1 |
Measurement of the arc force in GTA weldingBurleigh, Thomas David January 1980 (has links)
Thesis (M.S.)--Massachusetts Institute of Technology, Dept. of Materials Science and Engineering, 1980. / MICROFICHE COPY AVAILABLE IN ARCHIVES AND SCIENCE. / Vita. / Includes bibliographical references. / by Thomas David Burleigh. / M.S.
|
2 |
Welding and weld repair of nanostructured and amorphous materialsCadney, Sean. January 2007 (has links)
In recent years, nanostructured and amorphous metals have become more prominent in scientific research. Their unique characteristics and their vastly superior mechanical properties have lead to emerging technical applications however the use of these materials is only in its infancy. To further growth the industrial applications for these advanced materials, joining processes capable of maintaining the unique aspects of the microstructure are required. / Joining of two beveled plates has been accomplished by use of the Cold Spray process. This process uses a converging diverging nozzle to accelerate micron sized powder towards a substrate. The strength of the resulting joint has been compared to freeforms made of powder of the same composition. No significant difference was observed in the mechanical properties between the freeforms and the weldments and examination of the fracture surface showed that the strength of the interface is higher than the strength of the freeform itself. / A weld repair experiment has also been performed where the ElectroSpark Deposition process (ESD) has successfully been used to transfer amorphous material from an electrode to an amorphous substrate without crystallizing either material. This result is of crucial importance as it signifies that these extremely expensive and heat sensitive materials can be repaired when in-service wear causes damage. This process, due to its inherently fast cooling rate, has also successfully been used to transform a crystalline AlCoCe alloy into an amorphous deposit atop both amorphous and crystalline substrates.
|
3 |
Welding and weld repair of nanostructured and amorphous materialsCadney, Sean. January 2007 (has links)
No description available.
|
4 |
Principles for open-arc weld deposition of high-chromium white iron surface layers / John Anthony Francis.Francis, John A. January 1999 (has links)
Bibliography: leaves 191-198. / xxi, 201 leaves : ill. ; 30 cm. / Title page, contents and abstract only. The complete thesis in print form is available from the University Library. / Examines the mechanisms controlling the dilution, geometry and wear performance of weld- deposited high-chromium white iron surface layers. Focuses on layers deposited by mechanised flux-cored-arc welding, as this process achieves higher deposition rates than manual-metal-arc welding and affords a greater degree of control over individual welding variables. / Thesis (Ph.D.)--University of Adelaide, Dept. of Mechanical Engineering, 1999
|