University of Alberta
Evaluating the synthesis, physicomechanical characteristics, and anti-bacterial response of an unfilled resin-based system incorporating a pH-responsive monomer
Abstract
dc:description.abstractSecondary caries caused by the overgrowth of acid-producing oral microbiota and tooth-adhesive interface degradation constitutes a crucial pathological mechanism for restoration failure. Development of resin-based dental materials with effective anti-bacterial activity while maintaining mechanical integrity (e.g., strength) is a key challenge. Despite extensive research on antimicrobial dental materials, few studies focus on pH-responsive monomers. 2-(Dimethylamino) ethyl methacrylate (DMAEMA), a widely used pH-responsive monomer, has a protonation potential of its tertiary amine group, which theoretically endows the material with both pH-neutralization and anti-bacterial properties. The mechanism of activation occurs through the tertiary amine (TA) group of a monomer component that can be charged and has potential for anti-bacterial properties. However, the influence of monomer-blend alterations at varying concentrations on the mechanical performance has not been characterized. The presented thesis aims to systematically explore the effect of introducing DMAEMA at varied mass fractions (0, 2.5, 5, 7,5, 10, 25 and 50 wt%) as a co-monomer into an experimental rein system (55 wt% BisGMA, 45 wt% HEMA) on material properties including flexural strength (FS), flexural modulus(FM), Vicker’s hardness (VH), water sorption (Wsp), water solubility (Wsl), and anti-bacterial effect with Counting Forming Unit (CFU). The statistical analysis of FS, FM, VH, Wsp, Wsl, and log transformed CFU data were performed with one-way ANOVA test at α=.05 and Tukey’s post hoc test was performed when appropriate for group comparisons. The results showed that, although a potential anti-bacterial effect can be observed at a high content of 50 wt% (n=3, Tukey’s test, p=.038), the FS significantly decreased when the DMAEMA content reached 7.5 wt% before water storage (n≥11, Tukey’s test, p=.018), and the Wsp and Wsl significantly increased when DMAEMA content reached 7.5 wt% (n=5, Tukey’s test, p=.020) and 5 wt% (n=5, Tukey’s test, p=.039), respectively. In summary, although the incorporation of DMAEMA into an experimental dental resin system endows potential anti-bacterial function, a negative impact on the key physicomechanical properties is shown as the DMAEMA content increases. Therefore, under the current system, DMAEMA is not an ideal candidate monomer for anti-bacterial dental resin. This study clarifies the limitations of introducing DMAEMA monomer for anti-bacterial purposes, and highlights in the development of novel resin-based dental materials, any exploration of secondary functions should be based on ensuring the primary functional performance.
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- Master's
- Grantor
- University of Alberta
- Year dc:date.issued
- 2026
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Liu, Zheyuan
- Advisors dc:contributor.advisor
-
- Romanyk, Dan (Department of Mechanical Engineering)
- Addison, Owen (Department of Dentistry)
Subjects
dc:subject × 3Rights
dc:rights- Statement dc:rights
-
- This thesis is made available by the University of Alberta Library with permission of the copyright owner solely for non-commercial purposes. This thesis, or any portion thereof, may not otherwise be copied or reproduced without the written consent of the copyright owner, except to the extent permitted by Canadian copyright law.
- Language dc:language.iso
- en
Identifiers
dc:identifier.*- DOI dc:identifier.doi
- https://doi.org/10.7939/84412