Experimental and Numerical Investigation of Fatigue Behavior of Pearlitic Rail Steels

Abstract

dc:description.abstract

In recent years, rail transport of Canadian crude oil and coal has grown. While transportation of oil and coal by rail has demonstrated benefits, it has also raised significant concerns about transportation safety and potential impacts to the environment. In this regards, rolling contact fatigue (RCF) of railway components is one of the most crucial subjects to the safety of rail transportation. The RCF cracking is very sensitive to the microstructure of the rails which are mostly manufactured from pearlitic steels. Therefore, complete understanding of the effects of microstructural characteristics on the RCF phenomenon is critical for mitigating damage and life predictions so that components can be repaired or replaced in time before catastrophic failure occurs. In the current study, microstructural changes in pearlitic rail steels under fatigue loadings and their effects on the RCF crack initiation and propagation have been investigated by experimental and numerical approaches. Optical microscopy and micro-hardness testing are utilized to perform failure analysis on the rails that have been in service in the US. The morphologies and geometrical characteristics of the RCF cracks are analyzed. Moreover, the extent of plastic deformation in different regions of the rails is evaluated through microstructural analysis. Besides, other microstructural constituents including MnS based inclusions and white etching layers are evaluated. A microstructure-based model is built using Voronoi tessellation and continuum damage mechanics. The experimental results reveal that the maximum depths of cracks were mainly dependent on the grade of rail steel rather than the duration of service life. The maximum depths of the cracks were dependent on the thickness of largely deformed layer near the surface of the rails. Results of numerical simulations show occurrence of preferential strain accumulation in pro-eutectoid (PE) ferrite. As a result, a higher content of PE ferrite leads to a lower fatigue life of pearlitic rail steels.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
Master's
Grantor
University of Alberta
Year dc:date.issued
2019

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Hassas Irani, Seyed Babak
Advisors dc:contributor.advisor
  • Chen, Zengtao (Mechanical Engineering)
  • Szablewski, Daniel (National Research Council of Canada)

Subjects

dc:subject × 4

Rights

dc:rights
Statement dc:rights
  • Permission is hereby granted to the University of Alberta Libraries to reproduce single copies of this thesis and to lend or sell such copies for private, scholarly or scientific research purposes only. Where the thesis is converted to, or otherwise made available in digital form, the University of Alberta will advise potential users of the thesis of these terms. The author reserves all other publication and other rights in association with the copyright in the thesis and, except as herein before provided, neither the thesis nor any substantial portion thereof may be printed or otherwise reproduced in any material form whatsoever without the author's prior written permission.
Language dc:language.iso
en

Identifiers

dc:identifier.*
DOI dc:identifier.doi
https://doi.org/10.7939/r3-aja8-bk02

Chain of custody

source
Harvested from
University of Alberta
Base URL
era.library.ualberta.ca/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Hassas Irani, Seyed Babak. Experimental and Numerical Investigation of Fatigue Behavior of Pearlitic Rail Steels. Master's thesis, University of Alberta, 2019. https://doi.org/10.7939/r3-aja8-bk02