Abstract
dc:description.abstractStress corrosion cracking (SCC) from the external surface of a buried pipeline is a serious matter and can cause significant economic and environmental losses. Despite of many research works which have been done on the understanding of crack initiation and propagation mechanisms, these mechanisms are still being debated. This research studied the crack growth behaviour of different pipeline steels including two types of X65, one X52 and one X80 pipeline steels in near-neutral pH environments. Crack growth behaviour of all steels has been found to be consistent with that of true corrosion fatigue. Crack growth rates were correlated with (K)2Kmax/f0.1. It was revealed that cracking behaviour of pipeline steels in near neutral pH environments is material dependent. Highest crack growth rate was seen in the steel which highest amount of hydrogen atoms could be generated and stored in its microstructure to contribute in cracking procedure due to hydrogen embrittlement effect.
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- Master's
- Grantor
- University of Alberta
- Year dc:date.issued
- 2010
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Marvasti, Mohammad Hassan
- Advisor dc:contributor.advisor
-
- Weixing Chen, Department of Chemical and Materials Engineering
Subjects
dc:subject × 5Rights
dc:rights- Statement dc:rights
-
- This thesis is made available by the University of Alberta Libraries with permission of the copyright owner solely for non-commercial purposes. This thesis, or any portion thereof, may not otherwise be copied or reproduced without the written consent of the copyright owner, except to the extent permitted by Canadian copyright law.
- Language dc:language.iso
- en
Identifiers
dc:identifier.*- DOI dc:identifier.doi
- https://doi.org/10.7939/R33P7B