{"id":{"repo_id":"whiterose","oai_identifier":"oai:etheses.whiterose.ac.uk:20585"},"canonical_url":"https://search.ndltd.org/etd/whiterose/oai:etheses.whiterose.ac.uk:20585","repository":{"repo_id":"whiterose","name":"White Rose University Consortium","base_url":"https://etheses.whiterose.ac.uk/cgi/oai2"},"display":{"title":"Transitioning of Spent Advanced Gas Reactor Fuel from Wet to Dry Storage","abstract":"Upon removal from a reactor spent nuclear fuel is placed into water storage for a period of time since water provides both a decay heat sink and radiation shielding. In the UK this fuel has traditionally been reprocessed however the decision has been made that this will cease in 2018 in favour of an open fuel cycle and direct disposal to a degological disposal facility, although this is not expected to be available until 2075. Current experience with pond storage has found that fuel can be safely stored in caustic dosed ponds for at least 25 years and therefore the current plan is to extend water storage until around 2040, however how the fuel will be stored for the remaining 35 years is yet to be decided. One option that is being considered is the use of dry storage which is being used successfully in the USA for the storage of fuel from Light Water Reactors. One of the most important factors when utilising dry stores is an effective drying step and this PhD is aiming to look at this area in particular. Commercial drying methods have been developed for use with Zircaloy and aluminium clad fuels however this PhD intends to develop a method that can be used to dry Stainless Steel clad fuels such as those used in the UK's Advanced Gas Reactors (AGR). Since intact AGR fuel has yet to be examined following storage the first part if this thesis looked at preparing samples for later macro scale testing. Samples were treated to induce defects known to be of concern and analysed with the conclusion being that bound water is of no concern for drying operations and can be disregarded when preparing samples. Since AGR is known to have failed by stress corrosion cracking water trapped within microcracked pins is a likely issue. A section of tube was prepared by compression and boiling in magnesium chloride which micro CT imaging found to have images of a similar size to known failures. This tube was prepared into a test piece for later testing. The second part of the thesis looks at macro scale testing using the test piece described above and a similar test piece with a 300 um pinhole. A multipurpose drying rig capable of vacuum drying and flowed gas drying was constructed. In the first phase of drying tests vacuum drying and flowed gas drying were compared using a test piece with a 300 um pinhole and the impact of different cover gas was assessed. vacuum drying was found to be significantly more effective than flowed gas drying with the type of cover gas having little impact. Most importantly this work guided further improvements to the rig. The second phase of this work carried out more detailed drying tests on vacuum drying and flowed gas drying and utilised the pinholed and cracked test piece. The greatest influencing factor on the drying rate (the rate at which water could be removed from inside the test piece) was found to be the water level inside the test piece with broadly similar rates being found in all conditions and with both test piece when the test piece was full. As the water level within the test piece dropped, vacuum drying quickly became more effective. This was not helped by considering energy usage. There was however a feeling that flowed gas drying was limited due to the pipework size. In the final phase of testing the ability to detect the point which all water was removed (the end point) from the test piece using online instrumentation was assessed. Currently a vacuum rebound test is used which is both time consuming and if flowed gas drying is being used requires additional plant equipment. It was found that dew point measurements appeared to give a relatively clear indication of the end point when for both vacuum drying and flowed gas drying. For vacuum drying only the measurement of mass flow and pressure also gave a reasonable indication of end point.","abstract_html":"Upon removal from a reactor spent nuclear fuel is placed into water storage for a period of time since water provides both a decay heat sink and radiation shielding. In the UK this fuel has traditionally been reprocessed however the decision has been made that this will cease in 2018 in favour of an open fuel cycle and direct disposal to a degological disposal facility, although this is not expected to be available until 2075. Current experience with pond storage has found that fuel can be safely stored in caustic dosed ponds for at least 25 years and therefore the current plan is to extend water storage until around 2040, however how the fuel will be stored for the remaining 35 years is yet to be decided. One option that is being considered is the use of dry storage which is being used successfully in the USA for the storage of fuel from Light Water Reactors. One of the most important factors when utilising dry stores is an effective drying step and this PhD is aiming to look at this area in particular. Commercial drying methods have been developed for use with Zircaloy and aluminium clad fuels however this PhD intends to develop a method that can be used to dry Stainless Steel clad fuels such as those used in the UK&#x27;s Advanced Gas Reactors (AGR). Since intact AGR fuel has yet to be examined following storage the first part if this thesis looked at preparing samples for later macro scale testing. Samples were treated to induce defects known to be of concern and analysed with the conclusion being that bound water is of no concern for drying operations and can be disregarded when preparing samples. Since AGR is known to have failed by stress corrosion cracking water trapped within microcracked pins is a likely issue. A section of tube was prepared by compression and boiling in magnesium chloride which micro CT imaging found to have images of a similar size to known failures. This tube was prepared into a test piece for later testing. The second part of the thesis looks at macro scale testing using the test piece described above and a similar test piece with a 300 um pinhole. A multipurpose drying rig capable of vacuum drying and flowed gas drying was constructed. In the first phase of drying tests vacuum drying and flowed gas drying were compared using a test piece with a 300 um pinhole and the impact of different cover gas was assessed. vacuum drying was found to be significantly more effective than flowed gas drying with the type of cover gas having little impact. Most importantly this work guided further improvements to the rig. The second phase of this work carried out more detailed drying tests on vacuum drying and flowed gas drying and utilised the pinholed and cracked test piece. The greatest influencing factor on the drying rate (the rate at which water could be removed from inside the test piece) was found to be the water level inside the test piece with broadly similar rates being found in all conditions and with both test piece when the test piece was full. As the water level within the test piece dropped, vacuum drying quickly became more effective. This was not helped by considering energy usage. There was however a feeling that flowed gas drying was limited due to the pipework size. In the final phase of testing the ability to detect the point which all water was removed (the end point) from the test piece using online instrumentation was assessed. Currently a vacuum rebound test is used which is both time consuming and if flowed gas drying is being used requires additional plant equipment. It was found that dew point measurements appeared to give a relatively clear indication of the end point when for both vacuum drying and flowed gas drying. For vacuum drying only the measurement of mass flow and pressure also gave a reasonable indication of end point.","abstract_has_math":false,"creators":["Goode, James Bruce"],"institution":"University of Leeds","degree_name":"Ph.D","degree_level":"doctoral","degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":["Hanson, Bruce C","Harbottle, David"],"committee_chairs":[],"committee_members":[],"year":2017,"date_issued":"2017-12","date_published":"2017-12","updated_at":"2026-11-18T22:27:18Z","subjects":[],"languages":["eng"],"rights":[],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier","label":"Identifier","values":["uk.bl.ethos.745516"],"render_values":[{"text":"uk.bl.ethos.745516","href":null,"code":true}]},{"key":"dc:identifier.grantnumber","label":"Dc Identifier Grantnumber","values":["EP/L014041/1"],"render_values":[{"text":"EP/L014041/1","href":null,"code":true}]}],"person_identifier_entries":[{"key":"person:identifier.orcid","label":"ORCID","values":["0000000249007153"],"render_values":[{"text":"0000-0002-4900-7153","href":"https://orcid.org/0000-0002-4900-7153","code":true}]}]},"links":{"outbound_url":null,"outbound_label":null,"outbound_source":null,"record_url":null,"record_label":null,"record_kind":null,"record_source":null,"download_url":"https://etheses.whiterose.ac.uk/id/eprint/20585/2/AGR%20Fuel%20Drying-Coloured%20links.pdf","download_label":"Download PDF","download_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://etheses.whiterose.ac.uk/cgi/oai2?verb=GetRecord&metadataPrefix=uketd_dc&identifier=oai%3Aetheses.whiterose.ac.uk%3A20585","prefix":"uketd_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Hanson, Bruce C","Harbottle, David"]},{"key":"dc:contributor.sponsor","label":"Sponsor","values":["EPSRC"]},{"key":"dc:creator","label":"Author","values":["Goode, James Bruce"]},{"key":"person:identifier.orcid","label":"ORCID","values":["0000000249007153"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2017-12"]},{"key":"dc:date.issued","label":"Date","values":["2017-12"]},{"key":"dc:publisher.commercial","label":"Dc Publisher Commercial","values":["University of Leeds"]},{"key":"dc:publisher.department","label":"Dc Publisher Department","values":["School of Chemical and Process Engineering (Leeds)"]},{"key":"dc:publisher.institution","label":"Dc Publisher Institution","values":["University of Leeds"]},{"key":"dc:relation.isreferencedby","label":"Dc Relation Isreferencedby","values":["https://etheses.whiterose.ac.uk/id/eprint/20585/"]},{"key":"dc:relation.references","label":"Dc Relation References","values":["[1] Nuclear Decommissioning Authority. Oxide Fuels - Preferred Option - Pub- lications - GOV.UK. Technical Report SMS/TS/C2-OF/001/Preferred Op- tion, June 2012. URL https://www.gov.uk/government/publications/ oxide-fuels-preferred-option. [2] R.L. Sindelar, Caskey Jr, G.R., Peacock Jr, H.B., and Lam, P.S. Evalua- tion of Degradation During Interim Dry Storage of Al SNF. In High level Radioactive Waste Management: Proceedings of the Sixth Annual Interna- tional Conference, Las Vegas, Nevada, May 1995. American Nuclear Society ; American Society of Civil Engineers. ISBN 0-7844-0082-2 978-0-7844-0082-1. [3] R. L. Sindelar, H. B. Peacock, P. S. Lam, N. C. Iyer, M. R. Louthan, and J. R. Murphy. Scientific Basis for Storage Criteria for Interim Dry Storage of Aluminum-clad Fuels. MRS Online Proceedings Library, 412:99{105, 1995. doi: 10.1557/PROC-412-99. [4] ASTM. Guide for Drying Behavior of Spent Nuclear Fuel. Technical Report C-1553, ASTM International, 2008. URL http://www.astm.org/ Standards/C1553.htm. [5] J.V. Best, W.J. Stephen, and A.J. Wickham. Radiolytic graphite oxida- tion. Progress in Nuclear Energy, 16(2):127{178, 1985. ISSN 0149-1970. doi: 10.1016/0149-1970(85)90002-2. URL http://www.sciencedirect. com/science/article/pii/0149197085900022. [6] Neale Brittain. EDF Energy - Nuclear Generation The AGR Design, Fukushima and More, February 2012. URL www-diva.eng.cam.ac.uk/ mphil-in-nuclear-energy/external-lectures/2011-12-lectures/ edf-energy-ng-cambridge-09022012.pdf/at_download/file. [7] J. Winton, M. M. Haberlin, D. Rhodes, R. B. Jones, J. S. Waddington, and A. C. Roberts. 7. The mechanical properties of AGR cladding. In Nuclear Fuel Performance, pages 7.1{7.5. Thomas Telford Publishing, January 1973. ISBN 978-0-7277-5160-7. URL http://www.icevirtuallibrary.com/doi/ full/10.1680/nfp.48977.0011. DOI: 10.1680/nfp.48977.0011. [8] John Kyffin. Technological Development to Support a Change in the United Kingdom's Strategy for Management of Spent AGR Oxide Fuel. In Pro- ceedings of the International Conference on Management of Spent Fuel from Nuclear Power Reactors, Vienna, June 2015. IAEA. [9] J.V. Best, A.J. Wickham, and C.J. Wood. Inhibition of Moderator Graphite Corrosion in CEGB Magnox Reactors 1. Laboratory measurements of the effect of coolant composition on the radiolytic Graphite/CO//2 Reaction. Journal of the British Nuclear Energy Society, 135(185):319{324, 1976. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0016983992& partnerID=40&md5=915c35fbb47bb51abf96e4726b4dc0fe. [10] J.V. Best, A.J. Wickham, and C.J. Wood. Inhibition of Mod- erator Graphite Corrosion in CEGB Magnox Reactors - 2. Hy- drogen Injections into Wylfa Reactor I Coolant Gas. Journal of the British Nuclear Energy Society, 135(185):325{331, 1976. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0016985985& partnerID=40&md5=f4aeea00cb2805b54d15a5cd33f4812b. [11] J.A. Cairns, J.P. Coad, E.W.T. Richards, and I.A. Stenhouse. Car- bon deposition on metallic surfaces studied by r.f. plasma discharge. Nature, 288(5792):686{687, 1980. URL http://www.scopus.com/ inward/record.url?eid=2-s2.0-0042260217&partnerID=40&md5= f4025f10064d6610aec7f2736563fc3b. [12] G.W. Horsley and J.A. Cairns. The inhibition of carbon deposition on stain- less steel by prior selective oxidation. Applied Surface Science, 18(3):273{ 286, 1984. URL http://www.scopus.com/inward/record.url?eid=2-s2. 0-0021468709&partnerID=40&md5=60bc28d98b47c716a564bb0f71611fb0. [13] M.L. Sykes, I.A.S. Edwards, and K.M. Thomas. Metal carbonyl decom- position and carbon deposition in the advanced gas-cooled nuclear reactor. Carbon, 31(3):467{472, 1993. ISSN 0008-6223. doi: 10.1016/0008-6223(93) 90135-W. URL http://www.sciencedirect.com/science/article/pii/ 000862239390135W. [14] Clive Mowforth. Suppression of Carbon Deposition in an AGR. In Con- ference on Chemistry in Nuclear Power Generation, Manchester, November 2014. [15] G.R. Millward, H.E. Evans, M. Aindow, and C.W. Mowforth. The influence of oxide layers on the initiation of carbon deposition on stainless steel. Oxidation of Metals, 56(3-4):231{250, 2001. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0013354192& partnerID=40&md5=14f7e80057f0ecd263b8f337c701c13c. [16] G.R. Millward, H.E. Evans, I.P. Jones, C.D. Eley, and C.W. Mowforth. The inuence of carbonyl sulphide on the inhibition of filamentary carbon deposi- tion on stainless steel. Materials and Corrosion, 54(11):864{869, 2003. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0344585500& partnerID=40&md5=609c82c48463f73743e82819b5ebd61f. [17] G.R. Millward, H.E. Evans, I.P. Jones, and C.D. Eley. Car- bon deposition on stainless steel in oxidising environments. Ma- terials at High Temperatures, 20(4):535{541, 2003. URL http: //www.scopus.com/inward/record.url?eid=2-s2.0-10844227558& partnerID=40&md5=34d871d3680f50df94784719a7d51797. [18] G.R. Millward, H.E. Evans, I.P. Jones, C.D. Eley, and K.A. Simpson. Burn-off of filamentous carbon and subsequent re- deposition on a 20cr25ni austenitic steel. Materials at High Tem- peratures, 26(1):57{61, 2009. URL http://www.scopus.com/ inward/record.url?eid=2-s2.0-72349086337&partnerID=40&md5= 10bc279a2d2654434c55872fad462ef6. [19] British Stainless Steel Association. What Is Stainless Steel? URL http: //www.bssa.org.uk/faq.php?id=1. [20] Oliver Kuhn. Science Break : Steel. Recorder-The Official Journal of Canadian Exploarion Geopyhsicists, 38(08), October 2013. URL http: //csegrecorder.com/features/view/science-break-201310. [21] Magmaweld. Stainless Steel Welding. URL http://www.magmaweld.com/ stainless_steel_welding.html. [22] Zhiliang Cao and Henry Gu Cao. Cubic Atom and Crystal Structures. International Journal of Physics, International Journal of Physics, 2(6): 277{281, January 2014. ISSN 2333-4878. doi: 10.12691/ijp-2-6-11. URL http://pubs.sciepub.com/ijp/2/6/11/abstract.html. [23] James Gordon Parr and Albert Hanson. An introduction to stainless steel. American Society for Metals, 1965. [24] Donald Peckner and I. M. Bernstein, editors. Handbook of stainless steels. McGraw-Hill, New York, 1977. ISBN 978-0-07-049147-2. [25] L. Hochmann and J. Colombier. Stainless and Heat Resisting Steels. Edward Arnold, second edition edition edition, 1967. [26] W. A. England, M. J. Bennett, D. A. Greenhalgh, S. N. Jenny, and C. F. Knights. The characterization by raman spectroscopy of oxide scales formed on a 20crn25ninNb stabilized stainless steel. Corrosion Sci- ence, 26(7):537{545, 1986. ISSN 0010-938X. doi: 10.1016/0010-938X(86) 90021-1. URL http://www.sciencedirect.com/science/article/pii/ 0010938X86900211. [27] J. Y. Jeng, B. E. Quayle, P. J. Modern, W. M. Steen, and B. D. Bastow. Laser surface treatments to improve the intergranular corrosion resistance of 18/13/Nb and 304l in nitric acid. Corrosion Science, 35(5):1289{1296, 1993. ISSN 0010-938X. doi: 10.1016/0010-938X(93)90350-P. URL http://www. sciencedirect.com/science/article/pii/0010938X9390350P. [28] M. F. Montemor, M. G. S. Ferreira, N. E. Hakiki, and M. Da Cunha Belo. Chemical composition and electronic structure of the oxide films formed on 316l stainless steel and nickel based alloys in high temperature aque- ous environments. Corrosion Science, 42(9):1635{1650, September 2000. ISSN 0010-938X. doi: 10.1016/S0010-938X(00)00012-3. URL http://www. sciencedirect.com/science/article/pii/S0010938X00000123. [29] S. S. M. Tavares, V. Moura, V. C. da Costa, M. L. R. Ferreira, and J. M. Pardal. Microstructural changes and corrosion resistance of AISI 310s steel exposed to 600-800 C. Materials Characterization, 60(6):573578, June 2009. ISSN 1044-5803. doi: 10.1016/j.matchar.2008.12.005. URL http://www. sciencedirect.com/science/article/pii/S1044580308003422. [30] Abdulla Al-Shater, Dirk Engelberg, Stuart Lyon, Cornelius Donohoe, Steve Walters, Guy Whillock, and Andrew Sherry. Characterization of the stress corrosion cracking behavior of thermally sensitized 20cr-25ni stainless steel in a simulated cooling pond environment. Journal of Nuclear Science and Tech- nology, 0(0):1{10, April 2017. ISSN 0022-3131. doi: 10.1080/00223131.2017. 1309305. URL http://dx.doi.org/10.1080/00223131.2017.1309305. [31] C. Tyzack and H.C. Cowen. The corrosion of reactor materials in carbon dioxide. Atomic Energy Review, 14(2):263{324, 1976. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0016963965& partnerID=40&md5=c3c8ed5610ba613cee9abf20b181440c. [32] J. M. Francis. Structure of Surface Oxides Formed on A 20% Cr/25% Ni/Nb-Stabilised Steel in Carbon Dioxide at High Temperatures. British Corrosion Journal, 3(3):113{119, May 1968. ISSN 0007-0599. doi: 10. 1179/000705968798326244. URL http://www.maneyonline.com/doi/abs/ 10.1179/000705968798326244. [33] J. A. Desport and M. J. Bennett. Investigation by fractography of the high- temperature oxidation of the 20%Cr-25%Ni-Nb stainless steel. Oxidation of Metals, 29(3-4):327{346, April 1988. ISSN 0030-770X, 1573-4889. doi: 10. 1007/BF00751803. URL http://link.springer.com/article/10.1007/ BF00751803. [34] M.J. Bennett, P.C. Blythe, G.H. Chaffey, K. Hand, J.W. McMillan, S.J. Webster, and J.E. Antill. The effect of fission neutron irradiation upon the oxidation of a 20 wt % Cr/25 wt % Ni/Nb stabilised stainless steel by carbon dioxide beween 580 and 840C. Journal of Nuclear Materials, 25(3):260{270, March 1968. ISSN 0022-3115. doi: 10.1016/0022-3115(68) 90169-4. URL http://www.sciencedirect.com/science/article/pii/ 0022311568901694. [35] M.J. Bennett, G.H. Chaffey, and J.E. Antill. Some aspects of the effects of fission fragment irradiation upon the oxidation of austenitic stainless steels by oxygen at 650C and 800C. Journal of Nuclear Materials, 32(2): 299{309, September 1969. ISSN 0022-3115. doi: 10.1016/0022-3115(69) 90079-8. URL http://www.sciencedirect.com/science/article/pii/ 0022311569900798. [36] William D. Callister. Materials science and engineering: an introduction. Wiley international edition. Wiley, New York, NY, 6th international edition, 2003. ISBN 0-471-22471-5 0-471-22471-5 0-555-00205-5 0-471-26456-3. [37] S. M Bruemmer, E. P Simonen, P. M Scott, P. L Andresen, G. S Was, and J. L Nelson. Radiation-induced material changes and susceptibility to intergranular failure of light-water-reactor core internals. Journal of Nuclear Materials, 274(3):299{314, September 1999. ISSN 0022-3115. doi: 10.1016/ S0022-3115(99)00075-6. URL http://www.sciencedirect.com/science/ article/pii/S0022311599000756. [38] E. A. Little. Development of radiation resistant materials for advanced nuclear power plant. Materials Science and Technol- ogy, 22(5):491{518, May 2006. ISSN 0267-0836. doi: 10.1179/ 174328406X90998. URL http://0-www.maneyonline.com.wam.leeds.ac. uk/doi/abs/10.1179/174328406X90998. [39] C Taylor. The formation of sensitised microstructures during the irra- diation of CAGR fuel pin cladding. In Symposium on the Radiation- induced Sensitisation of Stainless Steels;, Berkeley, UK, September 1986. URL https://inis.iaea.org/search/searchsinglerecord.aspx? recordsFor=SingleRecord&RN=18098354. [40] John Kyffin. The technical case for interim Storage of AGR fuel and devel- opment of a programme of further work. Manchester, April 2014. IChemE. [41] Kenneth R. Trethewey and John Chamberlain. Corrosion for science and engineering. Longman, Harlow, 2. ed., reprint edition, 1998. ISBN 0-582- 23869-2 0-582-23869-2. [42] A. V. Byalobzheskii. Radiation Corrosion. I.P.S.T., May 1970. ISBN 978-0- 7065-1013-3. [43] Robert S. Glass, George E. Overturf, Richard A. Van Konynenburg, and R. Daniel McCright. Gamma radiation effects on corrosion-I. Electro- chemical mechanisms for the aqueous corrosion processes of austenitic stainless steels relevant to nuclear waste disposal in tuff. Corrosion Sci- ence, 26(8):577{590, 1986. ISSN 0010-938X. doi: 10.1016/0010-938X(86) 90025-9. URL http://www.sciencedirect.com/science/article/pii/ 0010938X86900259. [44] W. G. Burns, W. R. Marsh, and W. S. Walters. The gamma irradiation- enhanced corrosion of stainless and mild steels by water in the pres- ence of air, argon and hydrogen. Radiation Physics and Chemistry (1977), 21(3):259{279, 1983. ISSN 0146-5724. doi: 10.1016/0146-5724(83) 90155-3. URL http://www.sciencedirect.com/science/article/pii/ 0146572483901553. [45] R. L. Sindelar, P. S. Lam, M. R. Louthan Jr., and N. C. Iyer. Corrosion of Metals and Alloys in High Radiation Fields. Materials Characterization, 43 (2-3):147{157, August 1999. ISSN 1044-5803. doi: 10.1016/S1044-5803(99) 00042-X. URL http://www.sciencedirect.com/science/article/pii/ S104458039900042X. [46] R. J. Guenther, A. B. Johnson Jr, A. L. Lund, and E. R. Gilbert. Initial Evaluation of Dry Storage Issues for Spent Nuclear Fuels in Wet Storage at the Idaho Chemical Processing Plant. Technical Report INEL{96/0140, Idaho National Engineering Lab., Idaho Falls, ID (United States), November 1994. URL http://www.osti.gov/scitech/biblio/285498. [47] R. Winston Revie, Herbert Henry Uhlig, and Herbert Henry Uhlig, editors. Uhlig's Corrosion Handbook. Electrochemical Society series. Wiley, New York, 2nd ed edition, 2000. ISBN 978-0-471-15777-9. [48] R. Priya, S. Ningshen, and U. Kamachi Mudali. In uence of Oxidizing Ion Concentration on the Corrosion Resistance of Type 304l Stainless Steel in Nitric Acid Medium. Corrosion, 69(4):335{344, April 2013. ISSN 0010-9312. doi: 10.5006/703. URL http://0-corrosionjournal.org.wam.leeds.ac. uk/doi/full/10.5006/703. [49] C. L. Briant. The Effects of Sulfur and Phosphorus on the In- tergranular Corrosion of 304 Stainless Steel. Corrosion, 36(9):497{ 509, September 1980. ISSN 0010-9312. doi: 10.5006/0010-9312-36.9. 497. URL http://0-corrosionjournal.org.wam.leeds.ac.uk/doi/abs/ 10.5006/0010-9312-36.9.497. [50] O. V. Kasparova. The effect of boron and carbon on the structure and corrosion-electrochemical behavior of Kh20n20 austenitic stainless steel. Protection of Metals and Physical Chemistry of Surfaces, 49(6): 734{739, November 2013. ISSN 2070-2051, 2070-206X. doi: 10.1134/ S2070205113060063. URL http://link.springer.com/article/10.1134/ S2070205113060063. [51] M. Mayuzumi, J. Ohta, and T. Arai. Efffects of Cold Work, Sensitization Treatment, and the Combination on Corrosion Behavior of Stainless Steels in Nitric Acid. Corrosion, 54(4):271{280, April 1998. ISSN 0010-9312. doi: 10. 5006/1.3284853. URL http://0-corrosionjournal.org.wam.leeds.ac. uk/doi/abs/10.5006/1.3284853. [52] ASTM International. Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels. Technical report, ASTM International, 2014. URL http://www.astm.org/Standards/A262.htm. [53] T. M. Devine, C. L. Briant, and B. J. Drummond. Mechanism of intergran- ular corrosion of 316l stainless steel in oxidizing acids. Scripta Metallur- gica, 14(11):1175{1179, November 1980. ISSN 0036-9748. doi: 10.1016/ 0036-9748(80)90251-3. URL http://www.sciencedirect.com/science/ article/pii/0036974880902513. [54] G. H. Aydogdu and M. K. Aydinol. Determination of susceptibility to in- tergranular corrosion and electrochemical reactivation behaviour of AISI 316l type stainless steel. Corrosion Science, 48(11):3565{3583, November 2006. ISSN 0010-938X. doi: 10.1016/j.corsci.2006.01.003. URL http: //www.sciencedirect.com/science/article/pii/S0010938X06000308. [55] Wenjie Bai, Mengyu Chai, Lichan Li, and Quan Duan. Comparative Study of Acoustic Emission Characteristics for Intergranular Corrosion of 316l Stain- less Steel Parent Material and Weldment. In ASME 2014 Pressure Vessels and Piping Conference Volume 5: High-Pressure Technology; ASME NDE Division; 22nd Scavuzzo Student Paper Symposium and Competition, Ana- heim, California, USA, July 2014. The American Society of Mechanical Engi- neers. URL http://0-proceedings.asmedigitalcollection.asme.org. wam.leeds.ac.uk/proceeding.aspx?articleid=1938090. [56] P. Fauvet, F. Balbaud, R. Robin, Q. T. Tran, A. Mugnier, and D. Espinoux. Corrosion mechanisms of austenitic stainless steels in nitric media used in reprocessing plants. Journal of Nuclear Materials, 375(1):52{64, March 2008. ISSN 0022-3115. doi: 10.1016/j.jnucmat.2007.10.017. URL http://www. sciencedirect.com/science/article/pii/S002231150701046X. [57] Fanny Balbaud, Gerard Sanchez, Gerard Santarini, and Gerard Pi- card. Cathodic Reactions Involved in Corrosion Processes Occur-ing in Concentrated Nitric Acid at 100C. European Journal of Inorganic Chemistry, 2000(4):665{674, 2000. ISSN 1099-0682. doi: 10.1002/(SICI)1099-0682(200004)2000:4h665::AID-EJIC665i3.0.CO;2-N. URL http://onlinelibrary.wiley.com/doi/10.1002/(SICI) 1099-0682(200004)2000:4<665::AID-EJIC665>3.0.CO;2-N/abstract. [58] K. Fukuya, S. Shima, H. Kayano, and M. Narui. Stress corrosion cracking and intergranular corrosion of neutron irradiated austenitic stainless steels. Journal of Nuclear Materials, 191-194, Part B:1007{1011, September 1992. ISSN 0022-3115. doi: 10.1016/0022-3115(92)90626-V. URL http://www. sciencedirect.com/science/article/pii/002231159290626V. [59] NACE International. Stress Corrosion Cracking (SCC). URL https://www.nace.org/Corrosion-Central/Corrosion-101/ Stress-Corrosion-Cracking-(SCC)/. [60] Philippe Marcus. Corrosion Mechanisms in Theory and Practice. CRC Press, July 2002. ISBN 978-0-203-90918-8. Google-Books-ID: 69bImhlRCdcC. [61] ASTM International. ASTM G38 - 01(2013) Standard Practice for Making and Using C-Ring Stress-Corrosion Test Specimens. Technical report, 2007. URL https://www.astm.org/Standards/G38.htm. [62] ASTM International. ASTM G36 - 94(2013) Standard Practice for Evalu- ating Stress-Corrosion-Cracking Resistance of Metals and Alloys in a Boil- ing Magnesium Chloride Solution. Technical report, 2007. URL https: //www.astm.org/Standards/G36.htm. [63] Heinz Kohl. A Contribution to the Examination of Stress Corrosion Crack- ing of Austenitic Stainless Steels in Magnesium Chloride Solutions. COR- ROSION, 23(2):39{49, February 1967. ISSN 0010-9312. doi: 10.5006/ 0010-9312-23.2.39. URL http://www.corrosionjournal.org/doi/abs/ 10.5006/0010-9312-23.2.39. [64] Osama M. Alyousif and Rokuro Nishimura. The stress corrosion cracking behavior of austenitic stainless steels in boiling magnesium chloride solu- tions. Corrosion Science, 49(7):3040{3051, July 2007. ISSN 0010-938X. doi: 10.1016/j.corsci.2006.12.023. URL http://www.sciencedirect.com/ science/article/pii/S0010938X07000248. [65] Osama M. Alyousif and Rokuro Nishimura. The effect of test tempera- ture on SCC behavior of austenitic stainless steels in boiling saturated mag- nesium chloride solution. Corrosion Science, 48(12):4283{4293, December 2006. ISSN 0010-938X. doi: 10.1016/j.corsci.2006.01.014. URL http: //www.sciencedirect.com/science/article/pii/S0010938X06000643. [66] C. Garcia, F. Martin, P. De Tiedra, J. A. Heredero, and M. L. Aparicio. Effects of prior cold work and sensitization heat treatment on chloride stress corrosion cracking in type 304 stainless steels. Corrosion science, 43(8): 1519{1539, 2001. ISSN 0010-938X. URL http://cat.inist.fr/?aModele= afficheN&cpsidt=14117343. [67] David Hambley. Technical Basis for Extending Storage of AGR Fuel. Salt Lake City, September 2013. URL https://www.researchgate.net/ profile/David_Hambley/publication/279058579_Technical_Basis_ for_Extending_Storage_of_the_UK's_Advanced_Gas-Cooled_Reactor_ Fuel/links/5589322308aed6bff80b421d.pdf. [68] Craig W. Jones. Environmental Application of Hydrogen Peroxide. In Applications of Hydrogen Peroxide and Derivatives, pages 213{217. Royal Society of Chemistry, Cambridge, 1999. ISBN 978-0-85404-536-5. Google-Books-ID: QLePlhTsE0oC. [69] Mark C. Biesinger, Brad P. Payne, Andrew P. Grosvenor, Leo W. M. Lau, Andrea R. Gerson, and Roger St. C. Smart. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni. Applied Surface Science, 257(7):2717{2730, January 2011. ISSN 0169-4332. doi: 10.1016/j.apsusc.2010.10.051. URL http:// www.sciencedirect.com/science/article/pii/S0169433210014170. [70] Thermo Scientific. XPS Interpretation of Calcium. URL https:// xpssimplified.com/elements/calcium.php. [71] P. Stefanov, D. Stoychev, M. Stoycheva, A. R. Gonzalez-Elipe, and Ts. Marinova. XPS, SEM and TEM characterization of stainless- steel 316l surfaces after electrochemical etching and oxidizing. Surface and Interface Analysis, 28(1):106{110, August 1999. ISSN 1096- 9918. doi: 10.1002/(SICI)1096-9918(199908)28:1h106::AID-SIA628i3.0. CO;2-J. URL http://onlinelibrary.wiley.com/doi/10.1002/(SICI) 1096-9918(199908)28:1<106::AID-SIA628>3.0.CO;2-J/abstract. [72] S. Jin and A. Atrens. ESCA-studies of the structure and composition of the passive film formed on stainless steels by various immersion times in 0.1 M NaCl solution. Applied Physics A, 42(2):149{165, January 1987. ISSN 0947- 8396, 1432-0630. doi: 10.1007/BF00616726. URL http://link.springer. com/article/10.1007/BF00616726. [73] P Stefanov, D Stoychev, M Stoycheva, and Ts Marinova. XPS and SEM studies of chromium oxide films chemically formed on stainless steel 316 L. Materials Chemistry and Physics, 65(2):212{215, July 2000. ISSN 0254-0584. doi: 10.1016/S0254-0584(00)00249-2. URL http://www.sciencedirect. com/science/article/pii/S0254058400002492. [74] V. Maurice, W. P. Yang, and P. Marcus. XPS and STM Study of Passive Films Formed on Fe-22cr(110) Single-Crystal Surfaces. Journal of The Elec- trochemical Society, 143(4):1182{1200, April 1996. ISSN 0013-4651, 1945- 7111. doi: 10.1149/1.1836616. URL http://0-jes.ecsdl.org.wam.leeds. ac.uk/content/143/4/1182. [75] R. Li, M. G. S. Ferreira, M. A. Anjos, and R. Vilar. Localized corrosion of laser surface cladded UNS S31254 superaustenitic stainless steel on mild steel. Surface and Coatings Technology, 88(1-3):90{95, January 1997. ISSN 0257-8972. doi: 10.1016/S0257-8972(96)02865-4. URL http://www. sciencedirect.com/science/article/pii/S0257897296028654. [76] M. A. Ashworth, D. I. R. Norris, and I. P. Jones. Radiation-induced segregation in Fe-20cr-25ni-Nb based austenitic stainless steels. Journal of Nuclear Materials, 189(3):289{302, August 1992. ISSN 0022-3115. doi: 10.1016/0022-3115(92)90383-V. URL http://www.sciencedirect.com/ science/article/pii/002231159290383V. [77] Jiang Hsieh. Computed Tomography: Principles, Design, Artifacts, and Recent Advances. SPIE PRESS, 2015. ISBN 978-1-62841-825- 5. URL http://ebooks.spiedigitallibrary.org/book.aspx?doi=10. 1117/3.2197756. DOI: 10.1117/3.2197756. [78] D. A. Horner, B. J. Connolly, S. Zhou, L. Crocker, and A. Turnbull. Novel images of the evolution of stress corrosion cracks from corrosion pits. Corrosion Science, 53(11):3466{3485, November 2011. ISSN 0010-938X. doi: 10.1016/j.corsci.2011.05.050. URL http://www.sciencedirect.com/ science/article/pii/S0010938X11002721. [79] L. Babout, T. J. Marrow, D. Engelberg, and P. J. Withers. X-ray microtomographic observation of intergranular stress corrosion cracking in sensitised austenitic stainless steel. Materials Science and Technology, 22(9):1068{ 1075, September 2006. ISSN 0267-0836. doi: 10.1179/174328406X114090. URL https://doi.org/10.1179/174328406X114090. [80] A. King, G. Johnson, D. Engelberg, W. Ludwig, and J. Marrow. Observations of Intergranular Stress Corrosion Cracking in a Grain-Mapped Polycrystal. Science, 321(5887):382{385, July 2008. ISSN 0036-8075, 1095- 9203. doi: 10.1126/science.1156211. URL http://science.sciencemag. org/content/321/5887/382. [81] W. Stephen Walters, Peter Durham, and Nicholas A. Hodge. The adsorption and desorption of water from a carbonaceous deposit layer on the surface of stainless steel representing spent AGR nuclear fuel cladding. Journal of Nuclear Science and Technology, 0(0):1{12, December 2017. ISSN 0022- 3131. doi: 10.1080/00223131.2017.1403384. URL https://doi.org/10. 1080/00223131.2017.1403384. [82] Yunus A. Cengel and Michael A. Boles. 2.1 Pure Substance. In Thermo- dynamics: an engineering approach, page 48. McGraw Hill, Boston, 3rd ed edition, 1998. ISBN 978-0-07-011927-7. [83] The Engineering Toolbox. Water Saturation Pressure. URL http://www. engineeringtoolbox.com/water-vapor-saturation-pressure-d_599. html. [84] Yunus A. Cengel and Michael A. Boles. 2.3 Phase-change Processes of Pure Substances. In Thermodynamics: an engineering approach, pages 49{55. McGraw Hill, Boston, 3rd ed edition, 1998. ISBN 978-0-07-011927-7. [85] Yunus A. Cengel and Michael A. Boles. 2.4 Property Diagrams for Phase- change Processes. In Thermodynamics: an engineering approach, pages 55{ 62. McGraw Hill, Boston, 3rd ed edition, 1998. ISBN 978-0-07-011927-7. [86] J.M.Sullivan Jr. ES 3001 Thermodynamics. URL http://users.wpi.edu/ ~sullivan/ES3001/Lectures/Lecture-A/Lecture-2-2011.htm. [87] Wikipedia, The Online Encyclopedia. Phase diagram. Novem- ber 2015. URL https://en.wikipedia.org/w/index.php?title=Phase_ diagram&oldid=692814655. Page Version ID: 692814655. [88] Yunus A. Cengel and Michael A. Boles. 2.5 Vapour Pressure and Phase Equlibrium. In Thermodynamics: an engineering approach, pages 62{66. McGraw Hill, Boston, 3rd ed edition, 1998. ISBN 978-0-07-011927-7. 127, [89] Robert J. Hunter. Thermodynamics of Surfaces. In Foundations of colloid science, pages 87{93. Oxford University Press, Oxford ; New York, 2nd ed edition, 2001. ISBN 978-0-19-850502-0. [90] Felix Casanova, Casey E Chiang, Chang-Peng Li, Igor V Roshchin, Anne M Ruminski, Michael J Sailor, and Ivan K Schuller. Gas adsorption and capillary condensation in nanoporous alumina films. Nanotechnology, 19(31): 315709, 2008. ISSN 0957-4484. URL http://stacks.iop.org/0957-4484/ 19/i=31/a=315709. [91] Yunus A Cengel. 1-3 Heat Transfer. In Introduction to thermodynamics and heat transfer, pages 5{6. McGraw-Hill, Dubuque, IA, 2008. ISBN 978-0-07- 128773-9. [92] 1.1 What and How. In Frank P. Incropera, David P. DeWitt, Theodore L. Bergman, and Adrienne S. Lavine, editors, Principles of heat and mass trans- fer, pages 3{5. Wiley, Singapore, 7. ed., international student version edition, 2013. ISBN 978-0-470-64615-1 978-0-470-50197-9. [93] Yunus A Cengel. 9-2 Conduction. In Introduction to thermodynamics and heat transfer, pages 374{381. McGraw-Hill, Dubuque, IA, 2008. ISBN 978- 0-07-128773-9. [94] J. P. Holman. 1-2 Thermal Conductivity. In Heat transfer, McGraw-Hill series in mechanical engineering, pages 5{9. McGraw-Hill, New York, 9th ed edition, 2002. ISBN 978-0-07-240655-9 978-0-07-112230-6. [95] Thermal Conductivity of common Materials and Gases. URL https://www. engineeringtoolbox.com/thermal-conductivity-d_429.html. [96] Yunus A Cengel. 9-3 Convection. In Introduction to thermodynamics and heat transfer, pages 382{383. McGraw-Hill, Dubuque, IA, 2008. ISBN 978- 0-07-128773-9. [97] J. P. Holman. 1-3 Convection Heat Transfer. In Heat transfer, McGraw-Hill series in mechanical engineering, pages 9{12. McGraw-Hill, New York, 9th ed edition, 2002. ISBN 978-0-07-240655-9 978-0-07-112230-6. [98] 1.2.2 Convection. In Frank P. Incropera, David P. DeWitt, Theodore L.Bergman, and Adrienne S. Lavine, editors, Principles of heat and mass transfer, pages 6{8. Wiley, Singapore, 7. ed., international student version edition, 2013. ISBN 978-0-470-64615-1 978-0-470-50197-9. [99] 14.1 Physical Origins and Rate Equations [Diffusion Mass Transfer]. In Frank P. Incropera, David P. DeWitt, Theodore L. Bergman, and Adri- enne . Lavine, editors, Principles of heat and mass transfer, pages 934{939. Wiley, Singapore, 7. ed., international student version edition, 2013. ISBN 978-0-470-64615-1 978-0-470-50197-9. [100] Jaime Benitez. 1.2 Molecular Mass Transfer. In Principles and modern applications of mass transfer operations, pages 3{15. Wiley-Interscience, New York, 2002. ISBN 978-0-471-20344-5. [101] A. H. P. Skelland. 2 Molecular Diffusion. In Diffusional Mass Transfer,pages 6{48. John Wiley & Sons Inc, New York, 1st edition edition edition, April 1974. ISBN 978-0-471-79374-8. [102] Jaime Benitez. 1.3 The Diffusion Coefficient. In Principles and modern applications of mass transfer operations, pages 15{34. Wiley-Interscience, New York, 2002. ISBN 978-0-471-20344-5 [103] E. L. Cussler. 5.1 Diffusion Coefficients in Gas. In Diffusion: mass transfer in fluid systems, pages 101{111. Cambridge University Press, New York, 2nd ed edition, 1997. ISBN 978-0-521-45078-2 978-0-521-56477-9. [104] E. L. Cussler. 6.5-Solute Boundary Interactions. In Diffusion: mass transfer in fluid systems. Cambridge University Press, New York, 2nd ed edition, 1997. ISBN 978-0-521-45078-2 978-0-521-56477-9. [105] Diffusion of Fluids in Porous Solids. In Robert H. Perry and Don W. Green, editors, Perry's chemical engineers' handbook, pages 5.48{5.49. McGraw-Hill, New York, 8th ed edition, 2008. ISBN 978-0-07-142294-9. [106] NRC: Glossary { Crud. URL http://www.nrc.gov/reading-rm/ basic-ref/glossary/crud.html. [107] W. S. Large. Review of Drying Methods for Spent Nuclear Fuel. Technical Report WSRC-TR-97-0075, Savannah River Site (US), Aiken, SC 29808, October 1999. URL http://www.osti.gov/scitech/biblio/14490. [108] G. E. Culley. Hanford's Progress Toward Dry Interim Storage of K Basin`s Spent Fuel. Technical Report WHC-SA{3107-FP; CONF-960804{, West- inghouse Hanford Co., Richland, WA (United States), May 1996. URL http://www.osti.gov/scitech/biblio/330736. [109] A. L. Pajunen. Cold Vacuum Drying Residual Free Water Test Descrip tion. Technical Report HNF{1851, Fluor Daniel Hanford Inc., Richland, WA (United States), December 1997. URL http://www.osti.gov/scitech/ biblio/10148296. [110] P. G. Loscoe. Transitioning Metallic Uranium Spent Nuclear Fuel from Wet to Dry Storage. In WM 2000 Proceedings, Tucson, Az, March 2000. URL https://www.wmsym.org/archives/2000/pdf/54/54-9.pdf. [111] L Rodrigo, L Therrien, and B. Surette. Low-Temperature, Vacuum-Assisted Drying of Degraded Spent Nuclear Fuel. In Waste Management, Decommissioning and Environmental Restoration for Canada's Nuclear Activities Current Practices and Future Needs. Canadian Nuclear Society, Toronto, 2005. ISBN 978-0-919784-81-9. [112] W.C.H Kupferschmidt and M.E. Stephens. AECL's Waste Management and Decommissioning Program. page 685. Australian Nuclear Association, 2006. [113] DS Cox, IB Bainbridge, and KR Greeneld. Management of Legacy Spent Nuclear Fuel Wastes at the Chalk River Laboratories: Operating Experi- ence and Progress Towards Waste Remediation. In Proceedings of WM'05 Conference, Tucson, Az, March 2005. [114] J.C. Crepeau, S. Reese, H.M. Mcllroy Jr., and R.E. Lords. Drying of Mock Spent Nuclear Fuel Elements. Drying Technology, 16(3-5):545{560, 1998.ISSN 07373937. [115] R. E. Lords, W. E. Windes, J. C. Crepeau, and R. W. Sidwell. Drying Studies of Simulated Doe Aluminum Plate Fuels. Technical Report INEL{95/00437; CONF-9606116{44, Idaho National Engineering Lab., Idaho Falls,ID (United States), May 1996. URL http://www.osti.gov/scitech/ biblio/236247. [116] R. E. Lords, W. E. Windes, J. C. Crepeau, and R. W. Sidwell. Drying Studies for Corroded Doe Aluminum Plate Fuels. Technical Report INEL{96/00134; CONF-960804{29, Idaho National Engineering Lab., Idaho Falls, ID (United States), May 1996. URL http://www.osti.gov/scitech/biblio/260992. [117] D. Caramelle, A. Bastianelli, F. Boussard, A. Milesi, G. Polydor, and G. Christin. CEA Spent Fuel: Reprocessing and Storage Management. In Proceedings of WM'97, Tucson, Az, March 1997. URL http://www.wmsym. org/archives/1997/sess12/12-04.htm. [118] P Michaille. Retrieval of Degraded Irradiated Fuel and Conditioning for a Safe Storage: the CEA Experience, October 2003. URL http://www.iaea.org/OurWork/ST/NE/NEFW/CEG/documents/ws102003_michaille3-e.pdf. [119] Krishna Pal Singh. Forced gas ow canister dehydration, June 2004. URL http://www.google.com/patents/EP1429344A2. International Classification G21C17/06, G21F5/14, G21C19/32, G21F5/00, G21F5/06, G21F9/36, F26B3/00, G21C19/06; Cooperative Classification G21F5/06, G21Y2004/40, G21Y2002/207, G21F9/34, G21Y2002/501, G21Y2002/201, G21Y2002/202; European Classification G21F5/06, G21F9/34. [120] J Morris, S Wickham, P Richardson, C Rhodes, and M Newland. Con- tingency Options for the Dry Storage of Magnox Spent Fuel in the UK. In Proceedings of the 12th International Conference on Radioactive Waste Management and Environmental Remediation, ICEM, volume 1, pages 817{ 823, Liverpool, October 2009. ISBN 978-0-7918-4407-6. doi: 10.1115/ ICEM2009-16331. [121] R. Sindelar, D. Vinson, N. Iyer, and D. Fisher. Overview of Crite- ria for Interim Wet and Dry Storage of Research Reactor Spent Nuclear Fuel. Technical report, SRS, 2010. URL http://sti.srs.gov/fulltext/ SRNL-STI-2010-00688.pdf. [122] Rick Springman. Forced Gas Dehydration (FGD) System for Drying Nuclear Fuel andWaste Packages. 17th Packaging and Transportation of Radioactive Materials Symposium (PATRAM 13). San Francisco, August 2013. [123] Engineering Toolbox. Specific Heat and Individual Gas Con- stant of Gases. URL http://www.engineeringtoolbox.com/ specific-heat-capacity-gases-d_159.html."]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"dc:type.qualificationlevel","label":"Dc Type Qualificationlevel","values":["doctoral"]},{"key":"dc:type.qualificationname","label":"Dc Type Qualificationname","values":["Ph.D"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.dcterms_iso639_2","label":"Language (ISO 639-2)","values":["eng"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["uk.bl.ethos.745516"]},{"key":"dc:identifier.grantnumber","label":"Dc Identifier Grantnumber","values":["EP/L014041/1"]},{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://etheses.whiterose.ac.uk/id/eprint/20585/2/AGR%20Fuel%20Drying-Coloured%20links.pdf"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Upon removal from a reactor spent nuclear fuel is placed into water storage for a period of time since water provides both a decay heat sink and radiation shielding. In the UK this fuel has traditionally been reprocessed however the decision has been made that this will cease in 2018 in favour of an open fuel cycle and direct disposal to a degological disposal facility, although this is not expected to be available until 2075. Current experience with pond storage has found that fuel can be safely stored in caustic dosed ponds for at least 25 years and therefore the current plan is to extend water storage until around 2040, however how the fuel will be stored for the remaining 35 years is yet to be decided. One option that is being considered is the use of dry storage which is being used successfully in the USA for the storage of fuel from Light Water Reactors. One of the most important factors when utilising dry stores is an effective drying step and this PhD is aiming to look at this area in particular. Commercial drying methods have been developed for use with Zircaloy and aluminium clad fuels however this PhD intends to develop a method that can be used to dry Stainless Steel clad fuels such as those used in the UK's Advanced Gas Reactors (AGR). Since intact AGR fuel has yet to be examined following storage the first part if this thesis looked at preparing samples for later macro scale testing. Samples were treated to induce defects known to be of concern and analysed with the conclusion being that bound water is of no concern for drying operations and can be disregarded when preparing samples. Since AGR is known to have failed by stress corrosion cracking water trapped within microcracked pins is a likely issue. A section of tube was prepared by compression and boiling in magnesium chloride which micro CT imaging found to have images of a similar size to known failures. This tube was prepared into a test piece for later testing. The second part of the thesis looks at macro scale testing using the test piece described above and a similar test piece with a 300 um pinhole. A multipurpose drying rig capable of vacuum drying and flowed gas drying was constructed. In the first phase of drying tests vacuum drying and flowed gas drying were compared using a test piece with a 300 um pinhole and the impact of different cover gas was assessed. vacuum drying was found to be significantly more effective than flowed gas drying with the type of cover gas having little impact. Most importantly this work guided further improvements to the rig. The second phase of this work carried out more detailed drying tests on vacuum drying and flowed gas drying and utilised the pinholed and cracked test piece. The greatest influencing factor on the drying rate (the rate at which water could be removed from inside the test piece) was found to be the water level inside the test piece with broadly similar rates being found in all conditions and with both test piece when the test piece was full. As the water level within the test piece dropped, vacuum drying quickly became more effective. This was not helped by considering energy usage. There was however a feeling that flowed gas drying was limited due to the pipework size. In the final phase of testing the ability to detect the point which all water was removed (the end point) from the test piece using online instrumentation was assessed. Currently a vacuum rebound test is used which is both time consuming and if flowed gas drying is being used requires additional plant equipment. It was found that dew point measurements appeared to give a relatively clear indication of the end point when for both vacuum drying and flowed gas drying. For vacuum drying only the measurement of mass flow and pressure also gave a reasonable indication of end point."]},{"key":"dc:format","label":"Dc Format","values":["text"]},{"key":"dcterms:accessrights","label":"Dcterms Accessrights","values":["public"]},{"key":"dc:title","label":"Title","values":["Transitioning of Spent Advanced Gas Reactor Fuel from Wet to Dry Storage"]}]}],"canonical_facts":{"dc:contributor.advisor":["Hanson, Bruce C","Harbottle, David"],"dc:contributor.sponsor":["EPSRC"],"dc:creator":["Goode, James Bruce"],"dc:date":["2017-12"],"dc:date.issued":["2017-12"],"dc:description.abstract":["Upon removal from a reactor spent nuclear fuel is placed into water storage for a period of time since water provides both a decay heat sink and radiation shielding. In the UK this fuel has traditionally been reprocessed however the decision has been made that this will cease in 2018 in favour of an open fuel cycle and direct disposal to a degological disposal facility, although this is not expected to be available until 2075. Current experience with pond storage has found that fuel can be safely stored in caustic dosed ponds for at least 25 years and therefore the current plan is to extend water storage until around 2040, however how the fuel will be stored for the remaining 35 years is yet to be decided. One option that is being considered is the use of dry storage which is being used successfully in the USA for the storage of fuel from Light Water Reactors. One of the most important factors when utilising dry stores is an effective drying step and this PhD is aiming to look at this area in particular. Commercial drying methods have been developed for use with Zircaloy and aluminium clad fuels however this PhD intends to develop a method that can be used to dry Stainless Steel clad fuels such as those used in the UK's Advanced Gas Reactors (AGR). Since intact AGR fuel has yet to be examined following storage the first part if this thesis looked at preparing samples for later macro scale testing. Samples were treated to induce defects known to be of concern and analysed with the conclusion being that bound water is of no concern for drying operations and can be disregarded when preparing samples. Since AGR is known to have failed by stress corrosion cracking water trapped within microcracked pins is a likely issue. A section of tube was prepared by compression and boiling in magnesium chloride which micro CT imaging found to have images of a similar size to known failures. This tube was prepared into a test piece for later testing. The second part of the thesis looks at macro scale testing using the test piece described above and a similar test piece with a 300 um pinhole. A multipurpose drying rig capable of vacuum drying and flowed gas drying was constructed. In the first phase of drying tests vacuum drying and flowed gas drying were compared using a test piece with a 300 um pinhole and the impact of different cover gas was assessed. vacuum drying was found to be significantly more effective than flowed gas drying with the type of cover gas having little impact. Most importantly this work guided further improvements to the rig. The second phase of this work carried out more detailed drying tests on vacuum drying and flowed gas drying and utilised the pinholed and cracked test piece. The greatest influencing factor on the drying rate (the rate at which water could be removed from inside the test piece) was found to be the water level inside the test piece with broadly similar rates being found in all conditions and with both test piece when the test piece was full. As the water level within the test piece dropped, vacuum drying quickly became more effective. This was not helped by considering energy usage. There was however a feeling that flowed gas drying was limited due to the pipework size. In the final phase of testing the ability to detect the point which all water was removed (the end point) from the test piece using online instrumentation was assessed. Currently a vacuum rebound test is used which is both time consuming and if flowed gas drying is being used requires additional plant equipment. It was found that dew point measurements appeared to give a relatively clear indication of the end point when for both vacuum drying and flowed gas drying. For vacuum drying only the measurement of mass flow and pressure also gave a reasonable indication of end point."],"dc:format":["text"],"dc:identifier":["uk.bl.ethos.745516"],"dc:identifier.grantnumber":["EP/L014041/1"],"dc:identifier.uri":["https://etheses.whiterose.ac.uk/id/eprint/20585/2/AGR%20Fuel%20Drying-Coloured%20links.pdf"],"dc:language.dcterms_iso639_2":["eng"],"dc:publisher.commercial":["University of Leeds"],"dc:publisher.department":["School of Chemical and Process Engineering (Leeds)"],"dc:publisher.institution":["University of Leeds"],"dc:relation.isreferencedby":["https://etheses.whiterose.ac.uk/id/eprint/20585/"],"dc:relation.references":["[1] Nuclear Decommissioning Authority. Oxide Fuels - Preferred Option - Pub- lications - GOV.UK. Technical Report SMS/TS/C2-OF/001/Preferred Op- tion, June 2012. URL https://www.gov.uk/government/publications/ oxide-fuels-preferred-option. [2] R.L. Sindelar, Caskey Jr, G.R., Peacock Jr, H.B., and Lam, P.S. Evalua- tion of Degradation During Interim Dry Storage of Al SNF. In High level Radioactive Waste Management: Proceedings of the Sixth Annual Interna- tional Conference, Las Vegas, Nevada, May 1995. American Nuclear Society ; American Society of Civil Engineers. ISBN 0-7844-0082-2 978-0-7844-0082-1. [3] R. L. Sindelar, H. B. Peacock, P. S. Lam, N. C. Iyer, M. R. Louthan, and J. R. Murphy. Scientific Basis for Storage Criteria for Interim Dry Storage of Aluminum-clad Fuels. MRS Online Proceedings Library, 412:99{105, 1995. doi: 10.1557/PROC-412-99. [4] ASTM. Guide for Drying Behavior of Spent Nuclear Fuel. Technical Report C-1553, ASTM International, 2008. URL http://www.astm.org/ Standards/C1553.htm. [5] J.V. Best, W.J. Stephen, and A.J. Wickham. Radiolytic graphite oxida- tion. Progress in Nuclear Energy, 16(2):127{178, 1985. ISSN 0149-1970. doi: 10.1016/0149-1970(85)90002-2. URL http://www.sciencedirect. com/science/article/pii/0149197085900022. [6] Neale Brittain. EDF Energy - Nuclear Generation The AGR Design, Fukushima and More, February 2012. URL www-diva.eng.cam.ac.uk/ mphil-in-nuclear-energy/external-lectures/2011-12-lectures/ edf-energy-ng-cambridge-09022012.pdf/at_download/file. [7] J. Winton, M. M. Haberlin, D. Rhodes, R. B. Jones, J. S. Waddington, and A. C. Roberts. 7. The mechanical properties of AGR cladding. In Nuclear Fuel Performance, pages 7.1{7.5. Thomas Telford Publishing, January 1973. ISBN 978-0-7277-5160-7. URL http://www.icevirtuallibrary.com/doi/ full/10.1680/nfp.48977.0011. DOI: 10.1680/nfp.48977.0011. [8] John Kyffin. Technological Development to Support a Change in the United Kingdom's Strategy for Management of Spent AGR Oxide Fuel. In Pro- ceedings of the International Conference on Management of Spent Fuel from Nuclear Power Reactors, Vienna, June 2015. IAEA. [9] J.V. Best, A.J. Wickham, and C.J. Wood. Inhibition of Moderator Graphite Corrosion in CEGB Magnox Reactors 1. Laboratory measurements of the effect of coolant composition on the radiolytic Graphite/CO//2 Reaction. Journal of the British Nuclear Energy Society, 135(185):319{324, 1976. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0016983992& partnerID=40&md5=915c35fbb47bb51abf96e4726b4dc0fe. [10] J.V. Best, A.J. Wickham, and C.J. Wood. Inhibition of Mod- erator Graphite Corrosion in CEGB Magnox Reactors - 2. Hy- drogen Injections into Wylfa Reactor I Coolant Gas. Journal of the British Nuclear Energy Society, 135(185):325{331, 1976. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0016985985& partnerID=40&md5=f4aeea00cb2805b54d15a5cd33f4812b. [11] J.A. Cairns, J.P. Coad, E.W.T. Richards, and I.A. Stenhouse. Car- bon deposition on metallic surfaces studied by r.f. plasma discharge. Nature, 288(5792):686{687, 1980. URL http://www.scopus.com/ inward/record.url?eid=2-s2.0-0042260217&partnerID=40&md5= f4025f10064d6610aec7f2736563fc3b. [12] G.W. Horsley and J.A. Cairns. The inhibition of carbon deposition on stain- less steel by prior selective oxidation. Applied Surface Science, 18(3):273{ 286, 1984. URL http://www.scopus.com/inward/record.url?eid=2-s2. 0-0021468709&partnerID=40&md5=60bc28d98b47c716a564bb0f71611fb0. [13] M.L. Sykes, I.A.S. Edwards, and K.M. Thomas. Metal carbonyl decom- position and carbon deposition in the advanced gas-cooled nuclear reactor. Carbon, 31(3):467{472, 1993. ISSN 0008-6223. doi: 10.1016/0008-6223(93) 90135-W. URL http://www.sciencedirect.com/science/article/pii/ 000862239390135W. [14] Clive Mowforth. Suppression of Carbon Deposition in an AGR. In Con- ference on Chemistry in Nuclear Power Generation, Manchester, November 2014. [15] G.R. Millward, H.E. Evans, M. Aindow, and C.W. Mowforth. The influence of oxide layers on the initiation of carbon deposition on stainless steel. Oxidation of Metals, 56(3-4):231{250, 2001. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0013354192& partnerID=40&md5=14f7e80057f0ecd263b8f337c701c13c. [16] G.R. Millward, H.E. Evans, I.P. Jones, C.D. Eley, and C.W. Mowforth. The inuence of carbonyl sulphide on the inhibition of filamentary carbon deposi- tion on stainless steel. Materials and Corrosion, 54(11):864{869, 2003. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0344585500& partnerID=40&md5=609c82c48463f73743e82819b5ebd61f. [17] G.R. Millward, H.E. Evans, I.P. Jones, and C.D. Eley. Car- bon deposition on stainless steel in oxidising environments. Ma- terials at High Temperatures, 20(4):535{541, 2003. URL http: //www.scopus.com/inward/record.url?eid=2-s2.0-10844227558& partnerID=40&md5=34d871d3680f50df94784719a7d51797. [18] G.R. Millward, H.E. Evans, I.P. Jones, C.D. Eley, and K.A. Simpson. Burn-off of filamentous carbon and subsequent re- deposition on a 20cr25ni austenitic steel. Materials at High Tem- peratures, 26(1):57{61, 2009. URL http://www.scopus.com/ inward/record.url?eid=2-s2.0-72349086337&partnerID=40&md5= 10bc279a2d2654434c55872fad462ef6. [19] British Stainless Steel Association. What Is Stainless Steel? URL http: //www.bssa.org.uk/faq.php?id=1. [20] Oliver Kuhn. Science Break : Steel. Recorder-The Official Journal of Canadian Exploarion Geopyhsicists, 38(08), October 2013. URL http: //csegrecorder.com/features/view/science-break-201310. [21] Magmaweld. Stainless Steel Welding. URL http://www.magmaweld.com/ stainless_steel_welding.html. [22] Zhiliang Cao and Henry Gu Cao. Cubic Atom and Crystal Structures. International Journal of Physics, International Journal of Physics, 2(6): 277{281, January 2014. ISSN 2333-4878. doi: 10.12691/ijp-2-6-11. URL http://pubs.sciepub.com/ijp/2/6/11/abstract.html. [23] James Gordon Parr and Albert Hanson. An introduction to stainless steel. American Society for Metals, 1965. [24] Donald Peckner and I. M. Bernstein, editors. Handbook of stainless steels. McGraw-Hill, New York, 1977. ISBN 978-0-07-049147-2. [25] L. Hochmann and J. Colombier. Stainless and Heat Resisting Steels. Edward Arnold, second edition edition edition, 1967. [26] W. A. England, M. J. Bennett, D. A. Greenhalgh, S. N. Jenny, and C. F. Knights. The characterization by raman spectroscopy of oxide scales formed on a 20crn25ninNb stabilized stainless steel. Corrosion Sci- ence, 26(7):537{545, 1986. ISSN 0010-938X. doi: 10.1016/0010-938X(86) 90021-1. URL http://www.sciencedirect.com/science/article/pii/ 0010938X86900211. [27] J. Y. Jeng, B. E. Quayle, P. J. Modern, W. M. Steen, and B. D. Bastow. Laser surface treatments to improve the intergranular corrosion resistance of 18/13/Nb and 304l in nitric acid. Corrosion Science, 35(5):1289{1296, 1993. ISSN 0010-938X. doi: 10.1016/0010-938X(93)90350-P. URL http://www. sciencedirect.com/science/article/pii/0010938X9390350P. [28] M. F. Montemor, M. G. S. Ferreira, N. E. Hakiki, and M. Da Cunha Belo. Chemical composition and electronic structure of the oxide films formed on 316l stainless steel and nickel based alloys in high temperature aque- ous environments. Corrosion Science, 42(9):1635{1650, September 2000. ISSN 0010-938X. doi: 10.1016/S0010-938X(00)00012-3. URL http://www. sciencedirect.com/science/article/pii/S0010938X00000123. [29] S. S. M. Tavares, V. Moura, V. C. da Costa, M. L. R. Ferreira, and J. M. Pardal. Microstructural changes and corrosion resistance of AISI 310s steel exposed to 600-800 C. Materials Characterization, 60(6):573578, June 2009. ISSN 1044-5803. doi: 10.1016/j.matchar.2008.12.005. URL http://www. sciencedirect.com/science/article/pii/S1044580308003422. [30] Abdulla Al-Shater, Dirk Engelberg, Stuart Lyon, Cornelius Donohoe, Steve Walters, Guy Whillock, and Andrew Sherry. Characterization of the stress corrosion cracking behavior of thermally sensitized 20cr-25ni stainless steel in a simulated cooling pond environment. Journal of Nuclear Science and Tech- nology, 0(0):1{10, April 2017. ISSN 0022-3131. doi: 10.1080/00223131.2017. 1309305. URL http://dx.doi.org/10.1080/00223131.2017.1309305. [31] C. Tyzack and H.C. Cowen. The corrosion of reactor materials in carbon dioxide. Atomic Energy Review, 14(2):263{324, 1976. URL http://www.scopus.com/inward/record.url?eid=2-s2.0-0016963965& partnerID=40&md5=c3c8ed5610ba613cee9abf20b181440c. [32] J. M. Francis. Structure of Surface Oxides Formed on A 20% Cr/25% Ni/Nb-Stabilised Steel in Carbon Dioxide at High Temperatures. British Corrosion Journal, 3(3):113{119, May 1968. ISSN 0007-0599. doi: 10. 1179/000705968798326244. URL http://www.maneyonline.com/doi/abs/ 10.1179/000705968798326244. [33] J. A. Desport and M. J. Bennett. Investigation by fractography of the high- temperature oxidation of the 20%Cr-25%Ni-Nb stainless steel. Oxidation of Metals, 29(3-4):327{346, April 1988. ISSN 0030-770X, 1573-4889. doi: 10. 1007/BF00751803. URL http://link.springer.com/article/10.1007/ BF00751803. [34] M.J. Bennett, P.C. Blythe, G.H. Chaffey, K. Hand, J.W. McMillan, S.J. Webster, and J.E. Antill. The effect of fission neutron irradiation upon the oxidation of a 20 wt % Cr/25 wt % Ni/Nb stabilised stainless steel by carbon dioxide beween 580 and 840C. Journal of Nuclear Materials, 25(3):260{270, March 1968. ISSN 0022-3115. doi: 10.1016/0022-3115(68) 90169-4. URL http://www.sciencedirect.com/science/article/pii/ 0022311568901694. [35] M.J. Bennett, G.H. Chaffey, and J.E. Antill. Some aspects of the effects of fission fragment irradiation upon the oxidation of austenitic stainless steels by oxygen at 650C and 800C. Journal of Nuclear Materials, 32(2): 299{309, September 1969. ISSN 0022-3115. doi: 10.1016/0022-3115(69) 90079-8. URL http://www.sciencedirect.com/science/article/pii/ 0022311569900798. [36] William D. Callister. Materials science and engineering: an introduction. Wiley international edition. Wiley, New York, NY, 6th international edition, 2003. ISBN 0-471-22471-5 0-471-22471-5 0-555-00205-5 0-471-26456-3. [37] S. M Bruemmer, E. P Simonen, P. M Scott, P. L Andresen, G. S Was, and J. L Nelson. Radiation-induced material changes and susceptibility to intergranular failure of light-water-reactor core internals. Journal of Nuclear Materials, 274(3):299{314, September 1999. ISSN 0022-3115. doi: 10.1016/ S0022-3115(99)00075-6. URL http://www.sciencedirect.com/science/ article/pii/S0022311599000756. [38] E. A. Little. Development of radiation resistant materials for advanced nuclear power plant. Materials Science and Technol- ogy, 22(5):491{518, May 2006. ISSN 0267-0836. doi: 10.1179/ 174328406X90998. URL http://0-www.maneyonline.com.wam.leeds.ac. uk/doi/abs/10.1179/174328406X90998. [39] C Taylor. The formation of sensitised microstructures during the irra- diation of CAGR fuel pin cladding. In Symposium on the Radiation- induced Sensitisation of Stainless Steels;, Berkeley, UK, September 1986. URL https://inis.iaea.org/search/searchsinglerecord.aspx? recordsFor=SingleRecord&RN=18098354. [40] John Kyffin. The technical case for interim Storage of AGR fuel and devel- opment of a programme of further work. Manchester, April 2014. IChemE. [41] Kenneth R. Trethewey and John Chamberlain. Corrosion for science and engineering. Longman, Harlow, 2. ed., reprint edition, 1998. ISBN 0-582- 23869-2 0-582-23869-2. [42] A. V. Byalobzheskii. Radiation Corrosion. I.P.S.T., May 1970. ISBN 978-0- 7065-1013-3. [43] Robert S. Glass, George E. Overturf, Richard A. Van Konynenburg, and R. Daniel McCright. Gamma radiation effects on corrosion-I. Electro- chemical mechanisms for the aqueous corrosion processes of austenitic stainless steels relevant to nuclear waste disposal in tuff. Corrosion Sci- ence, 26(8):577{590, 1986. ISSN 0010-938X. doi: 10.1016/0010-938X(86) 90025-9. URL http://www.sciencedirect.com/science/article/pii/ 0010938X86900259. [44] W. G. Burns, W. R. Marsh, and W. S. Walters. The gamma irradiation- enhanced corrosion of stainless and mild steels by water in the pres- ence of air, argon and hydrogen. Radiation Physics and Chemistry (1977), 21(3):259{279, 1983. ISSN 0146-5724. doi: 10.1016/0146-5724(83) 90155-3. URL http://www.sciencedirect.com/science/article/pii/ 0146572483901553. [45] R. L. Sindelar, P. S. Lam, M. R. Louthan Jr., and N. C. Iyer. Corrosion of Metals and Alloys in High Radiation Fields. Materials Characterization, 43 (2-3):147{157, August 1999. ISSN 1044-5803. doi: 10.1016/S1044-5803(99) 00042-X. URL http://www.sciencedirect.com/science/article/pii/ S104458039900042X. [46] R. J. Guenther, A. B. Johnson Jr, A. L. Lund, and E. R. Gilbert. Initial Evaluation of Dry Storage Issues for Spent Nuclear Fuels in Wet Storage at the Idaho Chemical Processing Plant. Technical Report INEL{96/0140, Idaho National Engineering Lab., Idaho Falls, ID (United States), November 1994. URL http://www.osti.gov/scitech/biblio/285498. [47] R. Winston Revie, Herbert Henry Uhlig, and Herbert Henry Uhlig, editors. Uhlig's Corrosion Handbook. Electrochemical Society series. Wiley, New York, 2nd ed edition, 2000. ISBN 978-0-471-15777-9. [48] R. Priya, S. Ningshen, and U. Kamachi Mudali. In uence of Oxidizing Ion Concentration on the Corrosion Resistance of Type 304l Stainless Steel in Nitric Acid Medium. Corrosion, 69(4):335{344, April 2013. ISSN 0010-9312. doi: 10.5006/703. URL http://0-corrosionjournal.org.wam.leeds.ac. uk/doi/full/10.5006/703. [49] C. L. Briant. The Effects of Sulfur and Phosphorus on the In- tergranular Corrosion of 304 Stainless Steel. Corrosion, 36(9):497{ 509, September 1980. ISSN 0010-9312. doi: 10.5006/0010-9312-36.9. 497. URL http://0-corrosionjournal.org.wam.leeds.ac.uk/doi/abs/ 10.5006/0010-9312-36.9.497. [50] O. V. Kasparova. The effect of boron and carbon on the structure and corrosion-electrochemical behavior of Kh20n20 austenitic stainless steel. Protection of Metals and Physical Chemistry of Surfaces, 49(6): 734{739, November 2013. ISSN 2070-2051, 2070-206X. doi: 10.1134/ S2070205113060063. URL http://link.springer.com/article/10.1134/ S2070205113060063. [51] M. Mayuzumi, J. Ohta, and T. Arai. Efffects of Cold Work, Sensitization Treatment, and the Combination on Corrosion Behavior of Stainless Steels in Nitric Acid. Corrosion, 54(4):271{280, April 1998. ISSN 0010-9312. doi: 10. 5006/1.3284853. URL http://0-corrosionjournal.org.wam.leeds.ac. uk/doi/abs/10.5006/1.3284853. [52] ASTM International. Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels. Technical report, ASTM International, 2014. URL http://www.astm.org/Standards/A262.htm. [53] T. M. Devine, C. L. Briant, and B. J. Drummond. Mechanism of intergran- ular corrosion of 316l stainless steel in oxidizing acids. Scripta Metallur- gica, 14(11):1175{1179, November 1980. ISSN 0036-9748. doi: 10.1016/ 0036-9748(80)90251-3. URL http://www.sciencedirect.com/science/ article/pii/0036974880902513. [54] G. H. Aydogdu and M. K. Aydinol. Determination of susceptibility to in- tergranular corrosion and electrochemical reactivation behaviour of AISI 316l type stainless steel. Corrosion Science, 48(11):3565{3583, November 2006. ISSN 0010-938X. doi: 10.1016/j.corsci.2006.01.003. URL http: //www.sciencedirect.com/science/article/pii/S0010938X06000308. [55] Wenjie Bai, Mengyu Chai, Lichan Li, and Quan Duan. Comparative Study of Acoustic Emission Characteristics for Intergranular Corrosion of 316l Stain- less Steel Parent Material and Weldment. In ASME 2014 Pressure Vessels and Piping Conference Volume 5: High-Pressure Technology; ASME NDE Division; 22nd Scavuzzo Student Paper Symposium and Competition, Ana- heim, California, USA, July 2014. The American Society of Mechanical Engi- neers. URL http://0-proceedings.asmedigitalcollection.asme.org. wam.leeds.ac.uk/proceeding.aspx?articleid=1938090. [56] P. Fauvet, F. Balbaud, R. Robin, Q. T. Tran, A. Mugnier, and D. Espinoux. Corrosion mechanisms of austenitic stainless steels in nitric media used in reprocessing plants. Journal of Nuclear Materials, 375(1):52{64, March 2008. ISSN 0022-3115. doi: 10.1016/j.jnucmat.2007.10.017. URL http://www. sciencedirect.com/science/article/pii/S002231150701046X. [57] Fanny Balbaud, Gerard Sanchez, Gerard Santarini, and Gerard Pi- card. Cathodic Reactions Involved in Corrosion Processes Occur-ing in Concentrated Nitric Acid at 100C. European Journal of Inorganic Chemistry, 2000(4):665{674, 2000. ISSN 1099-0682. doi: 10.1002/(SICI)1099-0682(200004)2000:4h665::AID-EJIC665i3.0.CO;2-N. URL http://onlinelibrary.wiley.com/doi/10.1002/(SICI) 1099-0682(200004)2000:4<665::AID-EJIC665>3.0.CO;2-N/abstract. [58] K. Fukuya, S. Shima, H. Kayano, and M. Narui. Stress corrosion cracking and intergranular corrosion of neutron irradiated austenitic stainless steels. Journal of Nuclear Materials, 191-194, Part B:1007{1011, September 1992. ISSN 0022-3115. doi: 10.1016/0022-3115(92)90626-V. URL http://www. sciencedirect.com/science/article/pii/002231159290626V. [59] NACE International. Stress Corrosion Cracking (SCC). URL https://www.nace.org/Corrosion-Central/Corrosion-101/ Stress-Corrosion-Cracking-(SCC)/. [60] Philippe Marcus. Corrosion Mechanisms in Theory and Practice. CRC Press, July 2002. ISBN 978-0-203-90918-8. Google-Books-ID: 69bImhlRCdcC. [61] ASTM International. ASTM G38 - 01(2013) Standard Practice for Making and Using C-Ring Stress-Corrosion Test Specimens. Technical report, 2007. URL https://www.astm.org/Standards/G38.htm. [62] ASTM International. ASTM G36 - 94(2013) Standard Practice for Evalu- ating Stress-Corrosion-Cracking Resistance of Metals and Alloys in a Boil- ing Magnesium Chloride Solution. Technical report, 2007. URL https: //www.astm.org/Standards/G36.htm. [63] Heinz Kohl. A Contribution to the Examination of Stress Corrosion Crack- ing of Austenitic Stainless Steels in Magnesium Chloride Solutions. COR- ROSION, 23(2):39{49, February 1967. ISSN 0010-9312. doi: 10.5006/ 0010-9312-23.2.39. URL http://www.corrosionjournal.org/doi/abs/ 10.5006/0010-9312-23.2.39. [64] Osama M. Alyousif and Rokuro Nishimura. The stress corrosion cracking behavior of austenitic stainless steels in boiling magnesium chloride solu- tions. Corrosion Science, 49(7):3040{3051, July 2007. ISSN 0010-938X. doi: 10.1016/j.corsci.2006.12.023. URL http://www.sciencedirect.com/ science/article/pii/S0010938X07000248. [65] Osama M. Alyousif and Rokuro Nishimura. The effect of test tempera- ture on SCC behavior of austenitic stainless steels in boiling saturated mag- nesium chloride solution. Corrosion Science, 48(12):4283{4293, December 2006. ISSN 0010-938X. doi: 10.1016/j.corsci.2006.01.014. URL http: //www.sciencedirect.com/science/article/pii/S0010938X06000643. [66] C. Garcia, F. Martin, P. De Tiedra, J. A. Heredero, and M. L. Aparicio. Effects of prior cold work and sensitization heat treatment on chloride stress corrosion cracking in type 304 stainless steels. Corrosion science, 43(8): 1519{1539, 2001. ISSN 0010-938X. URL http://cat.inist.fr/?aModele= afficheN&cpsidt=14117343. [67] David Hambley. Technical Basis for Extending Storage of AGR Fuel. Salt Lake City, September 2013. URL https://www.researchgate.net/ profile/David_Hambley/publication/279058579_Technical_Basis_ for_Extending_Storage_of_the_UK's_Advanced_Gas-Cooled_Reactor_ Fuel/links/5589322308aed6bff80b421d.pdf. [68] Craig W. Jones. Environmental Application of Hydrogen Peroxide. In Applications of Hydrogen Peroxide and Derivatives, pages 213{217. Royal Society of Chemistry, Cambridge, 1999. ISBN 978-0-85404-536-5. Google-Books-ID: QLePlhTsE0oC. [69] Mark C. Biesinger, Brad P. Payne, Andrew P. Grosvenor, Leo W. M. Lau, Andrea R. Gerson, and Roger St. C. Smart. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni. Applied Surface Science, 257(7):2717{2730, January 2011. ISSN 0169-4332. doi: 10.1016/j.apsusc.2010.10.051. URL http:// www.sciencedirect.com/science/article/pii/S0169433210014170. [70] Thermo Scientific. XPS Interpretation of Calcium. URL https:// xpssimplified.com/elements/calcium.php. [71] P. Stefanov, D. Stoychev, M. Stoycheva, A. R. Gonzalez-Elipe, and Ts. Marinova. XPS, SEM and TEM characterization of stainless- steel 316l surfaces after electrochemical etching and oxidizing. Surface and Interface Analysis, 28(1):106{110, August 1999. ISSN 1096- 9918. doi: 10.1002/(SICI)1096-9918(199908)28:1h106::AID-SIA628i3.0. CO;2-J. URL http://onlinelibrary.wiley.com/doi/10.1002/(SICI) 1096-9918(199908)28:1<106::AID-SIA628>3.0.CO;2-J/abstract. [72] S. Jin and A. Atrens. ESCA-studies of the structure and composition of the passive film formed on stainless steels by various immersion times in 0.1 M NaCl solution. Applied Physics A, 42(2):149{165, January 1987. ISSN 0947- 8396, 1432-0630. doi: 10.1007/BF00616726. URL http://link.springer. com/article/10.1007/BF00616726. [73] P Stefanov, D Stoychev, M Stoycheva, and Ts Marinova. XPS and SEM studies of chromium oxide films chemically formed on stainless steel 316 L. Materials Chemistry and Physics, 65(2):212{215, July 2000. ISSN 0254-0584. doi: 10.1016/S0254-0584(00)00249-2. URL http://www.sciencedirect. com/science/article/pii/S0254058400002492. [74] V. Maurice, W. P. Yang, and P. Marcus. XPS and STM Study of Passive Films Formed on Fe-22cr(110) Single-Crystal Surfaces. Journal of The Elec- trochemical Society, 143(4):1182{1200, April 1996. ISSN 0013-4651, 1945- 7111. doi: 10.1149/1.1836616. URL http://0-jes.ecsdl.org.wam.leeds. ac.uk/content/143/4/1182. [75] R. Li, M. G. S. Ferreira, M. A. Anjos, and R. Vilar. Localized corrosion of laser surface cladded UNS S31254 superaustenitic stainless steel on mild steel. Surface and Coatings Technology, 88(1-3):90{95, January 1997. ISSN 0257-8972. doi: 10.1016/S0257-8972(96)02865-4. URL http://www. sciencedirect.com/science/article/pii/S0257897296028654. [76] M. A. Ashworth, D. I. R. Norris, and I. P. Jones. Radiation-induced segregation in Fe-20cr-25ni-Nb based austenitic stainless steels. Journal of Nuclear Materials, 189(3):289{302, August 1992. ISSN 0022-3115. doi: 10.1016/0022-3115(92)90383-V. URL http://www.sciencedirect.com/ science/article/pii/002231159290383V. [77] Jiang Hsieh. Computed Tomography: Principles, Design, Artifacts, and Recent Advances. SPIE PRESS, 2015. ISBN 978-1-62841-825- 5. URL http://ebooks.spiedigitallibrary.org/book.aspx?doi=10. 1117/3.2197756. DOI: 10.1117/3.2197756. [78] D. A. Horner, B. J. Connolly, S. Zhou, L. Crocker, and A. Turnbull. Novel images of the evolution of stress corrosion cracks from corrosion pits. Corrosion Science, 53(11):3466{3485, November 2011. ISSN 0010-938X. doi: 10.1016/j.corsci.2011.05.050. URL http://www.sciencedirect.com/ science/article/pii/S0010938X11002721. [79] L. Babout, T. J. Marrow, D. Engelberg, and P. J. Withers. X-ray microtomographic observation of intergranular stress corrosion cracking in sensitised austenitic stainless steel. Materials Science and Technology, 22(9):1068{ 1075, September 2006. ISSN 0267-0836. doi: 10.1179/174328406X114090. URL https://doi.org/10.1179/174328406X114090. [80] A. King, G. Johnson, D. Engelberg, W. Ludwig, and J. Marrow. Observations of Intergranular Stress Corrosion Cracking in a Grain-Mapped Polycrystal. Science, 321(5887):382{385, July 2008. ISSN 0036-8075, 1095- 9203. doi: 10.1126/science.1156211. URL http://science.sciencemag. org/content/321/5887/382. [81] W. Stephen Walters, Peter Durham, and Nicholas A. Hodge. The adsorption and desorption of water from a carbonaceous deposit layer on the surface of stainless steel representing spent AGR nuclear fuel cladding. Journal of Nuclear Science and Technology, 0(0):1{12, December 2017. ISSN 0022- 3131. doi: 10.1080/00223131.2017.1403384. URL https://doi.org/10. 1080/00223131.2017.1403384. [82] Yunus A. Cengel and Michael A. Boles. 2.1 Pure Substance. In Thermo- dynamics: an engineering approach, page 48. McGraw Hill, Boston, 3rd ed edition, 1998. ISBN 978-0-07-011927-7. [83] The Engineering Toolbox. Water Saturation Pressure. URL http://www. engineeringtoolbox.com/water-vapor-saturation-pressure-d_599. html. [84] Yunus A. Cengel and Michael A. Boles. 2.3 Phase-change Processes of Pure Substances. In Thermodynamics: an engineering approach, pages 49{55. McGraw Hill, Boston, 3rd ed edition, 1998. ISBN 978-0-07-011927-7. [85] Yunus A. Cengel and Michael A. Boles. 2.4 Property Diagrams for Phase- change Processes. In Thermodynamics: an engineering approach, pages 55{ 62. McGraw Hill, Boston, 3rd ed edition, 1998. ISBN 978-0-07-011927-7. [86] J.M.Sullivan Jr. ES 3001 Thermodynamics. URL http://users.wpi.edu/ ~sullivan/ES3001/Lectures/Lecture-A/Lecture-2-2011.htm. [87] Wikipedia, The Online Encyclopedia. Phase diagram. Novem- ber 2015. URL https://en.wikipedia.org/w/index.php?title=Phase_ diagram&oldid=692814655. Page Version ID: 692814655. [88] Yunus A. Cengel and Michael A. Boles. 2.5 Vapour Pressure and Phase Equlibrium. In Thermodynamics: an engineering approach, pages 62{66. McGraw Hill, Boston, 3rd ed edition, 1998. ISBN 978-0-07-011927-7. 127, [89] Robert J. Hunter. Thermodynamics of Surfaces. In Foundations of colloid science, pages 87{93. Oxford University Press, Oxford ; New York, 2nd ed edition, 2001. ISBN 978-0-19-850502-0. [90] Felix Casanova, Casey E Chiang, Chang-Peng Li, Igor V Roshchin, Anne M Ruminski, Michael J Sailor, and Ivan K Schuller. Gas adsorption and capillary condensation in nanoporous alumina films. Nanotechnology, 19(31): 315709, 2008. ISSN 0957-4484. URL http://stacks.iop.org/0957-4484/ 19/i=31/a=315709. [91] Yunus A Cengel. 1-3 Heat Transfer. In Introduction to thermodynamics and heat transfer, pages 5{6. McGraw-Hill, Dubuque, IA, 2008. ISBN 978-0-07- 128773-9. [92] 1.1 What and How. In Frank P. Incropera, David P. DeWitt, Theodore L. Bergman, and Adrienne S. Lavine, editors, Principles of heat and mass trans- fer, pages 3{5. Wiley, Singapore, 7. ed., international student version edition, 2013. ISBN 978-0-470-64615-1 978-0-470-50197-9. [93] Yunus A Cengel. 9-2 Conduction. In Introduction to thermodynamics and heat transfer, pages 374{381. McGraw-Hill, Dubuque, IA, 2008. ISBN 978- 0-07-128773-9. [94] J. P. Holman. 1-2 Thermal Conductivity. In Heat transfer, McGraw-Hill series in mechanical engineering, pages 5{9. McGraw-Hill, New York, 9th ed edition, 2002. ISBN 978-0-07-240655-9 978-0-07-112230-6. [95] Thermal Conductivity of common Materials and Gases. URL https://www. engineeringtoolbox.com/thermal-conductivity-d_429.html. [96] Yunus A Cengel. 9-3 Convection. In Introduction to thermodynamics and heat transfer, pages 382{383. McGraw-Hill, Dubuque, IA, 2008. ISBN 978- 0-07-128773-9. [97] J. P. Holman. 1-3 Convection Heat Transfer. In Heat transfer, McGraw-Hill series in mechanical engineering, pages 9{12. McGraw-Hill, New York, 9th ed edition, 2002. ISBN 978-0-07-240655-9 978-0-07-112230-6. [98] 1.2.2 Convection. In Frank P. Incropera, David P. DeWitt, Theodore L.Bergman, and Adrienne S. Lavine, editors, Principles of heat and mass transfer, pages 6{8. Wiley, Singapore, 7. ed., international student version edition, 2013. ISBN 978-0-470-64615-1 978-0-470-50197-9. [99] 14.1 Physical Origins and Rate Equations [Diffusion Mass Transfer]. In Frank P. Incropera, David P. DeWitt, Theodore L. Bergman, and Adri- enne . Lavine, editors, Principles of heat and mass transfer, pages 934{939. Wiley, Singapore, 7. ed., international student version edition, 2013. ISBN 978-0-470-64615-1 978-0-470-50197-9. [100] Jaime Benitez. 1.2 Molecular Mass Transfer. In Principles and modern applications of mass transfer operations, pages 3{15. Wiley-Interscience, New York, 2002. ISBN 978-0-471-20344-5. [101] A. H. P. Skelland. 2 Molecular Diffusion. In Diffusional Mass Transfer,pages 6{48. John Wiley & Sons Inc, New York, 1st edition edition edition, April 1974. ISBN 978-0-471-79374-8. [102] Jaime Benitez. 1.3 The Diffusion Coefficient. In Principles and modern applications of mass transfer operations, pages 15{34. Wiley-Interscience, New York, 2002. ISBN 978-0-471-20344-5 [103] E. L. Cussler. 5.1 Diffusion Coefficients in Gas. In Diffusion: mass transfer in fluid systems, pages 101{111. Cambridge University Press, New York, 2nd ed edition, 1997. ISBN 978-0-521-45078-2 978-0-521-56477-9. [104] E. L. Cussler. 6.5-Solute Boundary Interactions. In Diffusion: mass transfer in fluid systems. Cambridge University Press, New York, 2nd ed edition, 1997. ISBN 978-0-521-45078-2 978-0-521-56477-9. [105] Diffusion of Fluids in Porous Solids. In Robert H. Perry and Don W. Green, editors, Perry's chemical engineers' handbook, pages 5.48{5.49. McGraw-Hill, New York, 8th ed edition, 2008. ISBN 978-0-07-142294-9. [106] NRC: Glossary { Crud. URL http://www.nrc.gov/reading-rm/ basic-ref/glossary/crud.html. [107] W. S. Large. Review of Drying Methods for Spent Nuclear Fuel. Technical Report WSRC-TR-97-0075, Savannah River Site (US), Aiken, SC 29808, October 1999. URL http://www.osti.gov/scitech/biblio/14490. [108] G. E. Culley. Hanford's Progress Toward Dry Interim Storage of K Basin`s Spent Fuel. Technical Report WHC-SA{3107-FP; CONF-960804{, West- inghouse Hanford Co., Richland, WA (United States), May 1996. URL http://www.osti.gov/scitech/biblio/330736. [109] A. L. Pajunen. Cold Vacuum Drying Residual Free Water Test Descrip tion. Technical Report HNF{1851, Fluor Daniel Hanford Inc., Richland, WA (United States), December 1997. URL http://www.osti.gov/scitech/ biblio/10148296. [110] P. G. Loscoe. Transitioning Metallic Uranium Spent Nuclear Fuel from Wet to Dry Storage. In WM 2000 Proceedings, Tucson, Az, March 2000. URL https://www.wmsym.org/archives/2000/pdf/54/54-9.pdf. [111] L Rodrigo, L Therrien, and B. Surette. Low-Temperature, Vacuum-Assisted Drying of Degraded Spent Nuclear Fuel. In Waste Management, Decommissioning and Environmental Restoration for Canada's Nuclear Activities Current Practices and Future Needs. Canadian Nuclear Society, Toronto, 2005. ISBN 978-0-919784-81-9. [112] W.C.H Kupferschmidt and M.E. Stephens. AECL's Waste Management and Decommissioning Program. page 685. Australian Nuclear Association, 2006. [113] DS Cox, IB Bainbridge, and KR Greeneld. Management of Legacy Spent Nuclear Fuel Wastes at the Chalk River Laboratories: Operating Experi- ence and Progress Towards Waste Remediation. In Proceedings of WM'05 Conference, Tucson, Az, March 2005. [114] J.C. Crepeau, S. Reese, H.M. Mcllroy Jr., and R.E. Lords. Drying of Mock Spent Nuclear Fuel Elements. Drying Technology, 16(3-5):545{560, 1998.ISSN 07373937. [115] R. E. Lords, W. E. Windes, J. C. Crepeau, and R. W. Sidwell. Drying Studies of Simulated Doe Aluminum Plate Fuels. Technical Report INEL{95/00437; CONF-9606116{44, Idaho National Engineering Lab., Idaho Falls,ID (United States), May 1996. URL http://www.osti.gov/scitech/ biblio/236247. [116] R. E. Lords, W. E. Windes, J. C. Crepeau, and R. W. Sidwell. Drying Studies for Corroded Doe Aluminum Plate Fuels. Technical Report INEL{96/00134; CONF-960804{29, Idaho National Engineering Lab., Idaho Falls, ID (United States), May 1996. URL http://www.osti.gov/scitech/biblio/260992. [117] D. Caramelle, A. Bastianelli, F. Boussard, A. Milesi, G. Polydor, and G. Christin. CEA Spent Fuel: Reprocessing and Storage Management. In Proceedings of WM'97, Tucson, Az, March 1997. URL http://www.wmsym. org/archives/1997/sess12/12-04.htm. [118] P Michaille. Retrieval of Degraded Irradiated Fuel and Conditioning for a Safe Storage: the CEA Experience, October 2003. URL http://www.iaea.org/OurWork/ST/NE/NEFW/CEG/documents/ws102003_michaille3-e.pdf. [119] Krishna Pal Singh. Forced gas ow canister dehydration, June 2004. URL http://www.google.com/patents/EP1429344A2. International Classification G21C17/06, G21F5/14, G21C19/32, G21F5/00, G21F5/06, G21F9/36, F26B3/00, G21C19/06; Cooperative Classification G21F5/06, G21Y2004/40, G21Y2002/207, G21F9/34, G21Y2002/501, G21Y2002/201, G21Y2002/202; European Classification G21F5/06, G21F9/34. [120] J Morris, S Wickham, P Richardson, C Rhodes, and M Newland. Con- tingency Options for the Dry Storage of Magnox Spent Fuel in the UK. In Proceedings of the 12th International Conference on Radioactive Waste Management and Environmental Remediation, ICEM, volume 1, pages 817{ 823, Liverpool, October 2009. ISBN 978-0-7918-4407-6. doi: 10.1115/ ICEM2009-16331. [121] R. Sindelar, D. Vinson, N. Iyer, and D. Fisher. Overview of Crite- ria for Interim Wet and Dry Storage of Research Reactor Spent Nuclear Fuel. Technical report, SRS, 2010. URL http://sti.srs.gov/fulltext/ SRNL-STI-2010-00688.pdf. [122] Rick Springman. Forced Gas Dehydration (FGD) System for Drying Nuclear Fuel andWaste Packages. 17th Packaging and Transportation of Radioactive Materials Symposium (PATRAM 13). San Francisco, August 2013. [123] Engineering Toolbox. Specific Heat and Individual Gas Con- stant of Gases. URL http://www.engineeringtoolbox.com/ specific-heat-capacity-gases-d_159.html."],"dcterms:accessrights":["public"],"dc:title":["Transitioning of Spent Advanced Gas Reactor Fuel from Wet to Dry Storage"],"dc:type":["Thesis"],"dc:type.qualificationlevel":["doctoral"],"dc:type.qualificationname":["Ph.D"],"person:identifier.orcid":["0000000249007153"]},"updated_at":"2026-11-18T22:27:18Z"}