Abstract

dc:description.abstract

The main part of this study concerned the evaluation of methods for measuring the elastic recovery of elastomeric dental impression materials following the application of various deforming strains. One brand from each chemical group of available elastomers was selected to allow for relative ranking of the results from each deformation test mode. The literature review and preliminary laboratory trials indicated a need to define certain test conditions. These were discussed with relevance to the clinical situation. The following conditions for clinical relevance were determined after clinical and laboratory tests. Firstly the storage temperature for specimen moulds and polymerization of specimens was set at 32 degrees Celsius. Secondly, the time of strain application was set at 1.25 minutes after the manufacturer's recommended setting time. Thirdly, the duration of the deforming strain was set at 5.0 seconds. Elastic recovery was measured at 2 minute intervals for 20 minutes under the room temperature and humidity condition prevailing. Compression, tensile, bending, and torsional strains were imposed on specimens of varying configurations as described. Compression set was recorded using a British Standards Institute type of balanced beam (modified to reduce specimen loading during measurement), a metallurgical microscope and a stereomicroscope (both microscopes modified for depth measurement and without load on the specimen during recovery). A stainless steel and an acrylic mould were used to determine the effect of mould material on specimen polymerization. Tensile set was evaluated using one vertical and two horizontal test modes. The effect of frictional resistance to elastic recovery in the horizontal modes was discussed and found to be insignificant. permanent deformation following bending and. torsional strain application was determined with results similar to those from compression testing. Relative ranking of permanent deformation values for specimens from the stainless steel compression test moulds, the vertical and B.S.I. tensile test moulds, the two bend test moulds and the torsion test mould were all similar. This suggested that the relatively simple compression set test was sufficient to evaluate the materials selected. No statistically significant change in elastic recovery with time was observed for polyether or polysiloxane specimens after 6 minutes following strain release; for the polysutphide and the silicone materials no statistically significant change occurred after I0 minutes- The compression tests indicated that the balanced beam instrument resulted in a significantly greater set percent being recorded compared with optical measurement methods. This was attributed to specimen loading during measurement and instrument inertia and friction. A system without specimen loading or inertia and friction effects was recommended. The effects of the mould material and configuration were considered and the following conclusions made. Firstly, permanent deformation is dependent on the elastomer type and the thermodynamic characteristics of a particular mould. Secondly, the mould material should be specified to ensure that sufficient polymerization occurs before deformation thus improving comparative studies between materials.

Degree

thesis:*
College dc:contributor.school
Adelaide Dental School
Year dc:date.issued
1983

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Blomberg, Per Anders Hugo
Advisor dc:contributor.advisor
  • Makinson, O. F.

Rights

Language dc:language.iso
en

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/2440/122055

Chain of custody

source
Harvested from
University of Adelaide
Base URL
digital.library.adelaide.edu.au/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Blomberg, Per Anders Hugo. Permament deformation of some elastomeric dental impression materials. 1983. https://hdl.handle.net/2440/122055