Spelling suggestions: "subject:"lil agglomeration"" "subject:"lil gglomeration""
1 |
A study of surface and liberation characteristics in coal beneficiation by oil agglomerationTampy, Geatesh January 1988 (has links)
No description available.
|
2 |
Evaluation of the response of some Ohio coals to oil agglomerationTampy, Geatesh January 1983 (has links)
No description available.
|
3 |
Advancement of the Hydrophobic-Hydrophilic Separation ProcessJones, Alan Wayne III 19 April 2019 (has links)
Froth flotation has long been regarded as the best available technology for ultrafine particles separation. However, froth flotation has extreme deficiencies for recovering ultrafine particles that are less than 30-50 μm in size for coal and 10-20 μm for minerals. Furthermore, dewatering of flotation products is difficult and costly using currently available technologies. Due to these problems, coal and mineral fines are either lost to tailings streams inadvertently or discarded purposely prior to flotation. In light of this, researchers at Virginia Tech have developed a process called hydrophobic-hydrophilic separation (HHS), which is based originally on a concept known as dewatering by displacement (DbD). The process uses non-polar solvents (usually short-chain alkanes) to selectively displace water from particle surfaces and to agglomerate fine coal particles. The resulting agglomerates are subsequently broken (or destabilized) mechanically in the next stage of the process, whereby hydrophobic particles are dispersed in the oil phase and water droplets entrapped within the agglomerates coalesce and exit by gravity along with the hydrophilic particles dispersed in them. In the present work, further laboratory-scale tests have been conducted on various coal samples with the objective of commercial deployment of the HHS process. Test work has also been conducted to explore the possibility of using this process for the recovery of ultrafine minerals such as copper and rare earth minerals. Ultrafine streams produced less than 10% ash and moisture consistently, while coarse coal feed had no observable degradation to the HHS process. Middling coal samples were upgraded to high-value coal products when micronized by grinding. All coal samples performed better with the HHS process than with flotation in terms of separation efficiency. High-grade rare earth mineral concentrates were produced with the HHS process ranging from 600-2100 ppm of total rare earth elements, depending on the method and reagent. Additionally, the HHS process produced copper concentrates assaying greater than 30% Cu for both artificial and real feed samples, as well as, between 10-20% Cu for waste samples, which all performed better than flotation. / Master of Science / Froth flotation has long been regarded as the best available technology for separating fine particles. Due to limitations in particle size with froth flotation, and high downstream dewatering costs, a new process has been developed called the hydrophobic-hydrophilic separation (HHS) process. This process was originally based on a concept known as dewatering by displacement (DbD) which was developed by researchers at Virginia Tech in 1995. The process uses hydrocarbon oils, like pentane or heptane, to selectively collect hydrophobic particles, such as coal, for which it was originally developed. In coal preparation plants, a common practice is to purposefully discard the ultrafine stream that flotation cannot recover and has an increased dewatering cost. The HHS process can effectively recovery this waste stream and produce highgrade salable product, with significantly reduced cost of dewatering. In the work presented, laboratory-scale tests have been conducted on various coal samples with the objective of commercial deployment of the HHS process. In this respect, several varying plant streams have been tested apart from the traditional discard stream. Additionally, test work has expanded into mineral commodities such as copper and rare earth minerals. In this work, salable high-value coal products were achievable with the HHS process. Ultrafine streams consistently produced less than 10% ash and moisture. Coarse coal feeds had no observable degradation to the HHS process and were able to produce single digit ash and moisture values. Middling coal samples were upgraded to high-value coal products when micronized by grinding. All coal samples performed better with the HHS process than with flotation in terms of separation efficiency. High-grade rare earth mineral concentrates were produced with the HHS process ranging from 600- 2100 ppm of total rare earth elements depending on the method and reagent. Additionally, the HHS process produced copper concentrates assaying greater than 30% Cu for an artificial and feed samples, as well as, between 10-20% Cu for waste samples, which all performed better than flotation.
|
4 |
Methods of Improving Oil AgglomerationSmith, Sarah Ann 05 June 2012 (has links)
A simple thermodynamic analysis suggests that oil can spontaneously displace water from coal's surface if the coal particle has a water contact angle greater than 90°. However, the clean coal products obtained from laboratory-scale dewatering-by-displacement (DbD) test work assayed moistures substantially higher than expected. These high moisture contents were attributed to the formation of water-in-oil emulsions stabilized by coal particles. Four different approaches were taken to overcome this problem and obtain low-moisture agglomeration products. These included separating the water droplets by screening, breaking emulsions with ultrasonic energy, breaking agglomerates with ultrasonic energy, and breaking agglomerates using vibrating mesh plates. On the basis of the laboratory test work, a semi-continuous test circuit was built and tested using an ultrasonic vibrator to break the water-in-oil emulsions.
The most promising results were obtained agglomerates were broken using the ultrasonic probe and the vibrating mesh plates. Tests conducted on flotation feed from the Kingston coal preparation plant gave a clean coal product containing 1% by weigh of moisture with a 94% combustible recovery. The separation efficiency of 93% is substantially higher than results achievable using froth flotation. When agglomerates formed from thermal coal from the Bailey coal preparation plant were broken using either ultrasonic energy or vibrating mesh plates, the obtained results were very similar: clean coal products assayed less than 5% moisture with separation efficiencies of 86% in average. / Master of Science
|
5 |
The Production of Low Ash Coals Using the Hydrophobic-Hydrophilic Separation Process with Novel DevelopmentsYoumans, Nathan Charles 06 June 2023 (has links)
Master of Science / Froth flotation is a common method in mineral processing to separate material based on hydrophobicity. This process becomes less efficient, however, as particle size is reduced. Because of this ultrafine particles are often discarded prior to froth flotation, and contributes to a substantial amount of coal waste in impoundments. An impoundment is a dam built using coarse reject to hold fine reject in slurry. Because of the land-use and risk of an impoundment failure, these impoundments pose an environmental liability. To address ultrafine coal rejection, researchers at Virginia Tech development the hydrophobic-hydrophilic separation (HHS) process. Unlike in froth flotation, HHS uses an organic solvent to separate and dewater hydrophobic particles from hydrophilic minerals. Past work on the HHS process yielded promising results. In particular, the HHS process has produced a low-ash (<2%) and low moisture (<8%) product, which makes it viable for a feed stock for carbon products. With this in mind, the goal of this work is to make the HHS process more robust by improving the understanding of the effects of auxiliary processes, such as grinding, pre-concentration, and reagent conditioning, on the HHS process. This work also contains work on the interaction between two primary unit operations in the HHS process: oil agglomeration and de-emulsification. Lastly, to make the HHS process more viable for commercial scale-up, a novel unit operation called enhanced liquid flotation (ELF) was developed and tested that performs comparably to the current HHS process, but with less unit operations.
|
6 |
Processing of Low Rank Coal and Ultrafine Particle Processing by Hydrophobic-Hydrophilic Separation (HHS)Jain, Riddhika 05 September 2013 (has links)
This thesis pertains to the processing of ultra-fine mineral particles and low rank coal using the hydrophobic--hydrophilic separation (HHS) method. Several explorative experimental tests have been carried out to study the effect of the various physical and chemical parameters on the HHS process.
In this study, the HHS process has been employed to upgrade a chalcopyrite ore. A systematic experimental study on the effects of various physical and chemical parameters such as particle size, reagent dosage and reaction time on the separation efficiencies have been performed. For this, a copper rougher concentrate (assaying 15.9 %Cu) was wet ground and treated with a reagent to selectively hydrophobize the copper-bearing mineral (chalcopyrite), leaving the siliceous gangue minerals hydrophilic. The slurry was subjected to a high-shear agitation to selectively agglomerate the chalcopyrite and to leave the siliceous gangue dispersed in aqueous phase. The agglomerates were then separated from dispersed gangue minerals by screening and the agglomerates dispersed in a hydrophobic liquid (n-pentane) to liberate the water trapped in the agglomerates. The chalcopyrite dispersed in the hydrophobic liquid was separated from the medium to obtain a concentrate substantially free of gangue minerals and moisture. The copper recoveries were substantially higher than those obtained by flotation. The HHS process was also tested on ultrafine mono-sized silica beads. The results were superior to those obtained by flotation, particularly with ultrafine particles.
The HHS process has also been tested successfully for upgrading subbituminous coals. Low-rank coals are not as hydrophobic as high-rank coals such as bituminous and anthracite coals. In the present work, a low-rank coal from Wyoming was hydrophobized with appropriate reagents and subjected to the HHS in a similar manner as described for processing copper. The results showed that the HHS process reduced the moisture substantially and increased the heating value up to 50% without heating the coal. Laboratory-scale tests conducted under different conditions, e.g., particle size, reagent type, reaction time, and pretreatments, showed promising results. Implementation for the HHS process for upgrading low-rank coals should help reduce CO2 emissions by improving combustion efficiencies. / Master of Science
|
Page generated in 0.1227 seconds