Back to search

University of Alberta

Effect of Ti/N ratio on CTOD fracture toughness of girth welded X70

Abstract

dc:description.abstract

Multipass welding exposes pipeline material to a high heating and cooling rate, which can lead to the formation of regions with poor toughness. The most well-known region is the intercritically reheated coarse-grained heat-affected zone (ICCGHAZ), where martensite-austenite (M-A) constituents form predominantly along prior austenite grain (PAG) boundaries. The M-A constituents affect toughness by promoting the formation of micro-cracks. Therefore, it is essential to understand the parameters that control the PAG growth within the ICCGHAZ. Among the precipitates in high-strength low-alloyed steels (HSLAs), TiN precipitates are more effective in retarding PAG growth at elevated temperatures compared to other precipitates due to their low solubility (or high stability). It is well known that a small PAG size improves the heat-affected zone (HAZ) toughness. Almost all the previous investigations on ICCGHAZ fracture toughness have been conducted on simulated welds, and they have not thoroughly addressed the relationship between the Ti/N ratio and corresponding crack-tip opening displacement (CTOD) fracture toughness of girth-welded X70 to the best of the author’s knowledge. Therefore, microalloyed steels with Ti/N weight percentage ratios of 2.38 (Hypo), 3.29 (Sto), and 5.11 (Hyper) were selected to investigate the effect of precipitate size distribution and volume fraction on the prior austenite grain (PAG) size, microstructure, microhardness, and ultimately CTOD fracture toughness of ICCGHAZ in shielded metal arc welded (SMAW) X70 pipeline. The mean size to volume fraction of TiN, which reflects the effectiveness of particle size distribution on pinning the grain boundaries, was highest (2.48104 nm) for the Hypo sample, intermediate for the Sto sample (2.35104 nm), and lowest (1.54104 nm) for the Hyper sample. The prior austenite grain (PAG) sizes for the ICCGHAZ, measured using an optical microscope, were 27, 37 and 51 µm for the Hyper, Sto and Hypo samples, respectively. These results correlate well with the ratio of precipitate average size to the measured volume fraction for each sample. The Hypo had the largest size to volume fraction of precipitates, resulting in an increase in PAG size at ICCGHAZ. The microstructural assessment suggested that an increase in bainite and M-A area fraction resulted in an increase in hardness. The corresponding hardness values for the Hypo and Hyper samples were 250 HV0.05 and 240 HV0.05, respectively. The slightly higher hardness for the Hypo sample compared with the Hyper sample was attributed to its higher M-A area fraction. The Sto sample had the highest amount of Bainite. The high M-A area fraction in the Hypo sample stemmed from its large PAG size, which was a result of its high size-to-volume fraction of TiN precipitates in this sample. Finally, the crack-tip opening displacement (CTOD) fracture toughness test was designed to assess the toughness of the ICCGHAZ in the girth-welded X70 pipeline steel and to identify which microstructural characteristics have the most significant impact on fracture toughness. The crack tip opening displacement (CTOD) toughness for the tested samples was 0.07 mm, 0.34 mm, and 0.65 mm for the Hypo, Sto, and Hyper samples, respectively. The fracture surface analysis at the ICCGHAZ region exhibited a quasi-cleavage fracture mode, where the facet size was observed to be the largest for the Hypo sample and the smallest for the Hyper sample. The analysis of the M-A constituents’ morphology showed a similar distribution for both size and aspect ratio, whereas a significant difference was observed between the total number of M-A constituents. The number density of M-A constituents for the Hypo, Hyper, and Sto samples was 0.08, 0.05, and 0.03 μm-2 for the 300 µm x 300 µm scanned area, respectively. The results show that CTOD fracture toughness improves as the Ti/N ratio increases. The increase in fracture toughness is mainly attributed to the decrease in PAG size and, to a lesser extent, the M-A area fraction. The fracture mechanism within the ICCGHAZ was controlled by PAG size and debonding of M-As from the matrix, whereas the fracture mechanism in the base metal (BM) was mainly due to the void nucleation and growth mechanism. The void formation in the BM was initiated by the microcrack formed upon the precipitates’ fracture.

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
Doctoral
Discipline thesis:degree_discipline
Materials Engineering
Grantor
University of Alberta
Year dc:date.issued
2026

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Milani, Vanda
Advisor dc:contributor.advisor
  • Henein, Hani (Chemical and Materials Engineering)

Subjects

dc:subject × 6

Rights

dc:rights
Statement dc:rights
  • This thesis is made available by the University of Alberta Library with permission of the copyright owner solely for non-commercial purposes. This thesis, or any portion thereof, may not otherwise be copied or reproduced without the written consent of the copyright owner, except to the extent permitted by Canadian copyright law.
Language dc:language.iso
en

Identifiers

dc:identifier.*
DOI dc:identifier.doi
https://doi.org/10.7939/86235

Chain of custody

source
Harvested from
University of Alberta
Base URL
era.library.ualberta.ca/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Milani, Vanda. Effect of Ti/N ratio on CTOD fracture toughness of girth welded X70. Doctoral thesis, University of Alberta, 2026. https://doi.org/10.7939/86235