{"id":{"repo_id":"uoit","oai_identifier":"oai:ontariotechu.scholaris.ca:10155/2184"},"canonical_url":"https://search.ndltd.org/etd/uoit/oai:ontariotechu.scholaris.ca:10155/2184","repository":{"repo_id":"uoit","name":"Ontario Institute of Technology","base_url":"https://ontariotechu.scholaris.ca/server/oai/request"},"display":{"title":"Experimental investigation of solid state hydrogen storage capabilities of biochar derived from organic waste materials","abstract":"This study investigates the solid-state hydrogen storage potential of biochar derived from tea waste, coffee grounds, maple leaves, and pinecones. After pyrolysis, three different activation methods take place, which are chemical, physical, and magnetic, to create different adsorbents. It performs tests at 0 °C and 25 °C, under 1 to 4 kPa pressure, and using different amounts of adsorbents between 1 to 6 grams of material. The highest capacity is 0.54 wt.% with chemically activated commercial carbon, and 0.39 wt.% in activated pinecone biochar. Tea waste shows the best performance under chemical activation with 0.36 wt.%, and magnetic activation with 0.33 wt.%. Coffee grounds show the lowest capacity with 0.33 wt.% in magnetic activation. The electrochemical tests range between 0.014 wt.% and 0.008 wt.%. SEM images show that pore structure affects hydrogen uptake. The study concludes that low temperature and chemical activation significantly improve storage performance.","abstract_html":"This study investigates the solid-state hydrogen storage potential of biochar derived from tea waste, coffee grounds, maple leaves, and pinecones. After pyrolysis, three different activation methods take place, which are chemical, physical, and magnetic, to create different adsorbents. It performs tests at 0 °C and 25 °C, under 1 to 4 kPa pressure, and using different amounts of adsorbents between 1 to 6 grams of material. The highest capacity is 0.54 wt.% with chemically activated commercial carbon, and 0.39 wt.% in activated pinecone biochar. Tea waste shows the best performance under chemical activation with 0.36 wt.%, and magnetic activation with 0.33 wt.%. Coffee grounds show the lowest capacity with 0.33 wt.% in magnetic activation. The electrochemical tests range between 0.014 wt.% and 0.008 wt.%. SEM images show that pore structure affects hydrogen uptake. The study concludes that low temperature and chemical activation significantly improve storage performance.","abstract_has_math":false,"creators":["Capoglu, Ayca"],"institution":"University of Ontario Institute of Technology","degree_name":"Master of Applied Science (MASc)","degree_level":null,"degree_discipline":"Mechanical Engineering","degree_department":null,"school":null,"contributors":[],"advisors":["Dincer, Ibrahim"],"committee_chairs":[],"committee_members":[],"year":2025,"date_issued":"2025-08-01","date_published":"2025-08-01","updated_at":"2026-11-19T09:02:25Z","subjects":["Hydrogen storage","Solid state storage","Activated charcoal","Renewable energy","Energy storage"],"languages":["en"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/10155/2184","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/10155/2184","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Auoit%3Aoai%3Aontariotechu.scholaris.ca%3A10155%2F2184","prefix":"oai_dc"},"source_record":{"url":"https://ontariotechu.scholaris.ca/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Aontariotechu.scholaris.ca%3A10155%2F2184","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Dincer, Ibrahim"]},{"key":"dc:creator","label":"Author","values":["Capoglu, Ayca"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2026-09-28T18:22:47Z"]},{"key":"dc:date.issued","label":"Date","values":["2025-08-01"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Mechanical Engineering"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Applied Science (MASc)"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of Ontario Institute of Technology"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject.other","label":"Dc Subject Other","values":["Hydrogen storage","Solid state storage","Activated charcoal","Renewable energy","Energy storage"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/10155/2184"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["This study investigates the solid-state hydrogen storage potential of biochar derived from tea waste, coffee grounds, maple leaves, and pinecones. After pyrolysis, three different activation methods take place, which are chemical, physical, and magnetic, to create different adsorbents. It performs tests at 0 °C and 25 °C, under 1 to 4 kPa pressure, and using different amounts of adsorbents between 1 to 6 grams of material. The highest capacity is 0.54 wt.% with chemically activated commercial carbon, and 0.39 wt.% in activated pinecone biochar. Tea waste shows the best performance under chemical activation with 0.36 wt.%, and magnetic activation with 0.33 wt.%. Coffee grounds show the lowest capacity with 0.33 wt.% in magnetic activation. The electrochemical tests range between 0.014 wt.% and 0.008 wt.%. SEM images show that pore structure affects hydrogen uptake. The study concludes that low temperature and chemical activation significantly improve storage performance."]},{"key":"dc:title","label":"Title","values":["Experimental investigation of solid state hydrogen storage capabilities of biochar derived from organic waste materials"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:contributor.advisor":["Dincer, Ibrahim"],"dc:creator":["Capoglu, Ayca"],"dc:date.accessioned":["2026-09-28T18:22:47Z"],"dc:date.issued":["2025-08-01"],"dc:description.abstract":["This study investigates the solid-state hydrogen storage potential of biochar derived from tea waste, coffee grounds, maple leaves, and pinecones. After pyrolysis, three different activation methods take place, which are chemical, physical, and magnetic, to create different adsorbents. It performs tests at 0 °C and 25 °C, under 1 to 4 kPa pressure, and using different amounts of adsorbents between 1 to 6 grams of material. The highest capacity is 0.54 wt.% with chemically activated commercial carbon, and 0.39 wt.% in activated pinecone biochar. Tea waste shows the best performance under chemical activation with 0.36 wt.%, and magnetic activation with 0.33 wt.%. Coffee grounds show the lowest capacity with 0.33 wt.% in magnetic activation. The electrochemical tests range between 0.014 wt.% and 0.008 wt.%. SEM images show that pore structure affects hydrogen uptake. The study concludes that low temperature and chemical activation significantly improve storage performance."],"dc:identifier.uri":["https://hdl.handle.net/10155/2184"],"dc:language.iso":["en"],"dc:subject.other":["Hydrogen storage","Solid state storage","Activated charcoal","Renewable energy","Energy storage"],"dc:title":["Experimental investigation of solid state hydrogen storage capabilities of biochar derived from organic waste materials"],"dc:type":["Thesis"],"others:access_status":["open.access"],"thesis:degree_discipline":["Mechanical Engineering"],"thesis:degree_name":["Master of Applied Science (MASc)"],"thesis:institution_name":["University of Ontario Institute of Technology"]},"updated_at":"2026-11-19T09:02:25Z"}