{"id":{"repo_id":"umn","oai_identifier":"oai:conservancy.umn.edu:11299/146450"},"canonical_url":"https://search.ndltd.org/etd/umn/oai:conservancy.umn.edu:11299/146450","repository":{"repo_id":"umn","name":"University of Minnesota","base_url":"https://conservancy.umn.edu/server/oai/request"},"display":{"title":"Size effect on fatigue crack growth of a quasibrittle material","abstract":"The Paris-Erdogan law describes the rate of fatigue crack growth as a function of the amplitude of the applied stress intensity factor. This equation, however, does not include a dependence of the crack growth on the structure size, which has been observed experimentally for concrete. The size effect on the fatigue crack growth is derived based on two hypotheses: (1) the scaling of the critical energy dissipation for fatigue crack growth has the same form as that of fracture energy for monotonic loading; (2) the difference in transitional sizes between the fatigue and monotonic loading is purely due to the difference in the fracture process zone (FPZ) size. The size-dependent fatigue crack growth law is verified experimentally through size effect tests on Berea sandstone. Using digital image correlation, it is shown that the FPZ length is approximately 7 mm and 11 mm for monotonic and cyclic loading, respectively. Optimal fitting resulted in transitional sizes of 34 mm and 54 mm for monotonic loading and cyclic loading, respectively, which shows a proportional relationship between the FPZ length and the transitional size.","abstract_html":"The Paris-Erdogan law describes the rate of fatigue crack growth as a function of the amplitude of the applied stress intensity factor. This equation, however, does not include a dependence of the crack growth on the structure size, which has been observed experimentally for concrete. The size effect on the fatigue crack growth is derived based on two hypotheses: (1) the scaling of the critical energy dissipation for fatigue crack growth has the same form as that of fracture energy for monotonic loading; (2) the difference in transitional sizes between the fatigue and monotonic loading is purely due to the difference in the fracture process zone (FPZ) size. The size-dependent fatigue crack growth law is verified experimentally through size effect tests on Berea sandstone. Using digital image correlation, it is shown that the FPZ length is approximately 7 mm and 11 mm for monotonic and cyclic loading, respectively. Optimal fitting resulted in transitional sizes of 34 mm and 54 mm for monotonic loading and cyclic loading, respectively, which shows a proportional relationship between the FPZ length and the transitional size.","abstract_has_math":false,"creators":["Manning, Jonathan"],"institution":null,"degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2013,"date_issued":"2013-01","date_published":"2013-01","updated_at":"2026-11-19T08:37:19Z","subjects":["Fatigue","Fracture","Paris Law","Quasibrittle","Sandstone","Size effect"],"languages":["en_US"],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier.citation","label":"Dc Identifier Citation","values":["Manning, Jonathan. (2013). Size effect on fatigue crack growth of a quasibrittle material. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/146450."],"render_values":[{"text":"Manning, Jonathan. (2013). Size effect on fatigue crack growth of a quasibrittle material. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/146450.","href":null,"code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"http://purl.umn.edu/146450","outbound_label":"Repository record","outbound_source":"dc:identifier.uri","record_url":"http://purl.umn.edu/146450","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier.uri","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://conservancy.umn.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Aconservancy.umn.edu%3A11299%2F146450","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Manning, Jonathan"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2013-03-13T16:09:27Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2013-03-13T16:09:27Z"]},{"key":"dc:date.issued","label":"Date","values":["2013-01"]},{"key":"dc:type","label":"Dc Type","values":["Thesis or Dissertation"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Fatigue","Fracture","Paris Law","Quasibrittle","Sandstone","Size effect"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en_US"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.citation","label":"Dc Identifier Citation","values":["Manning, Jonathan. (2013). Size effect on fatigue crack growth of a quasibrittle material. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/146450."]},{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://purl.umn.edu/146450"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["University of Minnesota M.S. thesis. January 2013. Major: Civil Engineering. Advisors:Joseph F. Labuz and Jia-Liang Le. 1 computer file (PDF); iv, 67 pages."]},{"key":"dc:description.abstract","label":"Abstract","values":["The Paris-Erdogan law describes the rate of fatigue crack growth as a function of the amplitude of the applied stress intensity factor. This equation, however, does not include a dependence of the crack growth on the structure size, which has been observed experimentally for concrete. The size effect on the fatigue crack growth is derived based on two hypotheses: (1) the scaling of the critical energy dissipation for fatigue crack growth has the same form as that of fracture energy for monotonic loading; (2) the difference in transitional sizes between the fatigue and monotonic loading is purely due to the difference in the fracture process zone (FPZ) size. The size-dependent fatigue crack growth law is verified experimentally through size effect tests on Berea sandstone. Using digital image correlation, it is shown that the FPZ length is approximately 7 mm and 11 mm for monotonic and cyclic loading, respectively. Optimal fitting resulted in transitional sizes of 34 mm and 54 mm for monotonic loading and cyclic loading, respectively, which shows a proportional relationship between the FPZ length and the transitional size."]},{"key":"dc:title","label":"Title","values":["Size effect on fatigue crack growth of a quasibrittle material"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:creator":["Manning, Jonathan"],"dc:date.accessioned":["2013-03-13T16:09:27Z"],"dc:date.available":["2013-03-13T16:09:27Z"],"dc:date.issued":["2013-01"],"dc:description":["University of Minnesota M.S. thesis. January 2013. Major: Civil Engineering. Advisors:Joseph F. Labuz and Jia-Liang Le. 1 computer file (PDF); iv, 67 pages."],"dc:description.abstract":["The Paris-Erdogan law describes the rate of fatigue crack growth as a function of the amplitude of the applied stress intensity factor. This equation, however, does not include a dependence of the crack growth on the structure size, which has been observed experimentally for concrete. The size effect on the fatigue crack growth is derived based on two hypotheses: (1) the scaling of the critical energy dissipation for fatigue crack growth has the same form as that of fracture energy for monotonic loading; (2) the difference in transitional sizes between the fatigue and monotonic loading is purely due to the difference in the fracture process zone (FPZ) size. The size-dependent fatigue crack growth law is verified experimentally through size effect tests on Berea sandstone. Using digital image correlation, it is shown that the FPZ length is approximately 7 mm and 11 mm for monotonic and cyclic loading, respectively. Optimal fitting resulted in transitional sizes of 34 mm and 54 mm for monotonic loading and cyclic loading, respectively, which shows a proportional relationship between the FPZ length and the transitional size."],"dc:identifier.citation":["Manning, Jonathan. (2013). Size effect on fatigue crack growth of a quasibrittle material. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/146450."],"dc:identifier.uri":["http://purl.umn.edu/146450"],"dc:language.iso":["en_US"],"dc:subject":["Fatigue","Fracture","Paris Law","Quasibrittle","Sandstone","Size effect"],"dc:title":["Size effect on fatigue crack growth of a quasibrittle material"],"dc:type":["Thesis or Dissertation"],"others:access_status":["open.access"]},"updated_at":"2026-11-19T08:37:19Z"}