{"id":{"repo_id":"ucl","oai_identifier":"oai:eprints.ucl.ac.uk.OAI2:10102009"},"canonical_url":"https://search.ndltd.org/etd/ucl/oai:eprints.ucl.ac.uk.OAI2:10102009","repository":{"repo_id":"ucl","name":"University College London","base_url":"https://discovery.ucl.ac.uk/cgi/oai2"},"display":{"title":"Chemical vapour deposition of tungsten oxide thin films from single-source precursors","abstract":"This thesis describes the chemical vapour deposition (CVD) of tungsten oxide thin films on glass from a wide range of single-source precursors. Chapter 1 describes previous work that has motivated this research. Chapter 2 discusses the synthesis of conventional style candidates for single-source precursors. Reactions of WOCl4 with 3-methyl salicylic acid (MesaliH2) and 3,5-di-iso-propyl salicylic acid (di-i-PrsaliH2) yielded the ditungsten complexes [WO(Mesali)(MesaliH)2(μ-O)], 1, and [WO(di-i-Prsali)(di-i-PrsaliH)2(μ-O)], 2, and the monotungsten complex [WO(di-i-Pr sali)(di-i-PrsaliH)Cl], 3. Tungsten(VI) dioxo complexes were prepared by ligand exchange reactions of [WO2(acac)2], 4, yielding [WO2(catH)2], 5, and [WO2(malt)2], 6, (catH2 = 3,5-di-tert-butyl-catechol; maltH = maltol). Chapter 3 describes thermal analyses of the complexes 1 - 6 and tungsten hexaphenoxide, and consequently their suitability for CVD. The use of [W(OPh)6] and 2 - 6 in aerosol assisted CVD is reported in Chapter 4. Brown tungsten oxide was deposited from 2 and 3 at 600 °C; blue partially-reduced WO3-x thin films were deposited from [W(OPh)6] from 300 to 500 °C, from 4 at 600 °C and 6 at 620 °C. Sintering all of the coatings in air at 550 °C afforded yellow films of stoichiometric WO3. Raman spectroscopy and glancing angle XRD showed that coatings deposited from [W(OPh)6] at 300 °C were amorphous, whereas all the other films were the monoclinic phase γ-tungsten oxide. Taking full advantage of the aerosol vaporisation technique led to the CVD of tungsten oxide films from polyoxometalate single-source precursors, as described in Chapter 5. The isopolyanion [nBu4N]2[W6O19], 7, afforded WO3 at 410 °C; the heteropolyanions [nBu4N]4H3[PW11O39], 8, and [nBu4N]4[PNbW11O40], 9, were used to deposit doped WO3 thin films in a highly-controlled manner at 480 °C. Thus, the unprecedented use of large, charged clusters for CVD was demonstrated. Chapter 6 describes investigations of the tungsten oxide films as photocatalysts for the destruction of organic pollutants. Fully-oxidised, yellow WO3 coatings showed excellent photocatalytic activity for the destruction of an over-layer of stearic acid. This could lead to the application of tungsten oxide films on glass as self-cleaning windows.","abstract_html":"This thesis describes the chemical vapour deposition (CVD) of tungsten oxide thin films on glass from a wide range of single-source precursors. Chapter 1 describes previous work that has motivated this research. Chapter 2 discusses the synthesis of conventional style candidates for single-source precursors. Reactions of WOCl4 with 3-methyl salicylic acid (MesaliH2) and 3,5-di-iso-propyl salicylic acid (di-i-PrsaliH2) yielded the ditungsten complexes [WO(Mesali)(MesaliH)2(μ-O)], 1, and [WO(di-i-Prsali)(di-i-PrsaliH)2(μ-O)], 2, and the monotungsten complex [WO(di-i-Pr sali)(di-i-PrsaliH)Cl], 3. Tungsten(VI) dioxo complexes were prepared by ligand exchange reactions of [WO2(acac)2], 4, yielding [WO2(catH)2], 5, and [WO2(malt)2], 6, (catH2 = 3,5-di-tert-butyl-catechol; maltH = maltol). Chapter 3 describes thermal analyses of the complexes 1 - 6 and tungsten hexaphenoxide, and consequently their suitability for CVD. The use of [W(OPh)6] and 2 - 6 in aerosol assisted CVD is reported in Chapter 4. Brown tungsten oxide was deposited from 2 and 3 at 600 °C; blue partially-reduced WO3-x thin films were deposited from [W(OPh)6] from 300 to 500 °C, from 4 at 600 °C and 6 at 620 °C. Sintering all of the coatings in air at 550 °C afforded yellow films of stoichiometric WO3. Raman spectroscopy and glancing angle XRD showed that coatings deposited from [W(OPh)6] at 300 °C were amorphous, whereas all the other films were the monoclinic phase γ-tungsten oxide. Taking full advantage of the aerosol vaporisation technique led to the CVD of tungsten oxide films from polyoxometalate single-source precursors, as described in Chapter 5. The isopolyanion [nBu4N]2[W6O19], 7, afforded WO3 at 410 °C; the heteropolyanions [nBu4N]4H3[PW11O39], 8, and [nBu4N]4[PNbW11O40], 9, were used to deposit doped WO3 thin films in a highly-controlled manner at 480 °C. Thus, the unprecedented use of large, charged clusters for CVD was demonstrated. Chapter 6 describes investigations of the tungsten oxide films as photocatalysts for the destruction of organic pollutants. Fully-oxidised, yellow WO3 coatings showed excellent photocatalytic activity for the destruction of an over-layer of stearic acid. This could lead to the application of tungsten oxide films on glass as self-cleaning windows.","abstract_has_math":false,"creators":["Cross, Warren Bradley"],"institution":"UCL (University College London)","degree_name":null,"degree_level":"Doctoral","degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2003,"date_issued":"2003","date_published":"2003","updated_at":"2026-11-26T06:24:24Z","subjects":[],"languages":["en","eng"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://discovery.ucl.ac.uk/id/eprint/10102009/","outbound_label":"Repository record","outbound_source":"dc:identifier.uri","record_url":"https://discovery.ucl.ac.uk/id/eprint/10102009/","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aucl%3Aoai%3Aeprints.ucl.ac.uk.OAI2%3A10102009","prefix":"oai_dc"},"source_record":{"url":"https://discovery.ucl.ac.uk/cgi/oai2?verb=GetRecord&metadataPrefix=uketd_dc&identifier=oai%3Aeprints.ucl.ac.uk.OAI2%3A10102009","prefix":"uketd_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Cross, Warren Bradley"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2003"]},{"key":"dc:date.issued","label":"Date","values":["2003"]},{"key":"dc:publisher.institution","label":"Dc Publisher Institution","values":["UCL (University College London)"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"dc:type.qualificationlevel","label":"Dc Type Qualificationlevel","values":["Doctoral"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["en","eng"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://discovery.ucl.ac.uk/id/eprint/10102009/"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["This thesis describes the chemical vapour deposition (CVD) of tungsten oxide thin films on glass from a wide range of single-source precursors. Chapter 1 describes previous work that has motivated this research. Chapter 2 discusses the synthesis of conventional style candidates for single-source precursors. Reactions of WOCl4 with 3-methyl salicylic acid (MesaliH2) and 3,5-di-iso-propyl salicylic acid (di-i-PrsaliH2) yielded the ditungsten complexes [WO(Mesali)(MesaliH)2(μ-O)], 1, and [WO(di-i-Prsali)(di-i-PrsaliH)2(μ-O)], 2, and the monotungsten complex [WO(di-i-Pr sali)(di-i-PrsaliH)Cl], 3. Tungsten(VI) dioxo complexes were prepared by ligand exchange reactions of [WO2(acac)2], 4, yielding [WO2(catH)2], 5, and [WO2(malt)2], 6, (catH2 = 3,5-di-tert-butyl-catechol; maltH = maltol). Chapter 3 describes thermal analyses of the complexes 1 - 6 and tungsten hexaphenoxide, and consequently their suitability for CVD. The use of [W(OPh)6] and 2 - 6 in aerosol assisted CVD is reported in Chapter 4. Brown tungsten oxide was deposited from 2 and 3 at 600 °C; blue partially-reduced WO3-x thin films were deposited from [W(OPh)6] from 300 to 500 °C, from 4 at 600 °C and 6 at 620 °C. Sintering all of the coatings in air at 550 °C afforded yellow films of stoichiometric WO3. Raman spectroscopy and glancing angle XRD showed that coatings deposited from [W(OPh)6] at 300 °C were amorphous, whereas all the other films were the monoclinic phase γ-tungsten oxide. Taking full advantage of the aerosol vaporisation technique led to the CVD of tungsten oxide films from polyoxometalate single-source precursors, as described in Chapter 5. The isopolyanion [nBu4N]2[W6O19], 7, afforded WO3 at 410 °C; the heteropolyanions [nBu4N]4H3[PW11O39], 8, and [nBu4N]4[PNbW11O40], 9, were used to deposit doped WO3 thin films in a highly-controlled manner at 480 °C. Thus, the unprecedented use of large, charged clusters for CVD was demonstrated. Chapter 6 describes investigations of the tungsten oxide films as photocatalysts for the destruction of organic pollutants. Fully-oxidised, yellow WO3 coatings showed excellent photocatalytic activity for the destruction of an over-layer of stearic acid. This could lead to the application of tungsten oxide films on glass as self-cleaning windows."]},{"key":"dc:format","label":"Dc Format","values":["text"]},{"key":"dcterms:accessrights","label":"Dcterms Accessrights","values":["public"]},{"key":"dc:title","label":"Title","values":["Chemical vapour deposition of tungsten oxide thin films from single-source precursors"]}]}],"canonical_facts":{"dc:creator":["Cross, Warren Bradley"],"dc:date":["2003"],"dc:date.issued":["2003"],"dc:description.abstract":["This thesis describes the chemical vapour deposition (CVD) of tungsten oxide thin films on glass from a wide range of single-source precursors. Chapter 1 describes previous work that has motivated this research. Chapter 2 discusses the synthesis of conventional style candidates for single-source precursors. Reactions of WOCl4 with 3-methyl salicylic acid (MesaliH2) and 3,5-di-iso-propyl salicylic acid (di-i-PrsaliH2) yielded the ditungsten complexes [WO(Mesali)(MesaliH)2(μ-O)], 1, and [WO(di-i-Prsali)(di-i-PrsaliH)2(μ-O)], 2, and the monotungsten complex [WO(di-i-Pr sali)(di-i-PrsaliH)Cl], 3. Tungsten(VI) dioxo complexes were prepared by ligand exchange reactions of [WO2(acac)2], 4, yielding [WO2(catH)2], 5, and [WO2(malt)2], 6, (catH2 = 3,5-di-tert-butyl-catechol; maltH = maltol). Chapter 3 describes thermal analyses of the complexes 1 - 6 and tungsten hexaphenoxide, and consequently their suitability for CVD. The use of [W(OPh)6] and 2 - 6 in aerosol assisted CVD is reported in Chapter 4. Brown tungsten oxide was deposited from 2 and 3 at 600 °C; blue partially-reduced WO3-x thin films were deposited from [W(OPh)6] from 300 to 500 °C, from 4 at 600 °C and 6 at 620 °C. Sintering all of the coatings in air at 550 °C afforded yellow films of stoichiometric WO3. Raman spectroscopy and glancing angle XRD showed that coatings deposited from [W(OPh)6] at 300 °C were amorphous, whereas all the other films were the monoclinic phase γ-tungsten oxide. Taking full advantage of the aerosol vaporisation technique led to the CVD of tungsten oxide films from polyoxometalate single-source precursors, as described in Chapter 5. The isopolyanion [nBu4N]2[W6O19], 7, afforded WO3 at 410 °C; the heteropolyanions [nBu4N]4H3[PW11O39], 8, and [nBu4N]4[PNbW11O40], 9, were used to deposit doped WO3 thin films in a highly-controlled manner at 480 °C. Thus, the unprecedented use of large, charged clusters for CVD was demonstrated. Chapter 6 describes investigations of the tungsten oxide films as photocatalysts for the destruction of organic pollutants. Fully-oxidised, yellow WO3 coatings showed excellent photocatalytic activity for the destruction of an over-layer of stearic acid. This could lead to the application of tungsten oxide films on glass as self-cleaning windows."],"dc:format":["text"],"dc:identifier.uri":["https://discovery.ucl.ac.uk/id/eprint/10102009/"],"dc:language":["en","eng"],"dc:publisher.institution":["UCL (University College London)"],"dcterms:accessrights":["public"],"dc:title":["Chemical vapour deposition of tungsten oxide thin films from single-source precursors"],"dc:type":["Thesis"],"dc:type.qualificationlevel":["Doctoral"]},"updated_at":"2026-11-26T06:24:24Z"}