{"id":{"repo_id":"vilnius","oai_identifier":"oai:vu.lt:elaba:308155835"},"canonical_url":"https://search.ndltd.org/etd/vilnius/oai:vu.lt:elaba:308155835","repository":{"repo_id":"vilnius","name":"Vilnius University","base_url":"https://epublications.vu.lt/oai"},"display":{"title":"Kofeinui jautraus molekulinių įspaudų fotopolimero matricoje jutiklio kūrimas ir tyrimas /","abstract":"In this thesis, a caffeine sensitive molecularly imprinted polymer (MIP) sensor was developed and characterised, with the recognition layer formed from a commercial 405 nm UV-curable urethane-acrylate photopolymer resin deposited on a 5 MHz AT cut gold coated quartz crystal microbalance (QCM) electrode. Previously reported caffeine MIP QCM sensors have relied either on the classical MAA/EDMA acrylate system or on electropolymerised polypyrrole; the novelty of this work lies in being the first to demonstrate that a commercial 3D printing photopolymer resin can serve as a functional MIP matrix for gravimetric caffeine detection. The solubility of the resin and caffeine was evaluated in several organic solvent systems, and the optimal composition was identified as acetone/ethanol (3:7 v/v) with 50 µL of resin and 8 mg of caffeine. MIP film formation and subsequent template removal by a deionised water flow (0,5 mL/min) were monitored in real time by QCM. It was established that films cured in air for 10 hours behaved viscoelastically and could not be interpreted by the Sauerbrey equation, whereas a 30 h curing period produced a sufficiently rigid film yielding a reproducible Sauerbrey compatible negative frequency shift (&#916;f = –7,5±0,5 Hz upon exposure to 4 mmol/L caffeine). An additional 10 % methanol wash did not produce a statistically significant increase in sensitivity and posed a risk of structural damage to the film. Comparison of the MIP sensor with a non-imprinted polymer (NIP) of identical composition yielded an imprinting factor of IF &#8776; 4,0. The MIP frequency response was linearly dependent on caffeine concentration in the range of 1–4 mmol/L (&#916;f = –1,5·c – 1,84; R² = 0,98), with a sensitivity approximately twice that of the NIP. Kinetic and thermodynamic parameters derived from the association and dissociation curves (k&#8336; = 0,298 M&#8315;¹s&#8315;¹, kd = 7,21·10&#8315;³ s&#8315;¹, KD = 2,42·10&#8315;² M, &#916;G = –9.06 kJ/mol) indicate a thermodynamically favourable, spontaneous complex formation, consistent with a recognition mechanism dominated by hydrogen bonding and electrostatic interactions. A four-day stability study revealed a gradual decrease in signal (~19 % over the first 24 h, ~32 % over the full period), attributable to swelling of the polymer matrix in aqueous medium; nevertheless, the sensor remained functional throughout the observation period. The work confirms that readily available commercial UV curable urethane-acrylate resins can be used as a functional MIP matrix in gravimetric sensors for small molecules. Selectivity towards structural caffeine analogues was not assessed in this work and remains a subject for further studies.","abstract_html":"In this thesis, a caffeine sensitive molecularly imprinted polymer (MIP) sensor was developed and characterised, with the recognition layer formed from a commercial 405 nm UV-curable urethane-acrylate photopolymer resin deposited on a 5 MHz AT cut gold coated quartz crystal microbalance (QCM) electrode. Previously reported caffeine MIP QCM sensors have relied either on the classical MAA/EDMA acrylate system or on electropolymerised polypyrrole; the novelty of this work lies in being the first to demonstrate that a commercial 3D printing photopolymer resin can serve as a functional MIP matrix for gravimetric caffeine detection. The solubility of the resin and caffeine was evaluated in several organic solvent systems, and the optimal composition was identified as acetone/ethanol (3:7 v/v) with 50 µL of resin and 8 mg of caffeine. MIP film formation and subsequent template removal by a deionised water flow (0,5 mL/min) were monitored in real time by QCM. It was established that films cured in air for 10 hours behaved viscoelastically and could not be interpreted by the Sauerbrey equation, whereas a 30 h curing period produced a sufficiently rigid film yielding a reproducible Sauerbrey compatible negative frequency shift (&amp;#916;f = –7,5±0,5 Hz upon exposure to 4 mmol/L caffeine). An additional 10 % methanol wash did not produce a statistically significant increase in sensitivity and posed a risk of structural damage to the film. Comparison of the MIP sensor with a non-imprinted polymer (NIP) of identical composition yielded an imprinting factor of IF &amp;#8776; 4,0. The MIP frequency response was linearly dependent on caffeine concentration in the range of 1–4 mmol/L (&amp;#916;f = –1,5·c – 1,84; R² = 0,98), with a sensitivity approximately twice that of the NIP. Kinetic and thermodynamic parameters derived from the association and dissociation curves (k&amp;#8336; = 0,298 M&amp;#8315;¹s&amp;#8315;¹, kd = 7,21·10&amp;#8315;³ s&amp;#8315;¹, KD = 2,42·10&amp;#8315;² M, &amp;#916;G = –9.06 kJ/mol) indicate a thermodynamically favourable, spontaneous complex formation, consistent with a recognition mechanism dominated by hydrogen bonding and electrostatic interactions. A four-day stability study revealed a gradual decrease in signal (~19 % over the first 24 h, ~32 % over the full period), attributable to swelling of the polymer matrix in aqueous medium; nevertheless, the sensor remained functional throughout the observation period. The work confirms that readily available commercial UV curable urethane-acrylate resins can be used as a functional MIP matrix in gravimetric sensors for small molecules. Selectivity towards structural caffeine analogues was not assessed in this work and remains a subject for further studies.","abstract_has_math":false,"creators":["Daunys, Matas,"],"institution":"Institutional Repository of Vilnius University","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2026,"date_issued":"2026","date_published":"2026","updated_at":"2026-11-19T10:12:15Z","subjects":[],"languages":["lit"],"rights":["info:eu-repo/semantics/openAccess"],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://repository.vu.lt/VU:ELABAETD308155835&prefLang=en_US","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://repository.vu.lt/VU:ELABAETD308155835&prefLang=en_US","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":"open","embargo_until":null,"access_note":null},"source_record":{"url":"https://epublications.vu.lt/oai?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Avu.lt%3Aelaba%3A308155835","prefix":"oai_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Daunys, Matas,"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2026"]},{"key":"dc:publisher","label":"Institution","values":["Institutional Repository of Vilnius University"]},{"key":"dc:relation","label":"Dc Relation","values":["https://epublications.vu.lt/object/elaba:308155835/308155835.pdf"]},{"key":"dc:type","label":"Dc Type","values":["info:eu-repo/semantics/masterThesis"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["lit"]},{"key":"dc:rights","label":"Dc Rights","values":["info:eu-repo/semantics/openAccess"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://repository.vu.lt/VU:ELABAETD308155835&prefLang=en_US"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["In this thesis, a caffeine sensitive molecularly imprinted polymer (MIP) sensor was developed and characterised, with the recognition layer formed from a commercial 405 nm UV-curable urethane-acrylate photopolymer resin deposited on a 5 MHz AT cut gold coated quartz crystal microbalance (QCM) electrode. Previously reported caffeine MIP QCM sensors have relied either on the classical MAA/EDMA acrylate system or on electropolymerised polypyrrole; the novelty of this work lies in being the first to demonstrate that a commercial 3D printing photopolymer resin can serve as a functional MIP matrix for gravimetric caffeine detection. The solubility of the resin and caffeine was evaluated in several organic solvent systems, and the optimal composition was identified as acetone/ethanol (3:7 v/v) with 50 µL of resin and 8 mg of caffeine. MIP film formation and subsequent template removal by a deionised water flow (0,5 mL/min) were monitored in real time by QCM. It was established that films cured in air for 10 hours behaved viscoelastically and could not be interpreted by the Sauerbrey equation, whereas a 30 h curing period produced a sufficiently rigid film yielding a reproducible Sauerbrey compatible negative frequency shift (&#916;f = –7,5±0,5 Hz upon exposure to 4 mmol/L caffeine). An additional 10 % methanol wash did not produce a statistically significant increase in sensitivity and posed a risk of structural damage to the film. Comparison of the MIP sensor with a non-imprinted polymer (NIP) of identical composition yielded an imprinting factor of IF &#8776; 4,0. The MIP frequency response was linearly dependent on caffeine concentration in the range of 1–4 mmol/L (&#916;f = –1,5·c – 1,84; R² = 0,98), with a sensitivity approximately twice that of the NIP. Kinetic and thermodynamic parameters derived from the association and dissociation curves (k&#8336; = 0,298 M&#8315;¹s&#8315;¹, kd = 7,21·10&#8315;³ s&#8315;¹, KD = 2,42·10&#8315;² M, &#916;G = –9.06 kJ/mol) indicate a thermodynamically favourable, spontaneous complex formation, consistent with a recognition mechanism dominated by hydrogen bonding and electrostatic interactions. A four-day stability study revealed a gradual decrease in signal (~19 % over the first 24 h, ~32 % over the full period), attributable to swelling of the polymer matrix in aqueous medium; nevertheless, the sensor remained functional throughout the observation period. The work confirms that readily available commercial UV curable urethane-acrylate resins can be used as a functional MIP matrix in gravimetric sensors for small molecules. Selectivity towards structural caffeine analogues was not assessed in this work and remains a subject for further studies."]},{"key":"dc:format","label":"Dc Format","values":["application/pdf"]},{"key":"dc:title","label":"Title","values":["Kofeinui jautraus molekulinių įspaudų fotopolimero matricoje jutiklio kūrimas ir tyrimas /","Development and investigation of a caffeine sensitive molecular imprints in a photopolymer matrix."]}]}],"canonical_facts":{"dc:creator":["Daunys, Matas,"],"dc:date":["2026"],"dc:description":["In this thesis, a caffeine sensitive molecularly imprinted polymer (MIP) sensor was developed and characterised, with the recognition layer formed from a commercial 405 nm UV-curable urethane-acrylate photopolymer resin deposited on a 5 MHz AT cut gold coated quartz crystal microbalance (QCM) electrode. Previously reported caffeine MIP QCM sensors have relied either on the classical MAA/EDMA acrylate system or on electropolymerised polypyrrole; the novelty of this work lies in being the first to demonstrate that a commercial 3D printing photopolymer resin can serve as a functional MIP matrix for gravimetric caffeine detection. The solubility of the resin and caffeine was evaluated in several organic solvent systems, and the optimal composition was identified as acetone/ethanol (3:7 v/v) with 50 µL of resin and 8 mg of caffeine. MIP film formation and subsequent template removal by a deionised water flow (0,5 mL/min) were monitored in real time by QCM. It was established that films cured in air for 10 hours behaved viscoelastically and could not be interpreted by the Sauerbrey equation, whereas a 30 h curing period produced a sufficiently rigid film yielding a reproducible Sauerbrey compatible negative frequency shift (&#916;f = –7,5±0,5 Hz upon exposure to 4 mmol/L caffeine). An additional 10 % methanol wash did not produce a statistically significant increase in sensitivity and posed a risk of structural damage to the film. Comparison of the MIP sensor with a non-imprinted polymer (NIP) of identical composition yielded an imprinting factor of IF &#8776; 4,0. The MIP frequency response was linearly dependent on caffeine concentration in the range of 1–4 mmol/L (&#916;f = –1,5·c – 1,84; R² = 0,98), with a sensitivity approximately twice that of the NIP. Kinetic and thermodynamic parameters derived from the association and dissociation curves (k&#8336; = 0,298 M&#8315;¹s&#8315;¹, kd = 7,21·10&#8315;³ s&#8315;¹, KD = 2,42·10&#8315;² M, &#916;G = –9.06 kJ/mol) indicate a thermodynamically favourable, spontaneous complex formation, consistent with a recognition mechanism dominated by hydrogen bonding and electrostatic interactions. A four-day stability study revealed a gradual decrease in signal (~19 % over the first 24 h, ~32 % over the full period), attributable to swelling of the polymer matrix in aqueous medium; nevertheless, the sensor remained functional throughout the observation period. The work confirms that readily available commercial UV curable urethane-acrylate resins can be used as a functional MIP matrix in gravimetric sensors for small molecules. Selectivity towards structural caffeine analogues was not assessed in this work and remains a subject for further studies."],"dc:format":["application/pdf"],"dc:identifier":["https://repository.vu.lt/VU:ELABAETD308155835&prefLang=en_US"],"dc:language":["lit"],"dc:publisher":["Institutional Repository of Vilnius University"],"dc:relation":["https://epublications.vu.lt/object/elaba:308155835/308155835.pdf"],"dc:rights":["info:eu-repo/semantics/openAccess"],"dc:title":["Kofeinui jautraus molekulinių įspaudų fotopolimero matricoje jutiklio kūrimas ir tyrimas /","Development and investigation of a caffeine sensitive molecular imprints in a photopolymer matrix."],"dc:type":["info:eu-repo/semantics/masterThesis"]},"updated_at":"2026-11-19T10:12:15Z"}