{"id":{"repo_id":"unt","oai_identifier":"info:ark/67531/metadc2652568"},"canonical_url":"https://search.ndltd.org/etd/unt/info:ark/67531/metadc2652568","repository":{"repo_id":"unt","name":"University of North Texas","base_url":"https://digital.library.unt.edu/oai/"},"display":{"title":"Frequency Dependent Response of Additively Manufactured Electrical Steel Toroidal Transformer Cores","abstract":"Fe-6.5wt%Si possesses excellent soft-magnetic properties which offer increased efficiency compared to that of lower silicon content electrical steels. However, its inherently brittle nature makes it economically infeasible to process using traditional thermomechanical deformation methods. Additive Manufacturing (AM) has been identified as a potential means of circumventing these processing difficulties. Among the AM methods, Laser Powder Bed Fusion (LPBF) processing of Fe-6.5wt%Si is of particular interest because of its near-net shape fabrication and uniquely fast cooling rates which suppress the development of ordered phases while also allowing for the implementation of disruptive design methodologies, such as thin-wall geometries. This work seeks to further the understanding of the dynamic magnetic response of additively produced electrical steels, and how it is affected by frequency, thermal treatment, and alloy composition. To this end, quasistatic magnetic tests were performed on coupons, and dynamic magnetic tests were performed on toroidal core geometries of LPBF produced samples of Fe-6.5wt%Si and Fe-3.8wt%Si materials. These materials were examined in both the as-printed and post-print heat-treated conditions. Results indicated superior soft magnetic properties in the Fe-6.5wt%Si sample due to the development of ordered phases and the restriction of eddy currents at higher frequencies. Microstructure analysis confirmed typical LPBF columnar microstructure in both as-printed samples and massive grains on the scale of millimeters in the annealed samples, with growth in the annealed Fe-3.8wt%Si condition notably progressed to a further extent than the growth seen in the annealed Fe-6.5wt%Si. This is consistent with grain growth retardation due to ordered phase formation. Phase analysis via X-ray diffraction confirmed the presence of ordered peaks with superlattice reflections in the Fe-6.5wt%Si sample. Further confirmation was obtained from microhardness tests, which found a significant increase in the annealed Fe-6.5wt%Si sample compared to its as-printed counterpart despite grain coarsening. On the other hand, the hardness of Fe-3.8wt%Si dropped with annealing due to an alleviation of the Hall-Petch effect with grain growth. Basic power-loss separation theory was utilized to qualitatively attribute the source of loss in each sample. The overall results indicate that the alleviation of internal stresses in the Fe-3.8wt%Si through annealing had the greatest effect in improving its soft magnetic properties, but the inherent higher resistivity and lower magnetostriction of the Fe-6.5wt%Si still surpassed its performance in both as-printed and annealed conditions.","abstract_html":"Fe-6.5wt%Si possesses excellent soft-magnetic properties which offer increased efficiency compared to that of lower silicon content electrical steels. However, its inherently brittle nature makes it economically infeasible to process using traditional thermomechanical deformation methods. Additive Manufacturing (AM) has been identified as a potential means of circumventing these processing difficulties. Among the AM methods, Laser Powder Bed Fusion (LPBF) processing of Fe-6.5wt%Si is of particular interest because of its near-net shape fabrication and uniquely fast cooling rates which suppress the development of ordered phases while also allowing for the implementation of disruptive design methodologies, such as thin-wall geometries. This work seeks to further the understanding of the dynamic magnetic response of additively produced electrical steels, and how it is affected by frequency, thermal treatment, and alloy composition. To this end, quasistatic magnetic tests were performed on coupons, and dynamic magnetic tests were performed on toroidal core geometries of LPBF produced samples of Fe-6.5wt%Si and Fe-3.8wt%Si materials. These materials were examined in both the as-printed and post-print heat-treated conditions. Results indicated superior soft magnetic properties in the Fe-6.5wt%Si sample due to the development of ordered phases and the restriction of eddy currents at higher frequencies. Microstructure analysis confirmed typical LPBF columnar microstructure in both as-printed samples and massive grains on the scale of millimeters in the annealed samples, with growth in the annealed Fe-3.8wt%Si condition notably progressed to a further extent than the growth seen in the annealed Fe-6.5wt%Si. This is consistent with grain growth retardation due to ordered phase formation. Phase analysis via X-ray diffraction confirmed the presence of ordered peaks with superlattice reflections in the Fe-6.5wt%Si sample. Further confirmation was obtained from microhardness tests, which found a significant increase in the annealed Fe-6.5wt%Si sample compared to its as-printed counterpart despite grain coarsening. On the other hand, the hardness of Fe-3.8wt%Si dropped with annealing due to an alleviation of the Hall-Petch effect with grain growth. Basic power-loss separation theory was utilized to qualitatively attribute the source of loss in each sample. The overall results indicate that the alleviation of internal stresses in the Fe-3.8wt%Si through annealing had the greatest effect in improving its soft magnetic properties, but the inherent higher resistivity and lower magnetostriction of the Fe-6.5wt%Si still surpassed its performance in both as-printed and annealed conditions.","abstract_has_math":false,"creators":["McKinstry, Michael Philip 2000-"],"institution":"University of North Texas","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":["Joshi, Sameehan S.","Dahotre, Narendra B.","Sharma, Shashank"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2026,"date_issued":"2026-07","date_published":"2026-07","updated_at":"2026-11-19T08:55:57Z","subjects":["Engineering, Materials Science","Additive Manufacturing","Laser Powder Bed Fusion"],"languages":["English"],"rights":["Public","McKinstry, Michael Philip 2000-","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["local-cont-no: submission_5082","ark: ark:/67531/metadc2652568"],"render_values":[{"text":"local-cont-no: submission_5082","href":null,"code":true},{"text":"ark: ark:/67531/metadc2652568","href":null,"code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://digital.library.unt.edu/ark:/67531/metadc2652568/","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://digital.library.unt.edu/ark:/67531/metadc2652568/","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digital.library.unt.edu/oai/?verb=GetRecord&metadataPrefix=oai_dc&identifier=info%3Aark%2F67531%2Fmetadc2652568","prefix":"oai_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Joshi, Sameehan S.","Dahotre, Narendra B.","Sharma, Shashank"]},{"key":"dc:creator","label":"Author","values":["McKinstry, Michael Philip 2000-"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2026-07"]},{"key":"dc:publisher","label":"Institution","values":["University of North Texas"]},{"key":"dc:type","label":"Dc Type","values":["Thesis or Dissertation"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Engineering, Materials Science","Additive Manufacturing","Laser Powder Bed Fusion"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:rights","label":"Dc Rights","values":["Public","McKinstry, Michael Philip 2000-","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["local-cont-no: submission_5082","https://digital.library.unt.edu/ark:/67531/metadc2652568/","ark: ark:/67531/metadc2652568"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["Fe-6.5wt%Si possesses excellent soft-magnetic properties which offer increased efficiency compared to that of lower silicon content electrical steels. However, its inherently brittle nature makes it economically infeasible to process using traditional thermomechanical deformation methods. Additive Manufacturing (AM) has been identified as a potential means of circumventing these processing difficulties. Among the AM methods, Laser Powder Bed Fusion (LPBF) processing of Fe-6.5wt%Si is of particular interest because of its near-net shape fabrication and uniquely fast cooling rates which suppress the development of ordered phases while also allowing for the implementation of disruptive design methodologies, such as thin-wall geometries. This work seeks to further the understanding of the dynamic magnetic response of additively produced electrical steels, and how it is affected by frequency, thermal treatment, and alloy composition. To this end, quasistatic magnetic tests were performed on coupons, and dynamic magnetic tests were performed on toroidal core geometries of LPBF produced samples of Fe-6.5wt%Si and Fe-3.8wt%Si materials. These materials were examined in both the as-printed and post-print heat-treated conditions. Results indicated superior soft magnetic properties in the Fe-6.5wt%Si sample due to the development of ordered phases and the restriction of eddy currents at higher frequencies. Microstructure analysis confirmed typical LPBF columnar microstructure in both as-printed samples and massive grains on the scale of millimeters in the annealed samples, with growth in the annealed Fe-3.8wt%Si condition notably progressed to a further extent than the growth seen in the annealed Fe-6.5wt%Si. This is consistent with grain growth retardation due to ordered phase formation. Phase analysis via X-ray diffraction confirmed the presence of ordered peaks with superlattice reflections in the Fe-6.5wt%Si sample. Further confirmation was obtained from microhardness tests, which found a significant increase in the annealed Fe-6.5wt%Si sample compared to its as-printed counterpart despite grain coarsening. On the other hand, the hardness of Fe-3.8wt%Si dropped with annealing due to an alleviation of the Hall-Petch effect with grain growth. Basic power-loss separation theory was utilized to qualitatively attribute the source of loss in each sample. The overall results indicate that the alleviation of internal stresses in the Fe-3.8wt%Si through annealing had the greatest effect in improving its soft magnetic properties, but the inherent higher resistivity and lower magnetostriction of the Fe-6.5wt%Si still surpassed its performance in both as-printed and annealed conditions."]},{"key":"dc:format","label":"Dc Format","values":["Text"]},{"key":"dc:title","label":"Title","values":["Frequency Dependent Response of Additively Manufactured Electrical Steel Toroidal Transformer Cores"]}]}],"canonical_facts":{"dc:contributor":["Joshi, Sameehan S.","Dahotre, Narendra B.","Sharma, Shashank"],"dc:creator":["McKinstry, Michael Philip 2000-"],"dc:date":["2026-07"],"dc:description":["Fe-6.5wt%Si possesses excellent soft-magnetic properties which offer increased efficiency compared to that of lower silicon content electrical steels. However, its inherently brittle nature makes it economically infeasible to process using traditional thermomechanical deformation methods. Additive Manufacturing (AM) has been identified as a potential means of circumventing these processing difficulties. Among the AM methods, Laser Powder Bed Fusion (LPBF) processing of Fe-6.5wt%Si is of particular interest because of its near-net shape fabrication and uniquely fast cooling rates which suppress the development of ordered phases while also allowing for the implementation of disruptive design methodologies, such as thin-wall geometries. This work seeks to further the understanding of the dynamic magnetic response of additively produced electrical steels, and how it is affected by frequency, thermal treatment, and alloy composition. To this end, quasistatic magnetic tests were performed on coupons, and dynamic magnetic tests were performed on toroidal core geometries of LPBF produced samples of Fe-6.5wt%Si and Fe-3.8wt%Si materials. These materials were examined in both the as-printed and post-print heat-treated conditions. Results indicated superior soft magnetic properties in the Fe-6.5wt%Si sample due to the development of ordered phases and the restriction of eddy currents at higher frequencies. Microstructure analysis confirmed typical LPBF columnar microstructure in both as-printed samples and massive grains on the scale of millimeters in the annealed samples, with growth in the annealed Fe-3.8wt%Si condition notably progressed to a further extent than the growth seen in the annealed Fe-6.5wt%Si. This is consistent with grain growth retardation due to ordered phase formation. Phase analysis via X-ray diffraction confirmed the presence of ordered peaks with superlattice reflections in the Fe-6.5wt%Si sample. Further confirmation was obtained from microhardness tests, which found a significant increase in the annealed Fe-6.5wt%Si sample compared to its as-printed counterpart despite grain coarsening. On the other hand, the hardness of Fe-3.8wt%Si dropped with annealing due to an alleviation of the Hall-Petch effect with grain growth. Basic power-loss separation theory was utilized to qualitatively attribute the source of loss in each sample. The overall results indicate that the alleviation of internal stresses in the Fe-3.8wt%Si through annealing had the greatest effect in improving its soft magnetic properties, but the inherent higher resistivity and lower magnetostriction of the Fe-6.5wt%Si still surpassed its performance in both as-printed and annealed conditions."],"dc:format":["Text"],"dc:identifier":["local-cont-no: submission_5082","https://digital.library.unt.edu/ark:/67531/metadc2652568/","ark: ark:/67531/metadc2652568"],"dc:language":["English"],"dc:publisher":["University of North Texas"],"dc:rights":["Public","McKinstry, Michael Philip 2000-","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."],"dc:subject":["Engineering, Materials Science","Additive Manufacturing","Laser Powder Bed Fusion"],"dc:title":["Frequency Dependent Response of Additively Manufactured Electrical Steel Toroidal Transformer Cores"],"dc:type":["Thesis or Dissertation"]},"updated_at":"2026-11-19T08:55:57Z"}