Steam Enhanced Calcination for CO2 Capture with CaOChampagne, Scott 16 April 2014 (has links)
Carbon capture and storage technologies are necessary to start lowering greenhouse gas emissions while continuing to utilize existing thermal power generation infrastructure. Calcium looping is a promising technology based on cyclic calcination/carbonation reactions which utilizes limestone as a sorbent. Steam is present in combustion flue gas and in the calciner used for sorbent regeneration. The effect of steam during calcination on sorbent performance has not been extensively studied in the literature. Here, experiments were conducted using a thermogravimetric analyzer (TGA) and subsequently a dual-fluidized bed pilot plant to determine the effect of steam injection during calcination on sorbent reactivity during carbonation.
In a TGA, various levels of steam (0-40% vol.) were injected during sorbent regeneration throughout 15 calcination/carbonation cycles. All concentrations of steam were found to increase sorbent reactivity during carbonation. A level of 15% steam during calcination had the largest impact. Steam changes the morphology of the sorbent during calcination, likely by shifting the pore volume to larger pores, resulting in a structure which has an increased carrying capacity. This effect was then examined at the pilot scale to determine if the phase contacting patterns and solids heat-up rates in a fluidized bed were factors. Three levels of steam (0%, 15%, 65%) were injected during sorbent regeneration throughout 5 hours of steady state operation. Again, all levels of steam were found to increase sorbent reactivity and reduce the required sorbent make-up rate with the best performance seen at 65% steam.
|
2 |
Steam Enhanced Calcination for CO2 Capture with CaOChampagne, Scott January 2014 (has links)
Carbon capture and storage technologies are necessary to start lowering greenhouse gas emissions while continuing to utilize existing thermal power generation infrastructure. Calcium looping is a promising technology based on cyclic calcination/carbonation reactions which utilizes limestone as a sorbent. Steam is present in combustion flue gas and in the calciner used for sorbent regeneration. The effect of steam during calcination on sorbent performance has not been extensively studied in the literature. Here, experiments were conducted using a thermogravimetric analyzer (TGA) and subsequently a dual-fluidized bed pilot plant to determine the effect of steam injection during calcination on sorbent reactivity during carbonation.
In a TGA, various levels of steam (0-40% vol.) were injected during sorbent regeneration throughout 15 calcination/carbonation cycles. All concentrations of steam were found to increase sorbent reactivity during carbonation. A level of 15% steam during calcination had the largest impact. Steam changes the morphology of the sorbent during calcination, likely by shifting the pore volume to larger pores, resulting in a structure which has an increased carrying capacity. This effect was then examined at the pilot scale to determine if the phase contacting patterns and solids heat-up rates in a fluidized bed were factors. Three levels of steam (0%, 15%, 65%) were injected during sorbent regeneration throughout 5 hours of steady state operation. Again, all levels of steam were found to increase sorbent reactivity and reduce the required sorbent make-up rate with the best performance seen at 65% steam.
|
3 |
Capture of Gaseous Sulfur Dioxide Using Graphene Oxide Based CompositesSanyal, Tanushree Sankar 31 March 2021 (has links)
Sulfur dioxide (SO₂), a well-known pollutant emitted from fossil fuel combustion, has major adverse health and environmental impacts. It is harmful at low concentration with a permissible exposure limit of two ppm for the eight-hour time-weighted average (TWA) value. Fortunately, its atmospheric concentration, like other air pollutants, has gradually reduced in Canada in the past years. However, despite the well-established flue gas desulfurization technologies, they have the disadvantages of being energy-intensive, not very efficient to achieve very low concentrations (at ppm level) and they operate at high temperatures. Moreover, emission standards are becoming more stringent.
Novel methods are therefore investigated to capture SO₂, such as adsorption processes using zeolites and metal oxides (e.g., Iron (Fe) and Vanadium (V) based) which tend to sustain wide ranges of temperatures and pressures. Graphene oxide (GO) was also shown to physisorb SO₂ at low temperatures. In this work, we propose to metal functionalize GO as a step forward on the path for efficient SO₂ capture, by promoting the SO₂ oxidation reaction into sulfur trioxide (SO₃) for increased capacity due to a possible higher affinity with the surface. The GO has a high surface area, high porosity, and controllable surface chemistry. The aim is to achieve outlet concentration of SO₂ as low as 1 ppm through combined physisorption and reaction promoted that the presence of GO and metal, at low operating temperature.
Iron oxide functionalized GO was synthesized using two different techniques: a polyol process (GO-FeₓOᵧ-P) and using a hydrolysis method (GO-FeₓOᵧ-H). The characterization analysis, scanning electron microscopy (SEM) and transmission electron microscopy (TEM), performed on the materials before and after SO₂ reaction show changes on the surface due to metal adding and to the sulfur capture. The breakthrough curves and the capacity calculations of the performed experiments have shown that with the addition of FeₓOᵧ on the surface of GO, the capturing capacity increases by a factor of three to four, indicating a possible change in the capturing mechanism. The evaluation of the temperature effect (from room temperature to 100℃) showed an increasing trend in the capture capacity for SO₂ with an increase in temperature, for both functionalized and non-functionalized GO, indicating it is not driven only by surface adsorption. The presence of sulfur species captured from the gas stream has been confirmed by energy-dispersive X-ray (EDXS) analysis. The future work would be focused on the investigation of the mechanisms and capturing phenomenon and the regeneration step for the materials in order to further improve the capturing capacity and process applicability.
|
4 |
Modélisation des phénomènes de corrosion du Zircaloy-4 sous mélanges oxygène-azote à haute température / Modelling of Zircaloy-4 degradation in oxygen and nitrogen mixtures at high temperatureLasserre-Gagnaire, Marina 17 December 2013 (has links)
Les gaines de zircaloy-4, assurent la première barrière de confinement des combustibles des Réacteurs à Eau Pressurisée. Plusieurs situations accidentelles au cours desquelles les gaines de crayons combustibles sont exposées l’air à haute température ont été envisagées. L’azote généralement utilisé en tant que gaz inerte, joue un rôle primordial lorsqu’il est combiné à l’oxygène à haute température. Les courbes cinétiques obtenues par la technique de thermogravimétrie révèlent la présence de deux domaines cinétiques : le domaine pré-transitoire et le domaine post-transitoire. Durant le domaine post-transitoire, la vitesse de corrosion augmente. Les images obtenues en microscopie optique révèlent l’existence de régions corrodées caractérisées par une couche de zircone poreuse et par la présence de précipités de nitrure de zirconium (ZrN) à l’interface métal - oxyde. La corrosion des plaquettes de Zy4 à 850°C sous mélanges oxygène - azote a été étudiée durant le domaine post-transitoire. Trois réactions successives permettent d’expliquer la présence des différentes phases. Ainsi, la dégradation catastrophique du métal est due à la progression auto-catalysée par ZrN du front de croissance des zones attaquées.Les hypothèses de modélisation ont été validées durant le domaine post-transitoire. L’étape déterminante a été identifiée. La réaction d’interface externe du mécanisme d’oxydation des précipités de ZrN impose sa vitesse aux autres étapes du mécanisme de croissance des régions corrodées. Par analogie avec les modèles de germination - croissance utilisés dans le cadre de la transformation thermique des poudres, nous avons pu décrire l’évolution des zones attaquées. / Zircaloy-4 claddings provide the first containment of UO2 fuel in Pressurised Water Reactors. It has been demonstrated that the fuel assemblies cladding could be exposed to air at high temperature in several accidental situations. When mixed to oxygen at high temperature, the nitrogen, usually used as an inert gas, causes the accelerated corrosion of the cladding.The kinetic curves obtained by thermogravimetry reveal two stages: a pre-transition and a post-transition one. In the post-transition stage, the kinetic rate increases with time. Images obtained by optical microscopy of a sample in the post-transition stage reveal the presence of corroded zones characterized by a porous scale with zirconium nitride precipitates at metal - oxide interface. Corrosion of Zy4 plates at 850°C under mixed oxygen - nitrogen atmospheres has been studied during the post-transition stage. A sequence of three reactions is proposed to explain the mechanism of nitrogen-enhanced corrosion. The accelerating effect of nitrogen in the corrosion scale can therefore be described on the basis of an autocatalytic effect of the zirconium nitride precipitates. Then, it is demonstrated that the steady-state approximation as well as the existence of an elementary step controlling the growth process are valid during the post-transition stage. The rate-determining step is identified as the external interface reaction step of the oxidation of the zirconium nitride precipitates. Finally, a nucleation and growth model used for thermal reactions in powders is used to describe both the nucleation and the growth of the attacked regions.
|