Back to search

University of Alberta

Kinetic Study of Steel Corrosion in Supercritical CO₂-Saturated Aqueous Environments

Abstract

dc:description.abstract

The long-term reliability of carbon capture, transportation, utilization, and storage (CCTUS) infrastructure depends on the corrosion resistance of steels used in supercritical CO₂ (s-CO₂) transmission systems. While dry s-CO₂ is non-corrosive to steels, the introduction of water, either from the capture processes or at geologic injection sites, creates aggressive corrosion environments that can threaten pipeline integrity. This study investigates the corrosion behaviour of five steels (X65, P110, 2Cr, P91, and SS316) with varying Cr levels in s-CO₂ saturated saline environments over exposure times up to 1000 h. Corrosion rates were determined through weight loss measurements, and corrosion product layers were characterized using X-ray diffraction (XRD), Raman spectroscopy, and scanning electron microscopy (SEM) with energy dispersive X-ray spectroscopy (EDS). The primary two objectives were to assess the role of chromium (Cr) content, and to investigate the kinetics of the corrosion process in s-CO₂ saturated saline environments. Corrosion rates consistently decline with increasing Cr content in the studied steels. A critical Cr threshold of approximately 9 wt.% was identified, above which the alloys exhibit satisfactory corrosion resistance in s-CO₂-saturated saline environments. For instance, both P91 and SS316 steels showed exceptional corrosion resistance (<0.01 mm/y), attributed to the formation of dense FeCO₃ layers over Cr-oxide-rich intermediates that effectively inhibited further metal dissolution. Across all steels, corrosion rates decreased exponentially with exposure time from 1 h to 1000 h due to the gradual development of protective FeCO₃ layers.\nCharacterization results indicate that the absence of Cr-oxide formation and the dominance of amorphous iron oxides on the steel surface hinder the development of a stable, protective film. This highlights that Cr content alone is not sufficient to predict corrosion behaviour. The findings suggest that additional factors, such as oxide morphology and environmental conditions, play a significant role in determining corrosion resistance in supercritical CO₂ environments. SS316 and P91 are recommended for applications involving unavoidable water-rich s-CO2 phases, while low-Cr steels may still be suitable for dry s-CO₂ transmission systems where moisture levels can be effectively controlled. The results also reveal that short testing durations tend to overestimate corrosion rates in s-CO₂-saturated aqueous environments. A minimum testing duration of 100 h is recommended to obtain a more accurate assessment of long-term corrosion performance; however, corrosion rates still continue to decrease up to the 1000 h mark.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
Master's
Discipline thesis:degree_discipline
Materials Engineering
Grantor
University of Alberta
Year dc:date.issued
2025

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Gross, Alexander
Advisor dc:contributor.advisor
  • Liu, Jing (Chemical and Materials Engineering)

Subjects

dc:subject × 4

Rights

dc:rights
Statement dc:rights
  • This thesis is made available by the University of Alberta Library with permission of the copyright owner solely for non-commercial purposes. This thesis, or any portion thereof, may not otherwise be copied or reproduced without the written consent of the copyright owner, except to the extent permitted by Canadian copyright law.
Language dc:language.iso
en

Identifiers

dc:identifier.*
DOI dc:identifier.doi
https://doi.org/10.7939/83099

Chain of custody

source
Harvested from
University of Alberta
Base URL
era.library.ualberta.ca/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Gross, Alexander. Kinetic Study of Steel Corrosion in Supercritical CO₂-Saturated Aqueous Environments. Master's thesis, University of Alberta, 2025. https://doi.org/10.7939/83099