{"id":{"repo_id":"unt","oai_identifier":"info:ark/67531/metadc2415980"},"canonical_url":"https://search.ndltd.org/etd/unt/info:ark/67531/metadc2415980","repository":{"repo_id":"unt","name":"University of North Texas","base_url":"https://digital.library.unt.edu/oai/"},"display":{"title":"The Effect of B2O3 Addition and Temperature Optimization on Mechanical Properties of Laminated Alumina and Yttria Stabilized Zirconia","abstract":"The effect of sintering aid B2O3 and the effect of sintering temperatures were evaluated in this thesis. A 7:3 ratio of alumina to 3 mol% yttria stabilized zirconia tape cast layers sintered at temperatures of 1500°C, 1550°C, and 1600°C were evaluated with an addition of 0 mol%, 1 mol%, and 3 mol% B2O3 additions to the yttria stabilized zirconia layer. X-ray microscopy were used to evaluate crack propagation to correlate with the flexural strengths found in three-point bend testing. Dilatometry was used to show the effect that the B2O3 addition had on the thermal expansion of the system. The addition of B2O3 was found to decrease the flexural strength of the alumina/YSZ laminate system. X-ray microscopy shows significant damage in the 1 mol% and 3 mol% B2O3 additions. The dilatometry suggests that 3 mol% destabilizes the YSZ layer, causing the YSZ to transform back into the monoclinic phase on cool down. The cracks rarely continued to propagate into the alumina layer, further confirming that the alumina/YSZ laminate combination has optimally weak interfaces. The temperature with the highest flexural strength for the 0 mol% B2O3 samples was shown to be 1600°C while the temperature with the highest flexural strength for the 1 mol% and 3 mol% B2O3 samples were shown to be 1550°C.","abstract_html":"The effect of sintering aid B2O3 and the effect of sintering temperatures were evaluated in this thesis. A 7:3 ratio of alumina to 3 mol% yttria stabilized zirconia tape cast layers sintered at temperatures of 1500°C, 1550°C, and 1600°C were evaluated with an addition of 0 mol%, 1 mol%, and 3 mol% B2O3 additions to the yttria stabilized zirconia layer. X-ray microscopy were used to evaluate crack propagation to correlate with the flexural strengths found in three-point bend testing. Dilatometry was used to show the effect that the B2O3 addition had on the thermal expansion of the system. The addition of B2O3 was found to decrease the flexural strength of the alumina/YSZ laminate system. X-ray microscopy shows significant damage in the 1 mol% and 3 mol% B2O3 additions. The dilatometry suggests that 3 mol% destabilizes the YSZ layer, causing the YSZ to transform back into the monoclinic phase on cool down. The cracks rarely continued to propagate into the alumina layer, further confirming that the alumina/YSZ laminate combination has optimally weak interfaces. The temperature with the highest flexural strength for the 0 mol% B2O3 samples was shown to be 1600°C while the temperature with the highest flexural strength for the 1 mol% and 3 mol% B2O3 samples were shown to be 1550°C.","abstract_has_math":false,"creators":["Ober, Evan Thomas"],"institution":"University of North Texas","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":["Reidy III, Richard F","Du, Jincheng","Wang, Ruocun"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2024,"date_issued":"2024-12","date_published":"2024-12","updated_at":"2026-11-19T08:55:14Z","subjects":["Materials Science Engineering","B2O3","zirconia tape"],"languages":["English"],"rights":["Public","Ober, Evan Thomas","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["local-cont-no: submission_4083","https://digital.library.unt.edu/ark:/67531/metadc2415980/","ark: ark:/67531/metadc2415980"],"render_values":[{"text":"local-cont-no: submission_4083","href":null,"code":true},{"text":"https://digital.library.unt.edu/ark:/67531/metadc2415980/","href":"https://digital.library.unt.edu/ark:/67531/metadc2415980/","code":true},{"text":"ark: ark:/67531/metadc2415980","href":null,"code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://doi.org/10.12794/metadc2415980","outbound_label":"DOI","outbound_source":"dc:identifier","record_url":"https://doi.org/10.12794/metadc2415980","record_label":"Repository record","record_kind":"doi","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digital.library.unt.edu/oai/?verb=GetRecord&metadataPrefix=oai_dc&identifier=info%3Aark%2F67531%2Fmetadc2415980","prefix":"oai_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Reidy III, Richard F","Du, Jincheng","Wang, Ruocun"]},{"key":"dc:creator","label":"Author","values":["Ober, Evan Thomas"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2024-12"]},{"key":"dc:publisher","label":"Institution","values":["University of North Texas"]},{"key":"dc:type","label":"Dc Type","values":["Thesis or Dissertation"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Materials Science Engineering","B2O3","zirconia tape"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:rights","label":"Dc Rights","values":["Public","Ober, Evan Thomas","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["local-cont-no: submission_4083","doi: 10.12794/metadc2415980","https://digital.library.unt.edu/ark:/67531/metadc2415980/","ark: ark:/67531/metadc2415980"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["The effect of sintering aid B2O3 and the effect of sintering temperatures were evaluated in this thesis. A 7:3 ratio of alumina to 3 mol% yttria stabilized zirconia tape cast layers sintered at temperatures of 1500°C, 1550°C, and 1600°C were evaluated with an addition of 0 mol%, 1 mol%, and 3 mol% B2O3 additions to the yttria stabilized zirconia layer. X-ray microscopy were used to evaluate crack propagation to correlate with the flexural strengths found in three-point bend testing. Dilatometry was used to show the effect that the B2O3 addition had on the thermal expansion of the system. The addition of B2O3 was found to decrease the flexural strength of the alumina/YSZ laminate system. X-ray microscopy shows significant damage in the 1 mol% and 3 mol% B2O3 additions. The dilatometry suggests that 3 mol% destabilizes the YSZ layer, causing the YSZ to transform back into the monoclinic phase on cool down. The cracks rarely continued to propagate into the alumina layer, further confirming that the alumina/YSZ laminate combination has optimally weak interfaces. The temperature with the highest flexural strength for the 0 mol% B2O3 samples was shown to be 1600°C while the temperature with the highest flexural strength for the 1 mol% and 3 mol% B2O3 samples were shown to be 1550°C."]},{"key":"dc:format","label":"Dc Format","values":["Text"]},{"key":"dc:title","label":"Title","values":["The Effect of B2O3 Addition and Temperature Optimization on Mechanical Properties of Laminated Alumina and Yttria Stabilized Zirconia"]}]}],"canonical_facts":{"dc:contributor":["Reidy III, Richard F","Du, Jincheng","Wang, Ruocun"],"dc:creator":["Ober, Evan Thomas"],"dc:date":["2024-12"],"dc:description":["The effect of sintering aid B2O3 and the effect of sintering temperatures were evaluated in this thesis. A 7:3 ratio of alumina to 3 mol% yttria stabilized zirconia tape cast layers sintered at temperatures of 1500°C, 1550°C, and 1600°C were evaluated with an addition of 0 mol%, 1 mol%, and 3 mol% B2O3 additions to the yttria stabilized zirconia layer. X-ray microscopy were used to evaluate crack propagation to correlate with the flexural strengths found in three-point bend testing. Dilatometry was used to show the effect that the B2O3 addition had on the thermal expansion of the system. The addition of B2O3 was found to decrease the flexural strength of the alumina/YSZ laminate system. X-ray microscopy shows significant damage in the 1 mol% and 3 mol% B2O3 additions. The dilatometry suggests that 3 mol% destabilizes the YSZ layer, causing the YSZ to transform back into the monoclinic phase on cool down. The cracks rarely continued to propagate into the alumina layer, further confirming that the alumina/YSZ laminate combination has optimally weak interfaces. The temperature with the highest flexural strength for the 0 mol% B2O3 samples was shown to be 1600°C while the temperature with the highest flexural strength for the 1 mol% and 3 mol% B2O3 samples were shown to be 1550°C."],"dc:format":["Text"],"dc:identifier":["local-cont-no: submission_4083","doi: 10.12794/metadc2415980","https://digital.library.unt.edu/ark:/67531/metadc2415980/","ark: ark:/67531/metadc2415980"],"dc:language":["English"],"dc:publisher":["University of North Texas"],"dc:rights":["Public","Ober, Evan Thomas","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."],"dc:subject":["Materials Science Engineering","B2O3","zirconia tape"],"dc:title":["The Effect of B2O3 Addition and Temperature Optimization on Mechanical Properties of Laminated Alumina and Yttria Stabilized Zirconia"],"dc:type":["Thesis or Dissertation"]},"updated_at":"2026-11-19T08:55:14Z"}