₂ and H₂O and at the low exhaust gas temperature (500-550°C) of natural gas vehicles (NGV). Although Pd is the most active catalyst for CH₄ oxidation, the presence of H₂O suppresses the catalyst activity. The effect of H₂O on the activity of Pd/Al₂O₃ catalysts with Pd loadings of 0.3, 2.6 and 6.5Pd (wt.%) and corresponding dispersions of 57%, 48%, and 33%, was well described by a kinetic model that accounted for the effect of H₂O. Langmuir adsorption was assumed to determine the amount of H₂O adsorbed on active sites for the catalysts with different Pd dispersions under wet and dry reaction conditions. The estimated kinetic parameters of apparent activation energy, Ea of 60.6±11.5 kJ.mol-¹ and heat of H₂O adsorption, ∆H(H₂O) of -81.5±9.1 kJ.mol-¹ indicate that CH₄ oxidation is independent of Pd dispersion. Using different preparation methods and varying Ce:Pd ratios, it was found that sequential impregnation of the Al₂O₃ support by Ce and Pd, with Ce:Pd ratio of 5, yielded a catalyst that had the least inhibition by H₂O. H₂O adsorption is the dominant mechanism for activity loss, although some sintering of the support may also occur. In a Time-on-Stream (TOS) study with extra H₂O added to the feed gas, the chemical and physical properties of the catalysts showed only small changes before and after use. The less negative effect of H₂O at higher temperature and at lower H₂O concentration was also confirmed by the kinetic study. The kinetic model is consistent with a Langmuir mechanism in which H₂O adsorption suppresses C-H bond activation on the active sites. The kinetic analysis shows that the Ce added to the PdO/Al₂O₃ catalyst suppresses the amount of H₂O adsorbed onto the catalyst, thereby reducing the H₂O inhibition effect in the presence of Ce."],"dc:format":["4050763","application/pdf"],"dc:identifier":["http://hdl.handle.net/2429/58950","http://circle.library.ubc.ca/bitstream/2429/58950/4/ubc_2016_september_alyani_mina.pdf"],"dc:language":["eng"],"dc:publisher":["University of British Columbia"],"dc:rights":["http://creativecommons.org/licenses/by-nc-nd/4.0/","Attribution-NonCommercial-NoDerivatives 4.0 International"],"dc:title":["Effect of H₂O on CH₄ oxidation over PdO/Al₂O₃ and CeOx/PdO/Al₂O₃ catalysts"],"dc:type":["Text"],"thesis:degree_discipline":["Chemical and Biological Engineering"],"thesis:degree_level":["doctoral"],"thesis:degree_name":["Doctor of Philosophy - PhD"],"thesis:institution_name":["University of British Columbia"]},"updated_at":"2026-11-19T15:00:29Z"}