{"id":{"repo_id":"vilnius","oai_identifier":"oai:vu.lt:elaba:1951857"},"canonical_url":"https://search.ndltd.org/etd/vilnius/oai:vu.lt:elaba:1951857","repository":{"repo_id":"vilnius","name":"Vilnius University","base_url":"https://epublications.vu.lt/oai"},"display":{"title":"Mažo tankio polietileno fotooksidacijos ir fotodestrukcijos tyrimas /","abstract":"The influence of ultraviolet radiation (=254 nm) on the low density polyethylene was analysed in this study. Infrared transmission spectra measured by FTIR spectrometer were used to find out the change of polyethylene chemical composition. The UV radiation at 254 nm caused photooxidation and photodestruction of polyethylene. It was determined that carbonyl, aldehyde, vinyl, hydroxyl groups were formed as the products of the photooxidation of the polyethylene. The relative amount of carbonyl groups and aldehyde groups increased exponentially in the course of UV exposition. The growth of absorbance of vinyl groups was linear during UV exposition. Formation of hydroxyl groups was found only after 150 hours of UV exposition.","abstract_html":"The influence of ultraviolet radiation (=254 nm) on the low density polyethylene was analysed in this study. Infrared transmission spectra measured by FTIR spectrometer were used to find out the change of polyethylene chemical composition. The UV radiation at 254 nm caused photooxidation and photodestruction of polyethylene. It was determined that carbonyl, aldehyde, vinyl, hydroxyl groups were formed as the products of the photooxidation of the polyethylene. The relative amount of carbonyl groups and aldehyde groups increased exponentially in the course of UV exposition. The growth of absorbance of vinyl groups was linear during UV exposition. Formation of hydroxyl groups was found only after 150 hours of UV exposition.","abstract_has_math":false,"creators":["Sruogytė, Violeta,"],"institution":"Institutional Repository of Vilnius University","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":["Sitonytė, Jūratė"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2012,"date_issued":"2012","date_published":"2012","updated_at":"2026-11-19T10:01:20Z","subjects":["Photooxidation ; photodestruction ; polyethylene"],"languages":["lit"],"rights":["info:eu-repo/semantics/openAccess"],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://repository.vu.lt/VU:ELABAETD1951857&prefLang=en_US","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://repository.vu.lt/VU:ELABAETD1951857&prefLang=en_US","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":"open","embargo_until":null,"access_note":null},"source_record":{"url":"https://epublications.vu.lt/oai?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Avu.lt%3Aelaba%3A1951857","prefix":"oai_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Sitonytė, Jūratė"]},{"key":"dc:creator","label":"Author","values":["Sruogytė, Violeta,"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2012"]},{"key":"dc:publisher","label":"Institution","values":["Institutional Repository of Vilnius University"]},{"key":"dc:relation","label":"Dc Relation","values":["https://epublications.vu.lt/object/elaba:1951857/1951857.pdf"]},{"key":"dc:type","label":"Dc Type","values":["info:eu-repo/semantics/bachelorThesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Photooxidation ; photodestruction ; polyethylene"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["lit"]},{"key":"dc:rights","label":"Dc Rights","values":["info:eu-repo/semantics/openAccess"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://repository.vu.lt/VU:ELABAETD1951857&prefLang=en_US"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["The influence of ultraviolet radiation (=254 nm) on the low density polyethylene was analysed in this study. Infrared transmission spectra measured by FTIR spectrometer were used to find out the change of polyethylene chemical composition. The UV radiation at 254 nm caused photooxidation and photodestruction of polyethylene. It was determined that carbonyl, aldehyde, vinyl, hydroxyl groups were formed as the products of the photooxidation of the polyethylene. The relative amount of carbonyl groups and aldehyde groups increased exponentially in the course of UV exposition. The growth of absorbance of vinyl groups was linear during UV exposition. Formation of hydroxyl groups was found only after 150 hours of UV exposition."]},{"key":"dc:format","label":"Dc Format","values":["application/pdf"]},{"key":"dc:title","label":"Title","values":["Mažo tankio polietileno fotooksidacijos ir fotodestrukcijos tyrimas /","A Research on Photo-Oxidation and Photo-Degradation of Low Density Polyethylene."]}]}],"canonical_facts":{"dc:contributor":["Sitonytė, Jūratė"],"dc:creator":["Sruogytė, Violeta,"],"dc:date":["2012"],"dc:description":["The influence of ultraviolet radiation (=254 nm) on the low density polyethylene was analysed in this study. Infrared transmission spectra measured by FTIR spectrometer were used to find out the change of polyethylene chemical composition. The UV radiation at 254 nm caused photooxidation and photodestruction of polyethylene. It was determined that carbonyl, aldehyde, vinyl, hydroxyl groups were formed as the products of the photooxidation of the polyethylene. The relative amount of carbonyl groups and aldehyde groups increased exponentially in the course of UV exposition. The growth of absorbance of vinyl groups was linear during UV exposition. Formation of hydroxyl groups was found only after 150 hours of UV exposition."],"dc:format":["application/pdf"],"dc:identifier":["https://repository.vu.lt/VU:ELABAETD1951857&prefLang=en_US"],"dc:language":["lit"],"dc:publisher":["Institutional Repository of Vilnius University"],"dc:relation":["https://epublications.vu.lt/object/elaba:1951857/1951857.pdf"],"dc:rights":["info:eu-repo/semantics/openAccess"],"dc:subject":["Photooxidation ; photodestruction ; polyethylene"],"dc:title":["Mažo tankio polietileno fotooksidacijos ir fotodestrukcijos tyrimas /","A Research on Photo-Oxidation and Photo-Degradation of Low Density Polyethylene."],"dc:type":["info:eu-repo/semantics/bachelorThesis"]},"updated_at":"2026-11-19T10:01:20Z"}