Synthesis and Characterization of Zirconium Carbonitride Thin Films: ALD Process Development, Optimization and Comparative Evaluation against Sputtered Transition Metals

Abstract

dc:description.abstract

Atomic layer deposition (ALD) is a key thin-film deposition technique for advanced micro- and nano-electronic applications due to its unparalleled thickness control, uniformity, and conformality on high-aspect-ratio structures. However, low-temperature ALD of electropositive transition metals and their compounds remains challenging due to incomplete precursor reduction, impurity incorporation, and limited electrical performance. In this work, the Plasma-Enhanced Atomic Layer Deposition (PEALD) of zirconium-based thin films using tetrakis(dimethylamido)zirconium (TDMAZr) and hydrogen plasma is investigated, with results benchmarked against a metallic baseline established by DC magnetron sputtering. Deposition and characterization of the sputtered metallic baselines demonstrated that while variations in working pressure, power, and base pressure yield consistent trends across the investigated refractory metals, the influence of substrate temperature is uniquely characteristic to each specific material system. As revealed by direct X-ray diffraction (XRD) and scanning electron microscopy (SEM) analysis, molybdenum thin films exhibited a marginal reduction in electrical resistivity with increasing substrate temperature while maintaining a stable body-centred cubic structure. Conversely, zirconium films showed a unique resistivity inversion above 244 °C. Detailed SEM microstructural tracking and XRD line profiling quantified that this transition toward higher resistivity was accompanied by a significant reduction in physical grain size from 124 nm to 36 nm and a concurrent resurgence in internal lattice strain. Analyzed via the Thornton structure zone model (SZM), this reveals a distinct thermal threshold where defect proliferation and competitive nucleation kinetics actively counteract the expected benefits of thermally driven adatom mobility. Tantalum showcased a significant resistivity drop reaching 4×10-5 Ω·cm at 474 °C, driven by a microstructural transition from a Zone 1 fibrous structure to a highly dense, columnar Zone T morphology associated with a partial β to α phase transformation, directly verified through cross-sectional SEM imaging and peak evolution in the XRD patterns. For zirconium based films deposited by ALD, detailed saturation curve analysis established a stable, self-limiting ALD processing window between 100 and 200 °C, yielding a constant Growth Per Cycle (GPC) of 0.51 Å. At the optimized substrate temperature of 150 °C, the surface chemistry required specific kinetic thresholds to achieve ideal monolayer growth; A minimum precursor dose of 0.05 s was necessary to saturate the surface, while a plasma exposure of ≥ 11 s was required to drive the reduction half-reaction to completion. Crucially, purge durations of ≥ 12 s for both the reactant and counter-reactant steps were identified as critical to effective gas-phase separation, effectively mitigating parasitic CVD-like growth. Characterization of the films revealed a fundamental divergence in phase formation. While magnetron sputtering of zirconium films produced highly textured, metallic zirconium films with a low electrical resistivity of 1.5×10-4 Ω·cm, the PEALD process resulted in a ternary zirconium carbonitride (ZrCxNy) solid solution. X-ray Photoelectron Spectroscopy (XPS) and XRD confirmed that carbon ligands were substitutionally incorporated into a rock-salt ZrN-type lattice, resulting in a higher resistivity of 13.8×10-4 Ω·cm. The effects of plasma parameters were systematic; while increasing power from 800 W to 1000 W yielded negligible changes in growth rate, the H2/Ar ratio proved critical in modulating ligand removal. modulating the H2/Ar ratio and step pressure proved critical in controlling chemical reduction, film composition, and growth kinetics. Shifting from the baseline to an intermediate hydrogen flow (50/160 sccm H2/Ar) at 150 °C successfully reduced bulk carbon impurities by half to approximately 8 at.%, though GPC dropped to 0.44 Å/cycle. Transitioning to a strongly hydrogen-rich, low-pressure condition (100/10 sccm H₂/Ar at 0.2 Torr) maintained a dominant rocksalt ZrN-type framework with a GPC of 0.46 Å/cycle, but led to an increased sensitivity to post-deposition surface oxidation. Isolating the effect of temperature under this hydrogen-rich gas ratio by heating the substrate to 300 °C accelerated the GPC to 0.91 Å/cycle, indicating a transition from self-limiting growth to thermally activated CVD-like contributions, while simultaneously triggering a texture shift toward more mixed, non-(111) nitride orientations. Post-deposition annealing at 380 °C demonstrated excellent thermal stability, with no structural relaxation or phase decomposition, whereas severe oxidative degradation at 500 °C induced distinct monoclinic ZrO2 crystallization. These results define a major performance divergence: sputtering offers a highly conductive metallic baseline, whereas ceramic ALD films exhibit higher resistivity due to solid-solution attributes but deliver the requisite conformality and phase stability for nanoscale electronic and diffusion barrier coatings.

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
Doctoral
Discipline thesis:degree_discipline
Materials Engineering
Grantor
University of Alberta
Year dc:date.issued
2026

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Mojir Shaibani, Parman
Advisors dc:contributor.advisor
  • Ken Cadien, CME
  • Hongbo Zeng, CME

Subjects

dc:subject × 8

Rights

dc:rights
Statement dc:rights
  • This thesis is made available by the University of Alberta Library with permission of the copyright owner solely for non-commercial purposes. This thesis, or any portion thereof, may not otherwise be copied or reproduced without the written consent of the copyright owner, except to the extent permitted by Canadian copyright law.
Language dc:language.iso
en

Identifiers

dc:identifier.*
DOI dc:identifier.doi
https://doi.org/10.7939/86014

Chain of custody

source
Harvested from
University of Alberta
Base URL
era.library.ualberta.ca/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Mojir Shaibani, Parman. Synthesis and Characterization of Zirconium Carbonitride Thin Films: ALD Process Development, Optimization and Comparative Evaluation against Sputtered Transition Metals. Doctoral thesis, University of Alberta, 2026. https://doi.org/10.7939/86014