{"id":{"repo_id":"umn","oai_identifier":"oai:conservancy.umn.edu:11299/200156"},"canonical_url":"https://search.ndltd.org/etd/umn/oai:conservancy.umn.edu:11299/200156","repository":{"repo_id":"umn","name":"University of Minnesota","base_url":"https://conservancy.umn.edu/server/oai/request"},"display":{"title":"Bond Behavior of Post-Installed GFRP Bars in Structural Connections","abstract":"This research presents an experimental study with GFRP bars from three manufacturers, each having different bar textures (silica coated with helical wraps, silica coated and ribbed) used as post-installed (epoxy and cementitious adhesive) and cast-in-place reinforcement. Twenty test specimens were constructed and tested under static load. A test specimen was composed of two identical vertical elements, which were anchored into the base of the specimen using post-installed GFRP bars. The variables tested among different specimens included: concrete compressive strength (3 and 6 ksi), embedment length of GFRP bars (6 and 11.5 in.), and size of the post-installed GFRP bars (#4, #6, and #8). Concrete breakout was the only failure mode in all of the specimens with post-installed GFRP. Bond strengths and peak applied loads improved by increasing concrete strengths and embedment depths. The larger diameter bars (#6 and #8) showed a loss of bond strength compared to #4 bars.","abstract_html":"This research presents an experimental study with GFRP bars from three manufacturers, each having different bar textures (silica coated with helical wraps, silica coated and ribbed) used as post-installed (epoxy and cementitious adhesive) and cast-in-place reinforcement. Twenty test specimens were constructed and tested under static load. A test specimen was composed of two identical vertical elements, which were anchored into the base of the specimen using post-installed GFRP bars. The variables tested among different specimens included: concrete compressive strength (3 and 6 ksi), embedment length of GFRP bars (6 and 11.5 in.), and size of the post-installed GFRP bars (#4, #6, and #8). Concrete breakout was the only failure mode in all of the specimens with post-installed GFRP. Bond strengths and peak applied loads improved by increasing concrete strengths and embedment depths. The larger diameter bars (#6 and #8) showed a loss of bond strength compared to #4 bars.","abstract_has_math":false,"creators":["Bajwa, Muhammad Shahraiz"],"institution":null,"degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2018,"date_issued":"2018-06","date_published":"2018-06","updated_at":"2026-11-19T08:39:07Z","subjects":["Anchorage","Bond Behavior","GFRP Bars","Post-Installed"],"languages":["en"],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier.citation","label":"Dc Identifier Citation","values":["Bajwa, Muhammad Shahraiz. (2018). Bond Behavior of Post-Installed GFRP Bars in Structural Connections. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/200156."],"render_values":[{"text":"Bajwa, Muhammad Shahraiz. (2018). Bond Behavior of Post-Installed GFRP Bars in Structural Connections. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/200156.","href":null,"code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/11299/200156","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/11299/200156","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aumn%3Aoai%3Aconservancy.umn.edu%3A11299%2F200156","prefix":"oai_dc"},"source_record":{"url":"https://conservancy.umn.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Aconservancy.umn.edu%3A11299%2F200156","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Bajwa, Muhammad Shahraiz"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2018-09-21T16:06:11Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2018-09-21T16:06:11Z"]},{"key":"dc:date.issued","label":"Date","values":["2018-06"]},{"key":"dc:type","label":"Dc Type","values":["Thesis or Dissertation"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Anchorage","Bond Behavior","GFRP Bars","Post-Installed"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.citation","label":"Dc Identifier Citation","values":["Bajwa, Muhammad Shahraiz. (2018). Bond Behavior of Post-Installed GFRP Bars in Structural Connections. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/200156."]},{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/11299/200156"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["University of Minnesota M.S. thesis.June 2018. Major: Civil Engineering. Advisors: Benjamin Dymond, Rania Al-Hammoud. 1 computer file (PDF); viii, 158 pages."]},{"key":"dc:description.abstract","label":"Abstract","values":["This research presents an experimental study with GFRP bars from three manufacturers, each having different bar textures (silica coated with helical wraps, silica coated and ribbed) used as post-installed (epoxy and cementitious adhesive) and cast-in-place reinforcement. Twenty test specimens were constructed and tested under static load. A test specimen was composed of two identical vertical elements, which were anchored into the base of the specimen using post-installed GFRP bars. The variables tested among different specimens included: concrete compressive strength (3 and 6 ksi), embedment length of GFRP bars (6 and 11.5 in.), and size of the post-installed GFRP bars (#4, #6, and #8). Concrete breakout was the only failure mode in all of the specimens with post-installed GFRP. Bond strengths and peak applied loads improved by increasing concrete strengths and embedment depths. The larger diameter bars (#6 and #8) showed a loss of bond strength compared to #4 bars."]},{"key":"dc:title","label":"Title","values":["Bond Behavior of Post-Installed GFRP Bars in Structural Connections"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:creator":["Bajwa, Muhammad Shahraiz"],"dc:date.accessioned":["2018-09-21T16:06:11Z"],"dc:date.available":["2018-09-21T16:06:11Z"],"dc:date.issued":["2018-06"],"dc:description":["University of Minnesota M.S. thesis.June 2018. Major: Civil Engineering. Advisors: Benjamin Dymond, Rania Al-Hammoud. 1 computer file (PDF); viii, 158 pages."],"dc:description.abstract":["This research presents an experimental study with GFRP bars from three manufacturers, each having different bar textures (silica coated with helical wraps, silica coated and ribbed) used as post-installed (epoxy and cementitious adhesive) and cast-in-place reinforcement. Twenty test specimens were constructed and tested under static load. A test specimen was composed of two identical vertical elements, which were anchored into the base of the specimen using post-installed GFRP bars. The variables tested among different specimens included: concrete compressive strength (3 and 6 ksi), embedment length of GFRP bars (6 and 11.5 in.), and size of the post-installed GFRP bars (#4, #6, and #8). Concrete breakout was the only failure mode in all of the specimens with post-installed GFRP. Bond strengths and peak applied loads improved by increasing concrete strengths and embedment depths. The larger diameter bars (#6 and #8) showed a loss of bond strength compared to #4 bars."],"dc:identifier.citation":["Bajwa, Muhammad Shahraiz. (2018). Bond Behavior of Post-Installed GFRP Bars in Structural Connections. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/200156."],"dc:identifier.uri":["http://hdl.handle.net/11299/200156"],"dc:language.iso":["en"],"dc:subject":["Anchorage","Bond Behavior","GFRP Bars","Post-Installed"],"dc:title":["Bond Behavior of Post-Installed GFRP Bars in Structural Connections"],"dc:type":["Thesis or Dissertation"],"others:access_status":["open.access"]},"updated_at":"2026-11-19T08:39:07Z"}