{"id":{"repo_id":"unt","oai_identifier":"info:ark/67531/metadc822792"},"canonical_url":"https://search.ndltd.org/etd/unt/info:ark/67531/metadc822792","repository":{"repo_id":"unt","name":"University of North Texas","base_url":"https://digital.library.unt.edu/oai/"},"display":{"title":"The Role of Crystallographic Texture in Achieving Low Friction Zinc Oxide Nanolaminate Films","abstract":"Metal oxide nanolaminate films are potential high temperature solid lubricants due to their ability to exhibit significant plasticity when grain size is reduced to the nanometer scale, and defective growth structure is achieved by condensation of oxygen vacancies to form intrinsic stacking faults. This is in contrast to conventional microcrystalline and single crystal oxides that exhibit brittle fracture during loading in a sliding contact. This study emphasizes the additional effect of growth orientation, in particular crystallographic texture, on determining the sliding friction behavior in nanocolumnar grain zinc oxide films grown by atomic layer deposition. It was determined that zinc oxide low (0002) versus higher (101 ̅3) surface energy crystallographic planes influenced the sliding friction coefficient. Texturing of the (0002) grains resulted in a decreased adhesive component of friction thereby lowering the sliding friction coefficient to ~0.25, while the friction coefficient doubled to ~0.5 with increasing contribution of surface (101 ̅3) grains. In addition, the variation of the x-ray grazing incident angle from 0.5° to 5° was studied to better understand the surface grain orientation as a function of ZnO layer thickness in one versus four bilayer nanolaminates where the under layer (seed layer) was load-bearing Zn(Ti,Zr)O3.","abstract_html":"Metal oxide nanolaminate films are potential high temperature solid lubricants due to their ability to exhibit significant plasticity when grain size is reduced to the nanometer scale, and defective growth structure is achieved by condensation of oxygen vacancies to form intrinsic stacking faults. This is in contrast to conventional microcrystalline and single crystal oxides that exhibit brittle fracture during loading in a sliding contact. This study emphasizes the additional effect of growth orientation, in particular crystallographic texture, on determining the sliding friction behavior in nanocolumnar grain zinc oxide films grown by atomic layer deposition. It was determined that zinc oxide low (0002) versus higher (101 ̅3) surface energy crystallographic planes influenced the sliding friction coefficient. Texturing of the (0002) grains resulted in a decreased adhesive component of friction thereby lowering the sliding friction coefficient to ~0.25, while the friction coefficient doubled to ~0.5 with increasing contribution of surface (101 ̅3) grains. In addition, the variation of the x-ray grazing incident angle from 0.5° to 5° was studied to better understand the surface grain orientation as a function of ZnO layer thickness in one versus four bilayer nanolaminates where the under layer (seed layer) was load-bearing Zn(Ti,Zr)O3.","abstract_has_math":false,"creators":["Mojekwu, Nneoma"],"institution":"University of North Texas","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":["Scharf, Thomas W.","Aouadi, Samir","Bouanani, Mohamed El"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2015,"date_issued":"2015-12","date_published":"2015-12","updated_at":"2026-11-19T08:54:28Z","subjects":["zinc oxide","friction","nanolaminotes","atomic layer","deposition","Zinc oxide thin films.","Crystallography.","Friction.","Nanostructured materials."],"languages":["English"],"rights":["Public","Mojekwu, Nneoma","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digital.library.unt.edu/ark:/67531/metadc822792/","ark: ark:/67531/metadc822792"],"render_values":[{"text":"https://digital.library.unt.edu/ark:/67531/metadc822792/","href":"https://digital.library.unt.edu/ark:/67531/metadc822792/","code":true},{"text":"ark: ark:/67531/metadc822792","href":null,"code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://doi.org/10.12794/metadc822792","outbound_label":"DOI","outbound_source":"dc:identifier","record_url":"https://doi.org/10.12794/metadc822792","record_label":"Repository record","record_kind":"doi","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://digital.library.unt.edu/oai/?verb=GetRecord&metadataPrefix=oai_dc&identifier=info%3Aark%2F67531%2Fmetadc822792","prefix":"oai_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Scharf, Thomas W.","Aouadi, Samir","Bouanani, Mohamed El"]},{"key":"dc:creator","label":"Author","values":["Mojekwu, Nneoma"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2015-12"]},{"key":"dc:publisher","label":"Institution","values":["University of North Texas"]},{"key":"dc:type","label":"Dc Type","values":["Thesis or Dissertation"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["zinc oxide","friction","nanolaminotes","atomic layer","deposition","Zinc oxide thin films.","Crystallography.","Friction.","Nanostructured materials."]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:rights","label":"Dc Rights","values":["Public","Mojekwu, Nneoma","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["doi: 10.12794/metadc822792","https://digital.library.unt.edu/ark:/67531/metadc822792/","ark: ark:/67531/metadc822792"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["Metal oxide nanolaminate films are potential high temperature solid lubricants due to their ability to exhibit significant plasticity when grain size is reduced to the nanometer scale, and defective growth structure is achieved by condensation of oxygen vacancies to form intrinsic stacking faults. This is in contrast to conventional microcrystalline and single crystal oxides that exhibit brittle fracture during loading in a sliding contact. This study emphasizes the additional effect of growth orientation, in particular crystallographic texture, on determining the sliding friction behavior in nanocolumnar grain zinc oxide films grown by atomic layer deposition. It was determined that zinc oxide low (0002) versus higher (101 ̅3) surface energy crystallographic planes influenced the sliding friction coefficient. Texturing of the (0002) grains resulted in a decreased adhesive component of friction thereby lowering the sliding friction coefficient to ~0.25, while the friction coefficient doubled to ~0.5 with increasing contribution of surface (101 ̅3) grains. In addition, the variation of the x-ray grazing incident angle from 0.5° to 5° was studied to better understand the surface grain orientation as a function of ZnO layer thickness in one versus four bilayer nanolaminates where the under layer (seed layer) was load-bearing Zn(Ti,Zr)O3."]},{"key":"dc:format","label":"Dc Format","values":["xii, 59 pages : illustrations (chiefly color)","Text"]},{"key":"dc:title","label":"Title","values":["The Role of Crystallographic Texture in Achieving Low Friction Zinc Oxide Nanolaminate Films"]}]}],"canonical_facts":{"dc:contributor":["Scharf, Thomas W.","Aouadi, Samir","Bouanani, Mohamed El"],"dc:creator":["Mojekwu, Nneoma"],"dc:date":["2015-12"],"dc:description":["Metal oxide nanolaminate films are potential high temperature solid lubricants due to their ability to exhibit significant plasticity when grain size is reduced to the nanometer scale, and defective growth structure is achieved by condensation of oxygen vacancies to form intrinsic stacking faults. This is in contrast to conventional microcrystalline and single crystal oxides that exhibit brittle fracture during loading in a sliding contact. This study emphasizes the additional effect of growth orientation, in particular crystallographic texture, on determining the sliding friction behavior in nanocolumnar grain zinc oxide films grown by atomic layer deposition. It was determined that zinc oxide low (0002) versus higher (101 ̅3) surface energy crystallographic planes influenced the sliding friction coefficient. Texturing of the (0002) grains resulted in a decreased adhesive component of friction thereby lowering the sliding friction coefficient to ~0.25, while the friction coefficient doubled to ~0.5 with increasing contribution of surface (101 ̅3) grains. In addition, the variation of the x-ray grazing incident angle from 0.5° to 5° was studied to better understand the surface grain orientation as a function of ZnO layer thickness in one versus four bilayer nanolaminates where the under layer (seed layer) was load-bearing Zn(Ti,Zr)O3."],"dc:format":["xii, 59 pages : illustrations (chiefly color)","Text"],"dc:identifier":["doi: 10.12794/metadc822792","https://digital.library.unt.edu/ark:/67531/metadc822792/","ark: ark:/67531/metadc822792"],"dc:language":["English"],"dc:publisher":["University of North Texas"],"dc:rights":["Public","Mojekwu, Nneoma","Copyright","Copyright is held by the author, unless otherwise noted. All rights Reserved."],"dc:subject":["zinc oxide","friction","nanolaminotes","atomic layer","deposition","Zinc oxide thin films.","Crystallography.","Friction.","Nanostructured materials."],"dc:title":["The Role of Crystallographic Texture in Achieving Low Friction Zinc Oxide Nanolaminate Films"],"dc:type":["Thesis or Dissertation"]},"updated_at":"2026-11-19T08:54:28Z"}